CN105227705B - Housing unit moulding process - Google Patents

Housing unit moulding process Download PDF

Info

Publication number
CN105227705B
CN105227705B CN201510552146.1A CN201510552146A CN105227705B CN 105227705 B CN105227705 B CN 105227705B CN 201510552146 A CN201510552146 A CN 201510552146A CN 105227705 B CN105227705 B CN 105227705B
Authority
CN
China
Prior art keywords
housing unit
moulding process
transparent panel
lateral surface
frame
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201510552146.1A
Other languages
Chinese (zh)
Other versions
CN105227705A (en
Inventor
唐义梅
孙毅
廖新风
李勇
张伟
邹宏
胡志勤
王晓辉
刘兵
陈伟
许宇初
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Oppo Mobile Telecommunications Corp Ltd
Original Assignee
Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangdong Oppo Mobile Telecommunications Corp Ltd filed Critical Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority to CN201510552146.1A priority Critical patent/CN105227705B/en
Publication of CN105227705A publication Critical patent/CN105227705A/en
Application granted granted Critical
Publication of CN105227705B publication Critical patent/CN105227705B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of housing unit moulding process, the housing unit moulding process includes step:A translucent plate member and frame are provided, the frame has medial surface and is connected to the masking face of the medial surface;Step is processed in the periphery of the translucent plate member, obtains transparent panel, and the transparent panel has with step described in upper surface to be connected to the lateral surface of the upper surface and be connected to the step surface of the lateral surface;It is sticked on the lateral surface and the step surface and covers film, is plated to tear after anti-fingerprint film on the upper surface and described cover film;Coarse processing is carried out to the lateral surface and the step surface;Viscose glue is set on the lateral surface and the step surface;Medial surface described in the frame is assembled around the transparent panel and is adhered to the lateral surface through the viscose glue, the masking face is adhered to the step surface through the viscose glue;Wherein, the transparent panel and the frame enclosed around the transparent panel form housing unit.

Description

Housing unit moulding process
Technical field
The present invention relates to machine-shaping field, more particularly to a kind of housing unit moulding process.
Background technology
The housing unit applied to handset shell generally includes transparent panel and encloses the side around transparent panel at present Frame.And increasing housing unit develops just towards narrow black surround, without black surround visual effect, the usual periphery in transparent panel Step is set to realize narrow black surround, without black surround visual effect.But the step of transparent panel jail bonding with frame in such a structure Gu not enough, cause the performance of housing unit bad so that the production yield of the moulding process of housing unit is relatively low at present.
The content of the invention
In view of this, the present invention provides a kind of housing unit moulding process for improving production yield.
The present invention provides a kind of housing unit moulding process, and for molding housing unit, the housing unit includes saturating Bright panel and the frame around the transparent panel is enclosed, wherein, the housing unit moulding process includes step:
A translucent plate member and frame are provided, the frame has medial surface and is connected to the masking face of the medial surface;
Step is processed in the periphery of the translucent plate member, obtains transparent panel, the transparent panel has upper surface, institute State step and have to be connected to and the lateral surface of the upper surface and be connected to the step surface of the lateral surface;
It is sticked on the lateral surface and the step surface and covers film;
Anti-fingerprint film is plated on the upper surface, and is torn and described covered film;
Coarse processing is carried out to the lateral surface and the step surface;
Viscose glue is set on the lateral surface and the step surface;
The frame is assembled around the transparent panel, the medial surface is adhered to the lateral surface through the viscose glue, The masking face is adhered to the step surface through the viscose glue;
Wherein, the transparent panel and the frame enclosed around the transparent panel form housing unit.
Wherein, the housing unit moulding process also includes:
Polish the upper surface.
Wherein, in a translucent plate member and frame step is provided, the frame, which also has, is connected to the outer of the medial surface Surface;In the step of assembling the frame around the transparent panel, the outer surface with the upper surface is smooth connects.
