CN107286940A - 一种环保型纳米固沙粘结剂及其制备方法与应用 - Google Patents

一种环保型纳米固沙粘结剂及其制备方法与应用 Download PDF

Info

Publication number
CN107286940A
CN107286940A CN201710567614.1A CN201710567614A CN107286940A CN 107286940 A CN107286940 A CN 107286940A CN 201710567614 A CN201710567614 A CN 201710567614A CN 107286940 A CN107286940 A CN 107286940A
Authority
CN
China
Prior art keywords
sand
water
nanometer
fixing binder
fixing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710567614.1A
Other languages
English (en)
Inventor
张彦
何学良
赵赏鑫
张贵赞
周永涛
李佳萌
姚瑶
陈吉祥
刘左军
张继义
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Lanzhou University of Technology
Petro China Beijing Natural Gas Pipeline Co Ltd
Original Assignee
Lanzhou University of Technology
Petro China Beijing Natural Gas Pipeline Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lanzhou University of Technology, Petro China Beijing Natural Gas Pipeline Co Ltd filed Critical Lanzhou University of Technology
Priority to CN201710567614.1A priority Critical patent/CN107286940A/zh
Publication of CN107286940A publication Critical patent/CN107286940A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种纳米固沙粘结剂及其应用。本发明粘结剂的制备过程为:将凹凸棒石、水按质量比(1~2):10混合,凹凸棒石在水中浸泡20h~28h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂,该纳米固沙粘结剂可应用在防风固沙方面。本发明所用材料为天然材料,性质稳定,不会带来二次污染,材料来源广泛,费用低廉,制备工艺简单,易于操作和大面积推广使用;本发明固沙粘结剂的使用能改良土壤性质,增强沙土的保水能力,促进天然植物的定居和生长繁殖,能加速沙地固定和生态恢复进程。

Description

一种环保型纳米固沙粘结剂及其制备方法与应用
技术领域
本发明属于环保材料领域,尤其涉及一种环保型纳米固沙粘结剂及其制备方法与应用。
背景技术
现有的技术多是采用高分子有机化合物作为粘结剂的主要成分,虽然粘结性和固沙效果尚可,但不环保、成本高,大面积喷洒高分子有机化合物具有潜在的环境风险。
发明内容
本发明的目的在于提供一种环保型纳米固沙粘结剂及其制备方法与应用,旨在解决上述背景技术中的不足。
本发明是这样实现的,一种纳米固沙粘结剂,该粘结剂的制备过程为:将凹凸棒石、水按质量比(1~2):10混合,凹凸棒石在水中浸泡20h~28h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂。
优选地,所述凹凸棒石、水按质量比1:10混合。
优选地,所述纳米固沙粘结剂中凹凸棒石和水的质量比为1:(100~200)。
本发明进一步公开了上述纳米固沙粘结剂在防风固沙方面的应用。将纳米固沙粘结剂用喷雾、喷洒设备在流动沙地表面进行喷洒,经自然干燥后,凹凸棒纳米粒子将松散的沙粒胶结起来,在沙地表层形成一个具有较强抗风蚀能力的稳定层,起到防风固沙作用。
相比于现有技术的缺点和不足,本发明具有以下有益效果:
(1)本发明所用材料为天然材料,性质稳定,不会带来二次污染,材料来源广泛,费用低廉,制备工艺简单,易于操作和大面积推广使用;
(2)本发明固沙粘结剂的使用能改良土壤性质,增强沙土的保水能力,促进天然植物的定居和生长繁殖,能加速沙地固定和生态恢复进程。
具体实施方式
为了使本发明的目的、技术方案及优点更加清楚明白,以下结合实施例,对本发明进行进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定本发明。
实施例1
将1质量份凹凸棒石加入到10质量份水中,浸泡24h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂1,纳米固沙粘结剂1中凹凸棒石和水的质量比为1:100。
将纳米固沙粘结剂1用喷雾、喷洒设备在流动沙地表面进行喷洒,经自然干燥后,凹凸棒纳米粒子将松散的沙粒胶结起来,在沙地表层形成一个具有较强抗风蚀能力的稳定层,起到防风固沙作用。
实施例2
将2质量份凹凸棒石加入到10质量份水中,浸泡20h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂2,纳米固沙粘结剂2中凹凸棒石和水的质量比为1:200。
将纳米固沙粘结剂2用喷雾、喷洒设备在流动沙地表面进行喷洒,经自然干燥后,凹凸棒纳米粒子将松散的沙粒胶结起来,在沙地表层形成一个具有较强抗风蚀能力的稳定层,起到防风固沙作用。
实施例3
将2质量份凹凸棒石加入到10质量份水中,浸泡28h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂3,纳米固沙粘结剂3中凹凸棒石和水的质量比为1:100。
将纳米固沙粘结剂3用喷雾、喷洒设备在流动沙地表面进行喷洒,经自然干燥后,凹凸棒纳米粒子将松散的沙粒胶结起来,在沙地表层形成一个具有较强抗风蚀能力的稳定层,起到防风固沙作用。
以上所述仅为本发明的较佳实施例而已,并不用以限制本发明,凡在本发明的精神和原则之内所作的任何修改、等同替换和改进等,均应包含在本发明的保护范围之内。

Claims (4)

1.一种纳米固沙粘结剂,其特征在于,该粘结剂的制备过程为:将凹凸棒石、水按质量比(1~2):10混合,凹凸棒石在水中浸泡20h~28h后,搅拌、捣碎直至成均匀悬浊液,加水稀释后得到纳米固沙粘结剂。
2.如权利要求1所述的纳米固沙粘结剂,其特征在于,所述凹凸棒石、水按质量比1:10混合。
3.如权利要求2所述的纳米固沙粘结剂,其特征在于,所述纳米固沙粘结剂中凹凸棒石和水的质量比为1:(100~200)。
4.权利要求1~3任一项所述的纳米固沙粘结剂在防风固沙方面的应用。
CN201710567614.1A 2017-07-12 2017-07-12 一种环保型纳米固沙粘结剂及其制备方法与应用 Pending CN107286940A (zh)