CN107236463A - A kind of solid wooden floor board wax - Google Patents
A kind of solid wooden floor board wax Download PDFInfo
- Publication number
- CN107236463A CN107236463A CN201710511082.XA CN201710511082A CN107236463A CN 107236463 A CN107236463 A CN 107236463A CN 201710511082 A CN201710511082 A CN 201710511082A CN 107236463 A CN107236463 A CN 107236463A
- Authority
- CN
- China
- Prior art keywords
- parts
- wax
- extract
- floor board
- solid wooden
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to a kind of solid wooden floor board wax, by weight, it is uniformly mixed by following material:100 120 parts of paraffin, 50 60 parts of Brazil wax, 10 20 parts of silicone oil, 10 15 parts of kerosene, 5 10 parts of mint extract, 5 10 parts of cinnamomum camphora extract, 5 10 parts of lemon extract, 24 parts of emulsifying agent, 12 parts of dispersant.By experiment, a kind of solid wooden floor board wax that the inventive method is provided, compared to paste solid wooden floor board wax conventional on the market, it is more preferable to the maintenance effect on floor, either non-skid property, anti-scratch performance have good effect after waxing, smell of the present invention is more naturally pure and fresh simultaneously, it is to avoid the harm that is caused using natural flavor to human body, and market potential is huge.
Description
Technical field
The invention belongs to daily living article field, and in particular to a kind of solid wooden floor board wax.
Background technology
Floor wax, the white senior solid wax of oiliness, band fragrance, high temperature is semi-solid in oiliness, and low temperature is in hard solid, can be quick
The pore of material is penetrated into, is processed by shot blasting with high-speed glazing machine or floor-cleaning machine, makes ground that there is very strong glossiness, it is higher
Wearability and feud effect, rough earth is formed hard diaphragm, it is especially anti-skidding, anti-scratch, wear-resisting, effectively prevent water
Part, greasy dirt and other materials corrode.The main component of floor wax has silicone oil, special antilubricant, antistatic additive, natural plants wax.
It is usually used in solid wooden floor board, composite floor board, marble, ceramic tile and rigid plastics, the ground such as paint.Floor wax can decompose dirt,
The stain and dirt of floor deep layer are removed, high-effective cleansing is reached.Wax in the woodbox timber floor or concrete floor in house, both
It is attractive in appearance and be easy to sweep cleaning, and floor can be protected, make its durable in use.
Floor wax on the market contains a large amount of kerosene, natural flavor composition at present, and peculiar smell is big when using, and having of volatilizing
Noxious material can influence our health.
The content of the invention
In order to overcome above mentioned problem, the invention provides a kind of solid wooden floor board wax.
The present invention is achieved through the following technical solutions:
A kind of solid wooden floor board wax, by weight, is uniformly mixed by following material:100-120 parts of paraffin, Brazil wax
50-60 parts, 10-20 parts of silicone oil, 10-15 parts of kerosene, 5-10 parts of mint extract, 5-10 parts of cinnamomum camphora extract, lemon extract
5-10 parts, 2-4 parts of emulsifying agent, 1-2 parts of dispersant;Its preparation method, specifically includes following steps:
(1)80-85 is heated to after being mixed after the paraffin, Brazil wax are mixed with the pure water of 0.5 times of Quality of Paraffin Waxes number
DEG C, using mixer 200r/min stir process 3-5 minutes, then it is poured into container, treats its natural cooling, wax is frozen into
After type, water removal, and scrape off after the impurity of wax surface accumulation, removal of impurities wax is obtained, paraffin collocation Brazil wax is being sufficiently reserved Brazil
While the premium properties of palm wax, production cost is effectively reduced, by way of the heating stirring that adds water, wax water is make use of not
Molten characteristic, effectively removes paraffin removal reclaimed water solubility impurity, then using impurity and the difference of the density of wax, fully removes and accumulates in wax
The impurity on surface, obtains removal of impurities wax, is the outstanding raw material of solid wooden floor board wax;
(2)The removal of impurities wax is heated into melting again, is sufficiently stirred for 10-15 minutes, wherein peculiar smell is fully volatilized, then add
After the silicone oil, kerosene, mint extract, cinnamomum camphora extract, lemon extract, emulsifying agent, dispersant, 70-80 DEG C of insulation is filled
Divide stirring mixing 10-12 minutes, produce the solid wooden floor board wax;Natural flavor is replaced using plant extracts, it is more green strong
Health, at the same active ingredient in plant extracts can with the noxious material reaction bonded in wax, further function as elimination peculiar smell and
The effect of non-simple covering smell.
