CN106760346A - A kind of metal lagging and production method - Google Patents
A kind of metal lagging and production method Download PDFInfo
- Publication number
- CN106760346A CN106760346A CN201710094889.8A CN201710094889A CN106760346A CN 106760346 A CN106760346 A CN 106760346A CN 201710094889 A CN201710094889 A CN 201710094889A CN 106760346 A CN106760346 A CN 106760346A
- Authority
- CN
- China
- Prior art keywords
- metal
- metallic plate
- side wall
- bending
- edge
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Include panel and side wall the invention discloses a kind of metal lagging and production method, the side wall is formed from the edge of metallic plate to the same side bending, a bending corner structure is configured between adjacent wall, the bending corner structure is formed by side wall crease extended line and metallic plate edge surround part to metal lagging internal bend.Pre-processed by metallic plate, bending side wall, treatment bending corner structure, smooth edge and later stage are processed and obtain metal finishing board finished product.The metal lagging produced using the method has more excellent decay resistance.
Description
Technical field
The present invention relates to building material field, particularly a kind of metal lagging and production method.
Background technology
At present, metal lagging is widely used in the decoration of exterior wall field of building.Metal lagging is simple and light,
Picture on surface can be customized as needed, while top layer good corrosion resistance.
Existing metal lagging needs punching press to fall each corner in process of production, is made with the bending of the rear wall for facilitating
Industry, but punch-out edge is not coated with surface corrosion-resistant erosion resisting coating and be partially exposed at outward, easily it is subject in use
Corrosion, influences the using effect and bulk strength of bulk metal decorative panel.
Because in consideration of it, special propose this invention.
The content of the invention
It is an object of the invention to provide a kind of metal lagging and production method, metal lagging can be effectively avoided
Corrosion of the edge portions caused by punching press.
To achieve these goals, a kind of metal lagging that the present invention is provided, including panel and side wall, its feature exist
In:The side wall is formed from the edge of metallic plate to the same side bending, and a bending corner structure is configured between adjacent wall, described
Bending corner structure is formed by side wall crease extended line and metallic plate edge surround part to metal lagging internal bend.
Preferably, the side of the metallic plate scribbles corrosion-resistant finishes, and side wall bends to the side without corrosion-resistant finishes.
Preferably, the metallic plate edge surrounds part and is rushed from metallic plate edge with the side wall crease extended line
Fall a part, form breach.
Preferably, the edge of the breach is arc or linear pattern.
Preferably, the side wall crease extended line surrounds part and is configured with metallic plate edge with the metallic plate edge
Wedge-like opening, the bending corner structure is first to be bent inwards again fill the part that surrounds to metal from wedge-like opening two side portions
Plaque internal bend is formed.
Preferably, the bending corner structure fits in the inside sidewalls through bending.
Preferably, it is provided with a thermal insulation packing layer in the metal lagging.
Preferably, the thermal insulation packing layer is rock wool heat-preservation packed layer or polyphenylene granule heat-insulating packed layer.
Preferably, the side of the metal lagging is provided with the hole for installation connecting element.
A kind of production method of metal lagging, follows the steps below successively:
(1) corrosion-resistant finishes is sprayed on a metal plate;
(2) side wall is bent, side wall crease extended line and metallic plate edge part is surrounded into curved to metal finishing intralamellar part
Folding, forms bending corner structure;
(3) flat metal plates edge.
A kind of metal lagging and production method that the present invention is provided, the method bend in metallic plate the corner of metallic plate
Inner side, so, it is to avoid the edge of metallic plate is exposed to outside, and then avoids the metal caused by four angles of metallic plate are fallen in punching press
Decorative panel edge does not have the problem that corrosion-resistant protective layer easily corrodes.
Brief description of the drawings
Fig. 1 is metal finishing plate structure schematic diagram provided by the present invention.
Fig. 2 is metal finishing plate producing process flow chart provided by the present invention.
Fig. 3 is folding line and bending method schematic diagram in embodiment one.
Fig. 4 is bending angle structural representation in embodiment one.
Fig. 5 is folding line schematic diagram in embodiment two.
Fig. 6 is folding line schematic diagram in embodiment three.
Fig. 7 is folding line schematic diagram in example IV.
Fig. 8 is folding line schematic diagram in embodiment five.
Fig. 9 is folding line schematic diagram in embodiment six.
Figure 10 is bending angle structural representation in embodiment six.
