CN106589995A - Decorative board with pest proof function - Google Patents

Decorative board with pest proof function Download PDF

Info

Publication number
CN106589995A
CN106589995A CN201611003631.4A CN201611003631A CN106589995A CN 106589995 A CN106589995 A CN 106589995A CN 201611003631 A CN201611003631 A CN 201611003631A CN 106589995 A CN106589995 A CN 106589995A
Authority
CN
China
Prior art keywords
parts
decorative board
decorative panel
pressure
stabilizer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201611003631.4A
Other languages
Chinese (zh)
Inventor
史兆武
屈山峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Golden Crown Green Wood Industry Co Ltd
Original Assignee
Anhui Golden Crown Green Wood Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Golden Crown Green Wood Industry Co Ltd filed Critical Anhui Golden Crown Green Wood Industry Co Ltd
Priority to CN201611003631.4A priority Critical patent/CN106589995A/en
Publication of CN106589995A publication Critical patent/CN106589995A/en
Pending legal-status Critical Current

Abstract

The invention belongs to the technical field of wood plastic composite boards, and in particular relates to a decorative board with a pest control function, and the decorative board comprises the following raw materials: a wood plastic stabilizer, polymer of rosin allyl alcohol ester, phosphogypsum, dihydrocumic acid, larch extract, tannin extract, total flavonoids of Lithocarpus polystachyus, bagasse fiber and water. Compared with the prior art, the decorative board has the advantages of good mechanical properties and low imbibition rate and low heat shrinkage rate, the dimensional stability of decorative board can be ensured, the raw materials are well compatible and strong in plasticity, and can be customized according to the need to achieve modeling; the decorative board can effectively prevent pests and termites, and is easy to clean, free of maintenance, highly environmental-friendly and pollution-free, the fire protection grade can reach B1 level, comprehensive performance are superior, and the decorative board is suitable for popularization and use.

