- CN107695614A CN107695614A CN201610642710.3A CN201610642710A CN107695614A CN 107695614 A CN107695614 A CN 107695614A CN 201610642710 A CN201610642710 A CN 201610642710A CN 107695614 A CN107695614 A CN 107695614A
- Authority
- CN
- China
- Prior art keywords
- welding
- plate
- associated methods
- rolling
- metallic plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23P—METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS
- B23P15/00—Making specific metal objects by operations not covered by a single other subclass or a group in this subclass
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Butt Welding And Welding Of Specific Article (AREA)
- Metal Rolling (AREA)
Abstract
本发明公开了一种多层金属板的结合方法,属于金属板技术领域;对于平整的金属板,需要滚压将两层(或多层)金属板紧密贴合以减少板间空隙;焊接以固定金属板;将焊接的位置通过多次折弯与滚压;将滚压的位置进行焊接,以达到产品性能要求。工艺设计合理,主要为通过焊接与滚压结合的方式以达到短时间屏蔽液体入侵的特性;提高产品对水以及特种油的防护性能。
Description
技术领域
本发明涉及金属板技术领域,具体涉及一种多层金属板的结合方法。
背景技术:
传统金属之间的连接方式主要为焊接,焊接为通过加热工件熔化形成熔池,熔池冷却凝固后结合,并借助焊料的毛细作用连接,并在相当于工件熔点的温度下辅以高压、或震动等使两工件间相互渗透接合。由于工件熔化后局部存在漏点,因此无法应对短时的液体入侵。
发明内容
针对上述问题,本发明要解决的技术问题是提供一种设计合理、操作方便、加工效率高且质量稳定的多层金属板的结合方法。
本发明的一种多层金属板的结合方法,它的工艺方案如下:
1、对于平整的金属板,需要滚压将两层(或多层)金属板紧密贴合以减少板间空隙;
2、焊接以固定金属板;
3、将焊接的位置通过多次折弯与滚压;
4、将滚压的位置进行焊接,以达到产品性能要求
作为优选,所述的金属板相邻两层的层间距低于0.01mm。
作为优选,所述的各个金属板存在3~5处折弯,产品的防护性能无衰减,对液体的隔绝与密闭性能随着折弯数量的增加而趋于稳定。产品的抗撕破性能随着折弯数量的增加而远超材料本身的撕破强度。
作为优选,所述的步骤4中焊接的部位分别处于金属板折叠的1/3与2/3位置,可采用单点焊或者滚焊焊接。
本发明操作时,为防止工作过程中脱落,产品采用焊接工艺每次折弯之后均对新产生的叠加处进行焊接,增加产品的抗拉强度与屈服强度,并能够承受航空发动机运作时产生的机械振动与冲击。产品在标准状况下可在短时间(5min)内抵抗水(质量吸湿率≤0.1%)、航空燃油(质量吸湿率≤2.5%)、航空液压油(质量吸湿率≤5%)的浸润。其抗拉强度≥1100MPa,屈服强度≥1230MPa,断裂伸长率≥60%。
本发明的有益效果:工艺设计合理,主要为通过焊接与滚压结合的方式以达到短时间屏蔽液体入侵的特性;提高产品对水以及特种油的防护性能。
具体实施方式
本具体实施方式采用以下技术方案:它的工艺方案如下:
1、对于平整的金属板,需要滚压将两层(或多层)金属板紧密贴合以减少板间空隙;
2、焊接以固定金属板;
3、将焊接的位置通过多次折弯与滚压;
4、将滚压的位置进行焊接,以达到产品性能要求
作为优选,所述的金属板相邻两层的层间距低于0.01mm。
作为优选,所述的各个金属板存在3~5处折弯,产品的防护性能无衰减,对液体的隔绝与密闭性能随着折弯数量的增加而趋于稳定。产品的抗撕破性能随着折弯数量的增加而远超材料本身的撕破强度。
作为优选,所述的步骤4中焊接的部位分别处于金属板折叠的1/3与2/3位置,可采用单点焊或者滚焊焊接。
本发明操作时,为防止工作过程中脱落,产品采用焊接工艺每次折弯之后均对新产生的叠加处进行焊接,增加产品的抗拉强度与屈服强度,并能够承受航空发动机运作时产生的机械振动与冲击。产品在标准状况下可在短时间(5min)内抵抗水(质量吸湿率≤0.1%)、航空燃油(质量吸湿率≤2.5%)、航空液压油(质量吸湿率≤5%)的浸润。其抗拉强度≥1100MPa,屈服强度≥1230MPa,断裂伸长率≥60%。
本发明的有益效果:工艺设计合理,主要为通过焊接与滚压结合的方式以达到短时间屏蔽液体入侵的特性;提高产品对水以及特种油的防护性能。
以上显示和描述了本发明的基本原理和主要特征以及本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (4)
1.一种多层金属板的结合方法,其特征在于它的工艺方案如下:
(1)、对于平整的金属板,需要滚压将两层金属板紧密贴合以减少板间空隙;
(2)、焊接以固定金属板;
(3)、将焊接的位置通过多次折弯与滚压;
