CN106189291A - Iran's natural rock asphalt modified pitch and preparation method thereof - Google Patents

Iran's natural rock asphalt modified pitch and preparation method thereof Download PDF

Info

Publication number
CN106189291A
CN106189291A CN201610560542.3A CN201610560542A CN106189291A CN 106189291 A CN106189291 A CN 106189291A CN 201610560542 A CN201610560542 A CN 201610560542A CN 106189291 A CN106189291 A CN 106189291A
Authority
CN
China
Prior art keywords
iran
parts
natural rock
rock asphalt
modified pitch
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201610560542.3A
Other languages
Chinese (zh)
Other versions
CN106189291B (en
Inventor
徐萌
祝序博
牟惠跃
李文辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhongxin Road & Bridge Material Co Ltd
Original Assignee
Zhongxin Road & Bridge Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhongxin Road & Bridge Material Co Ltd filed Critical Zhongxin Road & Bridge Material Co Ltd
Priority to CN201610560542.3A priority Critical patent/CN106189291B/en
Publication of CN106189291A publication Critical patent/CN106189291A/en
Application granted granted Critical
Publication of CN106189291B publication Critical patent/CN106189291B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention belongs to new material technology field, be specifically related to a kind of Iran natural rock asphalt modified pitch and preparation method thereof.There is blocking production equipment expensive, easy for processes of rock asphalt modified asphalt in prior art, be difficult to the defects such as storage, the present invention provides a kind of Iran natural rock asphalt modified pitch and preparation method thereof.This Iran's natural rock asphalt modified pitch, including the raw material of following parts by weight: Iran's natural rock asphalt 15~20 parts, matrix pitch 90~100 parts, aromatic naphtha 20~30 parts, thermoplastic elastomer (TPE) 15~30 parts, stabilizer 3~5 parts, compatilizer 3~5 parts, dispersant 0.5~1 part.The modified pitch prepared by special preparation method, the compatibility is good, is not easily blocked production equipment, and its preparation method operation safety, technique simple possible, provides a kind of brand-new selection for modified pitch.