Description

A kind of decorative panel with insect prevention function
Technical field
The invention belongs to wood-plastic composite panel technical field, and in particular to a kind of decorative panel with insect prevention function.
Background technology
Wood-plastic composite panel is one kind mainly by timber(Lignose, plant cellulose)Based on material and thermoplasticity it is high Molecular material(Plastics)With processing aid etc., after mix homogeneously again the heating extrusion molding of Jing die apparatus and made by high-tech it is green Colour circle protects new decorative material, has the performance and feature of timber and plastics concurrently, is the NEW TYPE OF COMPOSITE material that can substitute timber and plastics Material, with expanding economy, the improvement of people's living standards, people have higher wanting to the speed and quality of Decoration Industry Ask, wood-plastic composite panel compare common wood loss it is low, be not required to paint or water paint coating process, easy construction, price be adapted to, Long service life, maintenance cost are low, therefore are increasingly liked by masses, in actual use, according to wood-plastic composite panel The differentiation of purposes, needs to strengthen some functions again, as the material in wood-plastic composite panel includes the wooden material in part Material, therefore in some areas it is possible that situation about being eaten into by worm or Coptotermes formosanus Shtrari., it is therefore desirable to research is carried out to corresponding function and is changed Enter.
The content of the invention
The purpose of the present invention is for existing problem, there is provided a kind of decorative panel with insect prevention function.
The present invention is achieved by the following technical solutions:A kind of decorative panel with insect prevention function, by following weight portion Raw material make:Wood moulding stabilizer 3-5 parts, polymer of rosin allyl alcohol ester 5-8 parts, ardealite 6-10 parts, dihydrocumic acid 4-6 parts, Larch extract 8-12 parts, Pasania cuspidata total flavones 5-7 parts, sugarcane fiber 15-22 parts, water 18-22 parts;
Wherein, wood moulding stabilizer is made up of the raw material of following weight portion:Rare-earth stabilizer XT-2 8-10 parts, graphite powder 5-8 parts, Potassium pyrophosphate 3-5 parts, calcium stearate 2-4 parts, the double stearylamine 4-8 parts of vinyl, methyl acetate 7-10 parts, dichloromethane 2-3 parts, BBP(Butyl Benzyl Phthalate 2-3 part, diethylene glycol ether 2-4 parts, oxidized microcrystalline wax 3-4 parts, polyol ester 3-6 parts, tetrahydro-anthraquinone 1-2 parts, tremolite powder 6-8 parts, polyvinyl butyral resin 2-4 parts, amino silicane coupling agent 15-20 parts.
Used as further improvement of these options, the polymer of rosin allyl alcohol ester is obtained using microwave heating polymerization, soft Change point and be not less than 320 DEG C.
Used as further improvement of these options, it is 60-80 μ that the length of the sugarcane fiber is 0.4-1.6mm, width m。
A kind of decorative panel with insect prevention function, its preparation method are comprised the following steps:
(1)Ardealite, sugarcane fiber are ground to form into the powder that particle diameter is 300-400 μm, polymer of rosin allyl alcohol ester, larch is added Tannic extract mix homogeneously, is heated to melting in far-infrared baking oven, is subsequently adding surplus stock, with 200-300 rev/min of speed After stirring 15-20 minutes, slurry is obtained;
(2)Gained slurry is poured in mould, after pulp gel, the finish mix embryo of pressurizing and dehydrating is forced, moulding pressure is 4MPa, After the completion of cooling and demolding;
(3)Compressing product is put in steam-cured template, sending into pressure steaming kettle carries out autoclave curing;Maintenance processes are liter temperature rise Pressed as 6 hours, 140 DEG C are risen to from room temperature, rise to 1.2MPa from normal pressure;Constant temperature and pressure 3 hours, steam pressure is 0.9MPa, permanent 135 DEG C of temperature;Decrease temperature and pressure 6 hours, is down to room temperature from 140 DEG C, is down to normal pressure from 0.9MPa;Maintenance sloughs steam-cured template after terminating As semi-finished product;
(4)Obtain being adapted to the decorative panel of size according to dimensional requirement finishing, it is 10% that drying machine is dried to moisture content, is obtained final product.
The present invention has advantages below compared to existing technology:The present invention prepare decorative panel mechanical property it is good, imbibition rate and Percent thermal shrinkage is low, it is ensured that the dimensional stability of decorative panel, and between raw material, the compatibility is good, and plasticity is strong, can realize as needed Customization moulding;Can effectively insect prevention, termite-proof, easy cleaning, Maintenance free and maintenance, high-environmental, nuisanceless, fire-protection rating can Up to B1 levels, comprehensive performance is superior, is suitable to promote the use of.
Specific embodiment
Embodiment 1
A kind of decorative panel with insect prevention function, is made up of the raw material of following weight portion:3 parts of wood moulding stabilizer, polymerized rosin propylene 8 parts of alcohol ester, 6 parts of ardealite, 4 parts of dihydrocumic acid, 12 parts of larch extract, 5 parts of Pasania cuspidata total flavones, 16 parts of sugarcane fiber, 22 parts of water;
