CN106309490A - Active physiotherapy ring and preparation method thereof - Google Patents

Active physiotherapy ring and preparation method thereof Download PDF

Info

Publication number
CN106309490A
CN106309490A CN201610920778.3A CN201610920778A CN106309490A CN 106309490 A CN106309490 A CN 106309490A CN 201610920778 A CN201610920778 A CN 201610920778A CN 106309490 A CN106309490 A CN 106309490A
Authority
CN
China
Prior art keywords
ring
energy
energy powder
physical therapy
mesh
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201610920778.3A
Other languages
Chinese (zh)
Inventor
荆玉松
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qingdao Is First Co Ltd
Original Assignee
Qingdao Is First Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qingdao Is First Co Ltd filed Critical Qingdao Is First Co Ltd
Priority to CN201610920778.3A priority Critical patent/CN106309490A/en
Publication of CN106309490A publication Critical patent/CN106309490A/en
Withdrawn legal-status Critical Current

Abstract

The invention provides an active physiotherapy ring and a preparation method thereof, belonging to the field of articles of daily use. The active physiotherapy ring comprises a ring body and is characterized in that the main body of the ring body is made of an elastic material added with 0.5-1.5% of energy powder, wherein a certain amount of auxiliary materials composed of calcium gluconate, stone needles, zinc glutamate and dragon bones are added in the energy powder under the collocation of multiple mineral raw materials. The activity of the energy powder can be better excited, and a coordinated and unified comprehensive energy field can be formed. The preparation method of the physiotherapy ring is characterized in that a special temperature of 520-580 DEG C is kept in the grinding process of the energy powder used in the formula of the elastic material of the main body of the physiotherapy ring, and by virtue of grinding at the temperature, the energy fields of all materials can be ground and mixed in a specific exciting state, thereby showing a stronger field effect in a final physiotherapy ring.

Description

A kind of activity physical therapy ring and preparation method thereof
Technical field
A kind of activity physical therapy ring and preparation method thereof, belongs to consumer goods industries.
Background technology
Currently known many Ores can produce the energy to biological physiological function with certain role and influence , this energy field includes magnetic field, the infrared ray etc. that mineral self send, and its concrete mechanism of action is still not clear.But it is right The actively impact objective reality the most for a certainty of human body.This material can be to the effect of biological physiological function generation effect The present invention is referred to as energy field effect or referred to as field effect.Now with more product utilization this energy field effect system Standby medical health care products.
Bracelet, neck ring are always decoration, the function articles for use that people commonly use, the technique of the elastomeric material used by bracelet, neck ring Require there is the biggest granule in melted polymer, cause using monoblock even to keep the granule of function to have There is the raw material of field effect.And mineral material be crushed to cause the most afterwards field effect relatively overly soft pulse to disappearing, this is because powder Each does what he thinks is right in the magnetic field of the various raw material powders with field effect of last current state, does not form unified energy like that to bulk starting material Amount field, causes interfering, and reduces physiotheraping effect, and the curative effect causing entirety is little.
Summary of the invention
The technical problem to be solved in the present invention is: overcome the deficiencies in the prior art, it is provided that a kind of effect is mutually promoted, field effect Active physical therapy ring that should be stronger and preparation method thereof.
The technical solution adopted for the present invention to solve the technical problems is: this activity physical therapy ring, and including ring body, its feature exists In: the main body of described ring body is to be added with the elastomeric material of the energy powder that mass fraction accounts for 0.5% ~ 1.5%, described energy powder Weight portion consists of: Buddha's warrior attendant YAOSHI 3.4 ~ 3.5 parts, tourmaline 3.0 ~ 4.0 parts, 0.3 ~ 0.42 part of Khotan jade stone, obsidian 2 ~ 2.4 Part, yellow quartz 0.03 ~ 0.07 part, Maifanitum 3 ~ 7 parts and adjuvant;Described adjuvant is calcium gluconate 3.8 ~ 4.1 parts, stone needle 0.3 ~ 0.6 part, zinc glutamate 0.01 ~ 0.015 part, Os Draconis 0.2 ~ 0.3 part.