Further, the mint extract, is heated by the water of dried peppermint leaf plus 10 times of its mass fractions and distilled, must distilled
Liquid, by distillate in being handled 15 minutes in 200r/min centrifuges, it is the peppermint leaf extract to take supernatant liquor.
Further, the cinnamomum camphora extract, is cleaned by camphor tree branches and leaves, is crushed to 80 mesh, plus 2 times of branck of Lignum cinnamomi camphorae leaf qualities part
Several compound ferment treatment 150 minutes, then add the 0.1% sodium chloride solution heating of 5 times of branck of Lignum cinnamomi camphorae leaf quality numbers to boil 60 minutes,
Filter residue and filtrate are filtered to obtain, filtrate drying moisture to 1/3rd of original volume is produced into the camphor tree extract solution;It is described compound
Enzyme, quality parts ratio 3 is pressed by cellulase, hemicellulase, ligninase:1:5 mix.
Further, the lemon extract, squeezing is cleaned by lemon, and pressed liquor is obtained after filtering, pressed liquor is stood into 2-3
My god, it is the lemon extract to take supernatant liquor.
Beneficial effects of the present invention:Present invention side is being sufficiently reserved Brazil wax using paraffin collocation Brazil wax
Premium properties while, effectively reduce production cost, by way of the heating stirring that adds water, make use of the water-insoluble spy of wax
Property, paraffin removal reclaimed water solubility impurity is effectively removed, then using impurity and the difference of the density of wax, fully removes and accumulates in wax surface
Impurity, obtains removal of impurities wax, is the outstanding raw material of solid wooden floor board wax;Meanwhile, natural flavor is replaced using plant extracts, it is greener
Color health, while the active ingredient in plant extracts can further function as elimination different with the noxious material reaction bonded in wax
The effect of taste rather than simple covering smell.A kind of solid wooden floor board wax provided by experiment, the inventive method, compared to market
Upper conventional paste solid wooden floor board wax, more preferable to the maintenance effect on floor, either non-skid property, anti-scratch performance have after waxing
Good effect, while smell of the present invention is more naturally pure and fresh, it is to avoid the harm caused using natural flavor to human body, market
Have a high potential.
Embodiment
Embodiment 1
A kind of solid wooden floor board wax, by weight, is uniformly mixed by following material:100 parts of paraffin, Brazil wax 50
It is part, 10 parts of silicone oil, 10 parts of kerosene, 5 parts of mint extract, 5 parts of cinnamomum camphora extract, 5 parts of lemon extract, 2 parts of emulsifying agent, scattered
1 part of agent;Its preparation method, specifically includes following steps:
(1)80-85 is heated to after being mixed after the paraffin, Brazil wax are mixed with the pure water of 0.5 times of Quality of Paraffin Waxes number
DEG C, using mixer 200r/min stir process 3 minutes, then it is poured into container, treats its natural cooling, wax coagulation forming
Afterwards, remove water, and scrape off after the impurity of wax surface accumulation, obtain removal of impurities wax, paraffin collocation Brazil wax is being sufficiently reserved cohune
While the premium properties of palmitic acid wax, production cost is effectively reduced, by way of the heating stirring that adds water, make use of wax water insoluble
Characteristic, effectively remove paraffin removal reclaimed water solubility impurity, then using impurity and the difference of the density of wax, fully remove accumulate in wax table
The impurity in face, obtains removal of impurities wax, is the outstanding raw material of solid wooden floor board wax;
(2)The removal of impurities wax is heated into melting again, is sufficiently stirred for 10 minutes, wherein peculiar smell is fully volatilized, then add institute
State after silicone oil, kerosene, mint extract, cinnamomum camphora extract, lemon extract, emulsifying agent, dispersant, 70-80 DEG C of insulation, fully
Stirring mixing 10 minutes, produces the solid wooden floor board wax;Natural flavor is replaced using plant extracts, more green and healthy, together
When plant extracts in active ingredient can further function as elimination peculiar smell rather than simple with the noxious material reaction bonded in wax
Covering smell effect.
