CN107217514A - Have a shave the preparation method of coffee-like cladding - Google Patents

Have a shave the preparation method of coffee-like cladding Download PDF

Info

Publication number
CN107217514A
CN107217514A CN201710602090.5A CN201710602090A CN107217514A CN 107217514 A CN107217514 A CN 107217514A CN 201710602090 A CN201710602090 A CN 201710602090A CN 107217514 A CN107217514 A CN 107217514A
Authority
CN
China
Prior art keywords
parts
scytoblastema
agent
coffee
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710602090.5A
Other languages
Chinese (zh)
Inventor
唐志坚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Foshan Nanhai Hongsheng Shoes Industry Co Ltd
Original Assignee
Foshan Nanhai Hongsheng Shoes Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Foshan Nanhai Hongsheng Shoes Industry Co Ltd filed Critical Foshan Nanhai Hongsheng Shoes Industry Co Ltd
Priority to CN201710602090.5A priority Critical patent/CN107217514A/en
Publication of CN107217514A publication Critical patent/CN107217514A/en
Pending legal-status Critical Current

Abstract

A kind of preparation method for coffee-like cladding of having a shave, is related to the preparation of cladding, this method comprises the following steps:Step one, scytoblastema changes colour, pending scytoblastema is placed on flour milling machine first, flour milling is carried out using the sand paper of No. 120, then the scytoblastema after flour milling is placed on full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, finally the scytoblastema sprayed will be entered into rinsing machine, and softening agent is added in rinsing machine, color fixing agent and water, washed 15 20 minutes in rinsing machine, scytoblastema after washing is taken out and is placed into dryer, dried 10 15 minutes in dryer, scytoblastema is taken out, pass through cladding color more saturation made from the method, comfort level can be more preferable, there is antique effect, and color and luster is unique, make color more natural, colour fixation can be more preferable.

