CN107175733A - A kind of fabrication processing of family expenses bookshelf - Google Patents

A kind of fabrication processing of family expenses bookshelf Download PDF

Info

Publication number
CN107175733A
CN107175733A CN201710410130.6A CN201710410130A CN107175733A CN 107175733 A CN107175733 A CN 107175733A CN 201710410130 A CN201710410130 A CN 201710410130A CN 107175733 A CN107175733 A CN 107175733A
Authority
CN
China
Prior art keywords
bookshelf
paint
family expenses
fabrication processing
spraying
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710410130.6A
Other languages
Chinese (zh)
Inventor
曲振波
毛斌
田蕴
周超华
黄华群
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201710410130.6A priority Critical patent/CN107175733A/en
Publication of CN107175733A publication Critical patent/CN107175733A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of fabrication processing of family expenses bookshelf, the fabrication processing of the family expenses bookshelf carries out blanking using wood sawing machine, double spread edge sealing is carried out using semi-automatic edge banding machine, mortise and mortice opening are carried out using tenonen, carrying out sheet material using Semi-automatic feeding filature fixes.The present invention using automatic edger complete conveying banded plate, send band, up and down milling side, polishing reduce process, greatly improve operating efficiency;The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature, and tenon improves the precision of assembling with tongue and groove fit, improves the stability of bookshelf;Pass through the processing technology of priming paint, secondary priming paint, intermediate coat and finish paint so that bookshelf good appearance, service life is long, it is not perishable and scratch.

Description

A kind of fabrication processing of family expenses bookshelf
Technical field
The present invention relates to family expenses bookshelf manufacturing technology field, specially a kind of fabrication processing of family expenses bookshelf.
Background technology
Bookshelf refers to that broadly people are used for specially putting the utensil of book at us.Due to its form, structure not Together, have again book lattice, bookcase, bookcase, etc. other titles.It is the universal apparatus during we live;Bookshelf in library can be with It is divided into metal imperial decree frame and wooden bookshelf according to material.And can be subdivided into single column, biprism type, lamination book among metal bookshelf Frame, dense stack room also have slide bookshelf;Wooden bookshelf material, including passed through by solid wood, He plates, Wooden core board, plate containing nodular flakes etc. Jia Gong Zu He shape, with oil paint coating or use face finish material patch, rich soft texture.Library's common type is upright Formula, base tilting L-type bookshelf, is to help reader to read books, the type with different size.
The wooden bookshelf of family expenses would generally be used for family's books storage, there is work when carrying out wooden bookshelf processing at present Skill is relatively complicated, inefficiency;The precision of assembling is low, the less stable of bookshelf;Paint is more thin, and color and luster is poor, holds Easily scratch, reduce service life.
The content of the invention
It is an object of the invention to provide a kind of fabrication processing of family expenses bookshelf, to solve to carry in above-mentioned background technology The problem of going out.
To achieve the above object, the present invention provides following technical scheme:A kind of fabrication processing of family expenses bookshelf, it is described The fabrication processing of family expenses bookshelf carries out blanking using wood sawing machine, and double spread edge sealing is carried out using semi-automatic edge banding machine, Mortise and mortice opening are carried out using tenonen, carrying out sheet material using Semi-automatic feeding filature fixes;
The fabrication processing of the family expenses bookshelf includes following process:
Process 1. carries out blanking according to the sharp wood sawing machine of family expenses book-house structure;
Process 2. completes conveying banded plate using automatic edger, send band, up and down milling side, polishing, edge sealing tape thickness:0.4 ~3mm;Edge bonding belt height:10~60mm;Thickness of workpiece:12~55mm;Minimum widith:70mm;Minimum length:160mm;Conveying Speed:9.5m/min;Milling side motor up and down: 0.75kw18000rpm 300HZ;Motor is polished up and down: 0.18kwX21400rpm;
Process 3. carries out mortise and mortice opening using tenonen to the backboard of bookshelf, side plate, dividing plate and bottom plate;
Process 4. is assembled to the backboard of family expenses bookshelf, side plate, dividing plate and bottom plate, by tenon and tongue and groove fit, and is used The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature for self-tapping screw.