Wherein, wood moulding stabilizer is made up of the raw material of following weight portion:8 parts of rare-earth stabilizer XT-2,5 parts of graphite powder, pyrophosphoric acid 3 parts of potassium, 4 parts of calcium stearate, vinyl double 4 parts of stearylamine, 10 parts of methyl acetate, 2 parts of dichloromethane, BBP(Butyl Benzyl Phthalate 3 parts, 2 parts of diethylene glycol ether, 3 parts of oxidized microcrystalline wax, 6 parts of polyol ester, 1 part of tetrahydro-anthraquinone, 8 parts of tremolite powder, polyvinyl alcohol 2 parts of butyral, 20 parts of amino silicane coupling agent.
Wherein, the polymer of rosin allyl alcohol ester is obtained using microwave heating polymerization, and softening point is not less than 320 DEG C;The sugarcane The length of slag fiber is 0.4-1.6mm, width is 60-80 μm.
A kind of decorative panel with insect prevention function, its preparation method are comprised the following steps:
(1)Ardealite, sugarcane fiber are ground to form into the powder that particle diameter is 300-400 μm, polymer of rosin allyl alcohol ester, larch is added Tannic extract mix homogeneously, is heated to melting in far-infrared baking oven, is subsequently adding surplus stock, is stirred with 250 revs/min of speed After 20 minutes, slurry is obtained;
(2)Gained slurry is poured in mould, after pulp gel, the finish mix embryo of pressurizing and dehydrating is forced, moulding pressure is 4MPa, After the completion of cooling and demolding;
(3)Compressing product is put in steam-cured template, sending into pressure steaming kettle carries out autoclave curing;Maintenance processes are liter temperature rise Pressed as 6 hours, 140 DEG C are risen to from room temperature, rise to 1.2MPa from normal pressure;Constant temperature and pressure 3 hours, steam pressure is 0.9MPa, permanent 135 DEG C of temperature;Decrease temperature and pressure 6 hours, is down to room temperature from 140 DEG C, is down to normal pressure from 0.9MPa;Maintenance sloughs steam-cured template after terminating As semi-finished product;
(4)Obtain being adapted to the decorative panel of size according to dimensional requirement finishing, it is 10% that drying machine is dried to moisture content, is obtained final product.
Embodiment 2
A kind of decorative panel with insect prevention function, is made up of the raw material of following weight portion:4 parts of wood moulding stabilizer, polymerized rosin propylene 6 parts of alcohol ester, 8 parts of ardealite, 5 parts of dihydrocumic acid, 10 parts of larch extract, 5 parts of Pasania cuspidata total flavones, 19 parts of sugarcane fiber, 20 parts of water;
Wherein, wood moulding stabilizer is made up of the raw material of following weight portion:9 parts of rare-earth stabilizer XT-2,6 parts of graphite powder, pyrophosphoric acid 4 parts of potassium, 3 parts of calcium stearate, vinyl double 6 parts of stearylamine, 8 parts of methyl acetate, 2 parts of dichloromethane, BBP(Butyl Benzyl Phthalate 3 Part, the contracting of 3 parts of diethylene glycol ether, 4 parts of oxidized microcrystalline wax, 5 parts of polyol ester, 1 part of tetrahydro-anthraquinone, 7 parts of tremolite powder, polyvinyl alcohol 3 parts of butyraldehyde, 18 parts of amino silicane coupling agent.
Remainder is in the same manner as in Example 1.
Embodiment 3
A kind of decorative panel with insect prevention function, is made up of the raw material of following weight portion:5 parts of wood moulding stabilizer, polymerized rosin propylene 5 parts of alcohol ester, 10 parts of ardealite, 4 parts of dihydrocumic acid, 8 parts of larch extract, 5 parts of Pasania cuspidata total flavones, 15 parts of sugarcane fiber, 22 parts of water;
Wherein, wood moulding stabilizer is made up of the raw material of following weight portion:10 parts of rare-earth stabilizer XT-2,5 parts of graphite powder, burnt phosphorus 3 parts of sour potassium, 4 parts of calcium stearate, vinyl double 8 parts of stearylamine, 10 parts of methyl acetate, 3 parts of dichloromethane, phthalic acid fourth benzyls 2 parts of ester, 2 parts of diethylene glycol ether, 3 parts of oxidized microcrystalline wax, 6 parts of polyol ester, 1 part of tetrahydro-anthraquinone, 8 parts of tremolite powder, polyethylene 2 parts of butyral, 20 parts of amino silicane coupling agent.
Remainder is in the same manner as in Example 1.
In order to verify the using effect of decorative panel in the present invention, matched group is set, matched group is the fire prevention purchased by market Grade is the common PLASTIC LAMINATED of B1, and its performance is detected, as a result as follows:
Table 1
By data in table 1, in matched group, decorative panel rupture strength and impact strength are all close with embodiment, but real Applying bulking factor and percent thermal shrinkage in a 1-3 substantially reduces, and the decorative panel dimensional stability prepared in illustrating the present invention is high.
Coptotermes formosanus Shtrari. experiment is simultaneously set, by embodiment 1-3 and the made decorative panel of matched group cut into length and width specification for 50mm × The bar shaped plank of 20mm, weighs 2 ± 0.2g Coptotermes formosanus Shtrari. respectively and is put in independent experimental provision, in each assay device by each 10 pieces The distilled water of the fine sand and 5g of 200g cleanings is placed into, is raised 5 days at ambient temperature, bar shaped plank is respectively put into into phase then In the assay device answered, check decorative panel to receive moth degree after 24 hours, represented have by moth degree by the integrity value of bar shaped plank Body result is as follows:
Table 2
The mothproof effect that decorative panel in the present invention be can be seen that by data in table 2 is significantly improved, and can extend making for decorative panel Use the time limit.

