- CN105922806A CN105922806A CN201610289853.0A CN201610289853A CN105922806A CN 105922806 A CN105922806 A CN 105922806A CN 201610289853 A CN201610289853 A CN 201610289853A CN 105922806 A CN105922806 A CN 105922806A
- Authority
- CN
- China
- Prior art keywords
- mud
- pen container
- manufacturing
- manufactured
- model
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B43—WRITING OR DRAWING IMPLEMENTS; BUREAU ACCESSORIES
- B43M—BUREAU ACCESSORIES NOT OTHERWISE PROVIDED FOR
- B43M99/00—Subject matter not provided for in other groups of this subclass
- B43M99/008—Desk-receptacles for holding writing appliances
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B44—DECORATIVE ARTS
- B44C—PRODUCING DECORATIVE EFFECTS; MOSAICS; TARSIA WORK; PAPERHANGING
- B44C1/00—Processes, not specifically provided for elsewhere, for producing decorative surface effects
- B44C1/22—Removing surface-material, e.g. by engraving, by etching
- B44C1/225—Removing surface-material, e.g. by engraving, by etching by engraving
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B44—DECORATIVE ARTS
- B44C—PRODUCING DECORATIVE EFFECTS; MOSAICS; TARSIA WORK; PAPERHANGING
- B44C3/00—Processes, not specifically provided for elsewhere, for producing ornamental structures
- B44C3/04—Modelling plastic materials, e.g. clay
Abstract
本发明涉及一种砖雕笔筒的制作方法,包括以下步骤:(1)制模:制作笔筒的模型,按照客户的需要将模型制作成一定的形状;(2)制泥:将东泥和西泥分别粉碎成泥料,然后按照东泥:西泥8:1的重量比进行制泥;(3)制坯:在步骤(1)的模型上制坯;(4)雕刻:在步骤(3)中的坯料上进行雕刻,雕刻出客户需要的图案;(5)煅烧:将步骤(4)中的物品在窑炉内烧制20‑24小时;(6)打磨:在打磨机内将步骤(5)中的物品打磨至具有一定的光泽度;(7)验收入库:将步骤(6)中的产品验收合格后入库,并做好入库登记。本发明工艺简单、容易控制,且制得的笔筒外形美观,更具有收藏价值,弥补了市场的空缺。
Description
技术领域
本发明涉及一种砖雕笔筒的制作方法,属于笔筒制作方法的技术领域。
背景技术
笔筒是指用陶瓷、竹木等制成的筒形插笔器具,是搁放毛笔的专用器物,据文献记载,它的材质有镏金、翡翠、紫檀和乌木,现在我们能够见到的传世器物,大多是用瓷或者是竹木制作的,具有收藏价值。但目前市场上很少存在砖雕笔筒,为弥补市场的空缺,提出本发明。
发明内容
针对现有技术的上述技术问题,本发明的目的是提供一种砖雕笔筒的制作方法,其工艺简单、容易控制,且制得的笔筒外形美观,更具有收藏价值,弥补了市场的空缺。
为达到上述目的,本发明是通过以下技术方案实现的:
一种砖雕笔筒的制作方法,包括以下步骤:
(1)制模:制作笔筒的模型,按照客户的需要将模型制作成一定的形状;
(2)制泥:将东泥和西泥分别粉碎成泥料,然后按照东泥:西泥8:1的重量比进行制泥;
(3)制坯:在步骤(1)的模型上制坯;
(4)雕刻:在步骤(3)中的坯料上进行雕刻,雕刻出客户需要的图案;
(5)煅烧:将步骤(4)中的物品在窑炉内烧制20-24小时;
(6)打磨:在打磨机内将步骤(5)中的物品打磨至具有一定的光泽度;
(7)验收入库:将步骤(6)中的产品验收合格后入库,并做好入库登记。
本发明的有益效果如下:
本发明砖雕笔筒的制作方法,其工艺简单、容易控制,且制得的笔筒外形美观,更具有收藏价值,弥补了市场的空缺。
具体实施方式
下面结合具体实施例对本发明作进一步的说明,但本发明的保护范围并不限于此。
本发明砖雕笔筒的制作方法,包括以下步骤:
(1)制模:制作笔筒的模型,按照客户的需要将模型制作成一定的形状;
(2)制泥:将东泥和西泥分别粉碎成泥料,然后按照东泥:西泥8:1的重量比进行制泥;
(3)制坯:在步骤(1)的模型上制坯;
(4)雕刻:在步骤(3)中的坯料上进行雕刻,雕刻出客户需要的图案;
(5)煅烧:将步骤(4)中的物品在窑炉内烧制20-24小时;
(6)打磨:在打磨机内将步骤(5)中的物品打磨至具有一定的光泽度;
(7)验收入库:将步骤(6)中的产品验收合格后入库,并做好入库登记。
本发明砖雕笔筒的制作方法,其工艺简单、容易控制,且制得的笔筒外形美观,更具有收藏价值,弥补了市场的空缺。
