CN106707585B - A kind of method of panel defective products heavy industry - Google Patents
A kind of method of panel defective products heavy industry Download PDFInfo
- Publication number
- CN106707585B CN106707585B CN201611258430.9A CN201611258430A CN106707585B CN 106707585 B CN106707585 B CN 106707585B CN 201611258430 A CN201611258430 A CN 201611258430A CN 106707585 B CN106707585 B CN 106707585B
- Authority
- CN
- China
- Prior art keywords
- assembly
- environment
- display panel
- panel
- touch panel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The present invention provides a kind of method of panel defective products heavy industry, comprising: separates the touch panel of the panel defective products and the display panel;By the touch panel be stained with glue and the display panel be stained with glue while be labelled on an intermediary layer respectively, be not connected between the touch panel and the display panel, to form an assembly;The assembly is placed in temperature to be lower than in the environment of predetermined value with cold treatment;The assembly is taken out from the environment after the predetermined time, and the touch panel and the display panel are separated with the intermediary layer respectively.By the above-mentioned means, the present invention can greatly improve the yield of heavy industry, be conducive to cost reduction.
Description
Technical field
The present invention relates to panel attachment mounting technology fields, more particularly to a kind of method of panel defective products heavy industry.
Background technique
With the continuous development of technology, the display screen with touch function has been widely used in life, so that touch-control
The demand of display screen sharply rises, or even the case where drug on the market occurs, and many manufacturers is caused to be in loss of capital operation, because
This, the control of cost becomes the important determinant that can enterprise survive in severe market environment.
However, inevitably will appear by the component that glue bonds bad in the production process of touch display screen
Product, for example, the touch panel (TP, Touch Panel) and display panel that are bonded entirely by glue, the yield of fitting are about
93%, that is, there is about 7% defective products to need rework and (do over again).Existing rework method is usually that will be bonded undesirable touch surface
Plate and display panel separation, after the two separation, glue is easy the random distribution on the surface of touch panel and display panel, will
Display or touch action can be impacted, therefore remaining glue need to be cleaned out again to touch panel and display panel weight
New fitting.
In the prior art, the glue on touch panel and display panel is usually directly struck off using tool, it is then such
Mode is easy to cause touch panel and display panel to scratch even fragmentation, and panel is caused to scrap, so that production cost is soaring, heavy industry
Yield is lower.
Summary of the invention
The purpose of the present invention is to provide a kind of methods of panel defective products heavy industry, can reduce the damage for needing heavy industry panel
Rate improves heavy industry yield, is conducive to cost reduction.
The embodiment of the present invention provides a kind of method of panel defective products heavy industry, wherein the panel defective products includes passing through water
The touch panel and display panel that glue is bonded to each other, the described method includes:
The touch panel of the panel defective products and the display panel are separated;
By the touch panel be stained with glue and the display panel be stained with glue while be labelled in one respectively
It on interlayer, is not connected between the touch panel and the display panel, to form an assembly;
The assembly is placed in temperature to be lower than in the environment of predetermined value with cold treatment;
The assembly is taken out from the environment after the predetermined time, and by the touch panel and the display
Panel is separated with the intermediary layer respectively.
In the method for heavy industry of the present invention, it is described by the assembly be placed in temperature lower than predetermined value environment in
The step of cold treatment includes: that the assembly is placed in temperature to be lower than in subzero 50 ° of environment with cold treatment.
It is described that the assembly is placed in temperature lower than in subzero 50 ° of environment in the method for heavy industry of the present invention
It include: that the assembly is placed in temperature to be lower than in subzero 50 ° of refrigerator with cold treatment with the step of cold treatment.
It is described that the assembly is placed in temperature lower than in subzero 50 ° of environment in the method for heavy industry of the present invention
With the step of cold treatment include: by the assembly sealed package and immerse temperature lower than in subzero 50 ° of liquid with cold treatment.
It is described that the assembly is placed in temperature lower than in subzero 50 ° of environment in the method for heavy industry of the present invention
It include: that the assembly is placed in temperature is in subzero 50 °~subzero 60 ° of environment with the step of cold treatment.
It is described to take out combined body from the environment after the predetermined time in the method for heavy industry of the present invention
The step of include: to take out the assembly from the environment after 0.5 hour to 2.5 hours.
In the method for heavy industry of the present invention, it is described after 0.5 hour to 2.5 hours by the assembly from described
The step of taking out in environment includes: after 1 hour to take out the assembly from the environment.
In the method for heavy industry of the present invention, by the touch panel and the display panel respectively with the intermediary
The step of after layer separation includes: to remove remaining glue on the touch panel and the display panel using adhesive remover.