Wherein, the housing unit moulding process also includes:
Common plating sets functional membrane on the outer surface and the upper surface.
Wherein, the housing unit moulding process also includes:
Deviate from the upper surface side ink for screen printing layer in the transparent panel, the ink layer cover the step surface and Orthographic projection region of the medial surface on the ink layer.
Wherein, the housing unit moulding process also includes:
In the transparent panel optical cement layer is coated with away from the upper surface side;
A display panel is provided, the display panel is adhered into the optical cement layer deviates from the transparent panel side.
Wherein, the translucent plate member uses glass material, and the frame uses plastic cement material.
Wherein, before viscose glue step being set on the lateral surface and the step surface, the lateral surface is covered with film At the neighbouring upper surface.
Wherein, before viscose glue step being set on the lateral surface and the step surface, the upper table is covered with diaphragm Face.
Wherein, before setting viscose glue step on the lateral surface and the step surface, in the step surface and described outer Groove is processed on side.
The housing unit moulding process of the present invention, by be sticked on the step surface and the lateral surface cover it is right after film The upper surface plating anti-fingerprint film of the translucent plate member, so as to avoid the step surface and the lateral surface from being plated anti-fingerprint film, from And avoid the lateral surface and the step surface roughness from reducing, and then the lateral surface and the step surface can be carried out thick Rough processing, so as to improve the roughness of the lateral surface and the step surface, so as to increase the viscose glue to the frame and institute The bonding dynamics of transparent panel is stated, and then the housing unit moulding process improves production yield.
Brief description of the drawings
In order to illustrate more clearly of technical scheme, the required accompanying drawing used in embodiment will be made below Simply introduce, it should be apparent that, drawings in the following description are only some embodiments of the present invention, general for this area For logical technical staff, on the premise of not paying creative work, other accompanying drawings can also be obtained according to these accompanying drawings.
Fig. 1 is the flow chart of housing unit moulding process provided by the invention;
Fig. 2 is the machining sketch chart of Fig. 1 housing unit moulding process;
Fig. 3 is the structural representation for the housing unit that Fig. 1 housing unit moulding process processes.
Embodiment
Below in conjunction with the accompanying drawing in the embodiment of the present invention, the technical scheme in embodiment of the present invention is carried out it is clear, It is fully described by.Obviously, described embodiment is a part of embodiment of the present invention, rather than whole embodiments. Based on the embodiment in the present invention, what those of ordinary skill in the art were obtained on the premise of creative work is not made Every other embodiment, it should all belong to the scope of protection of the invention.
Also referring to Fig. 1 to Fig. 3, a kind of housing unit moulding process of embodiment of the present invention offer, for being molded Go out housing unit 100, the housing unit 100 includes transparent panel 10 and frame 20, and the frame 20 is enclosed in described transparent Around panel 10, it is to be understood that the housing unit 100 be applied to mobile terminal on, the mobile terminal can be mobile phone, Tablet personal computer, notebook computer or liquid crystal display etc., the housing unit 100 it is to be appreciated that mobile phone or tablet personal computer, Or the decoration protecgulum for passing through display screen light is realized in notebook computer.The housing unit moulding process comprises the following steps:
Step S01:A translucent plate member 11 and frame 20 are provided, the inner side of frame 20 has medial surface 21 and is connected to institute State the masking face 22 of medial surface 21.
In present embodiment, the translucent plate member 11 can use glass material.The translucent plate member 11 can be passed through Pressure roller moulding process is obtained or obtained by cutting technique, be can also be and is prolonged pressure technique acquisition by pouring.It is described The light transmittance of isotropic disk part 11 need to reach more than 90%, can be provided well so that the housing unit 100 is applied to terminal Display effect.The flatness of the translucent plate member 11 is in 0.005mm~0.01mm, specific preferred 0.005mm, so that The smooth surface of housing unit 100, outward appearance is good, while facilitates the translucent plate member 11 to carry out plating and set up defences fingerprint film, to avoid The presentation quality of the translucent plate member 11 is influenceed, so as to improve the yield of the housing unit moulding process.The frame 20 passes through Shooting Technique is molded.The frame 20 also includes the outer surface 23 for being connected to the medial surface 21.In other embodiments, institute The flatness for stating translucent plate member 11 can also be 0.008mm.
