CN105128561A - Manufacturing method of biting preventing wooden pencil - Google Patents

Manufacturing method of biting preventing wooden pencil Download PDF

Info

Publication number
CN105128561A
CN105128561A CN201510539345.9A CN201510539345A CN105128561A CN 105128561 A CN105128561 A CN 105128561A CN 201510539345 A CN201510539345 A CN 201510539345A CN 105128561 A CN105128561 A CN 105128561A
Authority
CN
China
Prior art keywords
pencil
board
parts
portions
pencil board
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510539345.9A
Other languages
Chinese (zh)
Inventor
朱建青
朱凯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bengbu Shenlong Pencils Co Ltd
Original Assignee
Bengbu Shenlong Pencils Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bengbu Shenlong Pencils Co Ltd filed Critical Bengbu Shenlong Pencils Co Ltd
Priority to CN201510539345.9A priority Critical patent/CN105128561A/en
Publication of CN105128561A publication Critical patent/CN105128561A/en
Pending legal-status Critical Current

Abstract

The invention relates to the field of pencil production and processing, in particular to a manufacturing method of a biting preventing wooden pencil. The manufacturing method is characterized by comprising the following steps: (1) steaming a pencil board, putting the steamed pencil board in a furnace kiln, and then steaming the pencil board again for 30 minutes; (2) leveling the steamed pencil board, pressing the pencil board leveled by a leveling machine, and heating the pencil board during the pressing process; (3) planing the pencil board into a grooved board, which is 4.1-4.2 mm thick and is provided with a core groove corresponding to a lead core in diameter, by a recessing machine, then gluing the lead core with the pencil board with an adhesive, and after heating at 50-120 DEG C and drying for 1-8 hours in the clamping state, processing the glued material into a white bar pencil, which is 178-180 mm long, by a bar planning machine; and (4) polishing the white bar pencil into the wooden pencil. Through the adoption of the manufacturing method, the condition that children bit pen points during the pencil using process can be effectively prevented.

Description

A kind of preparation method of anti-bite Wood pencil
Technical field:
The present invention relates to pencil production and processing field, more specifically to a kind of preparation method of anti-bite Wood pencil.
Background technology:
Pencil is a kind of class being used for writing and drawing sketch is special, apart from the history of modern existing more than 400 year, pencil type includes: " log penholder ", " sharpening penholder ", " band cap pencil ", " common penholder ", be exactly that pencil-lead rod is pushed down by pencil manufacturer, this pencil could use after needing consumer to be cut out by nib; A fritter rubber is had in addition at the end of common lead penholder, when clerical error, can pen erasure error conversely, more convenient, invented by artist Oman of the U.S.." sharpening penholder ", a kind of exactly pencil half product pencil shaft being processed certain length nib and carry out selling, " band cap pencil ", combined by pencil shaft and pencil cap exactly, in pencil use procedure, particularly children, have the hobby of stinging nib, pencil is containing a large amount of bacterium in process layer by layer, and children sting nib can produce harmful effect to health.
Summary of the invention:
Technical problem to be solved by this invention is to overcome the preparation method that existing technological deficiency provides a kind of anti-bite Wood pencil.
Technical problem to be solved by this invention adopts following technical scheme to realize:
A preparation method for anti-bite Wood pencil, is characterized in that comprising the following steps:
(1) spray is carried out to pencil board and steam process, be placed in stove, then spray steaming carried out 30 minutes to pencil board;
(2) steam to spray the pencil board terminated and carry out smooth process, pencil board by flattening, heats pencil board in pressing process by use planisher, by flattening 2 hours time, and heating-up temperature 130 DEG C, 1 hour heat time;
(3) thickness is become to be 4.1 ~ 4.2mm pencil board planer with keyway planer, and have the frid of the core groove adapted with lead core diameter, then adhesive is used lead for retractable pencil and pencil board gummed to be got up, heat (50 ~ 120 DEG C) in the clamp state after dry 1 ~ 8 hour, make through the machined of plane bar the white shaft pencil that length is 178 ~ 180mm;
(4) white shaft pencil sanding and polishing is become Wood pencil.
Further, what described spray sprayed in steaming and processing is herb liquid steam.
Further, described herb liquid is formed by following component infusion: 4 parts of HERBA HEDYOTIS DIFFUSAEs, 3 parts of subprostrate sophoras, 5 parts of giant knotweeds, 6 parts of barrenwort, 7 parts of fleece-flowers root, 5 parts of radix paeoniae rubrathe, 4 parts of capsules of weeping forsythia, 1 part of red sage root, 9 portions of reticulate millettias, 2 portions of root of herbaceous peonys, 4 portions of evodia rutaecarpas, 1 portion of fruit of glossy privet, 5 portions of japanese saussurea herbs, 9 portions of hydrangeas.
Further, described adhesive is made up of following component: butyl nitrile EP rubbers, polyisobutene, unsaturated polyester (UP), silicate, epoxy resin, PVC plasticizer and EP rubbers.
The present invention carries out Chinese medicine spray steaming process to buying the pencil board raw material come, the Chinese medicine used is for bitter and have certain benefit to health, make the Chinese medicinal ingredients containing bitter in pencil board, when children sting nib at use pencil out, because bitter, children are stung and once there will be no interest to sting second time afterwards, for a long time it, children can give up the bad habit of stinging nib, and the smooth process after spray steaming can allow pencil board more straight, improves the quality of pencil.The present invention effectively can prevent children from using in pencil process and sting written phenomenon.
Detailed description of the invention:
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, below in conjunction with specific embodiment, setting forth the present invention further.
A preparation method for anti-bite Wood pencil, is characterized in that comprising the following steps:
(1) spray is carried out to pencil board and steam process, be placed in stove, then spray steaming carried out 30 minutes to pencil board;
(2) steam to spray the pencil board terminated and carry out smooth process, pencil board by flattening, heats pencil board in pressing process by use planisher, by flattening 2 hours time, and heating-up temperature 130 DEG C, 1 hour heat time;
(3) thickness is become to be 4.2mm pencil board planer with keyway planer, and have the frid of the core groove adapted with lead core diameter, then adhesive is used lead for retractable pencil and pencil board gummed to be got up, heat (100 DEG C) in the clamp state after dry 5 hours, make through the machined of plane bar the white shaft pencil that length is 180mm;
(4) white shaft pencil sanding and polishing is become Wood pencil.
Further, what described spray sprayed in steaming and processing is herb liquid steam.
Further, described herb liquid is formed by following component infusion: 4 parts of HERBA HEDYOTIS DIFFUSAEs, 3 parts of subprostrate sophoras, 5 parts of giant knotweeds, 6 parts of barrenwort, 7 parts of fleece-flowers root, 5 parts of radix paeoniae rubrathe, 4 parts of capsules of weeping forsythia, 1 part of red sage root, 9 portions of reticulate millettias, 2 portions of root of herbaceous peonys, 4 portions of evodia rutaecarpas, 1 portion of fruit of glossy privet, 5 portions of japanese saussurea herbs, 9 portions of hydrangeas.
Further, described adhesive is made up of following component: butyl nitrile EP rubbers, polyisobutene, unsaturated polyester (UP), silicate, epoxy resin, PVC plasticizer and EP rubbers.
More than show and describe general principle of the present invention and principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (4)