Further, the mint extract, is heated by the water of dried peppermint leaf plus 10 times of its mass fractions and distilled, must distilled
Liquid, by distillate in being handled 15 minutes in 200r/min centrifuges, it is the peppermint leaf extract to take supernatant liquor.
Further, the cinnamomum camphora extract, is cleaned by camphor tree branches and leaves, is crushed to 80 mesh, plus 2 times of branck of Lignum cinnamomi camphorae leaf qualities part
Several compound ferment treatment 150 minutes, then add the 0.1% sodium chloride solution heating of 5 times of branck of Lignum cinnamomi camphorae leaf quality numbers to boil 60 minutes,
Filter residue and filtrate are filtered to obtain, filtrate drying moisture to 1/3rd of original volume is produced into the camphor tree extract solution;It is described compound
Enzyme, quality parts ratio 3 is pressed by cellulase, hemicellulase, ligninase:1:5 mix.
Further, the lemon extract, squeezing is cleaned by lemon, and pressed liquor is obtained after filtering, pressed liquor is stood into 2-3
My god, it is the lemon extract to take supernatant liquor.
Embodiment 2
A kind of solid wooden floor board wax, by weight, is uniformly mixed by following material:120 parts of paraffin, Brazil wax 60
Part, 20 parts of silicone oil, 15 parts of kerosene, 10 parts of mint extract, 10 parts of cinnamomum camphora extract, 10 parts of lemon extract, 4 parts of emulsifying agent,
2 parts of dispersant;Its preparation method, specifically includes following steps:
(1)80-85 is heated to after being mixed after the paraffin, Brazil wax are mixed with the pure water of 0.5 times of Quality of Paraffin Waxes number
DEG C, using mixer 200r/min stir process 5 minutes, then it is poured into container, treats its natural cooling, wax coagulation forming
Afterwards, remove water, and scrape off after the impurity of wax surface accumulation, obtain removal of impurities wax, paraffin collocation Brazil wax is being sufficiently reserved cohune
While the premium properties of palmitic acid wax, production cost is effectively reduced, by way of the heating stirring that adds water, make use of wax water insoluble
Characteristic, effectively remove paraffin removal reclaimed water solubility impurity, then using impurity and the difference of the density of wax, fully remove accumulate in wax table
The impurity in face, obtains removal of impurities wax, is the outstanding raw material of solid wooden floor board wax;
(2)The removal of impurities wax is heated into melting again, is sufficiently stirred for 15 minutes, wherein peculiar smell is fully volatilized, then add institute
State after silicone oil, kerosene, mint extract, cinnamomum camphora extract, lemon extract, emulsifying agent, dispersant, 70-80 DEG C of insulation, fully
Stirring mixing 12 minutes, produces the solid wooden floor board wax;Natural flavor is replaced using plant extracts, more green and healthy, together
When plant extracts in active ingredient can further function as elimination peculiar smell rather than simple with the noxious material reaction bonded in wax
Covering smell effect.
Further, the mint extract, is heated by the water of dried peppermint leaf plus 10 times of its mass fractions and distilled, must distilled
Liquid, by distillate in being handled 15 minutes in 200r/min centrifuges, it is the peppermint leaf extract to take supernatant liquor.
