CN107127975A - Pressure bladder adhering method - Google Patents

Pressure bladder adhering method Download PDF

Info

Publication number
CN107127975A
CN107127975A CN201710245714.2A CN201710245714A CN107127975A CN 107127975 A CN107127975 A CN 107127975A CN 201710245714 A CN201710245714 A CN 201710245714A CN 107127975 A CN107127975 A CN 107127975A
Authority
CN
China
Prior art keywords
pressure bladder
gland
base
pressure
bladder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710245714.2A
Other languages
Chinese (zh)
Inventor
王克臻
刘林文
王立恒
孙帅
宫超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China General Nuclear Power Corp
CGN Power Co Ltd
China Nuclear Power Operation Co Ltd
Original Assignee
China General Nuclear Power Corp
CGN Power Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China General Nuclear Power Corp, CGN Power Co Ltd filed Critical China General Nuclear Power Corp
Priority to CN201710245714.2A priority Critical patent/CN107127975A/en
Publication of CN107127975A publication Critical patent/CN107127975A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of pressure bladder adhering method, comprise the following steps:S1, the interface in pressure bladder butt end smear bonding agent and drying;S2, by two butt end abutting joints of the pressure bladder to the support on base, and the pressure bladder is pressed on the base;S3, gland is pressed on the pressure bladder, and be locked on the base;Wherein, two butt ends positioning of the pressure bladder is contained in the locating slot between the gland and base, and the support is supported on below the pressure bladder;S4, the base and/or gland are heated, and then the pressure bladder is heated vulcanized, the interface of two butt ends of the pressure bladder is bonded together.The pressure bladder adhering method of the present invention, it is adaptable to the bonding of pressure bladder on circulating pump, improves the response time of scene bonding processing, is shorten to 2 hours by 72 hours original response times, saves bonding processing cost;It is simple to operate.