Step S02:Step 12 is processed in the periphery of the translucent plate member 11, obtains the transparent panel 10, it is described Bright panel 10 has upper surface 111, and the step 12 has the lateral surface 121 for being connected to the upper surface 111 and is connected to institute State the step surface 122 of lateral surface 121.
In present embodiment, the vertical upper surface 111 of the lateral surface 121, the vertical outside of the step surface 122 Face 121, the lateral surface 121 protrude from the lateral surface 121.The step 12 can be in CNC milling machine, through milling plus Work forms, and the step 12 can also be in optics grinding machine, be formed through grinding.Processing the lateral surface 121 and described During step surface 122, roughing can be used, to increase the roughness of the lateral surface 121 and the step surface 122.At other In embodiment, the lateral surface 121 can also be with the upper surface 111 in obtuse angle or acute angle, the step surface 122 may be used also To be set with the lateral surface 121 in angle.
Step S03:Polish the upper surface 111.
In present embodiment, grinding process can be carried out to the upper surface 111 using sander, specifically, described The abrasive pastes that mesh number is F8000 are coated with upper surface 111, sanding and polishing are carried out to the upper surface 111 using sander, to increase Add the smoothness of the transparent panel 10, and then improve the light transmittance of the transparent panel 10.In other embodiments, also may be used To be to apply mesh number as F300 abrasive pastes in upper surface 111, it is processed by shot blasting.
Step S04:It is sticked on the lateral surface 121 and the step surface 122 and covers film 13, on the upper surface 111 Film 13 is covered described in being torn after plating anti-fingerprint film 131.
In present embodiment, the film 13 of covering can be PET film, and the film 13 of covering is to the He of lateral surface 121 The step surface 122 is protected.The film 13 of covering is completely covered by the lateral surface 121 and the step surface 122, so as to anti- Only the lateral surface 121 and the step surface 122 are coated with anti-fingerprint film, and then prevent the lateral surface 121 and the step The roughness in face 122 reduces, and then prevents that the lateral surface 121 and the adhesive strength of the step surface 122 are relatively low, so as to improve The bond strength of transparent panel 10 and the frame 20 is stated, after plating sets the anti-fingerprint film 131 in the upper surface 111, is torn It is described to cover film 13, continue to process on the step 12 to facilitate.In other embodiments, it is described cover film 13 can also It is hard transparent plate, the step surface 122 and the lateral surface 121 is covered with facilitating.
Step S05:Coarse processing is carried out to the lateral surface 121 and the step surface 122.
In present embodiment, tear it is described cover film 13 after, etch process can be used to the lateral surface 121 and described Step surface 122 etches decorative pattern, to increase the roughness of the lateral surface 121 and the step surface 122, so as to increase the outside Face 121 and the reinforcing degree bonding with viscose glue of the step surface 122, and then it is bonding with frame 20 strong to improve the transparent panel 10 Degree, to improve the production yield of the housing unit moulding process.In other embodiments, can also be using Milling Process Mode mill out coarse decorative pattern on the lateral surface 121 and the step surface 122, to increase the step surface 122 and institute State the roughness of lateral surface 121.
Step S06:Groove 123 is processed on the step surface 122 and the lateral surface 121.
Can use CNC milling machine equal milling on the lateral surface 121 and the step surface 122 in present embodiment Go out the groove 123 or the groove 123 is gone out using optics grinding machine.The section of the groove 123 is in semicircle Shape.In other embodiments, the groove 123 can also be rectangular recess, and the number of the groove can also be multiple;Institute It can also be after the step S04 to state step S06, implemented before the step S05.