Description

Have a shave the preparation method of coffee-like cladding
Technical field:
The present invention relates to the preparation of cladding, and in particular to a kind of preparation method for coffee-like cladding of having a shave.
Background technology:
Leather is widely used in the surface of people's livelihood articles for use, and such as tables and chairs, sofa, footwear material, clothing etc. increase people's livelihood articles for use Texture, aesthetic feeling or durability.Leather can be roughly divided into dermatine and natural leather.Natural leather, which refers to, to be taken animal fur and gives With drying, cleaning, softening, dyeing, deburring, the manufacture craft processing such as cut after, form surfacing and strong but pliable in texture skin Material.
There is following drawback in the finished product processed using existing processing method:1st, surface wound can not be repaired well It is residual, colour uneven, it is impossible to effective modification desalination cladding neck line;2nd, brightness is unnatural, and coloring effect is bad, and color is disorderly not It is resistance to see, it is impossible to which that, with effect modelled after an antique, in order to solve the above-mentioned technical problem, spy proposes a kind of new technical scheme.
The content of the invention:
The invention aims to overcome the weak point that above-mentioned prior art is present, and one kind is provided and had a shave coffee color The preparation method of cladding.
The technical solution adopted by the present invention is:A kind of preparation method for coffee-like cladding of having a shave, this method includes following step Suddenly:Step 1: scytoblastema changes colour, pending scytoblastema is placed on flour milling machine first, flour milling is carried out using the sand paper of No. 120, Then the scytoblastema after flour milling is placed on full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, will finally be sprayed Scytoblastema will enter into rinsing machine, and add softening agent, color fixing agent and water in rinsing machine, 15-20 points washed in rinsing machine Clock, the scytoblastema after washing is taken out and is placed into dryer, is dried 10-15 minutes in dryer, scytoblastema is taken out;
Step 2: finished product changes colour, the scytoblastema handled well in step one is placed into polishing machine first, passes through polishing machine Apply to apply after light footwear breast in light footwear breast, smearing in spreading on scytoblastema and spread receipts light auxiliary agent A, now the rotating speed of polishing machine is 19 Revolutions per second, finally apply and spread receipts light auxiliary agent B, now the rotating speed of polishing machine is 9 revolutions per seconds.
The composition and parts by weight of described spray dyeing liquor are coffee-like 40-50 parts of dyestuff, 10-20 parts of emulsifying agent, mixing 1-10 parts of wax, 20-30 parts of environment-friendly type solvent, 5-15 parts of polyurethane resin.
A kind of ratio of softening agent of described step is that the ratio of 45%, color fixing agent is 20% and the ratio of water is 35%.
The composition and parts by weight of described middle light footwear breast are bright pigment paste 20-40 parts, 14-16 parts of synthesis resin, feel 20-40 parts of agent, 20-30 parts of bleeding agent.
Described bleeding agent is made up of environment-friendly type solvent 45%, surfactant 15% and dispersant 40%, described point Powder is Sodium Polyacrylate or sulfonated melamine, and described surfactant is NPE, detergent alkylate Sulphur phenol calcium, alkyl polyoxyethylene ether phosphate, alkyl polyoxypropylene ether phosphate or thermally coupled distillation columns.
The composition and parts by weight of described receipts light auxiliary agent A are 40-50 parts of pigment paste palm wax, natural palm wax 15-25 Part, 5-15 parts of discoloration wax, 20-30 parts of hand feeling agent.
The composition and parts by weight of described receipts light auxiliary agent B be coffee-like 25-35 part of dyestuff, 10-20 parts of palm wax of green grass or young crops, comprehensive 10-20 parts of resin, 10-20 parts of hand feeling agent, 15-25 parts of surfactant, 15-25 parts of bleeding agent.
Described bleeding agent is made up of environment-friendly type solvent 65%, surfactant 15% and dispersant 20%.
Described hand feeling agent is the copolymer of silicone polyether.
Described softening agent is by nitrocotton, oiliness barras, the special bright resins of oiliness SK, polishes lubrication prescription and senior banana oil group Into;Described color fixing agent is condensation product, many amine cation type polymer or the cupric dihydro-amine formaldehyde tree of dicyandiamide and formaldehyde Fat water solubility initial reduced body.
Beneficial effects of the present invention are:By cladding color more saturation made from the method, comfort level can be more preferable, there is imitative Ancient effect, can effectively modify desalination cladding neck line, and color and luster is unique, makes color more natural, and colour fixation can be more preferable.
Embodiment:
The present invention is further described in conjunction with specific embodiments:
Embodiment one:
A kind of preparation method for coffee-like cladding of having a shave, this method comprises the following steps:Step 1: scytoblastema changes colour, first Pending scytoblastema is placed on flour milling machine, flour milling is carried out using the sand paper of No. 120, then the scytoblastema after flour milling is placed Onto full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, finally will be entered the scytoblastema sprayed into rinsing machine, and Softening agent, color fixing agent and water are added in rinsing machine, is washed 15 minutes in rinsing machine, the scytoblastema after washing is taken out and is placed into In dryer, dried 10 minutes in dryer, scytoblastema is taken out;
Step 2: finished product changes colour, the scytoblastema handled well in step one is placed into polishing machine first, passes through polishing machine Apply to apply after light footwear breast in light footwear breast, smearing in spreading on scytoblastema and spread receipts light auxiliary agent A, now the rotating speed of polishing machine is 19 Revolutions per second, finally apply and spread receipts light auxiliary agent B, now the rotating speed of polishing machine is 9 revolutions per seconds.