Figure 11 is folding line schematic diagram in embodiment seven.
In figure:
1. 2. side wall of panel 3. bends the connector mounting hole of corner structure 4.
Specific embodiment
In order that those skilled in the art more fully understand the present invention program, with reference to the accompanying drawings and detailed description
The present invention is described in further detail.
Embodiment one
Refer to Fig. 1-4, it is the sheet material of 0.2-2mm that metal lagging uses thickness, material include but is not limited to PCM plates,
Stainless steel plate and precoating plate.The overall processing flow of metal lagging includes metallic plate pretreatment, bending side wall, treatment bending
The steps such as corner structure, smooth edge and later stage treatment.
In the preprocessing process of metallic plate, by corrosion-resistant finishes on the side even spread of metallic plate, then according to institute
The width of the decorative panel side wall 2 for needing is bent, and the direction that side wall 2 bends is not coated with being furnished with the one of corrosion-resistant finishes for metallic plate
Side.The folding line area defined of side wall 2 is panel 1.
In the step of bending side wall, the folding line extended line of side wall 2 is surrounded with the edge of metallic plate in the corner of metallic plate
Region bends inwards (as shown in Figure 3), forms bending corner structure 3 as shown in Figure 4.The concrete mode for bending inwards is not constituted
Limitation of the invention, as long as ensureing to fold into the edge of metallic plate to metallic plate inner side.It is described in the middle of the present embodiment
Bending is that the diagonal for surrounding region along corner is bent inwards, and two isosceles three can be formed so during bending
Angled face, two isosceles triangle faces are gradually gathered, and the degree gathered is determined according to the decoration plate shape of final needs, for example,
In certain embodiments, if to form box-like decorative panel, the degree of the inside lateral bending folding in corner can cause folding corner region
Inner side folding line forms the rib of decorative panel.
Bending corner structure is processed afterwards, bending corner structure 3 is repaired, or bending is attached at the inner side of inwall 2,
Or angle portion total flattened and is attached between adjacent wall 2 is extruded with external force.
Behind the edge of flat metal plates, one can be entered according to the practical service environment of metal lagging and use demand
Step carries out the processing in later stage, and these processing include:
As needed, thermal insulation packing layer can be filled in metal finishing intralamellar part, thermal insulation packing layer can be rock wool heat-preservation
Packed layer or polyphenylene granule heat-insulating packed layer.
As needed, several connector mounting holes 4 can be on the side wall 2 constructed, such as corner brace is installed in order to after
Deng connector.The shape of mounting hole 4 can have various, and circular hole form is used in the present embodiment.
As needed, can be printed on panel 1 and draw out decorative pattern and pattern, such as wood grain, marble grain, to reach more
Good decorative effect.
Embodiment two
Fig. 5 is refer to, the corner of metallic plate has been fallen in metallic plate stamped arcuately line punching press before bending, remaining is with implementation
Example one.Behind the corner for having fallen metallic plate along arc line shaped punching press, an arc notch is formd, so when inside lateral bending is rolled over,
Because the area of folding corner region is smaller, therefore it is easier when being exerted a force to inner side, is conducive to bending the formation of corner structure.
Embodiment three
Fig. 6 is refer to, the corner of metallic plate has been fallen in metallic plate stamped punching press before bending, and remaining is with embodiment one.This
Edge is left in embodiment, after punching press for linear breach, in the present embodiment, the folding corner region for washing out accounts for whole corner
The ratio in region is less than 50%.
Example IV
Fig. 7 is refer to, the corner of metallic plate has been fallen in metallic plate stamped punching press before bending, and remaining is with embodiment one.This
Edge is left in embodiment, after punching press for linear breach, in the present embodiment, the folding corner region for washing out accounts for whole corner
The ratio in region is equal to 50%.
Embodiment five
Fig. 8 is refer to, the corner of metallic plate has been fallen in metallic plate stamped punching press before bending, and remaining is with embodiment one.This
Edge is left in embodiment, after punching press for linear breach, in the present embodiment, the folding corner region for washing out accounts for whole corner
The ratio in region is more than 50%.
Processing mode used by the present embodiment can leave one section of flash without corrosion-resistant finishes in side edge along place, but due to
The fillers such as marine glue can be filled during installation between metal lagging, while flash position presses close to wall and is not exposed to table
Face, therefore flash has no effect on the overall decay resistance of metal lagging.
