CN105750421A - Bending mold for back panel - Google Patents

Bending mold for back panel Download PDF

Info

Publication number
CN105750421A
CN105750421A CN201610288399.7A CN201610288399A CN105750421A CN 105750421 A CN105750421 A CN 105750421A CN 201610288399 A CN201610288399 A CN 201610288399A CN 105750421 A CN105750421 A CN 105750421A
Authority
CN
China
Prior art keywords
bending mould
bending
mould under
backboard according
mould subassembly
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610288399.7A
Other languages
Chinese (zh)
Inventor
唐彬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kunshan Dianziyu Electric Products Co Ltd
Original Assignee
Kunshan Dianziyu Electric Products Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kunshan Dianziyu Electric Products Co Ltd filed Critical Kunshan Dianziyu Electric Products Co Ltd
Priority to CN201610288399.7A priority Critical patent/CN105750421A/en
Publication of CN105750421A publication Critical patent/CN105750421A/en
Pending legal-status Critical Current

Abstract

The invention discloses a back plate downward bending die and relates to the technical field of back plate dies. This mould of bending under backplate includes mould subassembly and lower mould subassembly, it includes upper die base, mobilizable welt and cope match-plate pattern to go up the mould subassembly, lower mould subassembly includes lower bolster and die holder, be provided with into the son on the cope match-plate pattern, when last mould subassembly and lower mould subassembly are closed, go up the welt and go into to form between the son and be used for realizing the fashioned difference in height of bending under the product, go up and set up elastic positioning device between mould subassembly and the lower mould subassembly. The invention effectively solves the problems of low processing precision and poor production stability caused by the existing back plate lower bending die, and has the advantages of convenient operation, high processing precision, convenient maintenance and low processing cost.

Description

背板下折弯模具Bending mold for back panel

技术领域technical field

本发明涉及背板模具技术领域,尤其涉及一种背板下折弯模具。The invention relates to the technical field of backplane moulds, in particular to a backplane bottom bending mold.

背景技术Background technique

电化学在背板工件的加工过程中,有时需要进行下折弯处理,尤其需要进行直角下弯折处理。目前加工这种直角下折弯的背板工件的冲压设备一般都通过一种上下模滑块装置来对其进行加工,通过分别设置在上模和下模上的带有相配竖直面的滑块和顶块,来达到冲压成型并顺利脱模的目的,但是这种结构形式的缺点是:滑块和顶块分别位于上下模上,这样在二者接触的瞬间,冲击力较大,可能会影响到加工精度,其生产稳定性差,需要进行修理模具的次数较多,当大批量生产时,往往会因为修模而延误生产进程。In the process of electrochemical backplane workpiece processing, down-bending treatment is sometimes required, especially right-angle down-bending treatment. At present, the stamping equipment for processing this kind of right-angle down-bending back plate workpiece generally processes it through an upper and lower die slider device, and through slides with matching vertical surfaces respectively arranged on the upper die and the lower die However, the disadvantage of this structural form is that the slider and the top block are respectively located on the upper and lower molds, so that at the moment of contact between the two, the impact force is relatively large, which may It will affect the processing accuracy, its production stability is poor, and the mold needs to be repaired more times. When mass production, the production process is often delayed due to mold repair.

发明内容Contents of the invention

本发明的目的是提出一种背板下折弯模具,解决现有的背板下折弯模具造成的加工精度低,生产稳定性差的问题。The object of the present invention is to provide a back panel lower bending die to solve the problems of low processing precision and poor production stability caused by the existing back panel lower bending die.

