CN105317129A - Aluminum glass plate composite stalk board with prevention gnawing of worn ants, heat preservation, sound insulation and no combustibility at thousand degrees - Google Patents
Aluminum glass plate composite stalk board with prevention gnawing of worn ants, heat preservation, sound insulation and no combustibility at thousand degrees Download PDFInfo
- Publication number
- CN105317129A CN105317129A CN201410384846.XA CN201410384846A CN105317129A CN 105317129 A CN105317129 A CN 105317129A CN 201410384846 A CN201410384846 A CN 201410384846A CN 105317129 A CN105317129 A CN 105317129A
- Authority
- CN
- China
- Prior art keywords
- glass plate
- aluminium
- stalk
- stalk board
- aluminium glass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The existing stainless steel composite board is filled with foamed plastic, is inflammable and is low in strength; since the foamed plastic is combusted in flame, a wrapped stainless steel plate is damaged by generated gas. An aluminum glass plate composite stalk board is made from an aluminum glass plate and a non-combustible stalk board; water glass is a high-temperature-resisting flame retardant, so that stalks are prevented from combusting at the thousand degrees; the non-combustible stalk board is weakly basic, so the gnawing of the worm ants is avoided, and fungi cannot grow on the non-combustible stalk board; the non-combustible stalk board is provided with multiple hollow holes and has good heat preservation and heat insulation properties; the stalk board is hardened by the water glass; after being dried, the stalk board is hard like wood and is durable; the aluminum glass plate does not rust; on the basis of the characteristics, the service life of the aluminum glass plate composite stalk board exceeds hundred years; carbon molecules of the stalk board and silicon molecules of the water glass generate chemical reaction in flame to generate silicon carbide; the silicon carbide is a hard substance resisting high temperature of thousands of years, so when fire occurs, the aluminum glass plate composite stalk board has little change in rigidity and can prevent the fire from spreading. In conclusion, the aluminum glass plate composite stalk board is an optimal building material for setting up factory buildings and makeshift houses.
Description
Cornstalk or sorghum stalk easily burn; Present stainless steel clad plate, fills with foamed plastics, and it exists inflammable and shortcoming that is insufficient strength, its foamed plastics burning in flame, and the corrosion resistant plate of parcel can destroy by the gas of generation; Market has no aluminium glass plate compound stalk plate.
The worm ant that this technology proposes does not eat the aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree does not fire, and is called for short aluminium glass plate compound stalk plate, can helps the shortcoming overcoming above-mentioned existence.
Aluminium glass plate compound stalk plate, its beneficial effect is, thousand degree do not fire, and ant does not eat worm, and fungi does not grow, heat preservation and soundproof, hard durable, and the life-span is super century-old.
Worm ant does not eat the aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree does not fire, and the technical scheme that its technical solution problem adopts is, with aluminium glass plate, does not fire stalk plate, water glass and high-temperature-resistant adhesive composition; Its technique is: high-temperature-resistant adhesive makes, and makes with water glass and heating starch; Aluminium glass plate basin makes, and makes one or more pyroceram screen cloth by the molten slurry of aluminium, removes the molten slurry of unnecessary aluminium, obtains aluminium molten slurry parcel glass web fabric swatch, obtains aluminium glass plate (1); Aluminium glass plate point can be welded into shallow basin, three limits of shallow basin can exceed another side, and become 90 degree of angular distortions in basin, send kiln to fire, make each limit of shallow basin fusible, obtain aluminium glass plate basin (1) after cooling; Aluminium glass plate hollow body makes, and can be welded into hollow body with aluminium glass plate point again, hollow body is flat, three side seals; Send kiln to fire, make each limit of hollow body fusible, after cooling, obtain aluminium glass plate hollow body (1); Stalk slab (2) do not fire after can be coated with high-temperature-resistant adhesive, put in aluminium glass plate basin, get suitable aluminium glass plate, advance aluminium glass plate basin from the low limit of aluminium glass plate basin, stalk slab will not be fired and cover parcel closely, obtain aluminium glass plate compound stalk plate (3), or, after not firing the available high-temperature-resistant adhesive painting of stalk slab (2), advance aluminium glass plate hollow body by flat hollow body side, get suitable aluminium glass plate and be sealed side, obtain aluminium glass plate compound stalk plate (3); Thus aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree do not fire is run to make worm ant not eat.As Fig. 1
Existing combination principle introduces aluminium glass plate compound stalk plate:
Do not fire stalk plate to make, corn or sorghum stalk removal of impurities are arranged, soaks into corn or sorghum stalk with water glass, dry after removing unnecessary water glass, obtain and do not fire stalk plate; With high-temperature-resistant adhesive polylith do not fired stalk plate be bonded into slab after dry, during bonding, each layer does not fire stalk plate and can stagger alternately in length and breadth, obtains and does not fire stalk slab.
