CN107009091B - A kind of manufacturing method of metallic mobile phone shell - Google Patents

A kind of manufacturing method of metallic mobile phone shell Download PDF

Info

Publication number
CN107009091B
CN107009091B CN201610058107.0A CN201610058107A CN107009091B CN 107009091 B CN107009091 B CN 107009091B CN 201610058107 A CN201610058107 A CN 201610058107A CN 107009091 B CN107009091 B CN 107009091B
Authority
CN
China
Prior art keywords
blank
processing
bottom wall
cnc
forming
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201610058107.0A
Other languages
Chinese (zh)
Other versions
CN107009091A (en
Inventor
袁宏金
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yulong Computer Telecommunication Scientific Shenzhen Co Ltd
Original Assignee
Yulong Computer Telecommunication Scientific Shenzhen Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yulong Computer Telecommunication Scientific Shenzhen Co Ltd filed Critical Yulong Computer Telecommunication Scientific Shenzhen Co Ltd
Priority to CN201610058107.0A priority Critical patent/CN107009091B/en
Publication of CN107009091A publication Critical patent/CN107009091A/en
Application granted granted Critical
Publication of CN107009091B publication Critical patent/CN107009091B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention proposes a kind of manufacturing methods of metallic mobile phone shell, include: the nearly processing and forming step in blank front: the nearly processing and forming of CNC is carried out to the positive bottom wall of blank, so that the positive bottom wall thickness of blank is on the basis of mobile phone processing procedure product positive setting bottom wall thickness, remaining thickness surplus;The nearly processing and forming step in the blank back side: the nearly processing and forming of CNC is carried out to the bottom wall at the blank back side, so that the bottom wall thickness at the blank back side is the setting bottom wall size at the mobile phone processing procedure product back side;The net processing and forming step in blank front: the net processing and forming of CNC is carried out to the positive bottom wall of the blank, remove the thickness surplus, so that the positive bottom wall thickness of blank is the setting bottom wall thickness, solves the problems, such as handset shell deformation, and reduce the production cost of handset shell.