(4)、将滚压的位置进行焊接,以达到产品性能要求。
2.根据权利要求1所述的一种多层金属板的结合方法,其特征在于所述的金属板相邻两层的层间距低于0.01mm。
3.根据权利要求1所述的一种多层金属板的结合方法,其特征在于所述的各个金属板存在3~5处折弯。
4.根据权利要求1所述的一种多层金属板的结合方法,其特征在于所述的步骤(4)中焊接的部位分别处于金属板折叠的1/3与2/3位置,可采用单点焊或者滚焊焊接。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610642710.3A CN107695614A (zh) | 2016-08-08 | 2016-08-08 | 一种多层金属板的结合方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610642710.3A CN107695614A (zh) | 2016-08-08 | 2016-08-08 | 一种多层金属板的结合方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN107695614A true CN107695614A (zh) | 2018-02-16 |
Family
ID=61169237
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201610642710.3A Pending CN107695614A (zh) | 2016-08-08 | 2016-08-08 | 一种多层金属板的结合方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN107695614A (zh) |
Citations (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2354921A (en) * | 1941-05-31 | 1944-08-01 | Archie W Mcclary | Metal drum |
US4470717A (en) * | 1980-06-07 | 1984-09-11 | Daimler-Benz Aktiengesellschaft | Web seam for sheet-metal parts and method for producing the same |
EP0177945A1 (de) * | 1984-10-12 | 1986-04-16 | Bayerische Motoren Werke Aktiengesellschaft, Patentabteilung AJ-3 | Schweissnaht zur Verbindung zweier Dünnbleche |
JPH105858A (ja) * | 1996-06-28 | 1998-01-13 | Kana Flex Corp Kk | 鋼板補強芯入りダクトホース及びその製造方法 |
JPH11197764A (ja) * | 1998-01-12 | 1999-07-27 | Oyo Kikaku:Kk | 並列的に連結可能な型鋼と複合型鋼 |
CN1347351A (zh) * | 1999-04-19 | 2002-05-01 | Abb股份有限公司 | 接合方法 |
CN101678431A (zh) * | 2007-01-15 | 2010-03-24 | Edag有限公司 | 金属板组件、用于接合金属板的方法和接合装置 |
JP2012074321A (ja) * | 2010-09-30 | 2012-04-12 | Nisshin Steel Co Ltd | 金属製の有底又は密閉容器及びその製造方法 |
CN103328146A (zh) * | 2012-01-16 | 2013-09-25 | 丰田自动车株式会社 | 面板接合结构 |
EP2667073A1 (de) * | 2012-05-21 | 2013-11-27 | Zambelli Fertigungs GmbH & Co. KG | Rohrstück aus Metallblech und Verfahren zu dessen Herstellung, Streck-Biegevorrichtung zur Herstellung eines Rohrbogens und Verfahren zur Herstellung eines Rohrbogens |
-
2016
- 2016-08-08 CN CN201610642710.3A patent/CN107695614A/zh active Pending
Patent Citations (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2354921A (en) * | 1941-05-31 | 1944-08-01 | Archie W Mcclary | Metal drum |
US4470717A (en) * | 1980-06-07 | 1984-09-11 | Daimler-Benz Aktiengesellschaft | Web seam for sheet-metal parts and method for producing the same |
