CN106297554A - A kind of acrylic luminescence logo film coating process - Google Patents

A kind of acrylic luminescence logo film coating process Download PDF

Info

Publication number
CN106297554A
CN106297554A CN201610742814.1A CN201610742814A CN106297554A CN 106297554 A CN106297554 A CN 106297554A CN 201610742814 A CN201610742814 A CN 201610742814A CN 106297554 A CN106297554 A CN 106297554A
Authority
CN
China
Prior art keywords
film
acrylic
logo
luminescence
superposition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610742814.1A
Other languages
Chinese (zh)
Inventor
苏斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI KONGBO INDUSTRIAL Co Ltd
Original Assignee
SHANGHAI KONGBO INDUSTRIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI KONGBO INDUSTRIAL Co Ltd filed Critical SHANGHAI KONGBO INDUSTRIAL Co Ltd
Priority to CN201610742814.1A priority Critical patent/CN106297554A/en
Publication of CN106297554A publication Critical patent/CN106297554A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of acrylic luminescence logo film coating process, particularly as follows: first get out the acrylic of required processing specification, on monoblock acrylic, then completely paste layer of transparent film;One layer of mirror film of superposition patch on hyaline membrane, continues one layer of black film of superposition patch on mirror film, and the semi-finished product of trilamellar membrane superposition on acrylic posted put baking oven into;Utilize machine tool plastics sucking moulding logo;Utilize mould that colour image is dug and tear unwanted film, retain the film needing color.The present invention uses a kind of Novel film laminating technique, adapt to Environmental by force, blowing-resistant drenches with rain and sunlight irradiates, and meets the technological effect demand of different consumer product, it is ensured that consumer product is unique, color floridity, visual effect is good, and lighting effects are strong, it is an advantage of the invention that technique is advanced rationally, enhance the market competitiveness, create significant economic benefit.

Description

A kind of acrylic luminescence logo film coating process
Technical field
The present invention relates to a kind of acrylic luminescence logo film coating process, can be used in the industries such as advertising signboard.
Background technology
At present, acrylic pad pasting uses more and more extensive in all trades and professions, along with the progress and development of society, people's Aesthetic conceptions and visual effect require to step up, and multiple color should be had to arrange in pairs or groups, and have third dimension, artistic feeling.Meet pad pasting After luminous visual effect.Paste multilayer film on the same face, according to different needs, hollow out or retain the film of needs, commonly Film coating process can not meet this require that, be a difficult problem to existing film coating process, only utilize new technique new Technique could meet the requirement of new product.
Summary of the invention
Problem to be solved by this invention is how to paste the film of multiple color on acrylic luminescence logo, it is ensured that product Multicolour collocation and logo illumination effect.
In order to solve the problems referred to above, the technical scheme is that a kind of acrylic luminescence logo film coating process of offer, its It is characterised by, specifically comprises the following steps that
The first step: select to need the acrylic of specification;
Second step: paste layer of transparent film on acrylic;
3rd step: one layer of mirror film of superposition patch on hyaline membrane:
4th step: one layer of black film of superposition patch on mirror film;
5th step: the semi-finished product that superposition on acrylic posts trilamellar membrane put baking oven into, steams completely by the moisture in the middle of film Send out, drying course must guaranteeing, acrylic is indeformable;
6th step: the semi-finished product being baked are taken out, utilizes machine tool plastics sucking moulding logo;
7th step: according to pattern color, utilizes mould to dig and tears unwanted film, retains the film needing color.
Preferably, after in described second step, acrylic posts hyaline membrane, must the most naturally do more than 12 hours.
Preferably, the parameter dried in described 5th step is: oven temperature is maintained at 60 DEG C, and drying time is 48 hours Above.
Preferably, if also needing to paste the film of other color, can operate according to the following steps after described 7th step:
After need pasting and utilizing engraving machine hollow out at other color film, then stick this color film.
The present invention uses a kind of Novel film laminating technique, adapt to Environmental by force, blowing-resistant drenches with rain and sunlight irradiates, and meets difference The technological effect demand of consumer product, it is ensured that consumer product is unique, color floridity, and visual effect is good, lighting effects are strong, this The advantage of invention is that technique is advanced rationally, enhances the market competitiveness, creates significant economic benefit.
Accompanying drawing explanation
Fig. 1 is the schematic diagram of a kind of acrylic luminescence logo of embodiment 1 preparation.
Detailed description of the invention
For making the present invention become apparent, hereby with preferred embodiment, and accompanying drawing is coordinated to be described in detail below.
Embodiment
A kind of acrylic luminescence logo film coating process:
1, first get out the acrylic of required processing specification, on monoblock acrylic, then completely paste layer of transparent film, often The lower nature of temperature does more than 12 hours;
2, on the hyaline membrane after naturally dry, one layer of mirror film is completely pasted in superposition, continue superposition on hyaline membrane completely paste one layer black Film;
3, the semi-finished product of trilamellar membrane superposition on acrylic posted put baking oven into, and the temperature of baking oven is maintained at 60 DEG C, protect The time of depositing is more than 48 hours, guarantees that acrylic is indeformable in drying course, and the moisture in the middle of film evaporates completely;
4, the semi-finished product of the trilamellar membrane then baking oven acrylic superposition posted take out, and utilize machine tool plastics sucking moulding logo;
5, the logo that plastic uptake is good utilizes mould dig colour image and tear unwanted film, retain and need color Film;
6, mould is placed on the logo that plastic uptake is good, divides figure with blade according to mold graph, as it is shown in figure 1, a-quadrant Retaining all black films, B region hollows out black film and mirror film, retains acrylic primary colors, and C digs in region and tears all of black film, protects Stay mirror film;
7, according to figure contribution, carve required green film moulding and the part of hollow out English words with machine, then dig Empty green film position to be pasted, i.e. the trilamellar membrane in D region, post the film of green.

Claims (4)

1. an acrylic luminescence logo film coating process, it is characterised in that specifically comprise the following steps that
The first step: select to need the acrylic of specification;
Second step: paste layer of transparent film on acrylic;
3rd step: one layer of mirror film of superposition patch on hyaline membrane:
4th step: one layer of black film of superposition patch on mirror film;
5th step: the semi-finished product that superposition on acrylic posts trilamellar membrane put baking oven into, evaporates completely by the moisture in the middle of film, dries Must guarantee during Gan that acrylic is indeformable;
6th step: the semi-finished product being baked are taken out, utilizes machine tool plastics sucking moulding logo;
7th step: according to pattern color, utilizes mould to dig and tears unwanted film, retains the film needing color.
2. acrylic luminescence logo film coating process as claimed in claim 1, it is characterised in that acrylic patch in described second step After good hyaline membrane, must the most naturally do more than 12 hours.
3. acrylic luminescence logo film coating process as claimed in claim 1, it is characterised in that the ginseng dried in described 5th step Number is: oven temperature is maintained at 60 DEG C, and drying time is more than 48 hours.
4. acrylic luminescence logo film coating process as claimed in claim 1, it is characterised in that if also needing to paste other color Film, can operate after described 7th step according to the following steps:
After need pasting and utilizing, at other color film, the trilamellar membrane that engraving machine hollow out posts, then stick this color film of respective shapes i.e. Can.
CN201610742814.1A 2016-08-26 2016-08-26 A kind of acrylic luminescence logo film coating process Pending CN106297554A (en)