Description

Iran's natural rock asphalt modified pitch and preparation method thereof
Technical field
The invention belongs to new material technology field, be specifically related to a kind of Iran's natural rock asphalt modified pitch and preparation side thereof Method.
Background technology
Existing petroleum asphalt modified technology mainly has a thermoplastic elastomer class (SBS), rubber-like (SBR), resinae (EVA, PE).Relevant natural rock asphalt modification technology aspect, existing data shows, Modified Asphalt Mixture of Natural Rock Asphalt, incessantly at height The level of polymer modified asphalt it is all up on warm nature energy, cryogenic property and water stabilizing, and the most remote in other performances Exceed polymer modified asphalt compound.
But there is presently no the corresponding job specfication of natural rock asphalt and concrete exercisable foundation.In prior art useful The application in making asphalt road surface of China's Qing Chuan natural rock asphalt, but China's Qing Chuan kir yield is little, expensive, Ash is big, is easily generated equipment pipeline blockage, is difficult to the defects such as storage.
Iran's natural rock asphalt is the high-quality natural rock asphalt of Iran's import, and Iran's natural rock asphalt is compatible with asphalt Property good, production technology is simple, operates safety, properties of product stabilizing factor, and low in raw material price, kir compound cost performance Height, and Iran's natural rock asphalt abundance, can effectively solve the problem that existing energy problem of China.
Summary of the invention
There is blocking production equipment expensive, easy for processes of rock asphalt modified asphalt in prior art, be difficult to storage etc. and lack Falling into, the present invention provides a kind of Iran natural rock asphalt modified pitch and preparation method thereof.The modified pitch compatibility in the present invention Good, it is not easily blocked production equipment, and its preparation method operation safety, technique simple possible, provides for modified pitch a kind of complete New selection.
The present invention provides a kind of Iran natural rock asphalt modified pitch, including the raw material of following parts by weight: Iran is natural Kir 15~20 parts, matrix pitch 90~100 parts, aromatic naphtha 20~30 parts, thermoplastic elastomer (TPE) 15~30 parts, stabilizer 3 ~5 parts, compatilizer 3~5 parts, dispersant 0.5~1 part.
Preferably, above-mentioned Iran natural rock asphalt modified pitch, including the raw material of following parts by weight: Iran's natural rock drip Blue or green 20 parts, matrix pitch 90 parts, aromatic naphtha 25 parts, thermoplastic elastomer (TPE) 20 parts, stabilizer 4 parts, compatilizer 4 parts, dispersant 1 Part.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described Iran natural rock asphalt ash < 15%, granularity is 100~120 mesh.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described matrix pitch is asphalt, preferably 70# base Matter Colophonium and 90# matrix pitch.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described thermoplastic elastomer (TPE) is styrene~butadiene ~styrol copolymer and styrene~the mixture of isoprene, both weight ratios are 3~5: 6~7.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described aromatic hydrocarbons viscous crude is decompression distillation lube base Oil.
Wherein, above-mentioned Iran natural rock asphalt modified pitch in, described stabilizer be cumyl peroxide and, triolefin The mixture of propyl group isocyanuric acid ester weight ratio 1: 1.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described compatilizer is that maleic anhydride is grafted compatilizer.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described dispersant is sodium tripolyphosphate and hexa metaphosphoric acid The mixture of sodium by weight 2: 3.
Present invention also offers the preparation method of a kind of above-mentioned Iran natural rock asphalt modified pitch, comprise the following steps:
A, Iran's natural rock asphalt is mixed at 150~180 DEG C with matrix pitch, after stirring premix swelling 0.5~1h Preliminary shearing, is stirred for 1.5~2h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge In matrix pitch;
C, store while stirring at temperature 150~160 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mixing After react, reaction temperature 150~180 DEG C, the response time 3~4h, course of reaction high speed stir, mixing speed is 2000 ~3000r/min, obtain Iran's natural rock asphalt modified pitch.
The invention have the benefit that and the present invention selects Iran's natural rock asphalt be modified, utilize natural rock asphalt Good with the asphalt compatibility, production technology is simple, operates safety, properties of product stabilizing factor, and the drip of low in raw material price, rock The advantages such as blue or green compound cost performance is high, mix it with asphalt and are modified, add a certain amount of in preparation process Aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant so that the modified pitch of preparation has preferable high/low temperature Performance, water stabilizing, be especially suitable for deck paving, the mating formation of road junction, for the modified drip of China's road Green grass or young crops provides a kind of brand-new selection.
Detailed description of the invention
The present invention provides a kind of Iran natural rock asphalt modified pitch, including the raw material of following parts by weight: Iran is natural Kir 15~20 parts, matrix pitch 90~100 parts, aromatic naphtha 20~30 parts, thermoplastic elastomer (TPE) 15~30 parts, stabilizer 3 ~5 parts, compatilizer 3~5 parts, dispersant 0.5~1 part.
Preferably, above-mentioned Iran natural rock asphalt modified pitch, including the raw material of following parts by weight: Iran's natural rock drip Blue or green 20 parts, matrix pitch 90 parts, aromatic naphtha 25 parts, thermoplastic elastomer (TPE) 20 parts, stabilizer 4 parts, compatilizer 4 parts, dispersant 1 Part.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described Iran natural rock asphalt content of ashes < 15%, grain Degree is 100~120 mesh.The granularity of kir plays great role to the performance of modified pitch, and kir granularity is excessive, kir Long with matrix pitch time of fusion, in kir, the powder of sandstone and rock easily precipitates;Fineness is too small, and kir is floating to be difficult to Miscible, therefore, through choosing comprehensively, inventor find kir granularity be 100~120 mesh be optimum granularity.Additionally, rock The content of ashes of Colophonium is also the key influence factor of performance of modified bitumen, and ash is the index of a rock content, and ash contains Amount size to modified pitch stirring and shear time state have large effect, be also cost height crucial effect because of Element, the Iranian natural rock asphalt of preferred content of ashes < 15% in technical solution of the present invention.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described matrix pitch is asphalt, preferably 70# base Matter Colophonium and 90# matrix pitch.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described thermoplastic elastomer (TPE) is styrene~butadiene ~styrol copolymer and styrene~the mixture of isoprene, both weight ratios are 3~5: 6~7.
