CN106785117A - A kind of electric motor car lead-acid battery method for supplementing water - Google Patents

A kind of electric motor car lead-acid battery method for supplementing water Download PDF

Info

Publication number
CN106785117A
CN106785117A CN201611205735.3A CN201611205735A CN106785117A CN 106785117 A CN106785117 A CN 106785117A CN 201611205735 A CN201611205735 A CN 201611205735A CN 106785117 A CN106785117 A CN 106785117A
Authority
CN
China
Prior art keywords
electrolyte
lead
acid
steam vent
electric motor
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201611205735.3A
Other languages
Chinese (zh)
Other versions
CN106785117B (en
Inventor
邓衍虎
杨丛利
邓威
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Guowei Electric Vehicle Manufacturing Co Ltd
Original Assignee
Anhui Guowei Electric Vehicle Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Guowei Electric Vehicle Manufacturing Co Ltd filed Critical Anhui Guowei Electric Vehicle Manufacturing Co Ltd
Priority to CN201611205735.3A priority Critical patent/CN106785117B/en
Publication of CN106785117A publication Critical patent/CN106785117A/en
Application granted granted Critical
Publication of CN106785117B publication Critical patent/CN106785117B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of electric motor car lead-acid battery method for supplementing water, is related to battery recovery technique field, comprises the following steps successively, preparation, with distilled water and bright sulfur acid configuration electrolyte and activating agent, the allocation ratio of electrolyte is that 500ML distilled water adds the acid of 0.3ML bright sulfurs, and activating agent is 10~12ML;The cover plate above lead-acid accumulator is pried open along steam vent, when noting prying open cover plate, cover plate should not be damaged;Rubber cap is opened, debris are clearly filled;The electrolyte that configure is drawn with dropper and slowly uniformly instilled from steam vent, until electrolyte covers the position of 2~4mm on pole plate;The steam vent of the lead-acid accumulator for having filled electrolyte is blocked business covering with ventilative, is fallen as in steam vent with dust protection, after standing 24 hours, suction out the electrolyte of Nei Geli, after cover rubber cap;Discharge and recharge reparation is carried out using obturator.Moisturizing effect of the present invention is good, and speed is fast, is easy to operation, and the efficiency of battery recovery is high.

Description

A kind of electric motor car lead-acid battery method for supplementing water
Technical field:
The present invention relates to battery recovery technique field, specifically a kind of electric motor car lead-acid battery method for supplementing water.
Background technology:
Lead-acid battery phase after charging, electrolytic effect can be produced, evaporate the moist part in electrolyte.Battery is through long After time discharge and recharge use, moisture can evaporate more, raise concentration of electrolyte, and liquid level declines.And in the mistake of long-term use There is this sulfation in journey, cause sulfuric acid also to tail off, at this moment require supplementation with distilled water and electrolyte, make build-up of fluid original Highly, electrolyte maintains normal concentration, to ensure lead-acid accumulator service life.Here it is the effect of lead-acid battery moisturizing.It is existing Have in technology, moisturizing and electrolyte in battery reparation are all carried out separately, moisturizing again after supplement electrolyte, step is more It is cumbersome, electric motor car lead-acid battery method for supplementing water.
The content of the invention:
The technical problems to be solved by the invention are that a kind of moisturizing effect of offer is good, and speed is fast, is easy to the electronic of operation Car lead-acid battery method for supplementing water.
The technical problems to be solved by the invention are realized using following technical scheme.
A kind of electric motor car lead-acid battery method for supplementing water, it is characterised in that:Comprise the following steps successively,
1) preparation, with distilled water and bright sulfur acid configuration electrolyte and activating agent, the allocation ratio of electrolyte is 500ML Distilled water adds the acid of 0.3ML bright sulfurs, and activating agent is 10~12ML;
2) cover plate above lead-acid accumulator is pried open along steam vent, when noting prying open cover plate, cover plate should not be damaged, At this moment it can be seen that 6 rubber caps of air bleeding valve;
3) rubber cap is opened, exposes steam vent, clearly fill debris;
4) draw the electrolyte that configure with dropper and slowly uniformly instilled from steam vent, until electrolyte is covered on pole plate The position of 2~4mm;
5) steam vent of the lead-acid accumulator for having filled electrolyte is blocked business covering with ventilative, is fallen such as exhaust with dust protection In hole, stand 24 hours after, suction out Nei Geli electrolyte, after cover rubber cap;
6) discharge and recharge reparation is carried out using obturator.
To there is two lead-acid accumulators of red line, electrolyte must not exceed red line above, and electrolyte can be from lead when expiring very much Overflowed in the aperture of acid accumulator cover.
If plus there is thing to fall into accidentally during electrolyte, must not be gone to drag for metal, clamp impurity using wooden stick.
The ozone dosage 1-2mg/L that described ozone sterilization is, the duration is 5~10 minutes, and temperature is 15~25 Between DEG C.
Described activating agent includes following components, 10~12 parts of diammonium hydrogen phosphate, 6~8 parts of potassium peroxydisulfate, Jiao by weight 100~200 parts of 2~4 parts of sodium phosphate, 4~6 parts of sodium thiosulfate, 0.2~1 part of zinc sulfate and distilled water.
The electrolyte that the present invention is prepared can cause plus distilled water and electrolyte can be with one along with the effect of activating agent Secondary property is completed, it is only necessary to add this electrolyte of the invention and activating agent, more convenient operation, speed faster, and battery Efficiency after recovery more preferably, can reach the 75% of at least original battery efficiency.
The present invention is the use of special battery repairing activity agent, can greatly improve the efficiency of battery recovery.
The beneficial effects of the invention are as follows:Moisturizing effect of the present invention is good, and speed is fast, is easy to operation, and the efficiency of battery recovery is high.
Specific embodiment:
In order that technological means, creation characteristic, reached purpose and effect that the present invention is realized are easy to understand, tie below Specific embodiment is closed, the present invention is expanded on further.
A kind of electric motor car lead-acid battery method for supplementing water, comprises the following steps successively,
1) preparation, with distilled water and bright sulfur acid configuration electrolyte and activating agent, the allocation ratio of electrolyte is 500ML Distilled water adds the acid of 0.3ML bright sulfurs, and activating agent is 10~12ML;
2) cover plate above lead-acid accumulator is pried open along steam vent, when noting prying open cover plate, cover plate should not be damaged, At this moment it can be seen that 6 rubber caps of air bleeding valve;
3) rubber cap is opened, exposes steam vent, clearly fill debris;
4) draw the electrolyte that configure with dropper and slowly uniformly instilled from steam vent, until electrolyte is covered on pole plate The position of 2~4mm;
5) steam vent of the lead-acid accumulator for having filled electrolyte is blocked business covering with ventilative, is fallen such as exhaust with dust protection In hole, stand 24 hours after, suction out Nei Geli electrolyte, after cover rubber cap;
6) discharge and recharge reparation is carried out using obturator.
To there is two lead-acid accumulators of red line, electrolyte must not exceed red line above, and electrolyte can be from lead when expiring very much Overflowed in the aperture of acid accumulator cover.
If plus there is thing to fall into accidentally during electrolyte, must not be gone to drag for metal, clamp impurity using wooden stick.
The ozone dosage 1-2mg/L that ozone sterilization is, the duration is 5~10 minutes, and temperature is between 15~25 DEG C.
Activating agent includes following components, 10~12 parts of diammonium hydrogen phosphate, 6~8 parts of potassium peroxydisulfate, sodium pyrophosphate by weight 100~200 parts of 2~4 parts, 4~6 parts of sodium thiosulfate, 0.2~1 part of zinc sulfate and distilled water.
General principle of the invention and principal character and advantages of the present invention has been shown and described above.The technology of the industry Personnel it should be appreciated that the present invention is not limited to the above embodiments, simply explanation described in above-described embodiment and specification this The principle of invention, without departing from the spirit and scope of the present invention, various changes and modifications of the present invention are possible, these changes Change and improvement all fall within the protetion scope of the claimed invention.The claimed scope of the invention by appending claims and its Equivalent thereof.