Embodiment six
Refer to Fig. 9-10, it is the sheet material of 0.2-2mm that metal lagging uses thickness, material include but is not limited to PCM plates,
Stainless steel plate and precoating plate.
By corrosion-resistant finishes on the side even spread of metallic plate, wedge-shaped indentation (such as Fig. 9 is stamped out in the corner of metallic plate
It is shown), then the width of the decorative panel side wall 2 according to needed for is bent, and the direction that side wall 2 bends is not coated with being furnished with for metallic plate
The side of corrosion-resistant finishes.The folding line area defined of side wall 2 is panel 1.
After the part of wedge-like opening both sides is first bent inwards once, then by the side of the folding line extended line of side wall 2 and metallic plate
Bent inwards along region is surrounded in the corner of metallic plate, form bending corner structure 3 as shown in Figure 10.Forming wedge-like opening simultaneously
After the inside side of the two side portions of opening is bent to form into folding line, then when folding corner region is bent inwards, wedge-like opening can be in external force
In the presence of be gradually separated from each other along folding line, metallic plate body is because of resistance when being rolled over this reduces the inside lateral bending of folding corner region
Deform the resistance for producing, bending corner structure is more prone to shaping.
Bending corner structure 3 is repaired afterwards, or bending is attached at the inner side of inwall 2, or extruded and will entirely be tied with external force
Structure flattens the angle portion being attached between adjacent wall 2.
As needed, thermal insulation packing layer can be filled in metal finishing intralamellar part, thermal insulation packing layer can be rock wool heat-preservation
Packed layer or polyphenylene granule heat-insulating packed layer.
As needed, several connector mounting holes 4 can be on the side wall 2 constructed, the installation connecting element in order to after
Such as corner brace.
As needed, can be printed on panel 1 and draw out decorative pattern and pattern, such as wood grain, marble grain, to reach more
Good decorative effect.
Embodiment seven
Figure 11 is refer to, metallic plate is right angled triangle metallic plate, and two angles have been fallen in stamped punching press before bending, remaining
With embodiment 1.
A kind of metal lagging provided by the present invention and production method are described in detail above.It is used herein
Specific case is set forth to principle of the invention and implementation method, and the explanation of above example is only intended to help and understands
Core concept of the invention.It should be pointed out that for those skilled in the art, not departing from the principle of the invention
On the premise of, some improvement and modification can also be carried out to the present invention, these are improved and modification also falls into the claims in the present invention
Protection domain in.
Claims (10)
1. a kind of metal lagging, including panel and side wall, it is characterised in that:The side wall is the edge from metallic plate to same
Lateral bending folding is formed, and a bending corner structure is configured between adjacent wall, and the bending corner structure is side wall crease extended line and metal
Edges of boards edge surrounds part and is formed to metal lagging internal bend.
2. metal lagging according to claim 1, it is characterised in that:The side of the metallic plate scribbles corrosion-resistant painting
Layer, side wall bends to the side without corrosion-resistant finishes.
3. metal lagging according to claim 1, it is characterised in that prolong with the side wall crease at the metallic plate edge
Line long surrounds part and a part is washed out from metallic plate edge to form breach.
4. metal lagging according to claim 3, it is characterised in that the edge of the breach is arc or linear pattern.
5. metal lagging according to claim 1, it is characterised in that:The side wall crease extended line and the metallic plate
Edge surrounds part and is configured with wedge-like opening at metallic plate edge, and the bending corner structure is by wedge-like opening two side portions elder generation
Bend inwards the part that surrounds is formed to metal lagging internal bend again.
6. according to any described metal laggings of claim 1-5, it is characterised in that:The bending corner structure is fitted through bending
In the inside sidewalls.
7. according to any described metal laggings of claim 1-5, it is characterised in that:A guarantor is provided with the metal lagging
Warm packed layer.
8. metal lagging according to claim 7, it is characterised in that:The thermal insulation packing layer is rock wool heat-preservation packed layer
Or polyphenylene granule heat-insulating packed layer.
9. according to any described metal laggings of claim 1-5, it is characterised in that:Set on the side of the metal lagging
There is the hole for installation connecting element.
10. a kind of production method of metal lagging, it is characterised in that follow the steps below successively:
(1) corrosion-resistant finishes is sprayed on a metal plate;
(2) side wall is bent, side wall crease extended line and metallic plate edge is surrounded into part to metal lagging internal bend, shape
Into bending corner structure;
(3) flat metal plates edge.