CN105217587A
CN105217587A CN201510685665.5A CN201510685665A CN105217587A CN 105217587 A CN105217587 A CN 105217587A CN 201510685665 A CN201510685665 A CN 201510685665A CN 105217587 A CN105217587 A CN 105217587A
Authority
CN
China
Prior art keywords
phosphate rock
ground phosphate
acid sludge
binding agent
acidity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510685665.5A
Other languages
Chinese (zh)
Inventor
杜建学
吴祥
黄天江
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YUNNAN TIANAN CHEMICAL Co Ltd
Original Assignee
YUNNAN TIANAN CHEMICAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YUNNAN TIANAN CHEMICAL Co Ltd filed Critical YUNNAN TIANAN CHEMICAL Co Ltd
Priority to CN201510685665.5A priority Critical patent/CN105217587A/en
Publication of CN105217587A publication Critical patent/CN105217587A/en
Pending legal-status Critical Current

Links

Abstract

Concentrated for warp in the two water thing method Wet-process Phosphoric Acid Production solid content produced is 10% ~ 20%, P by stone flour type ground phosphate rock binding agent 2o 5percentage composition be 40% ~ 47% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add ground silica or the limestone powder of 1 ~ 10% of acid sludge gross weight, adjustment acid sludge acidity quotient, to Mk=0.5 ~ 1.0, makes ground phosphate rock binding agent.After this binding agent and ground phosphate rock are uniformly mixed in proportion, enter pressure ball molding, roasting or oven dry, produce phosphorus ore pelletizing.The intermediate product that the present invention makes full use of Production Flow Chart as auxiliary material direct reuse in Production Flow Chart, by P in ground phosphate rock pelletizing 2o 5content improve 8 ~ 10%.Also can enter the shaping use of stove to the ground phosphate rock of acidity quotient Mk < 0.75 or Mk > 0.85, the pellet produced can enter stove without the need to additionally adding silica.Achieve efficient circulation and the comprehensive utilization of phosphate rock resource.