Claims (4)

1. a kind of decorative panel with insect prevention function, it is characterised in that be made up of the raw material of following weight portion:Wood moulding stabilizer 3- 5 parts, polymer of rosin allyl alcohol ester 5-8 parts, ardealite 6-10 parts, dihydrocumic acid 4-6 parts, larch extract 8-12 parts, Pasania cuspidata Total flavones 5-7 parts, sugarcane fiber 15-22 parts, water 18-22 parts;
Wherein, wood moulding stabilizer is made up of the raw material of following weight portion:Rare-earth stabilizer XT-2 8-10 parts, graphite powder 5-8 parts, Potassium pyrophosphate 3-5 parts, calcium stearate 2-4 parts, the double stearylamine 4-8 parts of vinyl, methyl acetate 7-10 parts, dichloromethane 2-3 parts, BBP(Butyl Benzyl Phthalate 2-3 part, diethylene glycol ether 2-4 parts, oxidized microcrystalline wax 3-4 parts, polyol ester 3-6 parts, tetrahydro-anthraquinone 1-2 parts, tremolite powder 6-8 parts, polyvinyl butyral resin 2-4 parts, amino silicane coupling agent 15-20 parts.
2. as claimed in claim 1 a kind of decorative panel with insect prevention function, it is characterised in that the polymer of rosin allyl alcohol ester is adopted Obtained with microwave heating polymerization, softening point is not less than 320 DEG C.
3. as claimed in claim 1 a kind of decorative panel with insect prevention function, it is characterised in that the length of the sugarcane fiber is 0.4-1.6mm, width are 60-80 μm.
4. as claimed in claim 1 a kind of decorative panel with insect prevention function, it is characterised in that its preparation method includes following step Suddenly:
(1)Ardealite, sugarcane fiber are ground to form into the powder that particle diameter is 300-400 μm, polymer of rosin allyl alcohol ester, larch is added Tannic extract mix homogeneously, is heated to melting in far-infrared baking oven, is subsequently adding surplus stock, with 200-300 rev/min of speed After stirring 15-20 minutes, slurry is obtained;
(2)Gained slurry is poured in mould, after pulp gel, the finish mix embryo of pressurizing and dehydrating is forced, moulding pressure is 4MPa, After the completion of cooling and demolding;
(3)Compressing product is put in steam-cured template, sending into pressure steaming kettle carries out autoclave curing;Maintenance processes are liter temperature rise Pressed as 6 hours, 140 DEG C are risen to from room temperature, rise to 1.2MPa from normal pressure;Constant temperature and pressure 3 hours, steam pressure is 0.9MPa, permanent 135 DEG C of temperature;Decrease temperature and pressure 6 hours, is down to room temperature from 140 DEG C, is down to normal pressure from 0.9MPa;Maintenance sloughs steam-cured template after terminating As semi-finished product;
(4)Obtain being adapted to the decorative panel of size according to dimensional requirement finishing, it is 10% that drying machine is dried to moisture content, is obtained final product.
CN201611003631.4A 2016-11-15 2016-11-15 Decorative board with pest proof function Pending CN106589995A (en)