Description

A kind of manufacturing method of metallic mobile phone shell
Technical field
The present invention relates to the field shaping technique of handset shell more particularly to a kind of manufacturing methods of metallic mobile phone shell.
Background technique
Current phone is more and more thinner, and function is more and more, in the limited situation in interior of mobile phone space, only further subtracts The thickness of thin handset shell, such as integrated smart phone thickness of shell require to be no more than the flat of 0.5mm and handset shell Face degree is no more than 0.25mm, this is a greatly challenge for the smart phone that screen size is more than 5.2 inches.
Currently, there is apparent deformation, mobile phone using conventional computer numerical control processing CNC technology handset shell after molding The machining stress in shell front (towards the side of mobile phone screen) is much larger than the machine of the handset shell back side (towards outside) The flatness at the battery cover position of forming residual stress, especially handset shell is even up to 0.5mm, considerably beyond current phone The requirement of shell product.The method for correcting the deformation of aluminium alloy handset shell, can be after completing CNC technique, using shaping mould Correct the requirement of shape of product to finished product;CNC technique can also be changed using the methods of laser laser carving after completing CNC technique The stress distribution of generation, to correct shape of product to meet the requirement of finished product.But these use the side of subsequent assistant orthopedic Method increases the investment of other equipment, improves the production cost of handset shell.Therefore, it is necessary to a kind of systems of metallic mobile phone shell Method is made, to solve the above-mentioned technical problems in the prior art.
Summary of the invention
The technical problem to be solved in the present invention is to provide a kind of manufacturing methods of metallic mobile phone shell, solve handset shell The problem of deformation, and reduce the production cost of handset shell.
The technical solution adopted by the present invention is that:
A kind of manufacturing method of metallic mobile phone shell, comprising: the nearly processing and forming step in blank front: to the positive bottom of blank Wall carries out the nearly processing and forming of CNC, so that the positive bottom wall thickness of the blank is in the positive setting bottom wall thickness of mobile phone processing procedure product On the basis of, remaining thickness surplus;The nearly processing and forming step in the blank back side: to the bottom wall at the blank back side carry out CNC closely at Type processing, so that the bottom wall thickness at the blank back side is the setting bottom wall size at the mobile phone processing procedure product back side;Blank front only at Type procedure of processing: the net processing and forming of CNC is carried out to the positive bottom wall of the blank, the thickness surplus is removed, so that the base Expect that positive bottom wall thickness is the setting bottom wall thickness.
Preferably, the thickness surplus is 0.3mm~0.6mm.
Preferably, the thickness surplus is 0.3mm;The net processing and forming step in blank front, specifically includes: setting The speed of mainshaft of CNC board is 8000 revs/min, and the process velocity of the net processing and forming of CNC is 800MM/ points, removes the thickness Spend the 0.15mm in surplus;The speed of mainshaft that CNC board is arranged is 10000 revs/min, the processing speed of the net processing and forming of CNC Degree is 800MM/ points, removes the 0.1mm in the thickness surplus;The speed of mainshaft that CNC board is arranged is 12000 revs/min, described The process velocity of the net processing and forming of CNC is 600MM/ points, removes remaining 0.05mm in the thickness surplus.
Preferably, the CNC board is three axis machines, and the tool type of the three axis machine is face cutter, the end face milling The material of knife is hard alloy.
Preferably, between the nearly processing and forming step in the blank front and the nearly processing and forming step in the blank back side, institute State manufacturing method, further includes: remove the burr that the nearly processing and forming step in the blank front remains on the blank;Cleaning institute State clamp tool used in the nearly processing and forming step in blank front.
Preferably, after the net processing and forming step in blank front, the manufacturing method, further includes: remove the base The net processing and forming step in material front remains on the burr on the blank;The blank is surface-treated, mobile phone system is obtained Finished product.
Preferably, before the nearly processing and forming step in the blank front, the manufacturing method, further includes: according to the hand The size of mechanism finished product obtains the blank using hardware method for processing forming.
Preferably, the blank is aluminum alloy material.
By adopting the above technical scheme, the present invention at least has following effect:
The manufacturing method of metallic mobile phone shell of the invention solves the problems, such as metallic mobile phone housing distortion, especially super The thin more scabrous problem on deformation of large area aluminium alloy handset shell, improves the Product Precision of metallic mobile phone shell.In addition, should Manufacturing method is simple, without additionally increasing other process equipments, improves the output efficiency of metallic mobile phone shell, reduces production Cost.
Detailed description of the invention
Fig. 1 is the flow chart of the manufacturing method of the metallic mobile phone shell of first embodiment of the invention;
Fig. 2 is the flow chart of the manufacturing method of the metallic mobile phone shell of second embodiment of the invention;
Fig. 3 is the flow chart of the manufacturing method of the metallic mobile phone shell of third embodiment of the invention;
Fig. 4 is the flow chart of the manufacturing method of the metallic mobile phone shell of fourth embodiment of the invention;
Fig. 5 is the flow chart of the manufacturing method of the metallic mobile phone shell of fifth embodiment of the invention.
Specific embodiment
Further to illustrate the present invention to reach the technical means and efficacy that predetermined purpose is taken, below in conjunction with attached drawing And preferred embodiment, the present invention is described in detail as after.
The manufacturing method of metallic mobile phone shell provided by the invention, efficiently solves asking for metallic mobile phone housing distortion Topic, and reduce the production cost of metallic mobile phone shell.The system of metallic mobile phone shell of the invention will be described in detail belows Make method and its each step.
Term " processing procedure product " used in this application is not carry out the semi-finished product for the rear processing procedure process such as being surface-treated, so processing procedure The size of product includes the surplus that the size of manufactured goods need to be removed plus rear processing procedures such as surface treatments, for example polishing will remove 0.03mm, sandblasting or anodized need to remove 0.01mm.
First embodiment
The manufacturing method of metallic mobile phone shell as shown in Figure 1 includes: the nearly processing and forming step S10 in blank front, blank The nearly processing and forming step S20 in the back side and the net processing and forming step S30 in blank front, above-mentioned steps are completed in CNC machining center.
Wherein, the nearly processing and forming step S10 in blank front: carrying out the nearly processing and forming of CNC to the positive bottom wall of blank, so that The positive bottom wall thickness of blank is on the basis of mobile phone processing procedure product positive setting bottom wall thickness, remaining thickness surplus, to blank Positive bottom wall thickness carries out preparatory processing, retains the positive bottom wall thickness of mobile phone processing procedure product in the premise of setting bottom wall thickness Under, thickness surplus is reserved, avoids the prior art to the disposable processing in blank front, so that excessive machine occurs in blank front Forming residual stress.The material of blank can be aluminium alloy.