Thermoplastic elastomer (TPE) is conducive to the improvement of the high temperature performance of modified pitch in suitable content range.If it is hot The amount of thermoplastic elastic is less than 15 weight portions, then do not have the effect of the high temperature performance improving modified pitch;If thermoplasticity The amount of elastomer is more than 30 weight portions, then the viscosity that can make modified pitch is too high, affects the mixing of modified asphalt mixture and becomes Type.Therefore, the present invention uses the thermoplastic elastomer (TPE) of 15~30 weight portions.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described aromatic naphtha is decompression distillation lube base oil. Aromatic naphtha is conducive to the improvement of the cryogenic property of modified pitch in suitable content range.If the amount of aromatic naphtha is less than 20 weights Amount part, then improve DeGrain to the cryogenic property of modified pitch;If the amount of aromatic naphtha is more than 30 weight portions, then to low temperature The amplitude of performance improvement is the most inconspicuous, and can significantly affect the high-temperature behavior of modified pitch, therefore, the present invention use 20~ The aromatic naphtha of 30 weight portions.
Wherein, above-mentioned Iran natural rock asphalt modified pitch in, described stabilizer be cumyl peroxide and, triolefin The mixture of propyl group isocyanuric acid ester weight ratio 1: 1.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described compatilizer is that maleic anhydride is grafted compatilizer.
Wherein, in above-mentioned Iran natural rock asphalt modified pitch, described dispersant is sodium tripolyphosphate and hexa metaphosphoric acid The mixture of sodium by weight 2: 3.
Present invention also offers the preparation method of a kind of above-mentioned Iran natural rock asphalt modified pitch, comprise the following steps:
A, Iran's natural rock asphalt is mixed at 150~180 DEG C with matrix pitch, after stirring premix swelling 0.5~1h Preliminary shearing, is stirred for 1.5~2h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge In matrix pitch;
C, store while stirring at temperature 150~160 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mixing After react, reaction temperature 150~180 DEG C, the response time 3~4h, course of reaction high speed stir, mixing speed is 2000 ~3000r/min, obtain Iran's natural rock asphalt modified pitch.
Below by embodiment, the detailed description of the invention of the present invention is described further, but not by the protection of the present invention In the range of scope is limited in described in embodiment.
Each product described in embodiment is common commercially available prod.
Embodiment 1 technical solution of the present invention prepares modified pitch 1
The raw material of modified pitch 1 consists of: count by weight, Iran's natural rock asphalt 15 parts, matrix pitch 90 parts, virtue Hydrocarbon ils 20 parts, thermoplastic elastomer (TPE) 15 parts, stabilizer 3 parts, compatilizer 3 parts, dispersant 0.5 part.
Preparation method is as follows, comprises the following steps:
A, being mixed at 150 DEG C with matrix pitch by Iran's natural rock asphalt, stirring premixes preliminary shearing after swelling 0.5h, then stirs Mix 1.5h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge In matrix pitch;
C, store while stirring at temperature 150 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mixing After react, reaction temperature 150 DEG C, response time 3h, course of reaction high speed stir, mixing speed is 2000r/min, To Iran's natural rock asphalt modified pitch 1.
Embodiment 2 technical solution of the present invention prepares modified pitch 2
The raw material of modified pitch 2 consists of: count by weight, Iran's natural rock asphalt 20 parts, matrix pitch 100 parts, Aromatic naphtha 30 parts, thermoplastic elastomer (TPE) 30 parts, stabilizer 5 parts, compatilizer 5 parts, dispersant 1 part.
Preparation method is as follows, comprises the following steps:
A, being mixed at 180 DEG C with matrix pitch by Iran's natural rock asphalt, stirring premixes preliminary shearing after swelling 1h, is stirred for 2h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge In matrix pitch;
C, store while stirring at temperature 160 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mixing After react, reaction temperature 180 DEG C, response time 4h, course of reaction high speed stir, mixing speed is 3000r/min, To Iran's natural rock asphalt modified pitch 2.
Embodiment 3 technical solution of the present invention prepares modified pitch 3
The raw material of modified pitch 3 consists of: count by weight, Iran's natural rock asphalt 20 parts, matrix pitch 90 parts, virtue Hydrocarbon ils 25 parts, thermoplastic elastomer (TPE) 20 parts, stabilizer 4 parts, compatilizer 4 parts, dispersant 1 part.
Preparation method is as follows, comprises the following steps:
A, being mixed at 160 DEG C with matrix pitch by Iran's natural rock asphalt, stirring premixes preliminary shearing after swelling 1h, is stirred for 2h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge In matrix pitch;
C, store while stirring at temperature 160 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mixing After react, reaction temperature 180 DEG C, response time 4h, course of reaction high speed stir, mixing speed is 2500r/min, To Iran's natural rock asphalt modified pitch 3.
The kir that comparative example 4 substitutes the present invention by equivalent SBS prepares modified pitch 4
The raw material of modified pitch 4 is in addition to substituting the SBS of Iran's natural rock asphalt equivalent, and remaining raw material and step are with real Execute example 3.The modified pitch of embodiment and comparative example gained is carried out performance test, obtains result as shown in table 1 below.
The performance measurement table of table 1 modified pitch
As seen from the experiment, the modified pitch that technical solution of the present invention prepares meets " asphalt highway construction technology Specification " method of (JTGF40-2004) performance requirement to modified pitch, meanwhile, the modified drip of technical solution of the present invention gained It is very big that blue or green compound high-temperature behavior promotes amplitude, and cryogenic property is not affected, and water stabilizing is excellent, preferably Bridge floor or intersection are mated formation.