Process 5. passes through the fixed rubber feet of super glue gluing in the lower surface of the bottom plate of family expenses bookshelf.
Process 6. carries out a priming paint to family expenses bookshelf, and a priming paint avoids drain spray, show-through, viscous paint defect, film thickness 10~20 μ;
7. 2 priming paint of process:Per pass seam, angle, side hidden area must be examined and adjust before large area spray painting with brushing Construction equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjust nozzle And spraying rate makes spraying uniform, the μ of total film thickness 20~30;
The intermediate coat of process 8.:Road seam, angle, side hidden area must be examined before large area spray painting with brushing and adjust construction Equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjustment nozzle and spray Applying speed makes spraying uniform, the μ of thickness 20~50;
The finish paint of process 9.:Control paint specification examines species, color, diluent of paint etc., examines paint quality, produces day Phase, record product batch number.Paint wet-film thickness is checked, adjustment nozzle and spraying rate make spraying uniform, reach thickness thickness 20 ~50 μ.
Process 10. is examined and corrects the construction quality of paint, it is to avoid drain spray, show-through, pin hole, bubble, sagging etc. occur outer Defect is seen, local blemish in paint is repaired in time;
Process 11. is dried to family expenses bookshelf, is checked and is corrected the conditions such as temperature, flow time, the drying time of baking room, Drying time is 2~3 hours.
It is preferred that, the family expenses bookshelf can use any one in core-board, solid wood board, particieboard, high polymer door plank Kind.
It is preferred that, carrying out bookshelf surface requirements before process 6 is constructed:1st, sandblasting cleannes grade:Sa2.5.2nd, sandblasting table Face dust:All visible dusts are blown away with compressed air.3rd, greasy dirt:Organic solvent scrub process is used, all visible greasy dirts are removed.
It is preferred that, carrying out bookshelf surface requirements before process 7 is constructed:1st, after secondary sandblasting is finished, all welding bead surfaces are clear Except tobacco and oxide skin.2nd, after secondary blasting treatment, before paint spraying is carried out, the defect of sprayed surface is tackled, especially Weld defect is checked again for and repaired.3rd, dust, the greasy dirt of lacquered surface are gone through, to there are still dust and oil Dirty surface should be cleaned out.The qualified FCL of pretreatment should start priming paint construction into construction station as early as possible, and the time should not surpass Spend 8 hours.
Compared with prior art, the beneficial effects of the invention are as follows:
1st, the present invention using automatic edger complete conveying banded plate, send band, up and down milling side, polishing reduce process, greatly It is big to improve operating efficiency.
2nd, the present invention side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature, and tenon and Tongue and groove fit improves the precision of assembling, improves the stability of bookshelf.
3rd, the processing technology that the present invention passes through priming paint, secondary priming paint, intermediate coat and finish paint so that bookshelf beautiful outline form See, service life is long, not perishable and scuffing.
Brief description of the drawings
Fig. 1 is that a kind of fabrication processing workflow schematic diagram of family expenses bookshelf is invented in this practicality.
Embodiment
Below in conjunction with the scheme in the embodiment of the present invention, the technical scheme in the embodiment of the present invention is carried out clear, complete Site preparation is described, it is clear that described embodiment is only a part of embodiment of the invention, rather than whole embodiments.It is based on Embodiment in the present invention, it is every other that those of ordinary skill in the art are obtained under the premise of creative work is not made Embodiment, belongs to the scope of protection of the invention.