为达此目的,本发明采用以下技术方案:For reaching this purpose, the present invention adopts following technical scheme:

一种背板下折弯模具,包括上模组件和下模组件,所述上模组件包括上模座、可活动的上衬板和上模板,所述下模组件包括下模板和下模座,所述上模板上设置有入子,当上模组件与下模组件闭合时,所述上衬板与入子之间形成用于实现产品下折弯成型的高度差,所述上模组件和下模组件之间设置弹性定位装置。A lower bending mold for a back panel, comprising an upper mold assembly and a lower mold assembly, the upper mold assembly includes an upper mold base, a movable upper liner and an upper template, and the lower mold assembly includes a lower template and the lower mold base, the upper template is provided with an insert, when the upper mold assembly and the lower mold assembly are closed, a height difference is formed between the upper liner and the insert to realize the lower bending of the product , an elastic positioning device is arranged between the upper mold assembly and the lower mold assembly.

作为一种背板下折弯模具的优选方案,所述入子与下模板相对的一侧设置有凹槽。As a preferred solution of the lower bending mold for the back panel, a groove is provided on the side opposite to the lower formwork of the insert.

作为一种背板下折弯模具的优选方案,所述凹槽靠近上衬板的侧壁为竖直面。As a preferred solution of the lower bending mold for the back panel, the side wall of the groove close to the upper liner is a vertical surface.

作为一种背板下折弯模具的优选方案,所述入子与上衬板相对的一侧底端设置有圆弧倒角。As a preferred solution of the lower bending mold for the back plate, the bottom end of the insert on the side opposite to the upper liner is provided with an arc chamfer.

作为一种背板下折弯模具的优选方案,所述弹性定位装置包括定位销和对应的定位孔,定位孔设置在上模板的底部,定位销穿过下模板,定位销的底部设置有第一支撑弹簧,第一支撑弹簧的底面抵触下模座,定位销的下部往上挤压下模板。As a preferred solution for the lower bending mold of the back plate, the elastic positioning device includes a positioning pin and a corresponding positioning hole, the positioning hole is arranged at the bottom of the upper template, the positioning pin passes through the lower template, and the bottom of the positioning pin is provided with a One support spring, the bottom surface of the first support spring is in contact with the lower mold base, and the bottom of the positioning pin presses the lower template upwards.

作为一种背板下折弯模具的优选方案,所述定位孔底部设置有缓冲弹簧。As a preferred solution of the bending mold under the back panel, a buffer spring is arranged at the bottom of the positioning hole.

作为一种背板下折弯模具的优选方案,所述下模板上设置有定位冲,定位冲的底部设置有第二支撑弹簧。As a preferred solution of the lower bending mold for the back plate, a positioning punch is arranged on the lower template, and a second support spring is arranged at the bottom of the positioning punch.

作为一种背板下折弯模具的优选方案,所述上模板和上模座之间以及下模板和下模座之间均设置有压簧。As a preferred solution of the lower bending mold for the back plate, compression springs are provided between the upper template and the upper mold holder and between the lower template and the lower mold holder.

作为一种背板下折弯模具的优选方案,所述上模组件和下模组件之间设有导向机构。As a preferred solution of the lower bending mold for the back panel, a guide mechanism is provided between the upper mold assembly and the lower mold assembly.

作为一种背板下折弯模具的优选方案,所述导向机构包括设置在上模板上的导柱和设置在下模板上的导向槽,所述导柱上设置有减震弹簧,所述导向槽与导柱相匹配。As a preferred solution for the lower bending mold of the back plate, the guide mechanism includes a guide post arranged on the upper template and a guide groove arranged on the lower template, the guide post is provided with a damping spring, and the guide groove Matches the guide posts.

本发明的有益效果为:The beneficial effects of the present invention are:

本发明提出一种背板下折弯模具,该背板下折弯模具的上膜组件设置有可活动的上衬板和设置在上模板上的入子,当上模组件和下模组件闭合时,通过上衬板与入子之间形成高度差,实现产品的下折弯成型。本发明有效解决现有的背板下折弯模具造成的加工精度低,生产稳定性差的问题,操作方便,加工精度高,便于维修,加工成本低。The present invention proposes a lower bending mold for a back panel. The upper membrane assembly of the lower bending mold for a back panel is provided with a movable upper liner and an insert on the upper template. When the parts are closed, the bottom bending forming of the product is realized through the height difference formed between the upper liner and the insert. The invention effectively solves the problems of low processing precision and poor production stability caused by the existing back plate lower bending mold, and has the advantages of convenient operation, high processing precision, convenient maintenance and low processing cost.