Physical therapy ring can be with the form being bracelet, it is also possible to be the form of neck ring.
A kind of energy active energy powder is employed, it is possible to adapt to the preparation technology of elastomeric material on the physical therapy ring of the present invention. The energy powder that the present invention adds needs to add the crucial auxiliary material combination of the present invention, the inventors found that described in interpolation The adjuvant of calcium gluconate, stone needle, zinc glutamate, Os Draconis composition, it is possible to preferably retain the activity of each energy powder, make energy powder The energy field of each material form the complex energy field of the phase coordinating and unifying, each magnetic field adding component or the infrared field of line are in mutually Excited state, field effect strengthens, thus offsets the field effect loss that portion of material causes because crystalline structure destroys.In energy powder Other material beyond described adjuvant can discharge different energy field, keeps higher field effect on the physical therapy ring made, The magnetic field or the infrared field of line that keep each interpolation component are in mutual excited state.
Described Os Draconis, another name: Lu Hu lose life, that gal bone, Os Draconis, Os Draconis (calcined), five OS DRACONISs, green grass or young cropsization Os Draconis, OS DRACONIS, Os Draconis.For mammal in ancient times as if the fossil of skeleton of class, rhinoceros class, Hippocampal cortex etc..
Preferably, described calcium gluconate and the mass ratio of stone needle are 3.8 ~ 3.9:0.5.When above-mentioned adjuvant uses above-mentioned Quality than time enable that powder shows the highest field effect in ceramic material.
Preferably, described yellow quartz is 0.01:1 with the mass ratio of Maifanitum.Inventor finds when yellow quartz and wheat meal The mass ratio of stone can show higher field effect when this ratio.
Preferably, the principal goods material of described elastomeric material is natural rubber or silica gel.Natural rubber or silica gel and the present invention The containment of energy powder used is preferable, and the product ultimately formed is optimal with the comfort level of human contact.
Described elastomeric material accounts for the described energy powder of 0.75% ~ 1.25% mixed with mass fraction.Preferably using of energy powder Amount, had both ensured the action effect of field effect, had ensured again cost.
The preparation method of a kind of above-mentioned active physical therapy ring, it is characterised in that preparation process is:
1) weighed material by the weight portion composition of energy powder and be sufficiently mixed;First with grinder the temperature of 520 DEG C ~ 580 DEG C It is ground obtaining the energy powder of 2000 mesh ~ 6000 mesh under degree;
2) the energy powder of 2000 mesh ~ 6000 mesh and the resin raw material of elastomeric material are mixed to get activated elastic materials by proportioning, live Property elastomeric material makes physical therapy ring by ring technique processed;
Or,
The energy powder of 2000 mesh ~ 6000 mesh proceeds to nano-level grinder after the ethanol of the 12% ~ 16% of addition energy powder gross mass again The abrasive media inside utilizing 0.8mm ~ 2.5mm is ground, and is dried after crushing and obtains nanoscale energy powder;Nanoscale energy powder with The resin raw material of elastomeric material is mixed to get activated elastic materials by proportioning, and activated elastic materials makes physical therapy by ring technique processed Ring.
The present invention, in the preparation method of physical therapy ring, is either directly added into the energy of 2000 mesh ~ 6000 mesh in elastomeric material Amount powder or nanoscale energy powder, key point is all in step 1) to keep 520 DEG C ~ 580 DEG C in process of lapping at energy powder This specified temp, inventor finds to grind at this temperature to enable to the energy field of each material at specific excited state Under be ground mixing, thus show higher field effect in final energy powder.Use ceramic particle form time with Only need co-ground during the mixing of other Glaze Composition, both can guarantee that in the ceramic particle being eventually fabricated, kept each interpolation component Magnetic field or the infrared field of line are in mutual excited state.And fiber and elastomeric material all can add as auxiliary agent in the course of processing Add.
Step 2) in comprise two kinds of forms of physical therapy ring, it is therefore intended that by the main body of the energy powder of above-mentioned composition Yu physical therapy ring In conjunction with.Aforesaid way is only the preferred form of the present invention, and with this end in view other technologies means all can use.
