CN105199485A - 一种耐磨环保涂料及其制备方法 - Google Patents

一种耐磨环保涂料及其制备方法 Download PDF

Info

Publication number
CN105199485A
CN105199485A CN201510668906.5A CN201510668906A CN105199485A CN 105199485 A CN105199485 A CN 105199485A CN 201510668906 A CN201510668906 A CN 201510668906A CN 105199485 A CN105199485 A CN 105199485A
Authority
CN
China
Prior art keywords
parts
diatomite
water
silicon nitride
glass bead
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510668906.5A
Other languages
English (en)
Inventor
谢军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510668906.5A priority Critical patent/CN105199485A/zh
Publication of CN105199485A publication Critical patent/CN105199485A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种耐磨环保涂料,按质量分数包括:硅藻土30-50份、硅藻土负载纳米TiO2材料10-15份、坡缕石5-10份、玻化微珠8-12份、气相二氧化硅2-2.4份、羟丙基甲基纤维素3-6份、无机铝盐防水剂1-1.3份、硅酸镁铝0.5-1.5份、400目氮化硅3-5份、白竹炭5-6份、1076抗氧剂2-3份和水100-125份。将硅藻土、硅藻土负载纳米TiO2材料、坡缕石放入高速粉碎机中,密封,在8000-15000r/min的转速下剪切30-60秒,出主料:向主料中依次加入玻化微珠、气相二氧化硅、羟丙基甲基纤维素、无机铝盐防水剂、硅酸镁铝、400目氮化硅、白竹炭、1076抗氧剂、水后,搅拌5-8分钟即可。