附图说明Description of drawings

图1是本发明实施方式提供的背板下折弯模具开模状态时的结构示意图;Fig. 1 is a schematic view of the structure of the bending mold under the back plate provided by the embodiment of the present invention in the mold opening state;

图2是图1中A处的局部放大图;Fig. 2 is a partial enlarged view of place A in Fig. 1;

图3是本发明实施方式提供的背板下折弯模具闭合状态时的结构示意图;Fig. 3 is a schematic structural view of the closed state of the bending mold under the back panel provided by the embodiment of the present invention;

图4是图3中B处的局部放大图。Fig. 4 is a partial enlarged view of B in Fig. 3 .

图中:In the picture:

1、上托板;2、上模座;3、上垫板;4、上模板;5、下模板;6、下垫板;7、下模座;8、下托板;9、入子;10、凹槽;11、上衬板;12、定位冲;13、定位销;14、第一支撑弹簧;15、压簧;16、第二支撑弹簧;17、背板;91、圆弧倒角。1. Upper supporting plate; 2. Upper mold base; 3. Upper backing plate; 4. Upper formwork; 5. Lower formwork; 6. Lower backing plate; 7. Lower mold base; 8. Lower supporting plate; 9. Insert ; Chamfer.

具体实施方式detailed description

为使本发明解决的技术问题、采用的技术方案和达到的技术效果更加清楚,下面将结合附图对本发明实施方式的技术方案作进一步的详细描述,显然,所描述的实施方式仅仅是本发明一部分实施方式,而不是全部的实施方式。基于本发明中的实施方式,本领域技术人员在没有作出创造性劳动前提下所获得的所有其他实施方式,都属于本发明保护的范围。In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the embodiments of the present invention will be further described in detail below in conjunction with the accompanying drawings. Obviously, the described embodiments are only the technical solutions of the present invention. Some implementations, not all implementations. Based on the implementation manners in the present invention, all other implementation manners obtained by those skilled in the art without creative efforts fall within the protection scope of the present invention.

在本发明的描述中,需要理解的是,术语“中心”、“纵向”、“横向”、“前”、“后”、“左”、“右”、“竖直”、“水平”、“顶”、“底”、“内”、“外”等指示的方位或位置关系为基于附图所示的方位或位置关系,仅是为了便于描述本发明和简化描述,而不是指示或暗示所指的装置或元件必须具有特定的方位、以特定的方位构造和操作,因此不能理解为对本发明保护范围的限制。In describing the present invention, it is to be understood that the terms "central", "longitudinal", "transverse", "front", "rear", "left", "right", "vertical", "horizontal", The orientations or positional relationships indicated by "top", "bottom", "inner", "outer", etc. are based on the orientations or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying The devices or elements referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore should not be construed as limiting the scope of the invention.

本实施方式提出一种新型背板下折弯模具,如图1至图4所示,该背板下折弯模具包括上模组件和下模组件,其中,上模组件包括自上而下依次可拆卸连接的上托板1、上模座2、上垫板3、可活动的上衬板11和上模板4。下模组件包括自上而下依次可拆卸连接的下模板5、下垫板6、下模座7、下支架以及下托板8。其中,上托板1和下托板8的设置能够方便拆装,更换模具。上垫板3和下垫板6的设置能够防止冲击力过大进而损伤上模座2和下模座7,起到一定的缓冲作用。This embodiment proposes a new type of back panel lower bending mold, as shown in Figures 1 to 4, the back panel lower bending mold includes an upper mold assembly and a lower mold assembly, wherein the upper mold assembly includes a And the upper supporting plate 1, the upper mold base 2, the upper backing plate 3, the movable upper lining plate 11 and the upper template 4 which are detachably connected successively. The lower mold assembly includes a lower formwork 5, a lower backing plate 6, a lower mold base 7, a lower bracket and a lower supporting plate 8 which are detachably connected sequentially from top to bottom. Wherein, the arrangement of the upper supporting plate 1 and the lower supporting plate 8 can facilitate disassembly and assembly, and replace the mould. The arrangement of the upper backing plate 3 and the lower backing plate 6 can prevent the impact force from being too large and damage the upper mold base 2 and the lower mold base 7, and play a certain buffering effect.