Description

Stone flour type ground phosphate rock binding agent
Technical field
The present invention relates to a kind of ground phosphate rock binding agent.
Technical background
Rock Phosphate (72Min BPL) is from exploitation, transport, to factory through processing treatment fed to boiler such as fragmentation, oven dry, screenings, lump ore amount only has about 50%, buy the qualified lump ore phosphorus through cleaning, usually also 15% ~ 20% to be lost, the ground phosphate rock enormous amount that the screening of phosphorus production enterprise is remaining, is not used and will causes the significant wastage of phosphor resource and serious financial loss." Yellow Phosphorus Industry entry criteria " that country implements explicitly calls for the breeze utilization ratio of yellow phosphorus enterprise to reach 100%.The technique that part phosphorus production enterprise attempts adopting ground phosphate rock to add clay or water glass dries as pelletizing after binding agent, in the hope of reaching the valuable phosphate rock resource of comprehensive utilization, reducing the object of product cost, but after adding clay or water glass, all reduces P in phosphorus ore 2o 5content, add the silicone content in ground phosphate rock, be not suitable for high silicon ground phosphate rock use.CN102381690 discloses medicament that a kind of rare earth element, sodium-chlor, calcium chloride, zinc chloride, sodium carbonate and salt of wormwood makes and montmorillonite powder in proportion, the powdered rock phosphate oxygen-enriched binder made after mixing, slaking, drying, ball grinds, but have that to add raw material numerous, making processes is tediously long and loaded down with trivial details, is difficult to the defects such as control and additional subsequent process after pyroreaction to the chemical composition in finished product and waste.
Summary of the invention
The object of this invention is to provide a kind of binding agent utilizing the intermediate product in two water thing method Wet-process Phosphoric Acid Production to make, P in phosphorus ore pelletizing can be improved 2o 5content, also can enter the shaping use of stove to the ground phosphate rock of acidity quotient deviation comparatively large (Mk < 0.75 or Mk > 0.85).This binding agent effectively overcomes the defect that prior art exists, and proposes the new technical scheme of a kind of efficient circulation and utilize resources synthetically.
The present invention is achieved through the following technical solutions:
Concentrated for warp in the two water thing method Wet-process Phosphoric Acid Production solid content produced is 10% ~ 20%, P by a kind of ground phosphate rock binding agent 2o 5percentage composition be 40% ~ 47% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add ground silica or the limestone powder of 1 ~ 10% of acid sludge gross weight, adjustment acid sludge acidity quotient, to Mk=0.5 ~ 1.0, makes ground phosphate rock binding agent.
After the ground phosphate rock of this binding agent and acidity quotient Mk < 0.75 or Mk > 0.85 is uniformly mixed in proportion, dried by pressure ball molding or granulating roasting operation, with the production requirement of the phosphorus ore pellet that to meet into stove acidity quotient be Mk=0.75 ~ 0.85.
The intermediate product that the present invention makes full use of Production Flow Chart as auxiliary material direct reuse in Production Flow Chart, namely with the middle acid sludge of two water thing method wet method phosphoric acid manufacture process after adjustment acidity, make and produce ground phosphate rock pelletizing binding agent used, by P in ground phosphate rock pelletizing 2o 5content improve 8 ~ 10%.Also can enter the shaping use of stove to the ground phosphate rock of acidity quotient Mk < 0.75 or Mk > 0.85, the pellet produced can enter stove without the need to additionally adding silica.Achieve efficient circulation and the comprehensive utilization of phosphate rock resource.
Accompanying drawing explanation
Accompanying drawing 1 is production schematic diagram of the present invention.
Embodiment
Following embodiment is intended to describe in further detail and explain the present invention, instead of limits the present invention by any way.Those of ordinary skill in the art's any simple modifications made for the present invention and replacement, all should fall within protection scope of the present invention.
Embodiment 1
Concentrated for warp in the two water thing method Wet-process Phosphoric Acid Production solid content produced is 10%, P by a kind of ground phosphate rock binding agent 2o 5percentage composition be 47% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add the limestone powder of 10% of acid sludge gross weight, adjustment acid sludge acidity quotient, to Mk=0.5, makes ground phosphate rock binding agent.
After the ground phosphate rock of this binding agent and acidity quotient Mk=1.0 is uniformly mixed in proportion, is dried by pressure ball molding or granulating roasting operation, produce phosphorus ore pelletizing.With the production requirement of the phosphorus ore pellet that to meet into stove acidity quotient be Mk=0.80.P in ground phosphate rock pelletizing 2o 5content improve 10%.
Embodiment 2
Concentrated for warp in the two water thing method Wet-process Phosphoric Acid Production solid content produced is 15%, P by a kind of ground phosphate rock binding agent 2o 5percentage composition be 45% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add the ground silica of 1% of acid sludge gross weight, maintain acid sludge acidity quotient Mk=0.79, make ground phosphate rock binding agent.
This binding agent and acidity quotient are, after the ground phosphate rock of Mk=0.9 is uniformly mixed in proportion, is dried or granulating roasting operation, produce phosphorus ore pelletizing by pressure ball molding.With the production requirement of the phosphorus ore pellet that to meet into stove acidity quotient be Mk=0.81.P in ground phosphate rock pelletizing 2o 5content improve 9%.
Embodiment 3
Concentrated for warp in the two water thing method Wet-process Phosphoric Acid Production solid content produced is 20%, P by a kind of ground phosphate rock binding agent 2o 5percentage composition be 40% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add the ground silica of 10% of acid sludge gross weight, adjustment acid sludge acidity quotient, to Mk=1.0, makes ground phosphate rock binding agent.
After the ground phosphate rock of this binding agent and acidity quotient Mk=0.5 is uniformly mixed in proportion, is dried by pressure ball molding or granulating roasting operation, produce phosphorus ore pelletizing.With the production requirement of the phosphorus ore pellet that to meet into stove acidity quotient be Mk=0.80.P in ground phosphate rock pelletizing 2o 5content improve 8%.

Claims (1)

1. a stone flour type ground phosphate rock binding agent, is characterized in that: by two water thing method Wet-process Phosphoric Acid Production through the concentrated solid content produced be 10% ~ 20%, P 2o 5percentage composition be 40% ~ 47% acid sludge be stored in acid sludge groove, pump into acidity regulator with acid sludge pump, add ground silica or the limestone powder of 1 ~ 10% of acid sludge gross weight, adjustment acid sludge acidity quotient, to Mk=0.5 ~ 1.0, makes ground phosphate rock binding agent.
CN201510685665.5A 2015-10-22 2015-10-22 Stone flour type ground phosphate rock binding agent Pending CN105217587A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510685665.5A CN105217587A (en) 2015-10-22 2015-10-22 Stone flour type ground phosphate rock binding agent

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510685665.5A CN105217587A (en) 2015-10-22 2015-10-22 Stone flour type ground phosphate rock binding agent

Publications (1)