Description

Pressure bladder adhering method
Technical field
The present invention relates to pressure bladder adhesive technology field, more particularly to a kind of pressure bladder adhering method.
Background technology
Daya Gulf nuclear power CRF circulating pumps are for the safety that improves equipment and online in the important hydraulic of nuclear power, design The feasibility of maintenance, at the top plate shaft envelope of pump case, is designed with twice air sac sealing in structure, mechanical seal failure or Mechanical seal water is put into the case of need to isolating, and blocks pouring in for seawater.Air bag is seldom put under normal circumstances, but is needed It is always ensured that complete availability.Natural aging and the reason such as corrosion of seawater due to rubber, enter in overhaul to air bag Row suppresses inspection, has an other safety requirements for leakage phenomenon occur, can not meet equipment.For a long time, the replacing of air bag, Bonding, the problems such as due to the technology blockage of businessman, more complicated technique for sticking and construction condition limitation, overall technology needs Outsourcing, somewhat expensive also has certain hysteresis quality in the response of time, is also the hidden danger for influenceing overhaul to be smoothed out.
The content of the invention
The technical problem to be solved in the present invention is that there is provided a kind of low pressure bladder adhering method of simple to operate, cost.
The technical solution adopted for the present invention to solve the technical problems is:A kind of pressure bladder adhering method is provided, including Following steps:
S1, the interface in pressure bladder butt end smear bonding agent and drying;
S2, by two butt end abutting joints of the pressure bladder to the support on base, and by the blanket gas Capsule is pressed on the base;The inner circumferential shape of the support correspondence pressure bladder is set;
S3, gland is pressed on the pressure bladder, and be locked on the base;
Wherein, two butt ends positioning of the pressure bladder is contained in the locating slot between the gland and base, The support is supported on below the pressure bladder;
S4, the base and/or gland are heated, the pressure bladder is heated and vulcanized, makes the two of the pressure bladder The interface of individual butt end bonds together.
Preferably, step S4 comprises the following steps:
S4.1, it is heated to after 45-55 DEG C, constant temperature 5-10min;
S4.2, it is heated to after 95-105 DEG C, constant temperature 5-10min;
S4.3, it is heated to after 140-160 DEG C, constant temperature 25-30min.
Preferably, the base includes first base, is mobily connected in the second base of described first base one end;Institute Stating gland includes second of first gland and end gland, cooperation of the cooperation in the first base in the second base Gland, the end gland is located at side of first gland away from second gland;
Step S3 comprises the following steps:
S3.1, end gland pressed on described one butt end of pressure bladder, and be locked in first base, it is right The butt end is positioned;
S3.2, the second gland pressed on another butt end of the pressure bladder, and is locked in second base, The butt end is positioned;
S3.3, the first gland pressed on the pressure bladder, and be locked in first base.
Preferably, after step S3.2, the distance between the second base and the first base are adjusted so that described Two butt end closed butt joints of pressure bladder.
Preferably, in step S3.2, before the second gland pressing, increase frictional force is placed on the pressure bladder Fine sandpaper;After the second gland pressing, the fine sandpaper is located between the pressure bladder and the second gland.
Preferably, in step S3.3, before the first gland pressing, the interface in two butt ends of pressure bladder Locate spreading glue.
Preferably, it is further comprising the steps of:
S5, natural cooling, remove the pressure bladder after bonding.
Preferably, it is further comprising the steps of:
S6, to after bonding pressure bladder carry out suppress test.
Preferably, step S6 comprises the following steps:
S6.1, by the pressure bladder after bonding be arranged on air sac sealing component in;
S6.2, the air sac sealing component by pipeline connected into air compressor machine;Isolating valve, pressure regulator valve are housed on the pipeline And pressure gauge;
S6.3, it is inflated according to the bearing requirements of pressure bladder and suppressed.
Preferably, the air sac sealing component includes air bag seat, support ring and the pressure ring of ring-type;
Step S6.1 includes:
S6.1.1, the periphery that the pressure bladder is installed to support ring;
S6.1.2, the inner ring that the pressure bladder and support ring are loaded to the air bag seat;
S6.1.3, the pressure ring pressed on the pressure bladder and be locked on the air bag seat.
Beneficial effects of the present invention:Suitable for the bonding of pressure bladder on circulating pump, the sound of scene bonding processing is improved Between seasonable, it is shorten to 2 hours by 72 hours original response times, saves bonding processing cost;It is simple to operate.
Brief description of the drawings
Below in conjunction with drawings and Examples, the invention will be further described, in accompanying drawing:
Fig. 1 is base and the front view of gland cooperation in the present invention;
Fig. 2 is cross-sectional views of the Fig. 1 along line A-A;
Fig. 3 is that two butt ends of pressure bladder are positioned at the overlooking structure figure between gland and base in the present invention;
Fig. 4 is part section structural representation of the pressure bladder on air sac sealing component in the present invention.
Embodiment
In order to which technical characteristic, purpose and effect to the present invention are more clearly understood from, now compare accompanying drawing and describe in detail The embodiment of the present invention.
With reference to Fig. 1-3, the pressure bladder adhering method of one embodiment of the invention, it may include following steps:
S1, the interface in two butt ends 101,102 of pressure bladder 100 smear bonding agent and drying.
Generally, the pressure bladder material of circulating pump is neoprene, model MY Dwg H71128/1/2 (Wartsila Propulsion Singapore Pte Ltd are produced), possess good elasticity.For above-mentioned pressure bladder, bonding agent is excellent Select 6025 glue (CHCMOSIL X6025).
After bonding agent is smeared, 40min or so is spontaneously dried.
In addition, before step S1, being cleaned to the interface of the butt end 101,102 of pressure bladder 100, it is ensured that interface Cleannes.
S2, by the support 30 on two butt ends 101 of pressure bladder 100,102 abutting joints to base 10, and will Pressure bladder 100 is pressed on base 10.
Wherein, the inner circumferential shape of the shape correspondence pressure bladder 100 of support 30 is set so that support 30 can coincide twelve Earthly Branches Support is in the lower section of pressure bladder 100;The length of support 30 is consistent with the length of base 10, or the slightly smaller than length of base 10.It is close Envelope air bag 100 is pressed on base 10, it is impossible to have rake angle phenomenon.
The pressure bladder inner circumferential of circulating pump is generally T-shaped, so as to form the inner passage of pressure bladder;The correspondence of support 30 For T-shaped support.
S3, gland 20 is pressed on pressure bladder 100, and be locked on base 10.