在本实施方式中,上模板4上设置有入子9,该入子9紧贴上衬板11设置,且底面与上模板4的底面相齐平。当上模组件与下模组件闭合时,入子9与上衬板11之间形成用于实现产品下折弯成型的高度差H(参见图4),如此,钣金件背板17在压合过程中完成下折弯成型,有效保证了下折弯的稳定性和可靠性,减少了折弯过程中的折弯阻力,降低了背板17产品因为折弯过程中的磨损而产生的不合格率,操作方便,加工精度高,便于维修,加工成本低。In this embodiment, an insert 9 is provided on the upper template 4 , and the insert 9 is arranged in close contact with the upper liner 11 , and the bottom surface is flush with the bottom surface of the upper template 4 . When the upper mold assembly and the lower mold assembly are closed, a height difference H is formed between the insert 9 and the upper liner 11 to realize the lower bending of the product (see Figure 4), so that the sheet metal back plate 17 The lower bending is completed during the pressing process, which effectively ensures the stability and reliability of the lower bending, reduces the bending resistance during the bending process, and reduces the wear and tear of the back plate 17 products due to the bending process. The failure rate is high, the operation is convenient, the processing precision is high, the maintenance is convenient, and the processing cost is low.

如图2和图4所示,入子9与下模板5相对的一侧设置有凹槽10,凹槽10的设置可方便背板的端部在冲压时预先形成上折弯结构。进一步的,凹槽10靠近上衬板11的侧壁为竖直面,使得背板的端部在冲压时预先形成与水平背板形成直角的上折弯结构,以备之后的直角下折弯成型奠定基础。As shown in Fig. 2 and Fig. 4, a groove 10 is provided on the opposite side of the insert 9 to the lower template 5, and the arrangement of the groove 10 facilitates the pre-forming of an upper bending structure at the end of the back plate during stamping. Further, the side wall of the groove 10 close to the upper backing plate 11 is a vertical surface, so that the end of the back plate is pre-formed with an upward bending structure forming a right angle with the horizontal back plate during stamping, for subsequent right-angle downward bending Forming the foundation.

如图2和图4所示,入子9与上衬板11相对的一侧底端设置有圆弧倒角91,不仅方便背板下弯折的加工操作,而且有效避免入子9的尖锐角划损背板17,加工精度高,产品质量高。As shown in Figure 2 and Figure 4, the bottom end of the insert 9 opposite to the upper liner 11 is provided with a circular arc chamfer 91, which not only facilitates the processing operation of the lower bending of the back plate, but also effectively avoids the sharpness of the insert 9. The back plate 17 is scratched at the corner, the processing precision is high, and the product quality is high.

进一步的,下模板4上设置有定位冲12,定位冲12的底部设置有第二支撑弹簧16,能够精确定位待加工产品。Further, the lower template 4 is provided with a positioning punch 12, and the bottom of the positioning punch 12 is provided with a second support spring 16, which can precisely position the product to be processed.