Embodiment 1:
Process 1. chooses real woodwork plate as rapidoprint, and blanking is carried out according to the sharp wood sawing machine of family expenses book-house structure;
Process 2. completes conveying banded plate using automatic edger, send band, up and down milling side, polishing, edge sealing tape thickness: 2.5mm;Edge bonding belt height:40mm;Thickness of workpiece:30mm;Minimum widith:70mm;Minimum length:160mm;Transporting velocity: 9.5m/min;Milling side motor up and down:0.75kw18000rpm 300HZ;Motor is polished up and down:0.18kwX21400rpm;
Process 3. carries out mortise and mortice opening using tenonen to the backboard of bookshelf, side plate, dividing plate and bottom plate;
Process 4. is assembled to the backboard of family expenses bookshelf, side plate, dividing plate and bottom plate, by tenon and tongue and groove fit, and is used The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature for self-tapping screw.
Process 5. passes through the fixed rubber feet of super glue gluing in the lower surface of the bottom plate of family expenses bookshelf.
Process 6. carries out a priming paint to family expenses bookshelf, and a priming paint avoids drain spray, show-through, viscous paint defect, film thickness 10μ;
7. 2 priming paint of process:Per pass seam, angle, side hidden area must be examined and adjust before large area spray painting with brushing Construction equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjust nozzle And spraying rate makes spraying uniform, the μ of total film thickness 20;
The intermediate coat of process 8.:Road seam, angle, side hidden area must be examined before large area spray painting with brushing and adjust construction Equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjustment nozzle and spray Applying speed makes spraying uniform, the μ of thickness 50;
The finish paint of process 9.:Control paint specification examines species, color, diluent of paint etc., examines paint quality, produces day Phase, record product batch number.Paint wet-film thickness is checked, adjustment nozzle and spraying rate make spraying uniform, reach thickness thickness 50 μ。
Process 10. is examined and corrects the construction quality of paint, it is to avoid drain spray, show-through, pin hole, bubble, sagging etc. occur outer Defect is seen, local blemish in paint is repaired in time;
Process 11. is dried to family expenses bookshelf, is checked and is corrected the conditions such as temperature, flow time, the drying time of baking room, Drying time is 2 hours.
Existing process flow:1. improve operating efficiency(Process 2 improves 34%;Process 6, process 7 improve 21%;);2. improve Product Precision(Process 4 by tenon and tongue and groove fit, and using self-tapping screw by Semi-automatic feeding filature to tenon and tenon The side of groove connecting portion is fixed);3. improving paint effect, it is difficult to scratch, improves service life.
Embodiment 2:
Process 1. chooses core-board as rapidoprint, and blanking is carried out according to the sharp wood sawing machine of family expenses book-house structure;
Process 2. completes conveying banded plate using automatic edger, send band, up and down milling side, polishing, edge sealing tape thickness:3mm; Edge bonding belt height:60mm;Thickness of workpiece:55mm;Minimum widith: 70mm;Minimum length:160mm;Transporting velocity:9.5m/ min;Milling side motor up and down: 0.75kw18000rpm 300HZ;Motor is polished up and down: 0.18kwX21400rpm;
Process 3. carries out mortise and mortice opening using tenonen to the backboard of bookshelf, side plate, dividing plate and bottom plate;
Process 4. is assembled to the backboard of family expenses bookshelf, side plate, dividing plate and bottom plate, by tenon and tongue and groove fit, and is used The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature for self-tapping screw.
Process 5. passes through the fixed rubber feet of super glue gluing in the lower surface of the bottom plate of family expenses bookshelf.
Process 6. carries out a priming paint to family expenses bookshelf, and a priming paint avoids drain spray, show-through, viscous paint defect, film thickness 20μ;
7. 2 priming paint of process:Per pass seam, angle, side hidden area must be examined and adjust before large area spray painting with brushing Construction equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjust nozzle And spraying rate makes spraying uniform, the μ of total film thickness 20;
The intermediate coat of process 8.:Road seam, angle, side hidden area must be examined before large area spray painting with brushing and adjust construction Equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjustment nozzle and spray Applying speed makes spraying uniform, the μ of thickness 40;
The finish paint of process 9.:Control paint specification examines species, color, diluent of paint etc., examines paint quality, produces day Phase, record product batch number.Paint wet-film thickness is checked, adjustment nozzle and spraying rate make spraying uniform, reach thickness thickness 40 μ。
Process 10. is examined and corrects the construction quality of paint, it is to avoid drain spray, show-through, pin hole, bubble, sagging etc. occur outer Defect is seen, local blemish in paint is repaired in time;
Process 11. is dried to family expenses bookshelf, is checked and is corrected the conditions such as temperature, flow time, the drying time of baking room, Drying time is 2.5 hours.