Claims (5)

1. a kind of electric motor car lead-acid battery method for supplementing water, it is characterised in that:Comprise the following steps successively,
1) preparation, with distilled water and bright sulfur acid configuration electrolyte and activating agent, the allocation ratio of electrolyte is 500ML distillations Water adds the acid of 0.3ML bright sulfurs, and activating agent is 10~12ML;
2) cover plate above lead-acid accumulator is pried open along steam vent, when noting prying open cover plate, cover plate should not be damaged, at this moment It can be seen that 6 rubber caps of air bleeding valve;
3) rubber cap is opened, exposes steam vent, clearly fill debris;
4) draw the electrolyte that configure with dropper and slowly uniformly instilled from steam vent, until electrolyte cover 2 on pole plate~ The position of 4mm;
5) steam vent of the lead-acid accumulator for having filled electrolyte is blocked business covering with ventilative, is fallen such as steam vent with dust protection It is interior, stand 24 hours after, suction out Nei Geli electrolyte, after cover rubber cap;
6) discharge and recharge reparation is carried out using obturator.
2. a kind of electric motor car lead-acid battery method for supplementing water according to claim 1, it is characterised in that:To there is two red lines Lead-acid accumulator, electrolyte must not exceed red line above, and electrolyte can overflow when expiring very much from the aperture of lead-acid battery lid.
3. a kind of electric motor car lead-acid battery method for supplementing water according to claim 1, it is characterised in that:If plus having during electrolyte Thing is fallen into accidentally, must not be gone to drag for metal, and impurity is clamped using wooden stick.
4. a kind of electric motor car lead-acid battery method for supplementing water according to claim 1, it is characterised in that:Described ozone sterilization The ozone dosage 1-2mg/L for being, the duration is 5~10 minutes, and temperature is between 15~25 DEG C.
5. a kind of electric motor car lead-acid battery method for supplementing water according to claim 1, it is characterised in that:Described activating agent is pressed Weight portion includes following components, 10~12 parts of diammonium hydrogen phosphate, 6~8 parts of potassium peroxydisulfate, 2~4 parts of sodium pyrophosphate, thiosulfuric acid 100~200 parts of 4~6 parts of sodium, 0.2~1 part of zinc sulfate and distilled water.
CN201611205735.3A 2016-12-23 2016-12-23 A kind of electric vehicle lead-acid battery method for supplementing water Expired - Fee Related CN106785117B (en)