Claims (10)

1. an Iranian natural rock asphalt modified pitch, it is characterised in that include the raw material of following parts by weight: Iran's natural rock Colophonium 15~20 parts, matrix pitch 90~100 parts, aromatic naphtha 20~30 parts, thermoplastic elastomer (TPE) 15~30 parts, stabilizer 3~5 Part, compatilizer 3~5 parts, dispersant 0.5~1 part.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that include following parts by weight Raw material: Iran's natural rock asphalt 20 parts, matrix pitch 90 parts, aromatic naphtha 25 parts, thermoplastic elastomer (TPE) 20 parts, stabilizer 4 parts, phase Hold agent 4 parts, dispersant 1 part.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described Iran natural rock asphalt Ash < 15%, granularity is 100~120 mesh.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described matrix pitch is 70# matrix pitch or 90# matrix pitch.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described thermoplastic elastomer (TPE) For styrene~butadiene~styrol copolymer and styrene~the mixture of isoprene, both weight ratios are 3~5:6 ~7.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described aromatic hydrocarbons viscous crude is for subtracting Pressure distillation lube base oil.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described stabilizer is peroxide Change diisopropylbenzene (DIPB) and, the mixture of Triallyl isocyanurate weight ratio 1:1.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described compatilizer is Malaysia Acid anhydride-grafted compatilizer.
Iran the most according to claim 1 natural rock asphalt modified pitch, it is characterised in that: described dispersant is trimerization The mixture of sodium phosphate and sodium hexameta phosphate 2:3 by weight.
10., according to the preparation method of the Iranian natural rock asphalt modified pitch described in any one of claim 1~9, its feature exists In, comprise the following steps:
A, Iran's natural rock asphalt is mixed at 150~180 DEG C with matrix pitch, preliminary shearing after stirring premix swelling 0.5~1h, It is stirred for 1.5~2h;
B, stirred after, before storing use three grades of high-speed shearing machines carry out fine pruning, make Rock Powder uniformly merge in substrate In Colophonium;
C, store while stirring at temperature 150~160 DEG C;
D, aromatic naphtha, thermoplastic elastomer (TPE), stabilizer, compatilizer and dispersant are added in step C products therefrom, mix laggard Row reaction, reaction temperature 150~180 DEG C, the response time 3~4h, course of reaction high speed stir, mixing speed be 2000~ 3000r/min, obtains Iran's natural rock asphalt modified pitch.
CN201610560542.3A 2016-07-15 2016-07-15 Iranian natural rock asphalt modified pitch and preparation method thereof Active CN106189291B (en)