Then, it executes the nearly processing and forming step S20 in the blank back side: the nearly processing and forming of CNC is carried out to the bottom wall at the blank back side, So that the bottom wall thickness at the blank back side is the setting bottom wall size at the mobile phone processing procedure product back side.Due to the bottom wall at the mobile phone processing procedure product back side Thickness is much smaller than its positive bottom wall thickness, so in this step disposably by the bottom wall thickness milling at the blank back side to setting Bottom wall size biggish residual stress can't occur at the blank back side.
Finally, executing the net processing and forming step S30 in blank front: the net processing and forming of CNC is carried out to the positive bottom wall of blank, Thickness surplus is removed, so that the positive bottom wall thickness of blank is setting bottom wall thickness.In this step by step S10 reserve The removal of thickness surplus, the step is on the basis of step S10, the positive thickness surplus of milling blank, by the positive bottom wall of blank Thickness is machined to setting bottom wall thickness.
By above step, during CNC is processed, use discharges and corrects step by step mach the present embodiment Residual stress realizes that the surface stress of mobile phone processing procedure product front and back is balanced, solves the problems, such as metallic mobile phone housing distortion, The problem on deformation of especially ultra-thin large area aluminium alloy handset shell.
Preferably, the nearly processing and forming step S10 in blank front, the nearly processing and forming step S20 in the blank back side and blank Positive net processing and forming step S30 is using conventional CNC machined parameters.
Second embodiment
On the basis of first embodiment, the thickness surplus of the present embodiment is 0.3mm~0.6mm.Many experiments prove, thick Degree surplus is above range value, can effectively solve the problems, such as that handset shell deforms.
Further, thickness surplus can be 0.3mm.As shown in Fig. 2, in the net processing and forming step S30 in blank front, Specifically include: step S300: the speed of mainshaft of setting CNC board is 8000 revs/min, and the process velocity of the net processing and forming of CNC is 800MM/ points, remove the 0.15mm in thickness surplus.Step S301: the speed of mainshaft of setting CNC board is 10000 revs/min, The process velocity of the net processing and forming of CNC is 800MM/ points, removes the 0.1mm in thickness surplus.Step S302: setting CNC board The speed of mainshaft be 12000 revs/min, the process velocity of the net processing and forming of CNC is 600MM/ points, is removed remaining in thickness surplus 0.05mm。
Preferably, CNC board is three axis machines, and the tool type of three axis machines is face cutter, the material of face cutter The amount of feeding of cutter is set as 0.15mm, removes the 0.15mm in thickness surplus in step S300 for hard alloy;In step In rapid S301, the amount of feeding of cutter is set as 0.1mm, removes the 0.1mm in thickness surplus;In step s 302, cutter is set The amount of feeding be 0.05mm, remove thickness surplus in remaining 0.05mm.
In this embodiment, the thickness surplus reserved in step S10 is removed step by step, due to what is used in each step The speed of mainshaft of CNC board is different, and process velocity is also not close identical, can effectively reduce blank front in machining process Residual stress.
3rd embodiment
As shown in figure 3, on the basis of first embodiment and second embodiment, in the nearly processing and forming step in blank front Between S10 and the nearly processing and forming step S20 in the blank back side, the manufacturing method of the metallic mobile phone shell of the present embodiment, further includes: step Rapid S40: the nearly processing and forming step S10 in removal blank front remains on burr and step S50 on blank: cleaning blank is just Clamp tool used in the nearly processing and forming step S10 in face.Removal remains in base to step S40 in time after step S10 completion Burr on material keeps the cleaning of blank, and in step s 50 that the clamp tool used in step slo is cleaned, in case It is used in following step, improves the precision of blank processing.
Fourth embodiment
As shown in figure 4, on the basis of 3rd embodiment, after the net processing and forming step S30 in blank front, the present embodiment Metallic mobile phone shell manufacturing method, further includes: step S60: the removal blank net processing and forming step S30 in front remains on base Burr and step S70 on material: blank is surface-treated, mobile phone manufactured goods are obtained.The step S60 of the present embodiment is gone Except remaining on the burr on blank in step S30 implementation procedure, and step S70 is surface-treated blank, such as sandblasting, throws The processing such as light, finally obtains mobile phone manufactured goods.
5th embodiment
As shown in figure 5, on the basis of first embodiment, before the nearly processing and forming step S10 in blank front, the present embodiment Manufacturing method, further includes: step S80: according to the size of mobile phone manufactured goods, blank is obtained using hardware method for processing forming.Base Material can be the metal materials such as aluminium alloy, according to the size of mobile phone manufactured goods, obtain blank using hardware method for processing forming.
Below with the manufacturing method of a specific embodiment detailed description of the present invention metallic mobile phone shell.
Firstly, the size based on mobile phone manufactured goods in product structure design, using such as punching press of hardware method for processing forming, forging Pressure etc. obtains blank;
Secondly, setting CNC machined parameters, carry out the nearly positive bottom of processing and forming blank for the first time using CNC processing method Wall, on the basis of mobile phone processing procedure product positive setting bottom wall thickness, remaining thickness surplus is the positive bottom wall thickness of blank 0.3mm;
Then, removal CNC processes remaining burr, and cleans CNC and process the clamp tool used;
Then, the bottom wall at the blank back side is processed using CNC machined parameters identical with nearly processing and forming for the first time, So that the bottom wall thickness at the blank back side is the setting bottom wall size at the mobile phone processing procedure product back side;
Furthermore net processing and forming is carried out to blank front using CNC machined parameters identical with nearly processing and forming for the first time, Thickness surplus 0.3 is removed, the positive bottom wall thickness of product is finally processed as setting bottom wall thickness;
The detailed machined parameters of net processing and forming are as follows:
CNC board: tri- axis machine of BROTHER;
Cutter material: carbide cutter tool;
Tool type: face cutter.
First time net processing and forming parameter:
The speed of mainshaft: 8,000 revs/min;
Process velocity: 800MM/ points;
It feeds (bite): 0.15mm.
Second of net processing and forming parameter:
The speed of mainshaft: 10,000 revs/min;
Process velocity: 800MM/ points;
It feeds (bite): 0.10mm.
The net processing and forming parameter of third time:
The speed of mainshaft: 12,000 revs/min;
Process velocity: 600MM/ points;
It feeds (bite): 0.05mm.
Finally, removal remaining burr of the net processing and forming of CNC etc., and surface is carried out to blank under the protection of special fixture Processing, such as polishing, sandblasting and anodic oxidation etc., finally obtain mobile phone manufactured goods.
By the explanation of specific embodiment, the present invention can should be reached technological means that predetermined purpose is taken and Effect is able to more deeply and specifically understand, however appended diagram is only to provide reference and description and is used, and is not used to this Invention limits.

