CN106867303A - A kind of coating process of coating paint and its injection blank - Google Patents

A kind of coating process of coating paint and its injection blank Download PDF

Info

Publication number
CN106867303A
CN106867303A CN201710148473.XA CN201710148473A CN106867303A CN 106867303 A CN106867303 A CN 106867303A CN 201710148473 A CN201710148473 A CN 201710148473A CN 106867303 A CN106867303 A CN 106867303A
Authority
CN
China
Prior art keywords
coating
paint
diluent
blank
chew
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710148473.XA
Other languages
Chinese (zh)
Inventor
辛洪萍
胡胜哲
郑龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGZHOU JINZHONG AUTOMOBILE PART MANUFACTURING Co Ltd
Original Assignee
GUANGZHOU JINZHONG AUTOMOBILE PART MANUFACTURING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGZHOU JINZHONG AUTOMOBILE PART MANUFACTURING Co Ltd filed Critical GUANGZHOU JINZHONG AUTOMOBILE PART MANUFACTURING Co Ltd
Priority to CN201710148473.XA priority Critical patent/CN106867303A/en
Publication of CN106867303A publication Critical patent/CN106867303A/en
Pending legal-status Critical Current

Abstract

A kind of coating process for being molded blank, using paint spraying on the surface of blank, the paint includes coating and diluent, coating:Diluent=1:(0.6~1.0);The composition of the diluent includes:Acetone 25 ~ 35%, n-butanol 25 ~ 35%, white spirit 15 ~ 25% and anti-plain boiled water 15 ~ 25%.The present invention makes the paint spraying after dilution in being not in chew after workpiece surface using the diluent of special formulation.

Description

A kind of coating process of coating paint and its injection blank
Technical field
The present invention relates to the field of painting, especially a kind of coating paint and its coating process of injection blank.
Background technology
Because injection blank stress is excessive, with the supporting diluent of coating factory or the priming paint of the dilution dilution agent of process stipulation Or there is chew, chew because the stress line that Stress Release is produced after spraying workpiece surface causes in workpiece during colored paint spraying.Produce The chew influence on product surface has a strong impact on the outward appearance of product, causes production to be smoothed out.
The content of the invention
One of technical problems to be solved by the invention are to provide a kind of coating paint, prevent workpiece from occurring stinging after spray coating Glue phenomenon.
The two of the technical problems to be solved by the invention are to provide a kind of coating paint, prevent workpiece from occurring stinging after spray coating Glue phenomenon.
To solve one of above-mentioned technical problem, the technical scheme is that:A kind of coating paint, including coating and dilution Agent, coating:Diluent=1:(0.6~1.0);The composition of the diluent includes:Acetone 25 ~ 35%, n-butanol 25 ~ 35%, white appliances Oil 15 ~ 25% and anti-plain boiled water 15 ~ 25%.The present invention makes the paint spraying after dilution in workpiece table using the diluent of special formulation It is not in chew behind face.
As improvement, the coating of coating selection Jiangmen four directions Ying Tebao coating Co., Ltd or LKWZ.
To solve the two of above-mentioned technical problem, the technical scheme is that:A kind of coating process for being molded blank, profit With paint spraying on the surface of blank, the paint includes coating and diluent, coating:Diluent=1:(0.6~1.0);Institute The composition for stating diluent includes:Acetone 25 ~ 35%, n-butanol 25 ~ 35%, white spirit 15 ~ 25% and anti-plain boiled water 15 ~ 25%.The present invention Using the diluent of special formulation, make the paint spraying after dilution in being not in chew after workpiece surface.
As improvement, coating selection Jiangmen four directions Ying Tebao coating Co., Ltd and LKWZ(Chinese)Painting Material.
As improvement, in coating process, first in one layer of priming paint of blank workpiece surface spraying, anti-plain boiled water, priming paint are then sprayed again By being released the stress on blank workpiece surface after oven baking.
As improvement, paint is sprayed using spray gun, spray gun oil pump capacity is turned down, air pressure is tuned up.
Used as improvement, the material of the blank is the mixing of ABS or PC and ABS.
The beneficial effect brought compared with prior art of the present invention is:
The present invention makes the paint spraying after dilution in being not in chew after workpiece surface using the diluent of special formulation.
Specific embodiment
Embodiment 1
A kind of coating paint, including coating and diluent, the dilution ratio of paint is coating:Diluent=1:(0.6~1.0)If, Chew is not serious, can use 0.6 ratio, and chew is very serious, takes 1.0 ratio.Coating selection Jiangmen four directions Ying Tebao is applied Material Co., Ltd or the coating of LKWZ.Present invention paint is the moulding of the mixing of ABS or PC and ABS suitable for material.It is described The composition of diluent includes by weight percentage:Acetone 30%, n-butanol 30%, white spirit 20% and anti-plain boiled water 20%.The present invention is adopted With the diluent of special formulation, make the paint spraying after dilution in being not in chew after workpiece surface.
Chew still can not be completely eliminated with the paint spraying of above-mentioned formula, the anti-plain boiled water of one spray can be increased in chew position Operation, specific practice is:In priming paint room, point sprays anti-plain boiled water, and lower operation is flowed out to from primer furnace baking, obtains the stress of workpiece To release, workpiece can be seen and stung one piece " stress line " of appearance by slight.
If above-mentioned operation can't entirely prevent chew, some diluents can be added in paint, then adjusted Spraying method:Spray gun oil pump capacity is turned down, air pressure is tuned up, chew can also effectively be prevented using lancet spraying.
Contain n-butanol in anti-chew paint, can be reacted with curing agent, most 3~4 bottles of agent is reinforced every time, it is ensured that It was finished in 1 hour.
Embodiment 2
A kind of coating paint, including coating and diluent, the dilution ratio of paint is coating:Diluent=1:(0.6~1.0)If, Chew is not serious, can use 0.6 ratio, and chew is very serious, takes 1.0 ratio.Coating selection Jiangmen four directions Ying Tebao is applied Material Co., Ltd or the coating of LKWZ.Present invention paint is the moulding of the mixing of ABS or PC and ABS suitable for material.It is described The composition of diluent includes by weight percentage:Acetone 25%, n-butanol 25%, white spirit 25% and anti-plain boiled water 25%.The present invention is adopted With the diluent of special formulation, make the paint spraying after dilution in being not in chew after workpiece surface.
Chew still can not be completely eliminated with the paint spraying of above-mentioned formula, the anti-plain boiled water of one spray can be increased in chew position Operation, specific practice is:In priming paint room, point sprays anti-plain boiled water, and lower operation is flowed out to from primer furnace baking, obtains the stress of workpiece To release, workpiece can be seen and stung one piece " stress line " of appearance by slight.
If above-mentioned operation can't entirely prevent chew, some diluents can be added in paint, then adjusted Spraying method:Spray gun oil pump capacity is turned down, air pressure is tuned up, chew can also effectively be prevented using lancet spraying.
Contain n-butanol in anti-chew paint, can be reacted with curing agent, most 3~4 bottles of agent is reinforced every time, it is ensured that It was finished in 1 hour.
Embodiment 3
A kind of coating paint, including coating and diluent, the dilution ratio of paint is coating:Diluent=1:(0.6~1.0)If, Chew is not serious, can use 0.6 ratio, and chew is very serious, takes 1.0 ratio.Coating selection Jiangmen four directions Ying Tebao is applied Material Co., Ltd or the coating of LKWZ.Present invention paint is the moulding of the mixing of ABS or PC and ABS suitable for material.It is described The composition of diluent includes by weight percentage:Acetone 35%, n-butanol 35%, white spirit 15% and anti-plain boiled water 15%.The present invention is adopted With the diluent of special formulation, make the paint spraying after dilution in being not in chew after workpiece surface.
Chew still can not be completely eliminated with the paint spraying of above-mentioned formula, the anti-plain boiled water of one spray can be increased in chew position Operation, specific practice is:In priming paint room, point sprays anti-plain boiled water, and lower operation is flowed out to from primer furnace baking, obtains the stress of workpiece To release, workpiece can be seen and stung one piece " stress line " of appearance by slight.
If above-mentioned operation can't entirely prevent chew, some diluents can be added in paint, then adjusted Spraying method:Spray gun oil pump capacity is turned down, air pressure is tuned up, chew can also effectively be prevented using lancet spraying.
Contain n-butanol in anti-chew paint, can be reacted with curing agent, most 3~4 bottles of agent is reinforced every time, it is ensured that It was finished in 1 hour.

