CN105436826A - Surface treatment method of anti-theft door - Google Patents

Surface treatment method of anti-theft door Download PDF

Info

Publication number
CN105436826A
CN105436826A CN201510873164.XA CN201510873164A CN105436826A CN 105436826 A CN105436826 A CN 105436826A CN 201510873164 A CN201510873164 A CN 201510873164A CN 105436826 A CN105436826 A CN 105436826A
Authority
CN
China
Prior art keywords
theft door
drying room
surface treatment
temperature
antitheft door
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510873164.XA
Other languages
Chinese (zh)
Inventor
陈勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Jinchangcheng Technology Door Industry Co Ltd
Original Assignee
Suzhou Jinchangcheng Technology Door Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Jinchangcheng Technology Door Industry Co Ltd filed Critical Suzhou Jinchangcheng Technology Door Industry Co Ltd
Priority to CN201510873164.XA priority Critical patent/CN105436826A/en
Publication of CN105436826A publication Critical patent/CN105436826A/en
Pending legal-status Critical Current

Abstract

The invention discloses a surface treatment method of an anti-theft door. After a semi-finished anti-theft door is assembled and adjusted, the surface of the anti-theft door is cleaned and polished, surface treatment is performed through a scouring pad, and oil and dust on the surface are removed through a six-in-one phosphorizing solution; body powder is sprayed to the anti-theft door with oil removed, the anti-theft door is conveyed into a drying room to be dried at the temperature from 205 DEG C to 215 DEG C, the temperature is maintained for 18 min to 22 min, the anti-theft door is delivered out of the drying room, surface treatment is performed through the scouring pad, and therefore the adhesive force is higher; and high-intensity wood-grained paper is coated with transfer printing glue so that the surface of a door body can be covered with the high-intensity wood-grained paper, after color registration and shade drying are performed, the anti-theft door is fed into the high-temperature drying room, the drying temperature ranges from 145 DEG C to 155 DEG C, the temperature is maintained for 18 min to 22 min, the anti-theft door is delivered out of the drying room, the wood-grained paper is removed, surface treatment is performed for the third time through the scouring pad, electrostatic painting is performed, high-brightness glossy golden oil is sprayed, the anti-theft door is fed into the drying room again, the drying temperature ranges from 125 DEG C to 135 DEG C, the temperature is maintained for 14 min to 16 min, the anti-theft door is delivered out of the drying room, and the finished product is assembled. By the adoption of the method, the attractiveness and the feel of the anti-theft door are improved, the surface of the product is provided with pure solid wood grains, the grains are clean and are provided with the solid wood texture, the grade and the level of the anti-theft door are increased, and therefore the quality of the product is improved.