Preferably, the temperature in described grinder 540 DEG C ~ 555 DEG C.Field effect can be obtained the strongest under identical proportioning Physical therapy ring goods.
Preferably, described energy powder proceeds to nanometer after the ethanol of the 14% ~ 14.5% of addition energy powder gross mass again grind Grind in grinding machine.Can the activity of preferably excitation energy powder, and ensure the particle uniformity of nanoscale energy powder.
Containing Zn, Fe, Mn, Cu, Co, A1, Se, Cr, Ag, Sr, Ga, Ge, Li in the Buddha's warrior attendant YAOSHI used in the present invention, The various trace elements such as Ti, Mo, V, the Fe in Buddha's warrior attendant YAOSHI, the trace element such as Zn, Mn, Cu, Co promotes organic Growing up and grow, and blood circulation promoting, the element such as Cu, Zn, Mo, I strengthens resistance and the function Buddha's warrior attendant of immunocompetence YAOSHI has adsorption and bactericidal action because of special tectonic in structure and chemically.Learn that Buddha's warrior attendant YAOSHI is to unit by experiment The absorption affinity of element is Pb(lead): 63 ~ 95%, Cd(cadmium): 35 ~ 68%, As(arsenic): 37.2%, Hg(hydrargyrum): 80%, F(fluorine): 64 ~ 69%. In coliform culture vessel, put into Buddha's warrior attendant YAOSHI solution, have 97.55% adsorbed death.The ability specific activity charcoal of absorption abnormal flavour High several times, in addition with anticancer, prevent radiation, Auto-regulator metabolism and blood circulation, prolongation life-span, supplement energy etc. and make With, it is generally used for arteriosclerosis, leg ulcer that hypertension, diabetes, nephritis, vein occlusion cause, burn, depilation, wet Rash, tinea pedis, neurodermatitis, miliaria, increase, anticancer, prevent radiation etc..
The obsidian used in the present invention is among all spar, a kind of spar that the property received is the strongest.Can the most just incite somebody to action Near miscellaneous QI or negativity energy, inspiration in it invisible space in.Can draw crossing the energy contained in human body, releive Uncomfortable.
The yellow quartz used in the present invention is the most effective in cure for pancreas and endocrine nervous system, and to glycosuria, patient less may be used Or lack, it is possible to treatment swelling stomach function regulating knots, and main gastrointestinal function, dyspepsia or the unbalance person of diet suitably use.Also clear up tight Open emotion, help the function of the digestive system such as the intestines and stomach.
The Maifanitum used in the present invention is made up of 25000 Multiple components, can discharge several mineral materials.Maifanitum is all right Self component is utilized to pass through the method ionization noxious substance absorbing, decomposing.Released mineral matter also balances mineral quantity, Maifanitum The requisite various mineral of human body can be given out in water.Supplement by absorbing unnecessary mineral or released mineral matter It is not enough, and Maifanitum can balance the quantity of mineral.Maifanitum release various trace element such as: potassium, phosphorus, ferrum, sulphur, manganese, Magnesium etc., enzyme and hormonal synthesis are played an important role by these materials.Maifanitum can also be treated " dermatosis, swelling, skin scabies, Traumatic injury of skin etc. ".And Maifanitum is the most effective to removing various chemical toxicants.Also have in the present invention and most to pay attention to, Maifanitum energy Discharge the infrared ray useful to human body.
The stone needle used in the present invention can send many far ir rays useful to human body and ultrasonic pulse, promotes Blood microcirculation, conditioning metabolism, its effect is equivalent to far infrared therapeutic apparatus+ultrasonic therapeutic apparatus dual function.Stone needle energy Energy by himself containing carrys out the potential of exciting human, have calm the nerves, QI and blood regulating, dredging the meridian, the internal organs such as purification Liver and kidney, Get rid of unnecessary toxin, strengthen the effect of the immunocompetence of people comprehensively.