Step S07:The lateral surface 121 is covered at the upper surface 111 with film 14.
In present embodiment, there is provided a film 14, the film 14 is attached at into the lateral surface 121 close to the upper table The edge in face 111, so as to be protected using the film 14 to the upper surface 111, prevent viscous on the lateral surface 121 Glue is spilled on the upper surface 111, so as to improve the presentation quality of the transparent panel 10, and then improves the housing unit 100 presentation quality, in other embodiments, the film 14 can also be to be replaced using tool, and the tool can cover The lateral surface 121 is at the upper surface 111.
Step S08:The upper surface 111 is covered with diaphragm 15.
In present embodiment, the diaphragm 15 can be PET film, and the diaphragm 15 is completely covered by the upper surface 111, the upper surface 111 is protected, prevents the upper surface 111 to be bonded with viscose glue, impurity, dust, or particulate matter etc. Pollutant.In other embodiments, it can also be and the upper surface covered using tool.The step S08 also may be used To be before the step S07.
Step S09:Viscose glue 16 is set on the lateral surface 121 and the step surface 122.
In present embodiment, the viscose glue 16 can be sprayed at the lateral surface 121 and the step surface using glue sprayer On 122, so as to reduce the production cycle of the housing unit moulding process, and then the life of the housing unit moulding process is improved Produce efficiency.
Step S10:The frame 20 is assembled around the transparent panel 10, the medial surface 21 is viscous through the viscose glue 16 The lateral surface 121 is connected to, the masking face 22 is adhered to the step surface 122 through the viscose glue 16.
In present embodiment, the outer surface 23 with the top face 111 is smooth connects so that the housing unit 100 presentation qualities improve.In other embodiments, the outer surface 23 can also be sets with the upper surface 111 in angle Put, to increase the narrow side visual effect of the housing unit 100.
Step S11:Common plating sets functional membrane 30 on the outer surface 23 and the upper surface 111.
In present embodiment, outer surface 23 and the transparent panel 10 of the frame 20 is completely covered in the functional membrane 30 Upper surface 111.The functional membrane 30 is anti-reflection film, so as to improve the light transmission of the housing unit 100, improves experience Property.In other implementations, the functional membrane 30 can also be rupture pressure disc, or frosted film.
Step S12:Deviate from the side ink for screen printing layer 17 of upper surface 111, the ink layer in the transparent panel 10 The orthographic projection region of the 17 coverings step surface 122 and the medial surface 21 on the ink layer 17.
In present embodiment, the ink layer 17 is white ink, utilizes the relatively described step surface 121 of the ink layer 17 Set, so that the ink layer 17 can be to blocking inside housing unit 100, and then avoid the transparent panel 10 Through and reflect the internal light of housing unit 100, and then avoid because of visual difference effect caused by refraction, it is described so as to improve The performance of housing unit 100, and then cause the housing unit moulding process to improve product quality.In other embodiment In, the ink layer 17 can also be black ink.
Step S13:In the transparent panel 10 optical cement layer 40 is coated with away from the side of upper surface 111.Using described Optical cement layer 40 can be bonded display panel, and have no effect on the translucency of the housing unit 100.
Step S14:One display panel 50 is provided, the display panel 50 is adhered to the optical cement layer 40 away from described The side of transparent panel 10.
The display panel 50 is bonded on the transparent panel 10, increases the use function of the housing unit 100, carries The suitability of the high housing unit 100.In present embodiment, display panel 50 can be LCD (Liquid Crystal Display, liquid crystal flat panel display) liquid crystal display or LCM (LCD Module, liquid crystal display die set) component.Display surface Plate 50 especially can be wide variety of touch screen, such as the display panel 50 can be that touch control layer is embedded into liquid crystal pixel In-cell touch screens or touch control layer be arranged at on-cell touch screens on liquid crystal pixel, can also be touch control layer The complete full sticking touch control screen for fitting in cover plate.
