CN106315058A - 抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐 - Google Patents
抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐 Download PDFInfo
- Publication number
- CN106315058A CN106315058A CN201510359076.8A CN201510359076A CN106315058A CN 106315058 A CN106315058 A CN 106315058A CN 201510359076 A CN201510359076 A CN 201510359076A CN 106315058 A CN106315058 A CN 106315058A
- Authority
- CN
- China
- Prior art keywords
- glass
- resistant
- oil tank
- ceramic mud
- glass web
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
目前的石油罐用钢铁做成,工艺复杂,造价贵,虽然进行防腐蚀,但抗酸碱性能还是很差,用不了几年就报废。抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐,由陶瓷粘结耐高温玻璃网布烧制获得;它代替金属,抗酸碱腐蚀,寿命千年,工艺简单,成本低。玻璃网布耐1500度,陶瓷泥烧成陶瓷1250度,烧成陶瓷后不会破坏玻璃网布抗拉性能。石油罐为紧密封闭泡沫板,封闭泡沫受冲击时,泡沫面产生弯曲将冲击力吸收,并将余下冲击力分流给竖壁,多层框架泡沫板将冲击力全部吸收;所以耐碰撞。瓷玻石油罐为冷加工,不用焊接,降低劳动强度。耐高温玻璃网布价格比钢铁低。
Description
目前的石油罐用钢铁做成,工艺复杂,造价贵,虽然进行防腐蚀,但抗酸碱性能还是很差,用不了几年就报废。市场无见用陶瓷粘结玻璃网布做的完全抗酸碱腐蚀的瓷玻石油罐。
本技术提出的抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐,属贮罐领域,简称瓷玻石油罐,能帮助克服上述存在的缺点。
瓷玻石油罐,其有益效果是,代替钢铁,抗酸碱腐蚀,寿命千年,工艺简单,降低成本。
抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐,其解决技术问题所采用的技术方案是,由陶瓷粘结耐高温玻璃网布组成;其工艺是:使耐高温玻璃网布通过陶瓷泥浆,陶瓷泥浆可加入粘合剂,令陶瓷泥浆穿过玻璃网布孔,刮去多余陶瓷泥浆,令陶瓷泥浆包裹玻璃网布,成为陶瓷泥浆玻璃网布;按石油罐各部件要求,如罐身,罐盖等,将多块陶瓷泥浆玻璃网布重叠粘成直或弯曲的陶瓷泥浆玻璃网布板;按石油罐各部件要求,将直的陶瓷泥浆玻璃网布板,开成直的或开成弯曲的陶瓷泥浆玻璃网布板条;按石油罐各部件要求,在直或弯曲的陶瓷泥浆玻璃网布板条(1),等距离开窄缝(2),窄缝宽度等于板条厚度,窄缝长度略大于板条宽度一半;将相对应直或弯曲的陶瓷泥浆玻璃网布板条窄缝对扦,做成石油罐各部件框架(3);在直或弯曲陶瓷泥浆玻璃网布板上,放相对应的框架,在框架上放直或弯曲陶瓷泥浆玻璃网布板粘紧,直或弯曲陶瓷泥浆玻璃网布板、框架可相间重叠粘成,最后用陶瓷泥浆玻璃网布条封边,粘成泡沫板,获得石油罐各部件的泡沫板(4);将开好相关孔位的石油罐各部件泡沫板放入炉烧制,令陶瓷泥浆成为陶瓷;冷却后获得陶瓷粘结耐高温玻璃网布的石油罐各部件;石油罐各部件可再涂上釉浆放入炉烧制;如果罐身体积过大,可将罐身分为几部分;将石油罐各部件安装成瓷玻石油罐(5),从而使抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐得以运行。如图1
现结合原理介绍瓷玻石油罐:
耐高温玻璃网布耐一千五百度,陶瓷泥浆烧成陶瓷一千二百五十度,所以烧成陶瓷后不会破坏耐高温玻璃网布的抗拉等性能。
粘合剂可为淀粉糊,加入粘合剂,能使陶瓷泥浆不脱离玻璃网布。
当瓷玻石油罐受到冲击时,玻璃网布会将冲击力全部吸收,令石油罐完好;石油罐各部件内部为框架,和玻璃网布板构成紧密的封闭泡沫板,封闭泡沫受冲击时,泡沫面产生弯曲,将冲击力吸收,并将余下冲击力分流给竖壁,若有多层框架,就将冲击力全部吸收;陶瓷因很薄而有弹性,冲击力过后,泡沫面恢复平直,所以封闭泡沫板具有良好的耐冲击力性能。
目前的石油罐,是将钢板焊接做成,工艺复杂,造价贵。
陶瓷,玻璃网布抗酸碱腐蚀寿命千年。
瓷玻石油罐为冷加工,不用焊接,降低劳动强度。
耐高温玻璃网布价格比钢铁低。
再涂上釉浆放入炉烧制,能保证石油罐汽密,减少石油汽蒸发。
说明书附图
图1:抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐
1 玻璃网布板条,2 窄缝,3 各部件框架,4 各部件的泡沫板,5 瓷玻石油罐。
Claims (1)
1.抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐,其特征是,由陶瓷粘结耐高温玻璃网布组成;其工艺是:使耐高温玻璃网布通过陶瓷泥浆,陶瓷泥浆可加入粘合剂,令陶瓷泥浆穿过玻璃网布孔,刮去多余陶瓷泥浆,令陶瓷泥浆包裹玻璃网布,成为陶瓷泥浆玻璃网布;按石油罐各部件要求,如罐身,罐盖等,将多块陶瓷泥浆玻璃网布重叠粘成直或弯曲的陶瓷泥浆玻璃网布板;按石油罐各部件要求,将直的陶瓷泥浆玻璃网布板,开成直的或开成弯曲的陶瓷泥浆玻璃网布板条;按石油罐各部件要求,在直或弯曲的陶瓷泥浆玻璃网布板条,等距离开窄缝,窄缝宽度等于板条厚度,窄缝长度略大于板条宽度一半;将相对应直或弯曲的陶瓷泥浆玻璃网布板条窄缝对扦,做成石油罐各部件框架;在直或弯曲陶瓷泥浆玻璃网布板上,放相对应的框架,在框架上放直或弯曲陶瓷泥浆玻璃网布板粘紧,直或弯曲陶瓷泥浆玻璃网布板、框架可相间重叠粘成,最后用陶瓷泥浆玻璃网布条封边,粘成泡沫板,获得石油罐各部件的泡沫板;将开好相关孔位的石油罐各部件泡沫板放入炉烧制,令陶瓷泥浆成为陶瓷;冷却后获得陶瓷粘结耐高温玻璃网布的石油罐各部件;石油罐各部件可再涂上釉浆放入炉烧制;如果罐身体积过大,可将罐身分为几部分;将石油罐各部件安装成瓷玻石油罐,从而使抗酸碱腐蚀耐碰撞寿命千年的泡沫壁瓷玻石油罐得以运行。