Existing process flow:1. improve operating efficiency(Process 2 improves 35%;Process 6, process 7 improve 24%;);2. improve Product Precision(Process 4 by tenon and tongue and groove fit, and using self-tapping screw by Semi-automatic feeding filature to tenon and tenon The side of groove connecting portion is fixed);3. improving paint effect, it is difficult to scratch, improves service life.
Embodiment 3:
Process 1. chooses particieboard as rapidoprint, and blanking is carried out according to the sharp wood sawing machine of family expenses book-house structure;
Process 2. completes conveying banded plate using automatic edger, send band, up and down milling side, polishing, edge sealing tape thickness: 1.3mm;Edge bonding belt height:40mm;Thickness of workpiece:30mm;Minimum widith: 70mm;Minimum length:160mm;Transporting velocity: 9.5m/min;Milling side motor up and down: 0.75kw18000rpm 300HZ;Motor is polished up and down: 0.18kwX21400rpm;
Process 3. carries out mortise and mortice opening using tenonen to the backboard of bookshelf, side plate, dividing plate and bottom plate;
Process 4. is assembled to the backboard of family expenses bookshelf, side plate, dividing plate and bottom plate, by tenon and tongue and groove fit, and is used The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature for self-tapping screw.
Process 5. passes through the fixed rubber feet of super glue gluing in the lower surface of the bottom plate of family expenses bookshelf.
Process 6. carries out a priming paint to family expenses bookshelf, and a priming paint avoids drain spray, show-through, viscous paint defect, film thickness 10μ;
7. 2 priming paint of process:Per pass seam, angle, side hidden area must be examined and adjust before large area spray painting with brushing Construction equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjust nozzle And spraying rate makes spraying uniform, the μ of total film thickness 25;
The intermediate coat of process 8.:Road seam, angle, side hidden area must be examined before large area spray painting with brushing and adjust construction Equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjustment nozzle and spray Applying speed makes spraying uniform, the μ of thickness 50;
The finish paint of process 9.:Control paint specification examines species, color, diluent of paint etc., examines paint quality, produces day Phase, record product batch number.Paint wet-film thickness is checked, adjustment nozzle and spraying rate make spraying uniform, reach thickness thickness 50 μ。
Process 10. is examined and corrects the construction quality of paint, it is to avoid drain spray, show-through, pin hole, bubble, sagging etc. occur outer Defect is seen, local blemish in paint is repaired in time;
Process 11. is dried to family expenses bookshelf, is checked and is corrected the conditions such as temperature, flow time, the drying time of baking room, Drying time is 3 hours
Existing process flow:1. improve operating efficiency(Process 2 improves 14%;Process 6, process 7 improve 11%;);2. improve product Precision(Process 4 is connected by tenon and tongue and groove fit, and using self-tapping screw by Semi-automatic feeding filature to tenon and tongue-and-groove The side of socket part position is fixed);3. improving paint effect, it is difficult to scratch, improves service life.
Although an embodiment of the present invention has been shown and described, for the ordinary skill in the art, can be with A variety of changes, modification can be carried out to these embodiments, replace without departing from the principles and spirit of the present invention by understanding And modification, the scope of the present invention is defined by the appended.