Description

一种耐磨环保涂料及其制备方法
技术领域
本发明涉及一种涂料,具体说是一种卧室耐磨环保涂料及其制备方法。
背景技术
在装修中,家具板材、地板板材中无可避免的存在甲醛等有害物质,严重危害人体。现有市售比较流行的抗甲醛、吸甲醛涂料大都采用硅藻土作为原料,但现有涂料大量采用树脂、胶粉等传统涂料原料,堵塞硅藻土空隙,降低其吸附效果,影响其使用性能。
发明内容
针对现有技术的上述不足,本发明提供了一种使用性能优异、稳定、效果好的耐磨环保涂料及其制备方法。
本发明采用的技术方案是:一种耐磨环保涂料,其特征在于:按质量分数包括:硅藻土30-50份、硅藻土负载纳米TiO2材料10-15份、坡缕石5-10份、玻化微珠8-12份、气相二氧化硅2-2.4份、羟丙基甲基纤维素3-6份、无机铝盐防水剂1-1.3份、硅酸镁铝0.5-1.5份、400目氮化硅3-5份、白竹炭5-6份、1076抗氧剂2-3份和水100-125份。
一种耐磨环保涂料制备方法,其特征在于:包括以下步骤:将硅藻土30-50份、硅藻土负载纳米TiO2材料10-15份、坡缕石5-10份放入高速粉碎机中,密封,在8000-15000r/min的转速下剪切30-60秒,出主料:向主料中依次加入玻化微珠8-12份、气相二氧化硅2-2.4份、羟丙基甲基纤维素3-6份、无机铝盐防水剂1-1.3份、硅酸镁铝0.5-1.5份、400目氮化硅3-5份、白竹炭5-6份、1076抗氧剂2-3份、水100-125份后,搅拌5-8分钟即可。
采用上述技术方案,本发明的有益效果是:采用硅藻土、硅藻土负载纳米TiO2材料、坡缕石共混,有效扩大硅藻土主料孔径60-80%,提高和稳定吸附能力,避免涂料中辅料堵塞;玻化微珠结合坡缕石提高其绝热﹑耐热、防火﹑吸音﹑保温性能。气相二氧化硅用作涂料防沉、增稠、防流挂的助剂,调节自由流动和作为抗结块剂来改善性质,具有良好的补强、增稠、触变、消光、抗紫外线和杀菌等多种作用,辅助吸附有害物质。无机铝盐防水剂提高其防水性能,结合硅酸镁铝悬浮增稠,配合氮化硅提高其耐磨性能和促进摩擦耐热性能。1076抗氧剂抗氧化能力强,延长了其使用寿命,确保在高温高热高湿度的厨房场合下的使用稳定性和安全卫生。
具体实施方式
以下结合实施例作进一步说明。
实施例一
一种耐磨环保涂料,按质量分数包括:硅藻土30份、硅藻土负载纳米TiO2材料10份、坡缕石5份、玻化微珠8份、气相二氧化硅2份、羟丙基甲基纤维素3份、无机铝盐防水剂1份、硅酸镁铝0.5份、400目氮化硅3份、白竹炭5份、1076抗氧剂2份和水100份。
一种耐磨环保涂料制备方法,包括以下步骤:将硅藻土30份、硅藻土负载纳米TiO2材料10份、坡缕石5份放入高速粉碎机中,密封,在8000r/min的转速下剪切60秒,出主料:向主料中依次加入玻化微珠8份、气相二氧化硅2份、羟丙基甲基纤维素3份、无机铝盐防水剂1份、硅酸镁铝0.5份、400目氮化硅3份、白竹炭5份、1076抗氧剂2份、水100份后,搅拌5分钟即可。
实施例二
一种耐磨环保涂料,按质量分数包括:硅藻土50份、硅藻土负载纳米TiO2材料15份、坡缕石10份、玻化微珠12份、气相二氧化硅2.4份、羟丙基甲基纤维素6份、无机铝盐防水剂1.3份、硅酸镁铝1.5份、400目氮化硅5份、白竹炭6份、1076抗氧剂3份和水125份。
一种耐磨环保涂料制备方法,包括以下步骤:将硅藻土50份、硅藻土负载纳米TiO2材料15份、坡缕石10份放入高速粉碎机中,密封,在15000r/min的转速下剪切30秒,出主料:向主料中依次加入玻化微珠12份、气相二氧化硅2.4份、羟丙基甲基纤维素6份、无机铝盐防水剂1.3份、硅酸镁铝1.5份、400目氮化硅5份、白竹炭6份、1076抗氧剂3份、水125份后,搅拌8分钟即可。
实施例三
一种耐磨环保涂料,按质量分数包括:硅藻土40份、硅藻土负载纳米TiO2材料12份、坡缕石8份、玻化微珠10份、气相二氧化硅2.3份、羟丙基甲基纤维素5份、无机铝盐防水剂1.1份、硅酸镁铝1份、400目氮化硅4份、白竹炭5.5份、1076抗氧剂2.5份和水120份。
一种耐磨环保涂料制备方法,包括以下步骤:将硅藻土40份、硅藻土负载纳米TiO2材料12份、坡缕石8份放入高速粉碎机中,密封,在12000r/min的转速下剪切45秒,出主料:向主料中依次加入玻化微珠10份、气相二氧化硅2.3份、羟丙基甲基纤维素5份、无机铝盐防水剂1.1份、硅酸镁铝1份、400目氮化硅4份、白竹炭5.5份、1076抗氧剂2.5份、水120份后,搅拌6.5分钟即可。

Claims (2)

1.一种耐磨环保涂料,其特征在于:按质量分数包括:硅藻土30-50份、硅藻土负载纳米TiO2材料10-15份、坡缕石5-10份、玻化微珠8-12份、气相二氧化硅2-2.4份、羟丙基甲基纤维素3-6份、无机铝盐防水剂1-1.3份、硅酸镁铝0.5-1.5份、400目氮化硅3-5份、白竹炭5-6份、1076抗氧剂2-3份和水100-125份。
2.一种耐磨环保涂料制备方法,其特征在于:包括以下步骤:将硅藻土30-50份、硅藻土负载纳米TiO2材料10-15份、坡缕石5-10份放入高速粉碎机中,密封,在8000-15000r/min的转速下剪切30-60秒,出主料:向主料中依次加入玻化微珠8-12份、气相二氧化硅2-2.4份、羟丙基甲基纤维素3-6份、无机铝盐防水剂1-1.3份、硅酸镁铝0.5-1.5份、400目氮化硅3-5份、白竹炭5-6份、1076抗氧剂2-3份、水100-125份后,搅拌5-8分钟即可。
CN201510668906.5A 2015-10-13 2015-10-13 一种耐磨环保涂料及其制备方法 Pending CN105199485A (zh)