The composition and parts by weight of described spray dyeing liquor be coffee-like 40 parts of dyestuff, 10 parts of emulsifying agent, 1 part of blended wax, 20 parts of environment-friendly type solvent, 5 parts of polyurethane resin.
The composition and parts by weight of described middle light footwear breast be bright 20 parts of pigment paste, 14 parts of synthesis resin, 20 parts of hand feeling agent, 20 parts of bleeding agent.
The composition and parts by weight of described receipts light auxiliary agent A are 40 parts of pigment paste palm wax, 15 parts of natural palm wax, discoloration 5 parts of wax, 20 parts of hand feeling agent.
The composition and parts by weight of described receipts light auxiliary agent B are coffee-like 25 parts of dyestuff, blue or green 10 parts of palm wax, synthesis resin 10 parts, 10 parts of hand feeling agent, 15 parts of surfactant, 15 parts of bleeding agent.
Embodiment two:
A kind of preparation method for coffee-like cladding of having a shave, this method comprises the following steps:Step 1: scytoblastema changes colour, first Pending scytoblastema is placed on flour milling machine, flour milling is carried out using the sand paper of No. 120, then the scytoblastema after flour milling is placed Onto full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, finally will be entered the scytoblastema sprayed into rinsing machine, and Softening agent, color fixing agent and water are added in rinsing machine, is washed 18 minutes in rinsing machine, the scytoblastema after washing is taken out and is placed into In dryer, dried 13 minutes in dryer, scytoblastema is taken out;
Step 2: finished product changes colour, the scytoblastema handled well in step one is placed into polishing machine first, passes through polishing machine Apply to apply after light footwear breast in light footwear breast, smearing in spreading on scytoblastema and spread receipts light auxiliary agent A, now the rotating speed of polishing machine is 19 Revolutions per second, finally apply and spread receipts light auxiliary agent B, now the rotating speed of polishing machine is 9 revolutions per seconds.
The composition and parts by weight of described spray dyeing liquor be coffee-like 45 parts of dyestuff, 15 parts of emulsifying agent, 5 parts of blended wax, 25 parts of environment-friendly type solvent, 10 parts of polyurethane resin.
The composition and parts by weight of described middle light footwear breast be bright 30 parts of pigment paste, 15 parts of synthesis resin, 30 parts of hand feeling agent, 25 parts of bleeding agent.
The composition and parts by weight of described receipts light auxiliary agent A are 45 parts of pigment paste palm wax, 20 parts of natural palm wax, discoloration 10 parts of wax, 25 parts of hand feeling agent.
The composition and parts by weight of described receipts light auxiliary agent B are coffee-like 30 parts of dyestuff, blue or green 15 parts of palm wax, synthesis resin 15 parts, 15 parts of hand feeling agent, 20 parts of surfactant, 20 parts of bleeding agent.
Embodiment three:
A kind of preparation method for coffee-like cladding of having a shave, this method comprises the following steps:Step 1: scytoblastema changes colour, first Pending scytoblastema is placed on flour milling machine, flour milling is carried out using the sand paper of No. 120, then the scytoblastema after flour milling is placed Onto full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, finally will be entered the scytoblastema sprayed into rinsing machine, and Softening agent, color fixing agent and water are added in rinsing machine, is washed 20 minutes in rinsing machine, the scytoblastema after washing is taken out and is placed into In dryer, dried 15 minutes in dryer, scytoblastema is taken out;
Step 2: finished product changes colour, the scytoblastema handled well in step one is placed into polishing machine first, passes through polishing machine Apply to apply after light footwear breast in light footwear breast, smearing in spreading on scytoblastema and spread receipts light auxiliary agent A, now the rotating speed of polishing machine is 19 Revolutions per second, finally apply and spread receipts light auxiliary agent B, now the rotating speed of polishing machine is 9 revolutions per seconds.
The composition and parts by weight of described spray dyeing liquor be coffee-like 50 parts of dyestuff, 20 parts of emulsifying agent, 10 parts of blended wax, 30 parts of environment-friendly type solvent, 15 parts of polyurethane resin.
The composition and parts by weight of described middle light footwear breast be bright 40 parts of pigment paste, 16 parts of synthesis resin, 40 parts of hand feeling agent, 30 parts of bleeding agent.
The composition and parts by weight of described receipts light auxiliary agent A are 50 parts of pigment paste palm wax, 25 parts of natural palm wax, discoloration 15 parts of wax, 30 parts of hand feeling agent.
The composition and parts by weight of described receipts light auxiliary agent B are coffee-like 35 parts of dyestuff, blue or green 20 parts of palm wax, synthesis resin 20 parts, 20 parts of hand feeling agent, 25 parts of surfactant, 25 parts of bleeding agent.
Using effect is tested:
This research is handled cladding by randomly selecting 100 claddings, investigates the effect of this method each side.Test Project standards of grading are:Very satisfied 5 points, 4 points are satisfied with, general 3 points, 2 points, very dissatisfied 1 point are unsatisfied with.Wherein common group For common processing method;
In summary, the present invention its not only can effectively color saturation, reparation leather scar effect, antique effect and Color and luster problem, and use is safe and healthy, effective, colour fixation is also more preferable.The preparation method is by the processing to conventional leather Method makes breakthrough adjustment, and the proportioning of some unique raw material and raw material is equally added during adjustment, Make whole preparation method more smooth, and effect is apparent.
For those skilled in the art, other can be made various corresponding according to above technical scheme and design Change and deformation, and all these change and deformation should all belong within the protection domain of the claims in the present invention.