Compared with prior art, the above-mentioned activity physical therapy ring of the had the beneficial effect that present invention of the present invention, physical therapy ring The energy active energy powder carried can adapt to the preparation technology environment of physical therapy ring and uses environment, and the field keeping higher is imitated Should, keep the magnetic field of each interpolation component or the infrared field of line to be in mutual excited state.The technique scheme institute of the present invention simultaneously The energy active energy powder added needs to use the crucial auxiliary material combination of the present invention, the inventors found that interpolation is certain The adjuvant of the calcium gluconate of amount, stone needle, zinc glutamate, Os Draconis composition, it is possible to preferably excite the activity of each energy powder so that it is Energy field forms the complex energy field of the phase coordinating and unifying, and each magnetic field adding component or the infrared field of line are in mutual excited state, Field effect is higher.Described in energy powder, other mineral materials beyond adjuvant can discharge different energy field, and the present invention uses The means of the energy powder of above-mentioned adaptation physical therapy ring preparation technology environment.Energy after again prepared by the particular abrasive technique through the present invention Enough form more preferably activity, the energy powder added in preparation method of the present invention keep in process of lapping 520 DEG C ~ 580 DEG C this Specified temp, inventor finds to grind the energy field quilt under specific excited state enabling to each material at this temperature Ground and mixed, thus in final physical therapy ring, show higher field effect.This physical therapy ring utilizes the energy wherein added Amount powder, dirty in health can be removed, decompose the bio electricity in health, improve health body constitution, faintly acid body constitution is slowly transformed into Alkalescence body constitution, the effectively shielding external environment injury to health.
Detailed description of the invention
Below in conjunction with specific embodiment, the present invention will be further described.
Embodiment 1
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.012 part, Os Draconis 0.25 Part weighs material and is sufficiently mixed;Then it is ground obtaining 2000 mesh ~ 6000 mesh at a temperature of 550 DEG C with grinder Energy powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 0.9% in the resin raw material of elastomeric material obtains activity bullet Property material, activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 2
1) weight portion of energy powder consist of Buddha's warrior attendant YAOSHI 3.5 parts, tourmaline 3.3 parts, 0.38 part of Khotan jade stone, obsidian 2.3 parts, Yellow quartz 0.06 part, Maifanitum 6 parts, calcium gluconate 3.8 parts, stone needle 0.5 part, zinc glutamate 0.011 part, Os Draconis 0.27 part title Take material and be sufficiently mixed;Then at a temperature of 545 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Amount powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 1.25% in the resin raw material of elastomeric material obtains activity Elastomeric material, activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 3
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.8 parts, 0.4 part of Khotan jade stone, obsidian 2.1 parts, Yellow quartz 0.05 part, Maifanitum 5 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.013 part, Os Draconis 0.23 part title Take material and be sufficiently mixed;Then at a temperature of 540 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Amount powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 0.75% in the resin raw material of elastomeric material obtains activity Elastomeric material, activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 4
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 4.0 parts, 0.42 part of Khotan jade stone, obsidian 2 parts, Yellow quartz 0.07 part, Maifanitum 3 parts, calcium gluconate 4.1 parts, stone needle 0.3 part, zinc glutamate 0.01 part, Os Draconis 0.3 part weigh Material is also sufficiently mixed;First at a temperature of 555 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 1.5% in the resin raw material of elastomeric material obtains activity bullet Property material, activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 5
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.5 parts, tourmaline 3.0 parts, 0.3 part of Khotan jade stone, obsidian 2.4 parts, Yellow quartz 0.03 part, Maifanitum 7 parts, calcium gluconate 3.8 parts, stone needle 0.6 part, zinc glutamate 0.015 part, Os Draconis 0.2 part title Take material and be sufficiently mixed;First at a temperature of 580 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 0.5% in the resin raw material of elastomeric material obtains activity bullet Property material, activated elastic materials makes physical therapy ring by ring technique processed.
Comparative example 1
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts weigh material and are sufficiently mixed;Then enter at a temperature of 550 DEG C with grinder Row grinding obtains the energy powder of 2000 mesh ~ 6000 mesh;
3) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 0.9% in the resin raw material of elastomeric material obtains activity bullet Property material, activated elastic materials makes physical therapy ring by ring technique processed.
