CN105437326A - Solid wood plyboard resistant to pests, ants and water soaking - Google Patents
Solid wood plyboard resistant to pests, ants and water soaking Download PDFInfo
- Publication number
- CN105437326A CN105437326A CN201410521088.1A CN201410521088A CN105437326A CN 105437326 A CN105437326 A CN 105437326A CN 201410521088 A CN201410521088 A CN 201410521088A CN 105437326 A CN105437326 A CN 105437326A
- Authority
- CN
- China
- Prior art keywords
- solid wood
- plank
- plyboard
- plastic
- resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
An existing wood plyboard is not resistant to water soaking, and a solid wood plyboard resistant to water soaking is not available in the market. The biggest defect of solid wood is that the width of a board is not large enough, another defect of the solid wood is that the solid wood is prone to deformation, and all the defects can be overcome by making the solid wood into a wood plyboard. The bending resistance of a wood plyboard made of wood veneers is not as good as the solid wood. The bending resistance of the wood plyboard made of the solid wood can be greatly improved. However, an existing solid wood plyboard is not resistant to water soaking. A solid wood plyboard resistant to pests, ants and water soaking is formed by bonding a plurality of pieces of solid wood through plastic. Plastic molten paste has extremely high bonding performance, and the solid wood pieces can be tightly bonded after being cooled, so that the solid wood pieces are prevented from being separated, and the solid wood plyboard is kept complete. The plastic is a waterproof substance, the solid wood plyboard is wrapped in the plastic so that water can be prevented from entering the solid wood plyboard, and the service time of the solid wood plyboard is prolonged. Pests and ants do not eat the plastic, the solid wood plyboard is wrapped in the plastic so that the solid wood plyboard can be resistant to the infestation of pests, ants and fungi, and the service time of the solid wood plyboard is further prolonged.
Description
Immersion that current wooden splint is water funk, its bending resistance, not as good as solid wood, market has no not water funk solid wood clamping plate.
The maximum deficiency of solid wood is, plank width is large not, the easily distortion of another point, it is made wooden splint and just overcomes these deficiencies, but the present water funk immersion of solid wood clamping plate.
The pest-resistant ant that this technology proposes is not afraid of the solid wood clamping plate of water soaking, is called for short not water funk solid wood clamping plate, can helps the shortcoming overcoming above-mentioned existence.
Not water funk solid wood clamping plate, its beneficial effect is not afraid of water soaking, increases service time, expands range of application.
Pest-resistant ant is not afraid of the solid wood clamping plate of water soaking, and the technical scheme that its technical solution problem adopts is, with veneer, plank, plastics form; Its technique is: juggle is split into about one millimeter thin wood chip (1), the plank (2) of a few millimeters thick; Polylith plank, by plastic melting slurries, makes plastic melting slurries wrap up plank, and removing Unneeded plastic melts slurries (3), then pressurization makes plank be bonded together, plank can preheating, can being alternately staggered of each layer plank, obtains not water funk solid wood clamping plate (4) after cooling; Or, veneer is placed on the bottom surface of plank by after plank lid reality, simultaneously by plastic melting slurries, plastic melting slurries are made to wrap up wood chip plank, removing Unneeded plastic melts slurries, then pressurization makes plank wood chip be bonded together, and obtain the not water funk solid wood clamping plate (4) that veneer clamping plate are topped, thus the solid wood clamping plate making pest-resistant ant not be afraid of water soaking is run after cooling.As Fig. 1
The existing not water funk wooden splint of combination principle introduction:
With the wooden splint that veneer is made, its bending resistance, not as good as solid wood, makes wooden splint with solid wood, can increase substantially wooden splint bending resistance.
Plastics are water resistant materials, and water can be stoped to enter wooden splint.
Plastic melting pulp has very strong viscosity, wood tightly can be clung after cooling, makes wood not be separated, and makes wooden splint keep complete.
The preheating of wood chip plank, can make plastic melting slurries more easily enter in wood.
Plank is alternate to be staggered, and can improve solid wood clamping plate bending resistance.
Worm ant does not eat plastics, and wooden splint wraps up by plastics, can resist worm ant fungi and invade food, significantly increases wooden splint service time.
With the topped solid wood clamping plate of veneer clamping plate, solid wood clamping plate more beautiful can be made.
Figure of description illustrates:
Fig. 1: pest-resistant ant is not afraid of the solid wood clamping plate of water soaking
1 veneer, 2 planks, 3 plastic melting slurries, 4 not water funk solid wood clamping plate.
Claims (1)
1. pest-resistant ant is not afraid of the solid wood clamping plate of water soaking, it is characterized in that, with veneer, plank, plastics form; Its technique is: juggle is split into about one millimeter thin wood chip, the plank of a few millimeters thick; Polylith plank by plastic melting slurries, makes plastic melting slurries wrap up plank, and removing Unneeded plastic melts slurries, and then pressurization makes plank be bonded together, and plank can preheating, and can being alternately staggered of each layer plank, obtains not water funk solid wood clamping plate after cooling; Or, veneer is placed on the bottom surface of plank by after plank lid reality, simultaneously by plastic melting slurries, plastic melting slurries are made to wrap up wood chip plank, removing Unneeded plastic melts slurries, then pressurization makes plank wood chip be bonded together, and obtain the not water funk solid wood clamping plate that veneer clamping plate are topped, thus the solid wood clamping plate making pest-resistant ant not be afraid of water soaking is run after cooling.