Claims (10)

1. a kind of preparation method for coffee-like cladding of having a shave, it is characterised in that:This method comprises the following steps:
Step 1: scytoblastema changes colour, pending scytoblastema is placed on flour milling machine first, flour milling is carried out using the sand paper of No. 120, Then the scytoblastema after flour milling is placed on full-automatic spray skin machine, spray dyeing liquor is uniformly sprayed onto on scytoblastema, will finally be sprayed Scytoblastema will enter into rinsing machine, and add softening agent, color fixing agent and water in rinsing machine, 15-20 points washed in rinsing machine Clock, the scytoblastema after washing is taken out and is placed into dryer, is dried 10-15 minutes in dryer, scytoblastema is taken out;
Step 2: finished product changes colour, the scytoblastema handled well in step one is placed into polishing machine first, by polishing machine in skin Apply to spread to apply after light footwear breast in middle smooth footwear breast, smearing on embryo and spread receipts light auxiliary agent A, now the rotating speed of polishing machine is 19 revolutions per seconds, Finally apply and spread receipts light auxiliary agent B, now the rotating speed of polishing machine is 9 revolutions per seconds.
2. the preparation method of coffee-like cladding according to claim 1 of having a shave, it is characterised in that:Described spray dyeing liquor Composition and parts by weight are coffee-like 40-50 parts of dyestuff, 10-20 parts of emulsifying agent, 1-10 parts of blended wax, environment-friendly type solvent 20-30 Part, 5-15 parts of polyurethane resin.
3. the preparation method of coffee-like cladding according to claim 1 of having a shave, it is characterised in that:Described step is a kind of The ratio of softening agent is that the ratio of 45%, color fixing agent is 20% and the ratio of water is 35%.
4. the preparation method of coffee-like cladding according to claim 1 of having a shave, it is characterised in that:Described middle light footwear breast Composition and parts by weight are bright pigment paste 20-40 parts, 14-16 parts of synthesis resin, 20-40 parts of hand feeling agent, 20-30 parts of bleeding agent.
5. the preparation method of coffee-like cladding according to claim 4 of having a shave, it is characterised in that:Described bleeding agent is by ring Guarantor's type solvent 45%, surfactant 15% and dispersant 40% are constituted, and described dispersant is Sodium Polyacrylate or sulfonated Melamine, described surfactant is NPE, detergent alkylate sulphur phenol calcium, alkyl polyoxyethylene ether phosphoric acid Ester, alkyl polyoxypropylene ether phosphate or thermally coupled distillation columns.
6. the preparation method of coffee-like cladding according to claim 1 of having a shave, it is characterised in that:Described receipts light auxiliary agent A Composition and parts by weight be 40-50 parts of pigment paste palm wax, 15-25 parts of natural palm wax, 5-15 parts of discoloration wax, hand feeling agent 20-30 parts.
7. the preparation method of coffee-like cladding according to claim 1 of having a shave, it is characterised in that:Described receipts light auxiliary agent B Composition and parts by weight be coffee-like 25-35 part of dyestuff, 10-20 parts of palm wax of green grass or young crops, 10-20 parts of synthesis resin, hand feeling agent 10- 20 parts, 15-25 parts of surfactant, 15-25 parts of bleeding agent.
8. the preparation method of coffee-like cladding according to claim 7 of having a shave, it is characterised in that:Described bleeding agent is by ring Guarantor's type solvent 65%, surfactant 15% and dispersant 20% are constituted.
9. the preparation method of the coffee-like cladding of having a shave according to claim 4,6 or 7, it is characterised in that:Described feel Agent is the copolymer of silicone polyether.
10. the preparation method of coffee-like cladding according to claim 3 of having a shave, it is characterised in that:Described softening agent by The special bright resin of nitrocotton, oiliness barras, oiliness SK, polishes lubrication prescription and senior banana oil composition;Described color fixing agent is double cyanogen The water-soluble initial reduced body of the condensation product of amine and formaldehyde, many amine cation type polymer or cupric dihydro-amine formaldehyde resin.
CN201710602090.5A 2017-07-21 2017-07-21 Have a shave the preparation method of coffee-like cladding Pending CN107217514A (en)