Comparative example 2
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.012 part, Os Draconis 0.25 Part weighs material and is sufficiently mixed;Then it is ground obtaining the energy of 2000 mesh ~ 6000 mesh at normal temperatures with grinder Powder;
2) the energy powder adding 2000 mesh ~ 6000 mesh that mass fraction accounts for 0.9% in the resin raw material of elastomeric material obtains activity bullet Property material, activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 1 ~ 5 and comparative example is worn to 100 old peoples, 100 subhealth states, the middle age of 100 health overdraws 1,2 physical therapy ring prepared, carries out practical test after using one week, and the health of the user of embodiment 1 ~ 5 is significantly better than The health of the user of comparative example 1,2.Such as: in (1) heavy burden aptitude tests, the user of embodiment 1 bear ability The user mean height 7.1% of the user mean height 10.5% of relatively comparative example 1, relatively comparative example 2;(2) equilibrant (is stood with one foot to the knee and is stretched Straight single armed) in test, the equilibration time of the user of embodiment 1 is compared with the user mean height 15.4% of comparative example 1, relatively comparative example 2 User mean height 8.7%;(3) in pliability test, (feet station is vertical fixing, straight-arm revolution health, uses front hook Amax, after using Corner A " max, then A " arc length about 10 ~ 30cm(the heaviest effect of health corresponding to max > Amax and (A " max Amax) is the brightest Aobvious, it is meant that situation is become better), the pliability of the user of embodiment 1, compared with the user mean height 13.6% of comparative example 1, relatively contrasts The user mean height 8.0% of example 2.Embodiment 1 and comparative example 1,2 compare the physical therapy ring that can be seen that under this kind of form of the present invention The adjuvant of middle interpolation has excitation to the activity of each material, it is possible to make the energy field of each material unify mutually, thus keeps relatively High comprehensive field effect, counteracts the field effect loss that portion of material causes because crystalline structure destroys, uses rear human activin The activity of cell, blood circulation promoting, this physical therapy ring utilizes the energy powder wherein added, dirty in removing health, decomposes Bio electricity in health, improves health body constitution, and faintly acid body constitution is slowly transformed into alkalescence body constitution, effectively shielding external environment pair The injury of health.
Embodiment 6
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.012 part, Os Draconis 0.25 Part takes material and is sufficiently mixed;Then it is ground obtaining 2000 mesh ~ 6000 purposes at a temperature of 550 DEG C with grinder Energy powder;
2) the energy powder of 14.8 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 14% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 0.9% and obtain activated elastic materials, live Property elastomeric material makes physical therapy ring by ring technique processed.
Embodiment 7
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.5 parts, tourmaline 3.3 parts, 0.38 part of Khotan jade stone, obsidian 2.3 Part, yellow quartz 0.06 part, Maifanitum 6 parts, calcium gluconate 3.8 parts, stone needle 0.5 part, zinc glutamate 0.011 part, Os Draconis 0.27 Part weighs material and is sufficiently mixed;Then it is ground obtaining 2000 mesh ~ 6000 mesh at a temperature of 545 DEG C with grinder Energy powder;
2) the energy powder of 16.9 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 14.5% of addition energy powder gross mass again The abrasive media utilizing 0.8mm ~ 2.5mm in grinder is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 0.75% and obtain activated elastic materials, Activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 8
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.8 parts, 0.4 part of Khotan jade stone, obsidian 2.1 parts, Yellow quartz 0.05 part, Maifanitum 5 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.013 part, Os Draconis 0.23 part title Take material and be sufficiently mixed;Then at a temperature of 540 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Amount powder;3.9 ~ 4.0:0.5:0.12 ~ 0.13
2) the energy powder of 15.7 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 14% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 1.25% and obtain activated elastic materials, Activated elastic materials makes physical therapy ring by ring technique processed.
Embodiment 9
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 4.0 parts, 0.42 part of Khotan jade stone, obsidian 2 parts, Yellow quartz 0.07 part, Maifanitum 3 parts, calcium gluconate 4.1 parts, stone needle 0.3 part, zinc glutamate 0.01 part, Os Draconis 0.3 part weigh Material is also sufficiently mixed;First at a temperature of 555 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Powder;
2) the energy powder of 13.75 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 13% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 0.5% and obtain activated elastic materials, live Property elastomeric material makes physical therapy ring by ring technique processed.