Description

A kind of surface treatment method of antitheft door
Technical field
The present invention relates to a kind of production method of antitheft door, particularly relate to a kind of surface treatment method of antitheft door.
Background technology
Antitheft door is the shop front of every household, and its outward appearance is the same with quality important.Existing antitheft door production technology generally comprises 9 steps, wherein comprise in step: oil removing, rust cleaning, phosphatization: in phosphating pond, door leaf and doorframe must in each ponds of phosphating pond, accumulative immersion just can enter subsequent processing in about 30 minutes, can ensure that surface of steel plate acidity causes embroidery material and cleaned up like this, and last layer phosphating coat, after being convenient in plastic-blasting operation, the adhesive force of molding powder.Gummed electric welding: by after the door-plate mid portion filled honeycomb paper of front and back or after anti-guncotton welds, shop front hydraulic test---Hot gluing machine, fastening sizing, making that the shop front is smooth can not modification.Plastic-blasting, transfer printing, water mill: to the specially treated technique of the shop front, guarantee the beautiful of shop front color and wood grain.Painting workshop will through spraying paint shop front bottoming, and washing is dried, the hot transfer printing of wood grain and the multiple working procedures such as drying and processing that oil.Reviewer checks every one link.Baking oven Lacquer finish: for solving the anti-ability of fading on fade by ultraviolet strong illumination problem, the palpus increase surface of steel door.Reviewer checks, with or without holiday, and stream paint.
In order to improve aesthetic feeling and the feel of antitheft door further, product surface is made to have pure solid wood lines, and clean mark there is solid wood texture, improve class and the grade of antitheft door, thus Improving The Quality of Products, need to carry out reformed AHP to original technique.
Summary of the invention
For overcoming the deficiencies in the prior art, the invention provides a kind of aesthetic feeling and the feel that improve antitheft door, make product surface have pure solid wood lines, and clean mark there is solid wood texture, improve class and the grade of antitheft door, thus the surface treatment method of the antitheft door of Improving The Quality of Products.
For achieving the above object, the technical solution adopted in the present invention is: a kind of surface treatment method of antitheft door, after antitheft door semi-finished product assembly and adjustment, first cleared up, polished in antitheft door surface, then carry out surface treatment with scouring pad, then use the six directions one Phosphating Solution to remove surperficial putty; By the antitheft door spray end powder after oil removing, send into drying room, baking temperature 205 ~ 215 DEG C, insulation 18 ~ 22min comes out of the stove, and uses scouring pad surface treatment, makes adhesive force stronger; By high strength woodgrained paper brush transfer printing glue, cover a surface, after chromatography is dried in the shade, enter high temperature drying room, baking temperature 145 ~ 155 DEG C, insulation 18 ~ 22min comes out of the stove, and uses the process of scouring pad three subsurface again after removing woodgrained paper, then electrostatic painting, spraying high brightness Lacquer finish polishes, then enter drying room, baking temperature 125 ~ 135 DEG C, insulation 14 ~ 16min comes out of the stove, and carries out finished product assembling.
Advantageous Effects of the present invention is: the operation pattern changing transfer printing in prior art, plastic-blasting, metallic paint, by multi step strategy and baking, improve aesthetic feeling and the feel of antitheft door, product surface is made to have pure solid wood lines, and clean mark there is solid wood texture, improve class and the grade of antitheft door, thus Improving The Quality of Products.
Detailed description of the invention
A surface treatment method for antitheft door, after antitheft door semi-finished product assembly and adjustment, first clears up antitheft door surface, polishes, and then carries out surface treatment with scouring pad, then uses the six directions one Phosphating Solution to remove surperficial putty; By the antitheft door spray end powder after oil removing, send into drying room, baking temperature 205 ~ 215 DEG C, insulation 18 ~ 22min comes out of the stove, and uses scouring pad surface treatment, makes adhesive force stronger; By high strength woodgrained paper brush transfer printing glue, cover a surface, after chromatography is dried in the shade, enter high temperature drying room, baking temperature 145 ~ 155 DEG C, insulation 18 ~ 22min comes out of the stove, and uses the process of scouring pad three subsurface again after removing woodgrained paper, then electrostatic painting, spraying high brightness Lacquer finish polishes, then enter drying room, baking temperature 125 ~ 135 DEG C, insulation 14 ~ 16min comes out of the stove, and carries out finished product assembling.
The present invention changes the operation pattern of transfer printing in prior art, plastic-blasting, metallic paint, by multi step strategy and baking, improve aesthetic feeling and the feel of antitheft door, product surface is made to have pure solid wood lines, and clean mark there is solid wood texture, improve class and the grade of antitheft door, thus Improving The Quality of Products.
Above embodiment is the explanation to content of the present invention, not as the restriction to content of the present invention, every those skilled in the art on basis disclosed in the application without creationary variation, all in the protection domain of the application.

Claims (1)

1. a surface treatment method for antitheft door, after antitheft door semi-finished product assembly and adjustment, first clears up antitheft door surface, polishes, and then carries out surface treatment with scouring pad, then uses the six directions one Phosphating Solution to remove surperficial putty; By the antitheft door spray end powder after oil removing, send into drying room, baking temperature 205 ~ 215 DEG C, insulation 18 ~ 22min comes out of the stove, and uses scouring pad surface treatment, makes adhesive force stronger; By high strength woodgrained paper brush transfer printing glue, cover a surface, after chromatography is dried in the shade, enter high temperature drying room, baking temperature 145 ~ 155 DEG C, insulation 18 ~ 22min comes out of the stove, and uses the process of scouring pad three subsurface again after removing woodgrained paper, then electrostatic painting, spraying high brightness Lacquer finish polishes, then enter drying room, baking temperature 125 ~ 135 DEG C, insulation 14 ~ 16min comes out of the stove, and carries out finished product assembling.
CN201510873164.XA 2015-12-03 2015-12-03 Surface treatment method of anti-theft door Pending CN105436826A (en)