在本实施方式中,上模组件与下模组件之间设置有弹性定位装置。弹性定位装置包括定位销13和对应的定位孔(图中未示出),定位孔设置在上模板4的底部,定位销13穿过下模板5,定位销13的底部设置有第一支撑弹簧14,第一支撑弹簧14的底面抵触下模座7,定位销13的下部往上挤压下模板5。定位孔底部设置有缓冲弹簧。在缓冲弹簧自然伸展状态下,其下端部到定位孔外端面之间的长度为定位销13伸出工作面长度的二分之一至三分之二,使定位销13插入定位孔时能够收缩产生弹力。上模板4和上模座2之间设置有压簧15,下模板5和下模座7之间设置有压簧15,两处的压簧15可增加工作过程中的缓冲作用,提高冲压稳定性。In this embodiment, an elastic positioning device is provided between the upper mold assembly and the lower mold assembly. Elastic locating device comprises locating pin 13 and corresponding locating hole (not shown in the figure), and locating hole is arranged on the bottom of upper template 4, and locating pin 13 passes lower template 5, and the bottom of locating pin 13 is provided with first supporting spring 14. The bottom surface of the first support spring 14 is in contact with the lower mold base 7, and the lower part of the positioning pin 13 presses the lower mold plate 5 upward. A buffer spring is arranged at the bottom of the positioning hole. When the buffer spring is naturally stretched, the length between its lower end and the outer end surface of the positioning hole is 1/2 to 2/3 of the length of the positioning pin 13 protruding from the working surface, so that the positioning pin 13 can shrink when inserted into the positioning hole Produce elasticity. A compression spring 15 is provided between the upper template 4 and the upper mold base 2, and a compression spring 15 is provided between the lower template 5 and the lower mold base 7. The compression springs 15 at the two places can increase the buffering effect during the working process and improve the stamping stability. sex.

在使用过程中,上模组件向下运动,定位销13插入定位孔,上模组件继续向下运动,定位销13的上端面与缓冲弹簧下端部顶触,缓冲弹簧和第一支撑弹簧14、第二支撑弹簧16均收缩产生弹力,共同为上模板4的运动带来缓冲。第一支撑弹簧14和第二支撑弹簧16收缩使得定位销13底部挤压下模板5的力逐渐减小,即第一支撑弹簧14和第二支撑弹簧16对下模板5的支撑力逐渐减小,下模板5的压簧15和第一支撑弹簧14、第二支撑弹簧16共同支撑下模板5,当第一支撑弹簧14和第二支撑弹簧16对下模板5支撑力逐渐减小,下模板5的压簧15所受压力逐渐变大并收缩产生弹力,为上模板4接触下模板5时带来缓冲。上模组件向下运动速度越快,下模板5的压簧15给上模板4带来的缓冲作用越显著。上模板4接触下模板5之前,为缓冲弹簧、第一支撑弹簧14配合产生两重缓冲作用。上模板4接触下模板5时,缓冲弹簧、第一支撑弹簧14、第二支撑弹簧16、压簧15的配合共同产生缓冲作用。第一支撑弹簧14和第二支撑弹簧16对下模板5支撑力有一渐变过程,提高冲压稳定性和成品率,减少模具磨损,延长使用寿命。During use, the upper mold assembly moves downward, the positioning pin 13 is inserted into the positioning hole, the upper mold assembly continues to move downward, the upper end surface of the positioning pin 13 touches the lower end of the buffer spring, and the buffer spring and the first support spring 14. Both the second support springs 16 shrink to generate elastic force, which together provide buffer for the movement of the upper template 4 . The contraction of the first supporting spring 14 and the second supporting spring 16 makes the force that the bottom of the positioning pin 13 presses the lower template 5 gradually decrease, that is, the supporting force of the first supporting spring 14 and the second supporting spring 16 on the lower template 5 gradually decreases. , the compression spring 15 of the lower template 5, the first supporting spring 14, and the second supporting spring 16 jointly support the lower template 5, and when the first supporting spring 14 and the second supporting spring 16 gradually reduce the supporting force of the lower template 5, the lower template The suffered pressure of the stage clip 15 of 5 gradually increases and shrinks to generate elastic force, which brings buffering when the upper template 4 contacts the lower template 5. The faster the downward movement speed of the upper mold assembly, the more significant the buffering effect brought by the compression spring 15 of the lower template 5 to the upper template 4 . Before the upper template 4 contacts the lower template 5, the buffer spring and the first support spring 14 cooperate to produce double buffering effects. When the upper template 4 contacts the lower template 5, the cooperation of the buffer spring, the first supporting spring 14, the second supporting spring 16 and the compression spring 15 together produces a buffering effect. The first support spring 14 and the second support spring 16 have a gradual change process to the support force of the lower template 5, which improves stamping stability and yield, reduces die wear, and prolongs the service life.