Wherein, two butt ends 101,102 of pressure bladder 100 position the positioning being contained between gland 20 and base 10 In groove 40, support 30 is supported on the lower section of pressure bladder 100.
Further, base 10 may include first base 11, be mobily connected in the second base of the one end of first base 11 12;Gland 20 includes coordinating the first gland 21 in first base 11 and end gland 23, coordinated in second base 12 Second gland 22, end gland 23 is located at side of first gland 21 away from the second gland 22.Second base 12 can pass through regulation Component 13 is connected to one end of first base 11, and passes through the adjustable distance between the two of adjusting part 13.Adjusting part 13 include screw bolt and nut for being engaged etc..
Step S3 may include following steps:
S3.1, end gland 23 pressed on 100 1 butt ends 101 of pressure bladder, and be locked at first base On 11, butt end 101 is positioned.
Locking of the end gland 23 in first base 11, can be realized, such as bolt by latch assembly;Bolt preferably is selected from Pierced under above from end gland 23 in first base 11.
S3.2, the second gland 22 pressed on another butt end 102 of pressure bladder 100, and be locked at the second bottom On seat 12, butt end 102 is positioned.
Locking of second gland 22 in second base 12, can be realized, such as bolt by latch assembly;Bolt preferably is selected from Pierced under above from the second gland 22 in second base 12.
After step S3.2, the distance between second base 12 and first base 11 are adjusted so that pressure bladder 100 Two butt ends 101,102 closed butt joints, there is certain thrust.The distance between second base 12 and first base 11 are adjusted Section, can be realized by rotating the nut of adjusting part 13.
In addition, to prevent relative slip between the gland 22 of pressure bladder 100 and second, the pressing of the second gland 22 Before, the fine sandpaper of increase frictional force is placed on pressure bladder 100;After the pressing of second gland 22, fine sandpaper is located at pressure bladder 100 and second between gland 22.Before placement, by fine sandpaper doubling, the pressure of pressure bladder 100 and second is placed on coarse face outwardly Between lid 22, increase frictional force.
S3.3, the first gland 21 pressed on pressure bladder 100, and be locked in first base 11.
First gland 21 is compressed 100 two butt ends of pressure bladder 101,102, and thrust should not in compaction process Excessive, composition surface should be without gap between the first gland 21 and first base 11.Lock of first gland 21 in first base 11 Tightly, it can be realized by latch assembly, such as bolt.
In step S3.3, to ensure interface bonding quality, before the pressing of the first gland 21, in pressure bladder 100 two The interface spreading glue of butt end 101,102.It further can also stick high temperature adhesive plaster.
S4, base 10 and/or gland 20 are heated, pressure bladder 100 is heated and vulcanized, makes two of pressure bladder 100 The interface of butt end 101,102 bonds together, and forms the pressure bladder 100 of overall ring-type.
During heating, in the bottoming hole that heating rod (not shown) is plugged into the gland 21 of first base 11 and first respectively.Two The setting of individual bottoming hole, is heated simultaneously, it is to avoid single hole heats brought temperature gradient explained, improves the uniformity of heating.
Correspondence heating rod, the temperature that temp probe (not shown) is plugged into the gland 21 of first base 11 and first respectively is visited In gaging hole, with detection temperature.
On the gland 21 of first base 11 or first, the distance between bottoming hole and temperature sensing hole and bottoming hole and positioning Vertical range between the inner top surface of groove 40 (pressure bladder upper surface) is of substantially equal, improves the accuracy of measurement temperature.Preferably, The distance between bottoming hole and temperature sensing hole are slightly more than bottoming hole and the inner top surface of locating slot 40 (upper surface of pressure bladder 100) Between vertical range.
Specifically, step S4 may include following steps:
S4.1, it is heated to after 45-55 DEG C, constant temperature 5-10min;It is preferred that 50 DEG C, constant temperature 5min.
S4.2, it is heated to after 95-105 DEG C, constant temperature 5-10min;It is preferred that 100 DEG C, constant temperature 5min.
S4.3, it is heated to after 150-160 DEG C, constant temperature 25-30min;It is preferred that 150 DEG C, constant temperature 30min.The speed of heating should Suitably so that be heated to 150 DEG C of 1 hour or so used times.
Step S4 can be realized by heater.Heating rod is powered, while monitoring temperature variations.
Further, pressure bladder adhering method of the invention can also include the steps of:
S5, natural cooling, remove the pressure bladder after bonding.
Pressure bladder 100 is checked, Instant cement can be used to be bonded if any small breach, surface matter is checked Amount, is cleared up using fine sandpaper if any injustice, makes balloon surface smooth.
Further, pressure bladder adhering method of the invention can also include the steps of:
S6, to after bonding pressure bladder 100 carry out suppress test.
As shown in figure 4, step S6 may include following steps:
S6.1, by the pressure bladder 100 after bonding be arranged on air sac sealing component in.
S6.2, by air sac sealing component pass through pipeline it is (not shown) connection air compressor machine (not shown);Equipped with isolation on pipeline Valve, pressure regulator valve and pressure gauge.
S6.3, it is inflated according to the bearing requirements of pressure bladder 100 and suppressed.
Wherein, air sac sealing component includes air bag seat 51, support ring 52 and the pressure ring 53 of ring-type.
Step S6.1 further may include:
S6.1.1, the periphery that pressure bladder 100 is installed to support ring 52.
S6.1.2, the inner ring that pressure bladder 100 and support ring 52 are loaded to air bag seat 51.
S6.1.3, pressure ring 53 pressed on pressure bladder 100 and be locked on air bag seat 51.
In order to increase the sealing effectiveness of air bag, the physical length of pressure bladder 100 is more than the circumferential length of air bag seat 51.This Outside, appropriate lubricant can be smeared to be easily installed.
Air sac sealing component also includes the dummy shaft support 54 of ring-type.In step S6.1.3, blanket gas is pressed in pressure ring 53 Before on capsule 100, dummy shaft support 54 is loaded to the inner ring of air bag seat 51, so that pressure bladder 100 is positioned at the He of dummy shaft support 54 Between air bag seat 51.
In step S6.3, mounted pressure bladder 100 is inflated by air compressor machine, sealing is checked.
The blowing pressure is not less than 2.5bar, continues 30min;Pressure, which declines, is not more than 0.2bar, then illustrates pressure bladder 100 Bonding it is qualified, meet and use standard.
In air sac sealing component, air vent 55 is offered on the periphery of air bag seat 51, air vent 55 extends from air bag seat 51 Insertion is connected to the inner ring of air bag seat 51 with the inner passage with pressure bladder 100, and air compressor machine passes through 55 pairs of sealings of the air vent The inflation of air bag 100 is suppressed.
Embodiments of the invention are the foregoing is only, are not intended to limit the scope of the invention, it is every to utilize this hair Equivalent structure or equivalent flow conversion that bright specification and accompanying drawing content are made, or directly or indirectly it is used in other related skills Art field, is included within the scope of the present invention.

