CN106470013A - 一种检测pid光伏电池片的方法 - Google Patents
一种检测pid光伏电池片的方法 Download PDFInfo
- Publication number
- CN106470013A CN106470013A CN201510519348.6A CN201510519348A CN106470013A CN 106470013 A CN106470013 A CN 106470013A CN 201510519348 A CN201510519348 A CN 201510519348A CN 106470013 A CN106470013 A CN 106470013A
- Authority
- CN
- China
- Prior art keywords
- photovoltaic
- photovoltaic module
- photovoltaic cell
- pid
- cell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (3)