Embodiment 10
1) weight portion of energy powder consists of: Buddha's warrior attendant YAOSHI 3.5 parts, 0.3 part of 3.0 parts of Khotan jade stones of tourmaline, obsidian 2.4 parts, Yellow quartz 0.03 part, Maifanitum 7 parts, calcium gluconate 3.8 parts, stone needle 0.6 part, zinc glutamate 0.015 part, Os Draconis 0.2 part title Take material and be sufficiently mixed;First at a temperature of 520 DEG C, it is ground obtaining the energy of 2000 mesh ~ 6000 mesh with grinder Powder;
2) the energy powder of 17.9 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 12% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 1.5% and obtain activated elastic materials, live Property elastomeric material makes physical therapy ring by ring technique processed.
Comparative example 3
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts weigh material and are sufficiently mixed;Then enter at a temperature of 550 DEG C with grinder Row grinding obtains the energy powder of 2000 mesh ~ 6000 mesh;
2) the energy powder of 10.12 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 14% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 0.9% and obtain activated elastic materials, live Property elastomeric material makes physical therapy ring by ring technique processed.
Comparative example 4
1) weight portion pressing energy powder forms: Buddha's warrior attendant YAOSHI 3.4 parts, tourmaline 3.5 parts, 0.36 part of Khotan jade stone, obsidian 2.2 Part, yellow quartz 0.04 part, Maifanitum 4 parts, calcium gluconate 3.9 parts, stone needle 0.5 part, zinc glutamate 0.012 part, Os Draconis 0.25 Part weighs material and is sufficiently mixed;Then it is ground obtaining the energy of 2000 mesh ~ 6000 mesh at normal temperatures with grinder Powder;
2) the energy powder of 14.8 part of 2000 mesh ~ 6000 mesh proceeds to nanometer after the ethanol of the 14% of addition energy powder gross mass again grind The abrasive media utilizing 0.8mm ~ 2.5mm in grinding machine is ground, and is dried after crushing and obtains nanoscale energy powder;
3) resin raw material of elastomeric material adds mass fraction account for the nanoscale energy powder of 0.9% and obtain activated elastic materials, live Property elastomeric material makes physical therapy ring by ring technique processed.
Embodiment 6 ~ 10 and comparative example is worn to 100 old peoples, 100 subhealth states, the middle age of 100 health overdraws 3,4 physical therapy ring prepared, carries out practical test after using one week, and the health of the user of embodiment 6 ~ 10 is significantly better than The health of the user of comparative example 3,4.Such as: in (1) heavy burden aptitude tests, the user of embodiment 6 bear ability The user mean height 7.9% of the user mean height 11.5% of relatively comparative example 3, relatively comparative example 4;(2) equilibrant (is stood with one foot to the knee and is stretched Straight single armed) in test, the equilibration time of the user of embodiment 6 is compared with the user mean height 15.7% of comparative example 3, relatively comparative example 4 User mean height 8.5%;(3) in pliability test, (feet station is vertical fixing, straight-arm revolution health, uses front hook Amax, after using Corner A " max, then A " arc length about 10 ~ 30cm(the heaviest effect of health corresponding to max > Amax and (A " max Amax) is the brightest Aobvious, it is meant that situation is become better), the pliability of the user of embodiment 6, compared with the user mean height 13.7% of comparative example 3, relatively contrasts The user mean height 8.2% of example 4.Embodiment 6 and comparative example 3,4 compare the physical therapy ring that can be seen that under this kind of form of the present invention The adjuvant of middle interpolation has excitation to the activity of each material, it is possible to make the energy field of each material unify mutually, thus keeps relatively High comprehensive field effect, counteracts the field effect loss that portion of material causes because crystalline structure destroys, uses rear human activin The activity of cell, blood circulation promoting, this physical therapy ring utilizes the energy powder wherein added, dirty in removing health, decomposes Bio electricity in health, improves health body constitution, and faintly acid body constitution is slowly transformed into alkalescence body constitution, effectively shielding external environment pair The injury of health.