Further, the cinnamomum camphora extract, is cleaned by camphor tree branches and leaves, is crushed to 80 mesh, plus 2 times of branck of Lignum cinnamomi camphorae leaf qualities part
Several compound ferment treatment 150 minutes, then add the 0.1% sodium chloride solution heating of 5 times of branck of Lignum cinnamomi camphorae leaf quality numbers to boil 60 minutes,
Filter residue and filtrate are filtered to obtain, filtrate drying moisture to 1/3rd of original volume is produced into the camphor tree extract solution;It is described compound
Enzyme, quality parts ratio 3 is pressed by cellulase, hemicellulase, ligninase:1:5 mix.
Further, the lemon extract, squeezing is cleaned by lemon, and pressed liquor is obtained after filtering, pressed liquor is stood into 2-3
My god, it is the lemon extract to take supernatant liquor.
Embodiment 3
A kind of solid wooden floor board wax, by weight, is uniformly mixed by following material:110 parts of paraffin, Brazil wax 55
It is part, 15 parts of silicone oil, 12 parts of kerosene, 8 parts of mint extract, 8 parts of cinnamomum camphora extract, 6 parts of lemon extract, 3 parts of emulsifying agent, scattered
1 part of agent;Its preparation method, specifically includes following steps:
(1)80-85 is heated to after being mixed after the paraffin, Brazil wax are mixed with the pure water of 0.5 times of Quality of Paraffin Waxes number
DEG C, using mixer 200r/min stir process 4 minutes, then it is poured into container, treats its natural cooling, wax coagulation forming
Afterwards, remove water, and scrape off after the impurity of wax surface accumulation, obtain removal of impurities wax, paraffin collocation Brazil wax is being sufficiently reserved cohune
While the premium properties of palmitic acid wax, production cost is effectively reduced, by way of the heating stirring that adds water, make use of wax water insoluble
Characteristic, effectively remove paraffin removal reclaimed water solubility impurity, then using impurity and the difference of the density of wax, fully remove accumulate in wax table
The impurity in face, obtains removal of impurities wax, is the outstanding raw material of solid wooden floor board wax;
(2)The removal of impurities wax is heated into melting again, is sufficiently stirred for 12 minutes, wherein peculiar smell is fully volatilized, then add institute
State after silicone oil, kerosene, mint extract, cinnamomum camphora extract, lemon extract, emulsifying agent, dispersant, 70-80 DEG C of insulation, fully
Stirring mixing 11 minutes, produces the solid wooden floor board wax;Natural flavor is replaced using plant extracts, more green and healthy, together
When plant extracts in active ingredient can further function as elimination peculiar smell rather than simple with the noxious material reaction bonded in wax
Covering smell effect.
Further, the mint extract, is heated by the water of dried peppermint leaf plus 10 times of its mass fractions and distilled, must distilled
Liquid, by distillate in being handled 15 minutes in 200r/min centrifuges, it is the peppermint leaf extract to take supernatant liquor.
Further, the cinnamomum camphora extract, is cleaned by camphor tree branches and leaves, is crushed to 80 mesh, plus 2 times of branck of Lignum cinnamomi camphorae leaf qualities part
Several compound ferment treatment 150 minutes, then add the 0.1% sodium chloride solution heating of 5 times of branck of Lignum cinnamomi camphorae leaf quality numbers to boil 60 minutes,
Filter residue and filtrate are filtered to obtain, filtrate drying moisture to 1/3rd of original volume is produced into the camphor tree extract solution;It is described compound
Enzyme, quality parts ratio 3 is pressed by cellulase, hemicellulase, ligninase:1:5 mix.
Further, the lemon extract, squeezing is cleaned by lemon, and pressed liquor is obtained after filtering, pressed liquor is stood into 2-3
My god, it is the lemon extract to take supernatant liquor.
Comparative example 1
This comparative example 1 compared with Example 1, is added without the paraffin, and all uses Brazil wax, side in addition
Method step all same.
Comparative example 2
This comparative example 2 compared with Example 2, without using the Brazil wax, and all uses paraffin, side in addition
Method step all same.
Comparative example 3
This comparative example 3 compared with Example 3, without using the mint extract, cinnamomum camphora extract, lemon extract, changes
To use natural flavor, method and step all same in addition.
Control group
Conventional paste solid wooden floor board wax on the market.