In the method for heavy industry of the present invention, the touch panel and the display surface are removed using adhesive remover described
The step of on plate after remaining glue includes: to stick protection on the surface of the touch panel and the display panel respectively
Film.
In the method for heavy industry of the present invention, the intermediary layer is tempered glass.
Compared to the method for existing heavy industry, the method for heavy industry of the present invention is by being stained with water for touch panel and display panel
The one side of glue is labelled on the different surfaces of an intermediary layer respectively to form assembly, and assembly is placed in temperature lower than predetermined value
Cold treatment is carried out in environment, with using glue in low temperature environment adhesion strength die down even disappear characteristic and make touch surface
Glue on plate and display panel is detached from and is transferred on intermediary layer, without striking off to touch panel and display panel
Processing, reduces the damage ratio of touch panel and display panel, can be improved heavy industry yield, advantageously reduce production cost.
For above content of the invention can be clearer and more comprehensible, preferred embodiment is cited below particularly, and cooperate institute's accompanying drawings, makees
Detailed description are as follows:
Detailed description of the invention
Fig. 1 is the flow chart of one embodiment of method of heavy industry after the present invention is bonded;
Fig. 2 is after present invention fitting in one embodiment of method of heavy industry, touch panel and display panel respectively with intermediary
Schematic diagram after layer fitting;
Fig. 3 is after present invention fitting in one embodiment of method of heavy industry, touch panel and display panel respectively with intermediary
Schematic diagram after layer separation.
Specific embodiment
The explanation of following embodiment is to can be used to the particular implementation of implementation to illustrate the present invention with reference to additional schema
Example.The direction term that the present invention is previously mentioned, such as "upper", "lower", "front", "rear", "left", "right", "inner", "outside", " side "
Deng being only the direction with reference to annexed drawings.Therefore, the direction term used be to illustrate and understand the present invention, rather than to
The limitation present invention.
The similar unit of structure is to be given the same reference numerals in the figure.
Refering to fig. 1, in one embodiment of rework method of full fitting rear panel defective products heavy industry of the invention, panel is bad
Product include the touch panel and display panel being bonded to each other by glue, and described method includes following steps:
Step S101: the touch panel of panel defective products and display panel are separated.
Wherein, display panel can be liquid crystal display panel, be also possible to OLED display panel or other display panels.
Glue can be OCA optical cement (Optically Clear Adhesive), be also possible to LOCA optical cement (Liquid
Optical Clear Adhesive)。
Step S102: by touch panel be stained with glue and display panel be stained with glue while be labelled in one respectively
It on interlayer, is not connected between touch panel and display panel, to form an assembly.
Wherein, intermediary layer is tempered glass.It is one embodiment of method of heavy industry after present invention fitting in conjunction with Fig. 2, Fig. 2
In, touch panel and display panel be bonded respectively with intermediary layer after schematic diagram.In the present embodiment, touch panel 11 is stained with
Glue 111 is labelled on one side on the first surface of intermediary layer 13, and what display panel 12 was stained with glue 121 is labelled to intermediary layer 13 on one side
The second surface opposite with first surface on, to form assembly 10.
Certainly, in other embodiments, when the area of intermediary layer is sufficiently large, touch panel 11 and display panel 12 are viscous
The one side of some glues can be labelled on the same surface of intermediary layer.In addition, intermediary layer for example can also be plastic material or
Ceramic material is formed.
Step S103: assembly is placed in temperature and is lower than in the environment of predetermined value with cold treatment.
Wherein, in present embodiment, the predetermined value is subzero 50 °, i.e., assembly is placed in temperature and is lower than subzero 50 °
In environment.Further, the temperature of the environment can be subzero 50 °~subzero 60 ° of range, for example, can be subzero 51 °,
Subzero 55 ° or subzero 58 ° etc..In addition, the predetermined value for example can also be subzero 40 or other lower temperature values °, it is described
The temperature of environment can also be subzero 45 ° or subzero 48 ° etc., not limit this, as long as the adhesion strength of glue can be made more micro-
It is weak and glue is detached from from touch panel, display panel.
Assembly is wherein placed in temperature to specifically include lower than in the environment of predetermined value with the step of cold treatment: by assembly
Temperature is placed in be lower than in subzero 50 ° of refrigerator with cold treatment.It in other embodiments, can also will be after assembly sealed package
It immerses in liquid of the temperature lower than 50 ° to carry out cold treatment, the liquid for example can be liquid nitrogen.
Step S104: taking out assembly after the predetermined time from the environment, and by touch panel and display surface
Plate is separated with intermediary layer respectively.