Claims (4)

1. a kind of fabrication processing of family expenses bookshelf, under the fabrication processing of the family expenses bookshelf is carried out using wood sawing machine Material, double spread edge sealing is carried out using semi-automatic edge banding machine, is carried out mortise and mortice opening using tenonen, is utilized Semi-automatic feeding spiral shell Silk machine carries out sheet material and fixed;
It is characterized in that:The fabrication processing of the family expenses bookshelf includes following process:
Process 1. carries out blanking according to the sharp wood sawing machine of family expenses book-house structure;
Process 2. completes conveying banded plate using automatic edger, send band, up and down milling side, polishing, edge sealing tape thickness:0.4 ~3mm;Edge bonding belt height:10~60mm;Thickness of workpiece:12~55mm;Minimum widith:70mm;Minimum length:160mm;Conveying Speed:9.5m/min;Milling side motor up and down: 0.75kw18000rpm 300HZ;Motor is polished up and down: 0.18kwX21400rpm;
Process 3. carries out mortise and mortice opening using tenonen to the backboard of bookshelf, side plate, dividing plate and bottom plate;
Process 4. is assembled to the backboard of family expenses bookshelf, side plate, dividing plate and bottom plate, by tenon and tongue and groove fit, and is used The side of tenon and tongue-and-groove connecting portion is fixed by Semi-automatic feeding filature for self-tapping screw;
Process 5. passes through the fixed rubber feet of super glue gluing in the lower surface of the bottom plate of family expenses bookshelf;
Process 6. carries out a priming paint to family expenses bookshelf, and a priming paint avoids drain spray, show-through, viscous paint defect, and film thickness 10~ 20μ;
7. 2 priming paint of process:Per pass seam, angle, side hidden area must be examined and adjust before large area spray painting with brushing Construction equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjust nozzle And spraying rate makes spraying uniform, the μ of total film thickness 20~30;
The intermediate coat of process 8.:Road seam, angle, side hidden area must be examined before large area spray painting with brushing and adjust construction Equipment, drying condition and time, recoating interval etc., paint spraying defect is examined, examine paint wet-film thickness, adjustment nozzle and spray Applying speed makes spraying uniform, the μ of thickness 20~50;
The finish paint of process 9.:Control paint specification examines species, color, diluent of paint etc., examines paint quality, produces day Phase, record product batch number;
Paint wet-film thickness is checked, adjustment nozzle and spraying rate make spraying uniform, reach the μ of thickness thickness 20~50;
Process 10. is examined and corrects the construction quality of paint, it is to avoid the outward appearance such as drain spray, show-through, pin hole, bubble, sagging occurs and lacks Fall into, local blemish in paint is repaired in time;
Process 11. is dried to family expenses bookshelf, is checked and is corrected the conditions such as temperature, flow time, the drying time of baking room, Drying time is 2~3 hours.
2. a kind of fabrication processing of family expenses bookshelf according to claim 1, it is characterised in that:The family expenses bookshelf can Using any one in core-board, solid wood board, particieboard, high polymer door plank.
3. a kind of fabrication processing of family expenses bookshelf according to claim 1, it is characterised in that:Applied carrying out process 6 Bookshelf surface requirements before work:1st, sandblasting cleannes grade:Sa2.5;
2nd, sand blasted surface dust:All visible dusts are blown away with compressed air;
3rd, greasy dirt:Organic solvent scrub process is used, all visible greasy dirts are removed.
4. a kind of fabrication processing of family expenses bookshelf according to claim 1, it is characterised in that:Applied carrying out process 7 Bookshelf surface requirements before work:1st, after secondary sandblasting is finished, tobacco and oxide skin are removed in all welding bead surfaces;
2nd, after secondary blasting treatment, before paint spraying is carried out, the defect of sprayed surface is tackled, especially weld defect enters Row is checked again for and repaired;
3rd, dust, the greasy dirt of lacquered surface are gone through, to there are still dust and the surface of greasy dirt should clean out;
The qualified FCL of pretreatment should start priming paint construction into construction station as early as possible, and the time is not to be exceeded 8 hours.
CN201710410130.6A 2017-06-03 2017-06-03 A kind of fabrication processing of family expenses bookshelf Pending CN107175733A (en)