CN106673214A - Efficient green low-phosphorus scale and corrosion inhibitor - Google Patents
Efficient green low-phosphorus scale and corrosion inhibitor Download PDFInfo
- Publication number
- CN106673214A CN106673214A CN201510772008.4A CN201510772008A CN106673214A CN 106673214 A CN106673214 A CN 106673214A CN 201510772008 A CN201510772008 A CN 201510772008A CN 106673214 A CN106673214 A CN 106673214A
- Authority
- CN
- China
- Prior art keywords
- acrylic acid
- corrosion inhibitor
- green low
- efficient green
- phosphorus scale
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an efficient green low-phosphorus scale and corrosion inhibitor, and relates to the technical field of chemical water treatment. The efficient green low-phosphorus scale and corrosion inhibitor comprises the following components by weight: 10-25% of polyaspartic acid, 10-25% of polyepoxysuccinic acid, 5-15% of acrylic acid-acrylate-maleic anhydride copolymer, 5-10% of sodium lignosulfonate, 0.5-1.5% of tungstate, 2-8% of zinc chloride, 10-20% of acrylic acid/2-methyl-2-acrylic acid amine propane sulfonic acid polymer and the balance of water. The efficient green low-phosphorus scale and corrosion inhibitor provided by the invention has stable characteristics, easy storage, excellent scale and corrosion inhibition performance, simple post-processing, and environmental friendliness.
Description
Technical field:
The present invention relates to chemical industry water-treatment technology field, and in particular to suitable for superelevation cycles of concentration
A kind of efficient green low-phosphorus antiincrustation corrosion inhibitor.
Background technology:
The quality of cooling circulating water system operation, is directly connected to enterprise security, efficiently produces,
Must give and ensure.Under the premise of guaranteeing that production is normal, water-saving and emission-reducing work only one goes out
Road, that is, scientifically, reasonably adopt treatment technology, by current recirculated water cycles of concentration by
2~3 times carry to 5-7 times.With the raising of cycles of concentration, water quality running quality can be caused
Difficulty, such as produces fouling, corrosion or ooze and deposits new problem.
The content of the invention:
Present invention aims to the defect and deficiency of prior art, there is provided a kind of efficiently green
Color low-phosphorus antiincrustation corrosion inhibitor.
In order to solve the problems of background technology, a kind of recirculating cooling water system of the present invention
Low-phosphorus antiincrustation corrosion inhibitor, its component and weight proportion be:Poly-aspartate:10-25%,
Poly-epoxy succinic acid:10-25%, acrylic acid-acrylic ester-maleic anhydride multipolymer:
5-15%, sodium lignin sulfonate:5-10%, tungstates:0.5-1.5%, zinc chloride:2-8%,
Acrylic acid/2- methyl -2- acrylic acid amido propane sulfonic acids are birdsed of the same feather flock together compound:10-20%, water:Surplus.
The present invention has the beneficial effect that:With stable speciality, easily storage, excellent scale inhibitor
Performance, the later stage processes easy, and environmental sound.
Specific embodiment:
Specific embodiment one:This specific embodiment is adopted the following technical scheme that:Its component
And its weight proportion is:Poly-aspartate:10%th, poly-epoxy succinic acid:15%th, acrylic acid-
Acrylate-maleic anhydride multipolymer:5%th, sodium lignin sulfonate:10%th, tungstates:
0.5%th, zinc chloride:8%th, acrylic acid/2- methyl -2- acrylic acid amido propane sulfonic acids are birdsed of the same feather flock together compound:
10%th, water:41.5%.Preparation method:By sequentially adding under said components accurate weighing normal temperature,
Obtain final product after stirring and dissolving.
Specific embodiment two:This specific embodiment is adopted the following technical scheme that:Its component
And its weight proportion is:Poly-aspartate:15%th, poly-epoxy succinic acid:20%th, acrylic acid-
Acrylate-maleic anhydride multipolymer:10%th, sodium lignin sulfonate:5%th, tungstates:
1.0%th, zinc chloride:3%th, acrylic acid/2- methyl -2- acrylic acid amido propane sulfonic acids are birdsed of the same feather flock together compound:
15%th, water:31%.Preparation method:By sequentially adding under said components accurate weighing normal temperature, stir
Mix and obtained final product after dissolving.
Specific embodiment three:This specific embodiment is adopted the following technical scheme that:Component and its
Weight proportion is:Poly-aspartate:25%th, poly-epoxy succinic acid:25%th, acrylic acid-acrylic
Acid esters-maleic anhydride multipolymer:8%th, sodium lignin sulfonate:8%th, tungstates:1.5%th,
Zinc chloride:5%th, acrylic acid/2- methyl -2- acrylic acid amido propane sulfonic acids are birdsed of the same feather flock together compound:18%th,
Water:9.5%.
The above, only to illustrate technical scheme and unrestricted, this area is common
Other modifications or equivalent that technical staff is made to technical scheme, as long as not
Depart from the spirit and scope of technical solution of the present invention, the claim model in the present invention all should be covered
In the middle of enclosing.
Claims (1)
1. a kind of efficient green low-phosphorus antiincrustation corrosion inhibitor, it is characterised in that:Its component and weight
Measuring proportioning is:Poly-aspartate:10-25%, poly-epoxy succinic acid:10-25%, acrylic acid-
Acrylate-maleic anhydride multipolymer:5-15%, sodium lignin sulfonate:5-10%, tungsten
Hydrochlorate:0.5-1.5%, zinc chloride:2-8%, acrylic acid/2- methyl -2- acrylic acid amido propane
Sulphonic acids polymer:10-20%, water:Surplus.