The housing unit moulding process of the present invention, by providing the translucent plate member with flat upper surface, so that institute The matching precision for stating translucent plate member and die cavity is improved, and then the outer framework is integrally formed out around the translucent plate member, profit With the outer framework top surface and the upper surface flush, so as to improve the Forming Quality of the outer framework, then to described outer Framework and the translucent plate member carry out milling, so as to facilitate smooth first outer surface to connect of milling and second appearance Face, the housing unit being made up of the frame and the transparent panel finally being obtained, the housing unit presentation quality improves, from And the production efficiency of the housing unit moulding process is improved.
Above is the preferred embodiment of the present invention, it is noted that for those skilled in the art, Under the premise without departing from the principles of the invention, some improvements and modifications can also be made, these improvements and modifications are also considered as this hair Bright protection domain.

Claims (10)

1. a kind of housing unit moulding process, it is characterised in that the housing unit moulding process includes step:
A translucent plate member and frame are provided, the frame has medial surface and is connected to the masking face of the medial surface;
Step is processed in the periphery of the translucent plate member, obtains transparent panel, and the transparent panel has a upper surface, described Rank, which has, to be connected to the lateral surface of the upper surface and is connected to the step surface of the lateral surface;
It is sticked on the lateral surface and the step surface and covers film, described cover is torn after anti-fingerprint film is plated on the upper surface Film, to prevent the lateral surface and the step surface to be coated with the anti-fingerprint film, to prevent the lateral surface and the step The roughness in face reduces, and improves the bond strength of the transparent panel and the frame;The film of covering is PET film or hard Translucent plate member;
Coarse processing is carried out to the lateral surface and the step surface;
Viscose glue is set on the lateral surface and the step surface;
Medial surface described in the frame is assembled around the transparent panel and is adhered to the lateral surface, the screening through the viscose glue Lee-side is adhered to the step surface through the viscose glue;
Wherein, the transparent panel and the frame enclosed around the transparent panel form housing unit.
2. housing unit moulding process according to claim 1, it is characterised in that the housing unit moulding process is also wrapped Include:
Polish the upper surface.
3. housing unit moulding process according to claim 1 a, it is characterised in that translucent plate member and frame step are being provided In rapid, the frame also has the outer surface for being connected to the medial surface;The frame is assembled around the transparent panel In step, the outer surface with the upper surface is smooth connects.
4. housing unit moulding process according to claim 3, it is characterised in that the housing unit moulding process is also wrapped Include:
Common plating sets functional membrane on the outer surface and the upper surface.
5. housing unit moulding process according to claim 1, it is characterised in that the housing unit moulding process is also wrapped Include:
Deviate from the upper surface side ink for screen printing layer in the transparent panel, the ink layer covers the step surface and described Orthographic projection region of the medial surface on the ink layer.
6. housing unit moulding process according to claim 1, it is characterised in that the housing unit moulding process is also wrapped Include:
In the transparent panel optical cement layer is coated with away from the upper surface side;
A display panel is provided, the display panel is adhered into the optical cement layer deviates from the transparent panel side.
7. housing unit moulding process according to claim 1, it is characterised in that the translucent plate member uses glass material Matter, the frame use plastic cement material.
8. housing unit moulding process according to claim 1, it is characterised in that in the lateral surface and the step surface Before upper setting viscose glue step, the lateral surface is covered at the upper surface with film.
9. housing unit moulding process according to claim 1, it is characterised in that in the lateral surface and the step surface Before upper setting viscose glue step, the upper surface is covered with diaphragm.
10. housing unit moulding process according to claim 1, it is characterised in that in the lateral surface and the step Before viscose glue step is set on face, groove is processed on the step surface and the lateral surface.
CN201510552146.1A 2015-08-31 2015-08-31 Housing unit moulding process Active CN105227705B (en)