EP0177945A1 (de) * | 1984-10-12 | 1986-04-16 | Bayerische Motoren Werke Aktiengesellschaft, Patentabteilung AJ-3 | Schweissnaht zur Verbindung zweier Dünnbleche |
JPH105858A (ja) * | 1996-06-28 | 1998-01-13 | Kana Flex Corp Kk | 鋼板補強芯入りダクトホース及びその製造方法 |
JPH11197764A (ja) * | 1998-01-12 | 1999-07-27 | Oyo Kikaku:Kk | 並列的に連結可能な型鋼と複合型鋼 |
CN1347351A (zh) * | 1999-04-19 | 2002-05-01 | Abb股份有限公司 | 接合方法 |
CN101678431A (zh) * | 2007-01-15 | 2010-03-24 | Edag有限公司 | 金属板组件、用于接合金属板的方法和接合装置 |
JP2012074321A (ja) * | 2010-09-30 | 2012-04-12 | Nisshin Steel Co Ltd | 金属製の有底又は密閉容器及びその製造方法 |
CN103328146A (zh) * | 2012-01-16 | 2013-09-25 | 丰田自动车株式会社 | 面板接合结构 |
EP2667073A1 (de) * | 2012-05-21 | 2013-11-27 | Zambelli Fertigungs GmbH & Co. KG | Rohrstück aus Metallblech und Verfahren zu dessen Herstellung, Streck-Biegevorrichtung zur Herstellung eines Rohrbogens und Verfahren zur Herstellung eines Rohrbogens |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Rodrigues et al. | Ultracold-Wire and arc additive manufacturing (UC-WAAM) | |
US10946470B2 (en) | Resistance spot welding method and welded member production method | |
CN101564791B (zh) | 一种高强度压力容器用钢的埋弧焊接方法 | |
CN101270459B (zh) | 焊趾tig重熔后跟随激冷处理改善焊接接头疲劳强度的方法 | |
CN109694989B (zh) | 一种825/x70镍基合金复合板及其生产方法 | |
KR20170072948A (ko) | 저항 스폿 용접 방법 | |
CN102528336B (zh) | 一种利用脆性锡铋系合金制备焊接丝材的方法 | |
JP6108017B2 (ja) | スポット溶接方法 | |
CN105229201A (zh) | 具有钢制外层的再制铸铁部件 | |
CN106488825A (zh) | 立式窄坡口气体保护电弧焊方法 | |
CN110293149B (zh) | 一种双金属复合毛管的制作装置及制作方法 | |
CN107185961B (zh) | 一种大规格、薄复层镍基合金/管线钢复合板的制备方法 | |
KR102028435B1 (ko) | 저항 스폿 용접 방법 및 용접 부재의 제조 방법 | |
CN104690404A (zh) | T22和tp347h异种钢的焊接方法 | |
Zhang et al. | Microstructures and performances of the butt joint of TA1/Q235B bimetallic sheet with addition of a Mo interlayer by using narrow gap laser welding with filler wire | |
CN102233474A (zh) | 窄间隙热丝氩弧焊工艺 | |
CN106112391A (zh) | 一种冶金复合双金属管坯的生产工艺 | |
CN107695614A (zh) | 一种多层金属板的结合方法 | |
JP7329692B2 (ja) | 溶接構造物の製造方法、及びこれにより製造された溶接構造物 | |
CN108290239B (zh) | 立式窄坡口气体保护弧焊方法 | |
CN117042909A (zh) | 电阻点焊接头以及电阻点焊接头的制造方法 | |
CN104439648A (zh) | 一种3-5mm板厚的铝及其合金TIG焊焊接工艺 | |
CN107378197A (zh) | 一种防止换热器管板堆焊时变形的加工方法 | |
CN113814602A (zh) | 一种硬质合金钎焊用三明治复合钎料的生产方法及专用设备 | |
CN107775269A (zh) | 一种复合板及其制备方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PB01 | Publication | ||
PB01 | Publication | ||
SE01 | Entry into force of request for substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20180216 |