上模组件和下模组件之间设有导向机构。导向机构包括设置在上模板4上的导柱和设置在下模板5上的导向槽,导柱上设置有减震弹簧,导向槽与导柱相匹配。通过导向机构的设置,能够在加工过程中对模具进行精确定位,提高加工精度。A guiding mechanism is arranged between the upper mold assembly and the lower mold assembly. The guide mechanism includes a guide post arranged on the upper template 4 and a guide groove arranged on the lower template 5, the guide post is provided with a damping spring, and the guide groove matches the guide post. Through the setting of the guide mechanism, the mold can be precisely positioned during the processing, and the processing accuracy can be improved.

以上结合具体实施方式描述了本发明的技术原理。这些描述只是为了解释本发明的原理,而不能以任何方式解释为对本发明保护范围的限制。基于此处的解释,本领域技术人员不需要付出创造性劳动即可联想到本发明的其它具体实施方式,这些方式都将落入本发明的保护范围之内。The technical principle of the present invention has been described above in conjunction with the specific embodiments. These descriptions are only for explaining the principles of the present invention, and cannot be construed as limiting the protection scope of the present invention in any way. Based on the explanations herein, those skilled in the art can think of other specific implementation modes of the present invention without creative effort, and these modes will all fall within the protection scope of the present invention.

Claims (10)

1. Bending Mould under a backboard, including upper die component and lower mold assemblies, described upper die component includes upper bolster (2), mobilizable upper liner plate (11) and cope match-plate pattern (4), described lower mold assemblies includes lower bolster (5) and die shoe (7), it is characterized in that, described cope match-plate pattern (4) is provided with into son (9), when upper die component and lower mold assemblies Guan Bi, described upper liner plate (11) and entering is formed for realizing the difference in height of bending and molding under product between son (9), between described upper die component and lower mold assemblies, elastic positioning device is set.
2. Bending Mould under backboard according to claim 1, it is characterised in that described in enter son (9) side relative with lower bolster (5) and be provided with groove (10).
3. Bending Mould under backboard according to claim 2, it is characterised in that described groove (10) is vertical plane near the sidewall of upper liner plate (11).
4. Bending Mould under backboard according to claim 1, it is characterised in that described in enter son (9) the side bottom relative with upper liner plate (11) and be provided with circular arc chamfering (91).
5. Bending Mould under backboard according to claim 1, it is characterized in that, described elastic positioning device includes alignment pin (13) and corresponding hole, location, hole, location is arranged on the bottom of cope match-plate pattern (4), alignment pin (13) traverse lower bolster (5), the bottom of alignment pin (13) is provided with the first support spring (14), first bottom surface conflict die shoe (7) supporting spring (14), the bottom of alignment pin (13) up extrudes lower bolster (5).
6. Bending Mould under backboard according to claim 5, it is characterised in that described location is provided with buffer spring bottom hole.
7. Bending Mould under backboard according to claim 5, it is characterised in that being provided with location punching (12) on described lower bolster (5), the bottom of location punching (12) is provided with the second support spring (16).
8. Bending Mould under backboard according to claim 1, it is characterized in that, between described cope match-plate pattern (4) and upper bolster (2) and between lower bolster (5) and die shoe (7), be provided with stage clip (15).
9. Bending Mould under backboard according to claim 1, it is characterised in that be provided with guiding mechanism between described upper die component and lower mold assemblies.
10. Bending Mould under backboard according to claim 9, it is characterized in that, described guiding mechanism includes the guide pillar being arranged on cope match-plate pattern (4) and the gathering sill being arranged on lower bolster (5), being provided with damping spring on described guide pillar, described gathering sill and guide pillar match.
CN201610288399.7A 2016-05-04 2016-05-04 Bending mold for back panel Pending CN105750421A (en)