50 arrhythmia patients, 50 hyperpietics, 50 varicose vein patients are allowed to dress embodiment 1 ~ 10 respectively The physical therapy ring prepared, after dressing 10min, significantly alleviating all occurs in ARR symptom, and blood pressure starts back fall, and blood vessel is not Protrude again.Under the effect of the energy field put outside this physical therapy ring, have stimulated the activity of soma, add the bullet of blood vessel wall Property, excite the potential of human body.The rehabilitation required time of the experimenter of this physical therapy ring is dressed in the experiment coordinating Drug therapy (only record rehabilitation than the rehabilitation required time of the experimenter not dressed, have multidigit experimenter there is no health in the experimental stage Multiple) the shortest by 78.6%.
The above, be only presently preferred embodiments of the present invention, is not the restriction that the present invention makees other form, appoints What those skilled in the art changed possibly also with the technology contents of the disclosure above or be modified as equivalent variations etc. Effect embodiment.But every without departing from technical solution of the present invention content, the technical spirit of the foundation present invention is to above example institute Any simple modification, equivalent variations and the remodeling made, still falls within the protection domain of technical solution of the present invention.

Claims (8)

1. an active physical therapy ring, including ring body, it is characterised in that: the main body of described ring body accounts for for being added with mass fraction The elastomeric material of the energy powder of 0.5% ~ 1.5%, the weight portion of described energy powder consists of: Buddha's warrior attendant YAOSHI 3.4 ~ 3.5 parts, tourmaline 3.0 ~ 4.0 parts, 0.3 ~ 0.42 part of Khotan jade stone, obsidian 2 ~ 2.4 parts, yellow quartz 0.03 ~ 0.07 part, Maifanitum 3 ~ 7 parts, auxiliary Material;Described adjuvant is calcium gluconate 3.8 ~ 4.1 parts, stone needle 0.3 ~ 0.6 part, zinc glutamate 0.01 ~ 0.015 part, Os Draconis 0.2 ~ 0.3 part.
A kind of activity physical therapy ring the most according to claim 1, it is characterised in that: described calcium gluconate and the matter of stone needle Amount ratio is 3.8 ~ 3.9:0.5.
A kind of activity physical therapy ring the most according to claim 1, it is characterised in that: described yellow quartz and the quality of Maifanitum Ratio is 0.01:1.
A kind of activity physical therapy ring the most according to claim 1, it is characterised in that: the principal goods material of described elastomeric material is Natural rubber or silica gel.
A kind of activity physical therapy ring the most according to claim 1, it is characterised in that: described elastomeric material divides mixed with quality Number accounts for the described energy powder of 0.75% ~ 1.25%.
6. the preparation method of the active physical therapy ring described in an any one of claim 1 ~ 5, it is characterised in that preparation process is:
1) weighed material by the weight portion composition of energy powder and be sufficiently mixed;First with grinder the temperature of 520 DEG C ~ 580 DEG C It is ground obtaining the energy powder of 2000 mesh ~ 6000 mesh under degree;
2) the energy powder of 2000 mesh ~ 6000 mesh and the resin raw material of elastomeric material are mixed to get activated elastic materials by proportioning, live Property elastomeric material makes physical therapy ring by ring technique processed;
Or,
The energy powder of 2000 mesh ~ 6000 mesh proceeds to nano-level grinder after the ethanol of the 12% ~ 16% of addition energy powder gross mass again The abrasive media inside utilizing 0.8mm ~ 2.5mm is ground, and is dried after crushing and obtains nanoscale energy powder;Nanoscale energy powder with The resin raw material of elastomeric material is mixed to get activated elastic materials by proportioning, and activated elastic materials makes physical therapy by ring technique processed Ring.
The preparation method of a kind of activity physical therapy ring the most according to claim 6, it is characterised in that: the pottery described in step 1) Temperature in porcelain grinder is 540 DEG C ~ 555 DEG C.
The most according to claim 6 a kind of activity physical therapy ring preparation method, it is characterised in that: step 2) described in energy Grind in amount powder proceeds to after the ethanol of the 14% ~ 14.5% of addition energy powder gross mass nano-level grinder again.
CN201610920778.3A 2016-10-21 2016-10-21 Active physiotherapy ring and preparation method thereof Withdrawn CN106309490A (en)