CN107557822A - A kind of Sulphate Galvanizing Brightener - Google Patents

A kind of Sulphate Galvanizing Brightener Download PDF

Info

Publication number
CN107557822A
CN107557822A CN201610508194.5A CN201610508194A CN107557822A CN 107557822 A CN107557822 A CN 107557822A CN 201610508194 A CN201610508194 A CN 201610508194A CN 107557822 A CN107557822 A CN 107557822A
Authority
CN
China
Prior art keywords
sodium
parts
sulphate
benzylideneacetone
castor oil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610508194.5A
Other languages
Chinese (zh)
Inventor
吴明辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201610508194.5A priority Critical patent/CN107557822A/en
Publication of CN107557822A publication Critical patent/CN107557822A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of Sulphate Galvanizing Brightener to include benzylideneacetone, o-chlorobenzaldehyde, AEO Disodium sulfosuccinate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and deionized water, using benzylideneacetone, o-chlorobenzaldehyde and AEO Disodium sulfosuccinate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate matches, it is aided with nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and the mode for being dissolved in deionized water, synthesize a kind of Sulphate Galvanizing Brightener, the characteristics of being walked with zinc-plated bright and low unit.

Description

A kind of Sulphate Galvanizing Brightener
Technical field
The present invention relates to electroplating additive technical field, espespecially a kind of Sulphate Galvanizing Brightener.
Background technology
Zinc-plating brightener is mainly used in improving the brightness of zinc coat, increases the corrosion-resistant of zinc coat, improves case hardness, Make zinc coat light attractive in appearance, improve added value of product.The continuous zinc coating of steel wire and iron and steel material shaped, has that composition is simple, electric conductivity The features such as good, current efficiency height, maintenance management facilitate, it is widely used in the continuous electroplating of sheet material, wire rod, band, tubing, it is big absolutely Majority uses weakly acidic solutions using sulfate as main salt, but sulfate zinc plating with other it is zinc-plated compared with, its shortcoming is point Ability is dissipated, coating crystallization is more coarse.
The content of the invention
A kind of Sulphate Galvanizing Brightener of the present invention, it is characterized in that:Using benzylideneacetone, o-chlorobenzaldehyde and poly alkyl alcohol Oxygen vinethene Disodium sulfosuccinate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate matching, are aided with nicotinic acid, sodium benzoate winestone Sour potassium sodium is simultaneously dissolved in the mode of deionized water, there is provided a kind of Sulphate Galvanizing Brightener.
To achieve these goals, technical solution of the invention is:A kind of Sulphate Galvanizing Brightener includes benzal Acetone, o-chlorobenzaldehyde, AEO Disodium sulfosuccinate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, cigarette Acid, sodium benzoate sodium potassium tartrate tetrahydrate and deionized water, each component and its mass parts are:
2~4 parts of benzylideneacetone
1~3 part of o-chlorobenzaldehyde
10~20 parts of AEO Disodium sulfosuccinate
8~15 parts of castor oil polyoxyethylene ether ester
3~7 parts of sodium naphthalene sulfonate
1~2 part of nicotinic acid
0.05~0.2 part of sodium benzoate sodium potassium tartrate tetrahydrate
50~70 parts of deionized water;
The preparation method is that:Each component is quantitatively weighed by formula, first 50~70 parts of deionized water is added to folder In the agitator of set, 60~70 DEG C are warming up to, adds 2~4 parts of benzylideneacetone, 1~3 part of o-chlorobenzaldehyde, fatty alcohol polyoxy 10~20 parts of vinethene Disodium sulfosuccinate, 8~15 parts of castor oil polyoxyethylene ether ester, 3~7 parts of sodium naphthalene sulfonate, nicotinic acid 1~ 2 parts, 0.05~0.2 part of sodium benzoate sodium potassium tartrate tetrahydrate, stir 30~40 minutes, after each component mixing, stop stirring, go out Material, produces Sulphate Galvanizing Brightener.
Advantages of the present invention and feature are:Using benzylideneacetone, o-chlorobenzaldehyde and AEO butanedioic acid Ester sodium sulfonate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate matching, are aided with nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and are dissolved in The mode of ionized water, there is provided a kind of Sulphate Galvanizing Brightener, there is the characteristics of zinc-plated bright and low unit walks.
Embodiment
Embodiment 1
A kind of Sulphate Galvanizing Brightener includes benzylideneacetone, o-chlorobenzaldehyde, AEO succinate sulfonic acid Sodium, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and deionized water, each component and its matter Measuring part is:
3 kilograms of benzylideneacetone
2 kilograms of o-chlorobenzaldehyde
15 kilograms of AEO Disodium sulfosuccinate
11 kilograms of castor oil polyoxyethylene ether ester
3 kilograms of sodium naphthalene sulfonate
1.5 kilograms of nicotinic acid
0.15 kilogram of sodium benzoate sodium potassium tartrate tetrahydrate
60 kilograms of deionized water
Its preparation method is:By formula quantitatively weigh each component, first by deionized water 60 kilograms be added to the stirring with chuck In device, 60~70 DEG C are warming up to, adds 3 kilograms of benzylideneacetone, 2 kilograms of o-chlorobenzaldehyde, AEO amber 15 kilograms of acid esters sodium sulfonate, 11 kilograms of castor oil polyoxyethylene ether ester, 3 kilograms of sodium naphthalene sulfonate, 1.5 kilograms of nicotinic acid, sodium benzoate 0.15 kilogram of sodium potassium tartrate tetrahydrate, stir 30~40 minutes, after each component mixing, stop stirring, discharging, produce sulfate zinc plating Brightener
Embodiment 2
A kind of Sulphate Galvanizing Brightener includes benzylideneacetone, o-chlorobenzaldehyde, AEO succinate sulfonic acid Sodium, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and deionized water, each component and its matter Measuring part is:
4 kilograms of benzylideneacetone
1 kilogram of o-chlorobenzaldehyde
20 kilograms of AEO Disodium sulfosuccinate
8 kilograms of castor oil polyoxyethylene ether ester
5 kilograms of sodium naphthalene sulfonate
1 kilogram of nicotinic acid
0.2 kilogram of sodium benzoate sodium potassium tartrate tetrahydrate
70 kilograms of deionized water
The preparation method is that:By formula quantitatively weigh each component, first by deionized water 70 kilograms be added to chuck Agitator in, be warming up to 60~70 DEG C, add 4 kilograms of benzylideneacetone, 1 kilogram of o-chlorobenzaldehyde, aliphatic alcohol polyethenoxy 20 kilograms of ether Disodium sulfosuccinate, 8 kilograms of castor oil polyoxyethylene ether ester, 5 kilograms of sodium naphthalene sulfonate, 1 kilogram of nicotinic acid, benzoic acid 0.2 kilogram of sodium sodium potassium tartrate tetrahydrate, stir 30~40 minutes, after each component mixing, stop stirring, discharging, produce sulfate plating Zinc brightener.
Embodiment 3
A kind of Sulphate Galvanizing Brightener includes benzylideneacetone, o-chlorobenzaldehyde, AEO succinate sulfonic acid Sodium, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, nicotinic acid, sodium benzoate sodium potassium tartrate tetrahydrate and deionized water, each component and its matter Measuring part is:
2 kilograms of benzylideneacetone
3 kilograms of o-chlorobenzaldehyde
10 kilograms of AEO Disodium sulfosuccinate
15 kilograms of castor oil polyoxyethylene ether ester
7 kilograms of sodium naphthalene sulfonate
2 kilograms of nicotinic acid
0.05 kilogram of sodium benzoate sodium potassium tartrate tetrahydrate
50 kilograms of deionized water
The preparation method is that:By formula quantitatively weigh each component, first by deionized water 50 kilograms be added to chuck Agitator in, be warming up to 60~70 DEG C, add 2 kilograms of benzylideneacetone, 3 kilograms of o-chlorobenzaldehyde, aliphatic alcohol polyethenoxy 10 kilograms of ether Disodium sulfosuccinate, 15 kilograms of castor oil polyoxyethylene ether ester, 7 kilograms of sodium naphthalene sulfonate, 2 kilograms of nicotinic acid, benzene first Sour 0.05 kilogram of sodium sodium potassium tartrate tetrahydrate, stir 30~40 minutes, after each component mixing, stop stirring, discharging, produce sulfate Zinc-plating brightener.
Described above, embodiment is only that the preferred embodiment of the present invention is described, not to the present invention's Scope is defined, on the premise of the spirit of the technology of the present invention is not departed from, skill of this area engineers and technicians to the present invention The various modifications and improvement that art scheme is made, it all should fall into the protection domain of claims of the present invention determination.

