CN105885236A - Novel anti-aging woven bag - Google Patents
Novel anti-aging woven bag Download PDFInfo
- Publication number
- CN105885236A CN105885236A CN201610488720.6A CN201610488720A CN105885236A CN 105885236 A CN105885236 A CN 105885236A CN 201610488720 A CN201610488720 A CN 201610488720A CN 105885236 A CN105885236 A CN 105885236A
- Authority
- CN
- China
- Prior art keywords
- parts
- woven bag
- aging
- novel anti
- antioxidant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to the field of plastic woven bag production processes and in particular relates to a novel anti-aging woven bag. The novel anti-aging woven bag is prepared by carrying out mixing, melting, filtration, extrusion film discharging, water cooling, separating, drawing, rolling and other procedures on the following raw materials in parts by weight: 100 parts of polypropylene, 20-23 parts of linear low density polyethylene, 8-10 parts of polyglycolide, 0.2-0.4 part of polycaprolactone, 1.2-1.4 parts of polyethylene terephthalate, 3-3.5 parts of EVA (ethylene-vinyl acetate copolymer) resin, 0.2-0.4 part of 2,4,5,6-tetrachloro-3-benzenedicarbonitrile, 1-1.2 parts of antioxidant 1035, 0.2-0.3 part of nano-carbon black, 0.4-0.6 part of aluminium oxide and 3-3.5 parts of auxiliary. The novel anti-aging woven bag is simple in formula and low in cost, has excellent processability and mechanical properties and is anti-aging and durable in use.
Description
Technical field
The present invention relates to Polywoven Bag production technology field, a kind of aging resistance Novel woven bag.
Background technology
Polywoven Bag is divided into Polypropylene Bag, Polythene Bag by main material composition;It is divided into seam end bag, tape edge by method of sewing
End bag.It is now widely used for a kind of packaging material of the article such as fertilizer, chemical products.Its main production is to utilize to mould
The material extruded thin film of raw material, cutting, simple tension are flat filament, through obtaining product through knitting device, and commonly referred to as woven bag.
The packaging bag of the polypropylene flat-filament establishment that conventional art produces, weatherability is poor, easily occur hardening at north of china in winter, embrittlement,
The problems such as demoulding, peeling, fracture, in south owing to summer temperature is high, illumination is strong, ultraviolet penetration power is strong, easily lead
The problem such as cause that woven bag is aging, burn into poor toughness, intensity low service life is short, not only wastes resource but also pollute environment.
Summary of the invention
In order to make up the deficiencies in the prior art, heretofore described a kind of aging resistance Novel woven bag, this woven bag has good
Good aging-resistant durability.
The technical solution adopted for the present invention to solve the technical problems is: a kind of aging resistance Novel woven bag, by following weight portion
Raw material by dispensing, melt, filter, extrude the operations such as membrane, water-cooled, sub-wire, wire drawing, rolling and make: polypropylene
100, linear low density polyethylene 20-23, PGA 8-10, pla-pcl 0.2-0.4, polyethylene terephthalate
1.2-1.4, EVA resin 3-3.5, termil 0.2-0.4, antioxidant 10351-1.2, nanometer carbon black 0.2-0.3,
Aluminium oxide 0.4-0.6, auxiliary agent 3-3.5.
Described auxiliary agent is prepared by the raw materials in: clay 20-24, Alumen 5-6, altax 2-3, cross-linking agent
TAC2-3, antioxidant CA 1-2, Anhydrite 3-4, ferrocene 2-3, morpholine 1-2, molybdenum bisuphide 5-7, phthalic acid ester
35-40, propylgallate 3-4, green tea powder 1-2, coix seed oil 2-3, vanadium diboride 2-3.
Beneficial effect: inventive formulation is simple, low cost, processing characteristics is excellent, excellent in mechanical performance, and aging resistance is made
Polywoven Bag can effectively stop the oxidation reaction caused by ultraviolet illumination, durable in use.
Detailed description of the invention
For the technological means making the present invention realize, creation characteristic, reach purpose and be easy to understand with effect, below in conjunction with
Embodiment, is expanded on further the present invention.
A kind of aging resistance Novel woven bag, by the raw material of following weight portion by dispensing, melt, filter, extrude membrane,
The operations such as water-cooled, sub-wire, wire drawing, rolling are made: polypropylene 100, linear low density polyethylene 20-23, PGA
8-10, pla-pcl 0.2-0.4, polyethylene terephthalate 1.2-1.4, EVA resin 3-3.5, tetrachloro isophthalic diformazan
Nitrile 0.2-0.4, antioxidant 10351-1.2, nanometer carbon black 0.2-0.3, aluminium oxide 0.4-0.6, auxiliary agent 3-3.5.
Described auxiliary agent is prepared by the raw materials in: clay 20-24, Alumen 5-6, altax 2-3, cross-linking agent
TAC2-3, antioxidant CA 1-2, Anhydrite 3-4, ferrocene 2-3, morpholine 1-2, molybdenum bisuphide 5-7, phthalic acid ester
35-40, propylgallate 3-4, green tea powder 1-2, coix seed oil 2-3, vanadium diboride 2-3.
The ultimate principle of the present invention, principal character and advantage have more than been shown and described.Skilled person will appreciate that of the industry,
The present invention is not restricted to the described embodiments, the principle that the present invention is simply described of the description in above-described embodiment and description,
Without departing from the spirit and scope of the present invention, the present invention also has various changes and modifications, and these changes and improvements are all
Fall in scope of the claimed invention.Claimed scope is defined by appended claims and equivalent thereof.
Claims (2)
1. an aging resistance Novel woven bag, it is characterised in that: by the raw material of following weight portion by dispensing, melted, filter,
The extruding operation such as membrane, water-cooled, sub-wire, wire drawing, rolling is made: polypropylene 100, linear low density polyethylene 20-23,
PGA 8-10, pla-pcl 0.2-0.4, polyethylene terephthalate 1.2-1.4, EVA resin 3-3.5, four
Chlorine isophthalodinitrile 0.2-0.4, antioxidant 10351-1.2, nanometer carbon black 0.2-0.3, aluminium oxide 0.4-0.6, auxiliary agent
3-3.5。
A kind of aging resistance Novel woven bag the most according to claim 1, it is characterised in that: described auxiliary agent is by following weight
Part raw material make: clay 20-24, Alumen 5-6, altax 2-3, cross-linking agent TAC2-3, antioxidant CA 1-2,
Anhydrite 3-4, ferrocene 2-3, morpholine 1-2, molybdenum bisuphide 5-7, phthalic acid ester 35-40, propylgallate 3-4,
Green tea powder 1-2, coix seed oil 2-3, vanadium diboride 2-3.