CN105219364A - 钻井用堵漏材料 - Google Patents

钻井用堵漏材料 Download PDF

Info

Publication number
CN105219364A
CN105219364A CN201410267618.4A CN201410267618A CN105219364A CN 105219364 A CN105219364 A CN 105219364A CN 201410267618 A CN201410267618 A CN 201410267618A CN 105219364 A CN105219364 A CN 105219364A
Authority
CN
China
Prior art keywords
patching materials
drilling well
waste material
ceramic
material particle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410267618.4A
Other languages
English (en)
Inventor
祈琪
黄明
张宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHENGDU ZONGTONG PETROLEUM PARTS Co Ltd
Original Assignee
CHENGDU ZONGTONG PETROLEUM PARTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHENGDU ZONGTONG PETROLEUM PARTS Co Ltd filed Critical CHENGDU ZONGTONG PETROLEUM PARTS Co Ltd
Priority to CN201410267618.4A priority Critical patent/CN105219364A/zh
Publication of CN105219364A publication Critical patent/CN105219364A/zh
Pending legal-status Critical Current

Abstract

本发明提供一种钻井用堵漏材料,属于油田钻井工程领域。为解决现有石油天然气勘探中,井漏问题变得日益突出的问题,本发明提供一种廉价的钻井用堵漏材料,由以下重量份的原料组成:陶瓷废料颗粒20-30份;木质纤维素0.1-0.5份;聚丙烯酰胺2-5份;甲基纤维素0.2-0.5份。本发明提供的钻井用堵漏材料,堵漏效果好,具有较强的堵漏承压能力,相比纤维堵漏水泥浆该堵漏液堵漏能力更强,更能够适应复杂的井下漏失地层。

Description

钻井用堵漏材料
技术领域
本发明属于油田钻井工程领域,具体涉及一种钻井用堵漏材料。
背景技术
近年来,随着石油天然气勘探的进一步深入,井漏问题变得日益突出,因而堵漏成为许多井安全钻井所必需采取的措施,而结合漏层性质选择合适的堵漏材料是保证成功堵漏的必要条件。
随着社会经济及陶瓷工业的快速发展,陶瓷工业废料日益增多,它不仅对城市环境造成巨大压力,而且还限制了城市经济的发展及陶瓷工业的可持续发展,所以陶瓷工业废料的处理与利用非常重要。目前,我国陶瓷工业废料的处理与利用程度比较低,资金紧缺,致使大量废渣挤占耕地,使水和空气受到污染。特别是近20年的高速发展,陶瓷业随着产量的增加,废料的数量越来越多。根据不完全统计:仅佛山陶瓷产区,各种陶瓷废料的年产量已经超过400万吨,而全国陶瓷废料的年产量估计在1000万吨左右。如此大量的陶瓷废料已经不是简单填埋可以解决的问题,而且随着经济的日益发展和社会的进步,环境已经成为人们关注的焦点。陶瓷废料的堆积挤占土地,影响当地空气的粉尘含量;而陶瓷废料的填埋耗费人力物力,还污染地下水质。如何变废为宝,化废料为资源,已经成为科技和环保部门的当务之急。
目前,还未见将陶瓷废料作为原料进行生产堵漏材料。
发明内容
为解决上述问题,本发明提供一种钻井用堵漏材料,采用如下技术方案:
一种钻井用堵漏材料,其特征在于:所述堵漏材料按以下重量份的原料组成:
陶瓷废料颗粒20-30份;
木质纤维素0.1-0.5份;
聚丙烯酰胺2-5份;
甲基纤维素0.2-0.5份。
优选地,所述的陶瓷废料颗粒为粒径≦200目的陶瓷厂废料颗粒。
优选地,所述的陶瓷废料颗粒为有色废坯和废瓷砖中的一种或者两种的组合的粉碎颗粒。
本发明的有益效果如下:
1.本发明提供的一种钻井用堵漏材料,以采用陶瓷厂废料为主要原料,所以成本低,而且生产工艺简单,有利于工业化生产和推广应用。
2.本发明提供的一种钻井用堵漏材料,由于陶瓷容重小、内部多孔,形态、成分较均一,具有一定的强度和坚固性,因而制备而成的堵漏材料,具有较强的堵漏承压能力,相比纤维堵漏水泥浆该堵漏液堵漏能力更强,更能够适应复杂的井下漏失地层;采用本发明制成的堵漏液不仅具有良好的堵漏能力,且凝固后的水泥石强度较低,防止堵漏液凝固后钻塞较难而引起的“新井眼”问题。
具体实施方式
下面结合具体实施例对本发明进行详细说明。以下实施例将有助于本领域的技术人员进一步理解本发明,但不以任何形式限制本发明。应当指出的是,对本领域的普通技术人员来说,在不脱离本发明构思的前提下,还可以做出若干变形和改进。这些都属于本发明的保护范围。
实施例1
一种钻井用堵漏材料,其特征在于:所述堵漏材料按以下重量份的原料组成:
陶瓷废料颗粒20份;
木质纤维素0.5份;
聚丙烯酰胺2份;
甲基纤维素0.5份。
所述的陶瓷废料颗粒为粒径≦200目的陶瓷厂废料颗粒。
所述的陶瓷废料颗粒为有色废坯的粉碎颗粒。
实施例2
一种钻井用堵漏材料,其特征在于:所述堵漏材料按以下重量份的原料组成:
陶瓷废料颗粒30份;
木质纤维素0.1份;
聚丙烯酰胺5份;
甲基纤维素0.2份。
所述的陶瓷废料颗粒为粒径≦200目的陶瓷厂废料颗粒。
所述的陶瓷废料颗粒为废瓷砖的粉碎颗粒。
实施例3
一种钻井用堵漏材料,其特征在于:所述堵漏材料按以下重量份的原料组成:
陶瓷废料颗粒25份;
木质纤维素0.3份;
聚丙烯酰胺3份;
甲基纤维素0.4份。
所述的陶瓷废料颗粒为粒径≦200目的陶瓷厂废料颗粒。
所述的陶瓷废料颗粒为有色废坯和废瓷砖两种组合的粉碎颗粒。

Claims (3)

1.一种钻井用堵漏材料,其特征在于:所述堵漏材料按以下重量份的原料组成:
陶瓷废料颗粒20-30份;
木质纤维素0.1-0.5份;
聚丙烯酰胺2-5份;
甲基纤维素0.2-0.5份。
2.根据权利要求1所述的钻井用堵漏材料,其特征在于所述的陶瓷废料颗粒为粒径≦200目的陶瓷厂废料颗粒。
3.根据权利要求1所述的钻井用堵漏材料,其特征在于所述的陶瓷废料颗粒为有色废坯和废瓷砖中的一种或者两种的组合的粉碎颗粒。
CN201410267618.4A 2014-06-17 2014-06-17 钻井用堵漏材料 Pending CN105219364A (zh)