Claims (7)

1. a kind of manufacturing method of metallic mobile phone shell characterized by comprising
The nearly processing and forming step in blank front: the nearly processing and forming of CNC is carried out to the positive bottom wall of blank, so that the blank is positive Bottom wall thickness on the basis of mobile phone processing procedure product positive setting bottom wall thickness, remaining thickness surplus;
The nearly processing and forming step in the blank back side: the nearly processing and forming of CNC is carried out to the bottom wall at the blank back side, so that the blank The bottom wall thickness at the back side is the setting bottom wall size at the mobile phone processing procedure product back side;
The net processing and forming step in blank front: the net processing and forming of CNC is carried out to the positive bottom wall of the blank, removes the thickness Surplus, so that the positive bottom wall thickness of the blank is the setting bottom wall thickness;
The thickness surplus is 0.3mm;
The net processing and forming step in blank front, specifically includes:
The speed of mainshaft that CNC board is arranged is 8000 revs/min, and the process velocity of the net processing and forming of CNC is 800MM/ points, is removed Remove the 0.15mm in the thickness surplus;
The speed of mainshaft that CNC board is arranged is 10000 revs/min, and the process velocity of the net processing and forming of CNC is 800MM/ points, Remove the 0.1mm in the thickness surplus;
The speed of mainshaft that CNC board is arranged is 12000 revs/min, and the process velocity of the net processing and forming of CNC is 600MM/ points, Remove remaining 0.05mm in the thickness surplus.
2. the manufacturing method according to claim 1, which is characterized in that the thickness surplus is 0.3mm~0.6mm.
3. the manufacturing method according to claim 1, which is characterized in that the CNC board is three axis machines, the three axis machine Tool type is face cutter, and the material of the face cutter is hard alloy.
4. manufacturing method according to any one of claim 1 to 3, which is characterized in that close form in blank front adds Between the nearly processing and forming step in the rapid and described blank back side of work step, the manufacturing method, further includes:
Remove the burr that the nearly processing and forming step in the blank front remains on the blank;
Clean clamp tool used in the nearly processing and forming step in the blank front.
5. manufacturing method according to claim 4, which is characterized in that after the net processing and forming step in blank front, The manufacturing method, further includes:
Remove the burr that the net processing and forming step in blank front remains on the blank;
The blank is surface-treated, mobile phone manufactured goods are obtained.
6. manufacturing method according to claim 5, which is characterized in that before the closely processing and forming step of the blank front, The manufacturing method, further includes:
According to the size of the mobile phone manufactured goods, the blank is obtained using hardware method for processing forming.
7. the manufacturing method according to claim 1, which is characterized in that the blank is aluminum alloy material.
CN201610058107.0A 2016-01-28 2016-01-28 A kind of manufacturing method of metallic mobile phone shell Expired - Fee Related CN107009091B (en)