Claims (7)

1. a kind of coating paint, it is characterised in that:Including coating and diluent, coating:Diluent=1:(0.6~1.0);It is described dilute The composition for releasing agent includes:Acetone 25 ~ 35%, n-butanol 25 ~ 35%, white spirit 15 ~ 25% and anti-plain boiled water 15 ~ 25%.
2. a kind of coating paint according to claim 1, it is characterised in that:Coating selection Jiangmen four directions Ying Tebao is applied Material Co., Ltd or the coating of LKWZ.
3. it is a kind of be molded blank coating process, it is characterised in that:Using paint spraying on the surface of blank, the paint Including coating and diluent, coating:Diluent=1:(0.6~1.0);The composition of the diluent includes:Acetone 25 ~ 35%, positive fourth Alcohol 25 ~ 35%, white spirit 15 ~ 25% and anti-plain boiled water 15 ~ 25%.
4. it is according to claim 3 it is a kind of be molded blank coating process, it is characterised in that:Described coating selection Jiangmen Cubic Ying Tebao coating Co., Ltd and LKWZ(Chinese)Coating.
5. it is according to claim 3 it is a kind of be molded blank coating process, it is characterised in that:In coating process, first exist One layer of priming paint of blank workpiece surface spraying, then sprays anti-plain boiled water again, and priming paint after oven baking by making blank workpiece surface Stress is released.
6. it is according to claim 3 it is a kind of be molded blank coating process, it is characterised in that:Using spray gun to paint into Row spraying, spray gun oil pump capacity is turned down, and air pressure is tuned up.
7. it is according to claim 3 it is a kind of be molded blank coating process, it is characterised in that:The material of the blank It is the mixing of ABS or PC and ABS.
CN201710148473.XA 2017-03-14 2017-03-14 A kind of coating process of coating paint and its injection blank Pending CN106867303A (en)