上述实施例仅用于解释说明本发明的发明构思,而非对本发明权利保护的限定,凡利用此构思对本发明进行非实质性的改动,均应落入本发明的保护范围。
Claims (1)
1.一种砖雕笔筒的制作方法,其特征在于包括以下步骤:
(1)制模:制作笔筒的模型,按照客户的需要将模型制作成一定的形状;
(2)制泥:将东泥和西泥分别粉碎成泥料,然后按照东泥:西泥8:1的重量比进行制泥;
(3)制坯:在步骤(1)的模型上制坯;
(4)雕刻:在步骤(3)中的坯料上进行雕刻,雕刻出客户需要的图案;
(5)煅烧:将步骤(4)中的物品在窑炉内烧制20-24小时;
(6)打磨:在打磨机内将步骤(5)中的物品打磨至具有一定的光泽度;
(7)验收入库:将步骤(6)中的产品验收合格后入库,并做好入库登记。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610289853.0A CN105922806A (zh) | 2016-05-05 | 2016-05-05 | 一种砖雕笔筒的制作方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610289853.0A CN105922806A (zh) | 2016-05-05 | 2016-05-05 | 一种砖雕笔筒的制作方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN105922806A true CN105922806A (zh) | 2016-09-07 |
Family
ID=56835009
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201610289853.0A Pending CN105922806A (zh) | 2016-05-05 | 2016-05-05 | 一种砖雕笔筒的制作方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN105922806A (zh) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106364240A (zh) * | 2016-09-07 | 2017-02-01 | 深圳职业技术学院 | 一种防倾倒的智能笔架及其制备方法 |
-
2016
- 2016-05-05 CN CN201610289853.0A patent/CN105922806A/zh active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106364240A (zh) * | 2016-09-07 | 2017-02-01 | 深圳职业技术学院 | 一种防倾倒的智能笔架及其制备方法 |
CN106364240B (zh) * | 2016-09-07 | 2018-04-06 | 深圳职业技术学院 | 一种防倾倒的智能笔架及其制备方法 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103144207B (zh) | 水晶石材加工方法 | |
CN102837365A (zh) | 一种冰碛岩茶壶的制造方法 | |
US20070245682A1 (en) | Method for manufacturing synthetic decorative stone with inlays | |
CN104552578A (zh) | 一种激光雕刻陶瓷工艺 | |
CN107935632B (zh) | 一种陶瓷器修补方法 | |
CN105272180A (zh) | 一种陶瓷砖的生产工艺 | |
CN105313578A (zh) | 一种珍珠贝雕画工艺品的制作方法 | |
CN103524112B (zh) | 一种双面釉下五彩瓷板的制备方法 | |
CN105922806A (zh) | 一种砖雕笔筒的制作方法 | |
CN104290167A (zh) | 竹碗生产工艺及其产品 | |
CN104097443B (zh) | 铜胎与琉璃结合结构及其加工方法 | |
CN106045475A (zh) | 利用坯体废料制备珍珠瓷砂的方法及珍珠瓷砂创意陶瓷 | |
CN205058636U (zh) | 3d打印粉磨成型零件渗蜡升降台 | |
CN107149365A (zh) | 一种紫砂上釉杯具的制备方法 | |
CN104310954B (zh) | 免施釉仿白色系大理石花纹瓷器及其制作工艺 | |
KR100574846B1 (ko) | 도자기 제조방법 | |
CN204600038U (zh) | 一种透气性好、出水快的紫砂壶 | |
CN204845321U (zh) | 一种残古瓷镶嵌饰品 | |
CN101456757B (zh) | 带有浅浮雕装饰的紫砂陶瓷制品的制备方法 | |
CN100551653C (zh) | 一种艺术瓷砖的制作工艺方法 | |
CN203779608U (zh) | 扇骨仿形机用仿形板 | |
CN104157441A (zh) | 磁心成品制作工艺 | |
KR100584036B1 (ko) | 금분을 이용한 분청사기의 제조방법 | |
CN109080360A (zh) | 一种石材盘子器皿的数控雕刻铣削加工方法 | |
CN204819130U (zh) | 砖坯转向机 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
WD01 | Invention patent application deemed withdrawn after publication | ||
WD01 | Invention patent application deemed withdrawn after publication |
Application publication date: 20160907 |