Publication Number Publication Date
CN105217587A true CN105217587A (en) 2016-01-06

Family

ID=54986945

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510685665.5A Pending CN105217587A (en) 2015-10-22 2015-10-22 Stone flour type ground phosphate rock binding agent

Country Status (1)

Country Link
CN (1) CN105217587A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108249411A (en) * 2018-01-02 2018-07-06 昆明理工大学 A kind of ground phosphate rock or broken phosphorus ore binding agent preparation method and type ore deposit production method

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102381690A (en) * 2010-12-03 2012-03-21 宣威市恒邦磷化工业有限公司 Powdered rock phosphate oxygen-enriched binder
CN102701164A (en) * 2012-01-04 2012-10-03 张兴华 Processing method for preparing phosphate rock powder into pellet yellow phosphorus charge
CN103964404A (en) * 2014-04-24 2014-08-06 贵州省惠水川东化工有限公司 Method for producing powdered rock phosphate balls by using powdered rock phosphate
CN104229762A (en) * 2014-09-24 2014-12-24 云南天安化工有限公司 Short-process defluorination technology of phosphorite powder for producing yellow phosphorus
CN104261363A (en) * 2014-09-24 2015-01-07 云南天安化工有限公司 Method for granulating, molding and calcining ground phosphorite

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102381690A (en) * 2010-12-03 2012-03-21 宣威市恒邦磷化工业有限公司 Powdered rock phosphate oxygen-enriched binder
CN102701164A (en) * 2012-01-04 2012-10-03 张兴华 Processing method for preparing phosphate rock powder into pellet yellow phosphorus charge
CN103964404A (en) * 2014-04-24 2014-08-06 贵州省惠水川东化工有限公司 Method for producing powdered rock phosphate balls by using powdered rock phosphate
CN104229762A (en) * 2014-09-24 2014-12-24 云南天安化工有限公司 Short-process defluorination technology of phosphorite powder for producing yellow phosphorus
CN104261363A (en) * 2014-09-24 2015-01-07 云南天安化工有限公司 Method for granulating, molding and calcining ground phosphorite

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108249411A (en) * 2018-01-02 2018-07-06 昆明理工大学 A kind of ground phosphate rock or broken phosphorus ore binding agent preparation method and type ore deposit production method

Similar Documents

Publication Publication Date Title
CN104261363B (en) A kind of ground phosphate rock granulating and forming roasting method
CN101767972B (en) Mine tailing sand brick and preparation method thereof
CN103964404B (en) Ground phosphate rock is utilized to produce the method for the phosphorus ore sphere of powder
CN104891461A (en) Method for producing yellow phosphorus from phosphate rock powder and carbon powder
CN109734344A (en) A method of cement retarder is prepared using half water ardealite
CN104072003B (en) A kind of titanium gypsum prepares the method for cement retarder
CN102910888A (en) Mixed material for filling mine roadway
CN106435170B (en) A kind of Basic Pellets preparation method and preparation and mineral powder mixed material used
CN104710150A (en) Imitation wood grain decorative plate and preparation method thereof
CN105217587A (en) Stone flour type ground phosphate rock binding agent
US9309160B2 (en) Ceramic tile products and manufacturing method thereof
CN103468240B (en) Ultralow-density ceramsite proppant with flint clay tailings as raw materials and preparation method of ultralow-density ceramsite proppant
CN104261368B (en) A kind of method that ground phosphate rock pressure ball molding is dried
CN109809726B (en) Tungsten smelting waste residue ceramsite without additive components and preparation method thereof
CN104310416A (en) Method for preparing high-brightness superfine calcined kaolin
CN101913571B (en) Technological process for producing calcium superphosphate by using low-grade phosphate ores
CN104003742A (en) Method for preparing magnesium-silicon sand by high-silicon magnesite tailings
CN102910890A (en) Baked brick made of granulated slag and preparation process of baked bricks
CN105217586A (en) Liquid-solid phase adjusting type ground phosphate rock binding agent
CN104261362B (en) A kind of ground phosphate rock pressure ball molding method of roasting
CN104823748A (en) Method for preparing artificial soil combination from red mud by Bayer method and obtained artificial soil combination
CN103936308B (en) Excite the method for the slag early hydration activity for the production of cement
CN108341731A (en) A kind of fireworks solid flashing composition
CN104261365B (en) A kind of enrichment pelletizing method of low grade rock phosphate
CN107337359A (en) A kind of lime stone slag and stone powder waste material renovation process

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20160106

RJ01 Rejection of invention patent application after publication