Waxing maintenance is carried out to solid wooden floor board of the same race using above-mentioned 7 kinds of floor waxes respectively, after inviting volunteer to waxing
Effect is given a mark, 10 points of full marks, and fraction is higher, and the effect that represents is better, result such as table 1 after statistical average:
Table 1
It is anti-skidding | It is anti-scratch | Smell | |
Embodiment 1 | 7 | 8 | 8 |
Embodiment 2 | 7 | 8 | 8 |
Embodiment 3 | 7 | 8 | 8 |
Comparative example 1 | 7 | 8 | 8 |
Comparative example 2 | 5 | 7 | 8 |
Comparative example 3 | 7 | 8 | 7 |
Control group | 5 | 7 | 5 |
As shown in Table 1, a kind of solid wooden floor board wax that the inventive method is provided, compared to paste solid wooden floor board conventional on the market
Wax, more preferable to the maintenance effect on floor, either non-skid property, anti-scratch performance have good effect after waxing, while this hair
Bright smell is more natural pure and fresh, it is to avoid the harm caused using natural flavor to human body, and market potential is huge.
Claims (5)
1. a kind of solid wooden floor board wax, it is characterised in that by weight, is uniformly mixed by following material:Paraffin 100-120
Part, 50-60 parts of Brazil wax, 10-20 parts of silicone oil, 10-15 parts of kerosene, 5-10 parts of mint extract, cinnamomum camphora extract 5-10
Part, 5-10 parts of lemon extract, 2-4 parts of emulsifying agent, 1-2 parts of dispersant;Its preparation method, specifically includes following steps:
(1)80-85 is heated to after being mixed after the paraffin, Brazil wax are mixed with the pure water of 0.5 times of Quality of Paraffin Waxes number
DEG C, using mixer 200r/min stir process 3-5 minutes, then it is poured into container, treats its natural cooling, wax is frozen into
After type, water removal, and scrape off after the impurity of wax surface accumulation, obtain removal of impurities wax;
(2)The removal of impurities wax is heated into melting again, is sufficiently stirred for 10-15 minutes, then adds the silicone oil, kerosene, peppermint
After extract, cinnamomum camphora extract, lemon extract, emulsifying agent, dispersant, 70-80 DEG C of insulation is thoroughly mixed 10-12 points
Clock, produces the solid wooden floor board wax.
2. a kind of solid wooden floor board wax according to claim 1, it is characterised in that by weight, uniform by following material
Mix:110 parts of paraffin, 55 parts of Brazil wax, 15 parts of silicone oil, 12 parts of kerosene, 8 parts of mint extract, cinnamomum camphora extract 8
Part, 6 parts of lemon extract, 3 parts of emulsifying agent, 1 part of dispersant.
3. a kind of solid wooden floor board wax according to claim 1, it is characterised in that:The mint extract, by dried peppermint leaf plus
The water heating distillation of 10 times of its mass fractions, obtains distillate, by distillate in being handled 15 minutes in 200r/min centrifuges, takes
Layer clear liquid is the peppermint leaf extract.
4. a kind of solid wooden floor board wax according to claim 1, it is characterised in that:The cinnamomum camphora extract, by camphor tree branches and leaves
Clean, be crushed to 80 mesh, plus 2 times of branck of Lignum cinnamomi camphorae leaf quality numbers compound ferment treatment 150 minutes, then add 5 times of branck of Lignum cinnamomi camphorae leaf qualities
The 0.1% sodium chloride solution heating of number is boiled 60 minutes, filters to obtain filter residue and filtrate, and filtrate is dried into moisture to original volume
1/3rd produce the camphor tree extract solution;The complex enzyme, mass fraction is pressed by cellulase, hemicellulase, ligninase
Than 3:1:5 mix.
5. a kind of solid wooden floor board wax according to claim 1, it is characterised in that:The lemon extract, is cleaned by lemon
Squeezing, obtains pressed liquor after filtering, pressed liquor is stood into 2-3 days, it is the lemon extract to take supernatant liquor.