Wherein the predetermined time can be 0.5 hour to 2.5 hours range, or can be 1.5 hours to 3.5 small
When range.Specifically, in present embodiment, assembly is taken out from the environment after one hour.Certainly, described
Predetermined time can also be 1.5 hours, 2 hours or 2.5 hours, not limit this.
According to glue characteristic it is found that glue its adhesion strength under low-temperature condition will become very weak or even disappear.This reality
It applies in mode, assembly is placed on a period of time in the environment of lower temperature, thus may make the adhesion strength of glue more micro-
Weak or even disappearance, so that glue may make to be detached from from touch panel and display panel.Therefore, as shown in figure 3, by touch panel
11 and after display panel 12 separates with intermediary layer 13 respectively, the glue 111,121 of disengaging will be transferred on intermediary layer 13, by
This can remove the glue on touch panel and display panel completely, compared with traditional approach, the rework method of present embodiment
The damage to panel can be reduced, the yield done over again is improved, advantageously reduces cost.
Further, after separating touch panel and display panel with intermediary layer respectively the step of includes: to utilize to remove
Jelly removes remaining glue on touch panel and display panel.After the above-mentioned progress cold treatment to assembly, incited somebody to action
The even all of glue of major part on touch panel and display panel is detached from from touch panel and display panel, so that touching
It is a small amount of residue glue of residual without residue glue or only on panel and display panel.When there are a small amount of residue glue, adhesive remover can be cooperated to remove
Remaining a small amount of residue glue is removed, and since residual silkgum content is less, to touch panel and display panel when removing using adhesive remover
Influence is smaller, can substantially reduce the risk of damage of product than existing.
Further, after removing residue glue using adhesive remover, protection is sticked on the surface of touch panel and display panel
Film, to reduce the risk that touch panel and display panel are damaged in the handling process.
In conclusion although the present invention has been disclosed above in the preferred embodiment, but above preferred embodiment is not to limit
The system present invention, those skilled in the art can make various changes and profit without departing from the spirit and scope of the present invention
Decorations, therefore protection scope of the present invention subjects to the scope of the claims.
Claims (10)
1. a kind of method of panel defective products heavy industry, wherein the panel defective products includes the touch surface being bonded to each other by glue
Plate and display panel, the described method includes:
The touch panel of the panel defective products and the display panel are separated;
By the touch panel be stained with glue and the display panel be stained with glue while be labelled to an intermediary layer respectively
On, which is characterized in that the method also includes:
It is not connected between the touch panel and the display panel, to form an assembly;
The assembly is placed in temperature to be lower than in the environment of predetermined value with cold treatment;
The assembly is taken out from the environment after the predetermined time, and by the touch panel and the display panel
It is separated respectively with the intermediary layer.
2. the method according to claim 1, wherein described be placed in temperature lower than predetermined value for the assembly
In environment with the step of cold treatment include: by the assembly be placed in temperature lower than in subzero 50 ° of environment with cold treatment.
3. according to the method described in claim 2, it is characterized in that, described be placed in temperature lower than subzero 50 ° for the assembly
Environment in the step of cold treatment include: by the assembly be placed in temperature lower than in subzero 50 ° of refrigerator with cold treatment.
4. according to the method described in claim 2, it is characterized in that, described be placed in temperature lower than subzero 50 ° for the assembly
Environment in the step of cold treatment include: by the assembly sealed package and to immerse temperature lower than in subzero 50 ° of liquid
With cold treatment.
5. the method according to claim 3 or 4, which is characterized in that described that the assembly is placed in temperature lower than subzero
It with the step of cold treatment include: that the assembly is placed in temperature is in subzero 50 °~subzero 60 ° of environment in 50 ° of environment.
6. the method according to claim 3 or 4, which is characterized in that it is described after the predetermined time by combined body from institute
Stating the step of taking out in environment includes: to take out the assembly from the environment after 0.5 hour to 2.5 hours.
7. according to the method described in claim 6, it is characterized in that, it is described after 0.5 hour to 2.5 hours by the combination
Body from the environment take out the step of include: after 1 hour to take out the assembly from the environment.
8. the method according to claim 1, wherein by the touch panel and the display panel respectively with
The step of after the intermediary layer separation includes: using remaining on the adhesive remover removing touch panel and the display panel
Glue.
9. according to the method described in claim 8, it is characterized in that, removing the touch panel and institute using adhesive remover described
The step of stating on display panel after remaining glue includes: to paste respectively on the surface of the touch panel and the display panel
Upper protective film.
10. the method according to claim 1, wherein the intermediary layer is tempered glass.