Claims (2)

1. a kind of Sulphate Galvanizing Brightener, it is characterized in that:Described Sulphate Galvanizing Brightener includes benzylideneacetone, adjacent chlorine Benzaldehyde, AEO Disodium sulfosuccinate, castor oil polyoxyethylene ether ester, sodium naphthalene sulfonate, nicotinic acid, benzoic acid Sodium sodium potassium tartrate tetrahydrate and deionized water, each component and its mass parts are:
2~4 parts of benzylideneacetone
1~3 part of o-chlorobenzaldehyde
10~20 parts of AEO Disodium sulfosuccinate
8~15 parts of castor oil polyoxyethylene ether ester
3~7 parts of sodium naphthalene sulfonate
1~2 part of nicotinic acid
0.05~0.2 part of sodium benzoate sodium potassium tartrate tetrahydrate
50~70 parts of deionized water.
2. a kind of Sulphate Galvanizing Brightener according to claim 1, it is characterized in that:Described Sulphate Galvanizing Brightener Preparation method be:By formula quantitatively weigh each component, first by deionized water 50~70 parts be added to the agitator with chuck In, 60~70 DEG C are warming up to, adds 2~4 parts of benzylideneacetone, 1~3 part of o-chlorobenzaldehyde, AEO amber 10~20 parts of acid esters sodium sulfonate, 8~15 parts of castor oil polyoxyethylene ether ester, 3~7 parts of sodium naphthalene sulfonate, 1~2 part of nicotinic acid, benzoic acid 0.05~0.2 part of sodium sodium potassium tartrate tetrahydrate, stir 30~40 minutes, after each component mixing, stop stirring, discharging, produce sulfuric acid Salt zinc-plating brightener.
CN201610508194.5A 2016-07-01 2016-07-01 A kind of Sulphate Galvanizing Brightener Pending CN107557822A (en)