1. a preparation method for anti-bite Wood pencil, is characterized in that comprising the following steps:
(1) spray is carried out to pencil board and steam process, be placed in stove, then spray steaming carried out 30 minutes to pencil board;
(2) steam to spray the pencil board terminated and carry out smooth process, pencil board by flattening, heats pencil board in pressing process by use planisher, by flattening 2 hours time, and heating-up temperature 130 DEG C, 1 hour heat time;
(3) thickness is become to be 4.1 ~ 4.2mm pencil board planer with keyway planer, and have the frid of the core groove adapted with lead core diameter, then adhesive is used lead for retractable pencil and pencil board gummed to be got up, heat (50 ~ 120 DEG C) in the clamp state after dry 1 ~ 8 hour, make through the machined of plane bar the white shaft pencil that length is 178 ~ 180mm;
(4) white shaft pencil sanding and polishing is become Wood pencil.
2. the preparation method of a kind of anti-bite Wood pencil according to claim 1, is characterized in that: what described spray sprayed in steaming and processing is herb liquid steam.
3. the preparation method of a kind of anti-bite Wood pencil according to claim 2, is characterized in that described herb liquid is formed by following component infusion: 4 parts of HERBA HEDYOTIS DIFFUSAEs, 3 parts of subprostrate sophoras, 5 parts of giant knotweeds, 6 parts of barrenwort, 7 parts of fleece-flowers root, 5 parts of radix paeoniae rubrathe, 4 parts of capsules of weeping forsythia, 1 part of red sage root, 9 portions of reticulate millettias, 2 portions of root of herbaceous peonys, 4 portions of evodia rutaecarpas, 1 portion of fruit of glossy privet, 5 portions of japanese saussurea herbs, 9 portions of hydrangeas.
4. the preparation method of a kind of anti-bite Wood pencil according to claim 1, is characterized in that described adhesive is made up of following component: butyl nitrile EP rubbers, polyisobutene, unsaturated polyester (UP), silicate, epoxy resin, PVC plasticizer and EP rubbers.
CN201510539345.9A 2015-08-27 2015-08-27 Manufacturing method of biting preventing wooden pencil Pending CN105128561A (en)