CN105317153A - 虫蚁不食保温隔音千度不燃的铝玻板复合纸板 - Google Patents
虫蚁不食保温隔音千度不燃的铝玻板复合纸板 Download PDFInfo
- Publication number
- CN105317153A CN105317153A CN201410381772.4A CN201410381772A CN105317153A CN 105317153 A CN105317153 A CN 105317153A CN 201410381772 A CN201410381772 A CN 201410381772A CN 105317153 A CN105317153 A CN 105317153A
- Authority
- CN
- China
- Prior art keywords
- glass plate
- aluminium
- aluminium glass
- basin
- hollow body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
现在的不锈钢复合板用泡沫塑料填充,存在怕火和强度低,在火焰中其泡沫塑料燃烧,产生气体将包裹的不锈钢板破坏。铝玻板复合纸板,用铝玻板,不燃纸板做成;水玻璃是耐高温阻燃剂,使纸千度不燃;不燃纸板为弱碱性使虫蚁不食,真菌不生长;不燃纸板有许多空心孔,具有很好的保温隔音性能;水玻璃使纸板硬化,纸板燥干后质坚似木,坚硬耐用;铝玻板不会生锈;这些,使铝玻板复合纸板寿命超百年。纸板的碳分子和水玻璃的硅分子,在火焰中发生化学反应生成碳化硅。碳化硅是耐千几度高温的坚硬物质,所以火灾发生时,铝玻板复合纸板的刚性变化不大,能阻止火灾扩展。综上所述,铝玻板复合纸板是搭建厂房、简易房的最好建筑材料。
Description
纸容易燃烧;现在的不锈钢复合板,用泡沫塑料填充,它存在怕火和强度不够的缺点,在火焰中其泡沫塑料燃烧,产生的气体会将包裹的不锈钢板破坏;市场未见铝玻板复合纸板。
本技术提出的虫蚁不食保温隔音千度不燃的铝玻板复合纸板,简称铝玻板复合纸板,能帮助克服上述存在的缺点。
铝玻板复合纸板,其有益效果是,千度不燃,虫蚁不食,真菌不生长,保温隔音,坚硬耐用,寿命超百年。
虫蚁不食保温隔音千度不燃的铝玻板复合纸板,其解决技术问题所采用的技术方案是,用铝玻板,不燃纸板,水玻璃和耐高温粘合剂组成;其工艺是:耐高温粘合剂制作,用水玻璃和淀粉加热制成;铝玻板盆制作,使一块或多块耐高温玻璃网布通过铝熔浆,除去多余的铝熔浆,获得铝熔浆包裹玻璃网布板,得到铝玻板(1);可将铝玻板点焊成浅盆,浅盆的三边可高出另一边,并且向盆内成九十度角弯曲,送窑炉烧制,令浅盆各边熔粘,冷却后获得铝玻板盆(1);铝玻板空心体制作,可再用铝玻板点焊成空心体,空心体扁平,三侧面密封;送窑炉烧制,令空心体各边熔粘,冷却后获得铝玻板空心体(1);不燃纸厚板(2)可涂耐高温粘合剂后,放进铝玻板盆内,取合适的铝玻板,从铝玻板盆的低边推进铝玻板盆,将不燃纸厚板覆盖包裹紧密,获得铝玻板复合纸板(3),或者,不燃纸厚板(2)可用耐高温粘合剂涂后,由扁平的空心体侧面推进铝玻板空心体,取合适的铝玻板封密侧面,获得铝玻板复合纸板(3);从而令虫蚁不食保温隔音千度不燃的铝玻板复合纸板得以运行。如图1
现结合原理介绍铝玻板复合纸板:
不燃纸厚板制作,将废旧纸箱展平,用水玻璃浸透纸皮,除去多余的水玻璃后干燥,获得水玻璃纸皮;用耐高温粘合剂将多块水玻璃纸皮粘合成水玻璃纸皮厚板,可纵横错开相间排列的各块水玻璃纸皮板干燥后,获得不燃纸厚板。
水玻璃是耐高温阻燃剂,使纸皮千度不燃;水玻璃使纸皮硬化,纸板燥干后质坚似木;水玻璃为弱碱性物质,它使纸板含碱性,令虫蚁不能食、真菌不能生长,这样就令不燃纸厚板寿命超百年;铝玻板不会生锈,所以铝玻板复合纸板寿命超百年;将铝玻板做成盆或空心体,是为了使铝玻板能紧紧地将不燃纸厚板锁住,产生铝玻板紧紧包裹不燃纸厚板的作用,使铝玻板复合纸板的效果更好;各层不燃纸板纵横错开相间排列,能加强铝玻板复合纸板的抗弯曲性能;不燃纸厚板有很多空心孔,保温隔音性能良好;铝玻板复合纸板,以纸皮为主,不燃纸板厚度可超十几公分,铝玻板厚度不超二毫米,只起到作为不燃纸板的防水作用;铝只作为粘结玻璃网布使用,其用量不多,所以铝玻板,实际上是玻璃网布板;纸厚板的碳分子和水玻璃的硅分子,在火焰中发生化学反应生成碳化硅。碳化硅是耐千几度高温的坚硬物质,所以火灾发生时,铝玻板复合纸板的刚性变化不大,能阻止火灾扩展。
综上所述,铝玻板复合纸板是搭建厂房、简易房的最好建筑材料。
说明书附图说明:
图1:虫蚁不食保温隔音千度不燃的铝玻板复合纸板
1,铝玻板、铝玻板盆、铝玻板空心体,2不燃纸厚板,3铝玻板复合纸板。
Claims (1)
1.虫蚁不食保温隔音千度不燃的铝玻板复合纸板,其特征是,用铝玻板,不燃纸板,水玻璃和耐高温粘合剂组成;其工艺是:耐高温粘合剂制作,用水玻璃和淀粉加热制成;铝玻板盆制作,使一块或多块耐高温玻璃网布通过铝熔浆,除去多余的铝熔浆,获得铝熔浆包裹玻璃网布板,得到铝玻板;可将铝玻板点焊成浅盆,浅盆的三边可高出另一边,并且向盆内成九十度角弯曲,送窑炉烧制,令浅盆各边熔粘,冷却后获得铝玻板盆;铝玻板空心体制作,可再用铝玻板点焊成空心体,空心体扁平,三侧面密封;送窑炉烧制,令空心体各边熔粘,冷却后获得铝玻板空心体;不燃纸厚板可涂耐高温粘合剂后,放进铝玻板盆内,取合适的铝玻板,从铝玻板盆的低边推进铝玻板盆,将不燃纸厚板覆盖包裹紧密,获得铝玻板复合纸板,或者,不燃纸厚板可用耐高温粘合剂涂后,由扁平的空心体侧面推进铝玻板空心体,取合适的铝玻板封密侧面,获得铝玻板复合纸板;从而令虫蚁不食保温隔音千度不燃的铝玻板复合纸板得以运行。