Claims (10)

1. a kind of pressure bladder adhering method, it is characterised in that comprise the following steps:
S1, the interface in pressure bladder butt end smear bonding agent and drying;
S2, by two butt end abutting joints of the pressure bladder to the support on base, and by the blanket gas bag pressure Tightly on the base;The inner circumferential shape of the support correspondence pressure bladder is set;
S3, gland is pressed on the pressure bladder, and be locked on the base;
Wherein, two butt ends positioning of the pressure bladder is contained in the locating slot between the gland and base, described Support is supported on below the pressure bladder;
S4, the base and/or gland are heated, the pressure bladder are heated and vulcanized, make two of the pressure bladder it is right The interface for connecing end bonds together.
2. pressure bladder adhering method according to claim 1, it is characterised in that step S4 comprises the following steps:
S4.1, it is heated to after 45-55 DEG C, constant temperature 5-10min;
S4.2, it is heated to after 95-105 DEG C, constant temperature 5-10min;
S4.3, it is heated to after 140-160 DEG C, constant temperature 25-30min.
3. pressure bladder adhering method according to claim 1, it is characterised in that the base includes first base, can Second base of the mobile link in described first base one end;The gland includes coordinating the first pressure in the first base Lid and end gland, the second gland coordinated in the second base, it is remote that the end gland is located at first gland The side of second gland;
Step S3 comprises the following steps:
S3.1, end gland pressed on described one butt end of pressure bladder, and be locked in first base, to described Butt end is positioned;
S3.2, the second gland pressed on another butt end of the pressure bladder, and be locked in second base, to institute Butt end is stated to be positioned;
S3.3, the first gland pressed on the pressure bladder, and be locked in first base.
4. pressure bladder adhering method according to claim 3, it is characterised in that after step S3.2, described the is adjusted The distance between two bases and the first base so that two butt end closed butt joints of the pressure bladder.
5. pressure bladder adhering method according to claim 3, it is characterised in that in step S3.2, second gland Before pressing, the fine sandpaper of increase frictional force is placed on the pressure bladder;After the second gland pressing, the fine sandpaper Between the pressure bladder and the second gland.
6. pressure bladder adhering method according to claim 3, it is characterised in that in step S3.3, first gland Before pressing, the interface spreading glue in described two butt ends of pressure bladder.
7. the pressure bladder adhering method according to claim any one of 1-6, it is characterised in that further comprising the steps of:
S5, natural cooling, remove the pressure bladder after bonding.
8. pressure bladder adhering method according to claim 7, it is characterised in that further comprising the steps of:
S6, to after bonding pressure bladder carry out suppress test.
9. pressure bladder adhering method according to claim 8, it is characterised in that step S6 comprises the following steps:
S6.1, by the pressure bladder after bonding be arranged on air sac sealing component in;
S6.2, the air sac sealing component by pipeline connected into air compressor machine;Isolating valve, pressure regulator valve and pressure are housed on the pipeline Power table;
S6.3, it is inflated according to the bearing requirements of pressure bladder and suppressed.
10. pressure bladder adhering method according to claim 9, it is characterised in that the air sac sealing component includes ring Air bag seat, support ring and the pressure ring of shape;
Step S6.1 includes:
S6.1.1, the periphery that the pressure bladder is installed to support ring;
S6.1.2, the inner ring that the pressure bladder and support ring are loaded to the air bag seat;
S6.1.3, the pressure ring pressed on the pressure bladder and be locked on the air bag seat.
CN201710245714.2A 2017-04-14 2017-04-14 Pressure bladder adhering method Pending CN107127975A (en)