Water glass is heat-resistant fireproof agent, and corn or sorghum stalk thousand degree are not fired; Water glass makes the stalk plate matter after dry doing hard like wood; Water glass is alkalescent material, and it makes stalk plate containing alkalescence, makes that worm ant can not eat, fungi can not grow, makes the aluminium glass plate compound stalk plate life-span super century-old; Aluminium glass plate is made basin or hollow body, is to make aluminium glass plate pin not firing stalk slab tightly, producing aluminium glass plate and tightly wrapping up the effect of not firing stalk slab, making the better effects if of aluminium glass plate compound stalk plate; Each layer does not fire stalk plate and staggers in length and breadth alternately, can strengthen the bending resistance of aluminium glass plate compound stalk plate; Do not fire stalk slab and have a lot of hollow hole, heat preservation and soundproof is functional; Aluminium glass plate compound stalk plate, based on corn or sorghum stalk, do not fire stalk plate thickness and can surpass tens centimeters, aluminium glass plate thickness does not surpass two millimeters, only plays the waterproof action as not firing stalk plate; Aluminium only uses as adhesive glass screen cloth, and its consumption is few, so aluminium glass plate, is actually glass web fabric swatch; , in flame, there is chemical reaction Formed SiClx in the carbon molecule of stalk plate and the silicon molecule of water glass.Carborundum is the hard material of resistance to thousand several years high temperature, so when fire occurs, the variation in rigidity of aluminium glass plate compound stalk plate is little, and fire can be stoped to expand.
In sum, aluminium glass plate compound stalk plate is the best constructional materials building factory building, lightly constructed and simply equipped building.
Figure of description illustrates:
Fig. 1: worm ant does not eat the aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree does not fire
1, aluminium glass plate, aluminium glass plate basin, aluminium glass plate hollow body, 2 do not fire stalk slab, 3 aluminium glass plate compound stalk plates.
Claims (1)
1. worm ant does not eat the aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree does not fire, and it is characterized in that, with aluminium glass plate, does not fire stalk plate, water glass and high-temperature-resistant adhesive composition; Its technique is: high-temperature-resistant adhesive makes, and makes with water glass and heating starch; Aluminium glass plate basin makes, and makes one or more pyroceram screen cloth by the molten slurry of aluminium, removes the molten slurry of unnecessary aluminium, obtains aluminium molten slurry parcel glass web fabric swatch, obtains aluminium glass plate; Aluminium glass plate point can be welded into shallow basin, three limits of shallow basin can exceed another side, and become 90 degree of angular distortions in basin, send kiln to fire, make each limit of shallow basin fusible, obtain aluminium glass plate basin after cooling; Aluminium glass plate hollow body makes, and can be welded into hollow body with aluminium glass plate point again, hollow body is flat, three side seals; Send kiln to fire, make each limit of hollow body fusible, after cooling, obtain aluminium glass plate hollow body; Stalk slab do not fire after can be coated with high-temperature-resistant adhesive, put in aluminium glass plate basin, get suitable aluminium glass plate, advance aluminium glass plate basin from the low limit of aluminium glass plate basin, stalk slab will not be fired and cover parcel closely, obtain aluminium glass plate compound stalk plate, or not firing stalk slab with after high-temperature-resistant adhesive painting, can advance aluminium glass plate hollow body by flat hollow body side, get suitable aluminium glass plate and be sealed side, obtain aluminium glass plate compound stalk plate; Thus aluminium glass plate compound stalk plate that heat preservation and soundproof thousand degree do not fire is run to make worm ant not eat.