CN105089694A - 一种尾矿固结后充填到塌陷坑的方法 - Google Patents

一种尾矿固结后充填到塌陷坑的方法 Download PDF

Info

Publication number
CN105089694A
CN105089694A CN201410201221.5A CN201410201221A CN105089694A CN 105089694 A CN105089694 A CN 105089694A CN 201410201221 A CN201410201221 A CN 201410201221A CN 105089694 A CN105089694 A CN 105089694A
Authority
CN
China
Prior art keywords
cement
enters
sequence
diameter
tailings
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410201221.5A
Other languages
English (en)
Inventor
祁建东
窦梅林
张法胜
朱利军
石现杰
李生龙
商百涛
祁维学
王延文
宁忠超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
XISHIMEN IRON MINE OF MINMETALS HANXING MINING CO Ltd
Original Assignee
XISHIMEN IRON MINE OF MINMETALS HANXING MINING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by XISHIMEN IRON MINE OF MINMETALS HANXING MINING CO Ltd filed Critical XISHIMEN IRON MINE OF MINMETALS HANXING MINING CO Ltd
Priority to CN201410201221.5A priority Critical patent/CN105089694A/zh
Publication of CN105089694A publication Critical patent/CN105089694A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种尾矿固结后充填到塌陷坑的方法,其一种尾矿固结后充填到塌陷坑的工艺过程为16道序,其各序工艺过程为:1、全尾砂料进入直径45m浓缩机,2、经过直径45m浓缩机处理的全尾砂料进入直径18m浓缩机,3、直径18m浓缩机处理的全尾砂料矿浆浓度达到45~55%,矿浆浓度达到45~55%的全尾砂料部分进入5序渣浆泵,清水部分进入溢流槽4序,4、溢流槽中的清水返回尾矿车间直径50m浓缩机,5、浓度达到45~55%全尾砂料浆通过渣浆泵输送给搅拌桶,6序,7、水泥入料进入水泥仓,8、水泥仓中的水泥进入螺旋给料机。本发明缓解了尾矿库库容,治理了受采矿活动破坏的地表环境,为土地复垦和生态环境重建创造条件。

Description

一种尾矿固结后充填到塌陷坑的方法
技术领域
本发明涉及一种充填方法,尤其涉及一种尾矿固结后充填到塌陷坑的方法。
背景技术
由于尾矿库库容严重不足,按2013年推算,剩余尾矿库库容只能满足矿山生产2-3年。因此,解决铁矿今后尾矿排放问题是矿山生产持续的当务之急。若采取一定的技术措施,在不影响井下采矿安全的前提下,利用矿山现有的地表塌陷坑进行尾矿固结排放,就可以解决铁矿今后的尾矿堆存问题。
发明内容
为了弥补现有技术的不足,解决铁矿今后的尾矿堆存问题,发明了一种尾矿固结后充填到塌陷坑的方法。
本发明解决问题的技术方案可以是:
一种尾矿固结后充填到塌陷坑的方法,其一种尾矿固结后充填到塌陷坑的工艺过程为16道序,其工序工艺过程为:1、全尾砂料进入直径45m浓缩机,2、经过直径45m浓缩机处理的全尾砂料进入直径18m浓缩机,3、直径18m浓缩机处理的全尾砂料矿浆浓度达到45~55%,矿浆浓度达到45~55%的全尾砂料部分进入5序渣浆泵,清水部分进入溢流槽4序,4、溢流槽中的清水返回直径45m浓缩机,5、浓度达到45~55%全尾砂料浆通过渣浆泵输送给搅拌桶6序,7、水泥入料进入水泥仓,8、水泥仓中的水泥进入螺旋给料机,9、螺旋给料机中的水泥进入皮带计量装置,10、皮带计量装置按照水泥占全尾砂干重的2~3%的比例送给斗式提升机,11、斗式提升机将水泥占全尾砂干重的2~3%的水泥送进搅拌桶6序,6、搅拌桶中的全尾砂料与加入2~3%的水泥充分搅拌后输送到4台盘式真空过滤机,12、4台盘式真空过滤机将加入2~3%水泥的料浆充分搅拌后的全尾砂料浆过滤后,清水排入循环水池13序,固结滤饼晴天时直接通过皮带运输机Ⅰ14序和皮带运输机Ⅱ15序排入塌陷区16序。
固结滤饼晴天时直接排入塌陷坑,雨天需在晾晒棚晾晒三天再输送到塌陷坑。固结滤饼浓度为75~80%,全尾砂固结体28天单轴抗压强度达到0.382~0.910MPa。
本发明的有益效果是:
1、本发明全尾砂固结体28天单轴抗压强度达到0.382~0.910MPa,固结体遇水不泥化、不粉化。
2、本发明缓解了尾矿库库容,治理了受采矿活动破坏的地表环境,为土地复垦和生态环境重建创造条件。
附图说明
图1为全尾砂固结排放工艺流程图。
具体实施方式
一种尾矿固结后充填到塌陷坑的方法,其一种尾矿固结后充填到塌陷坑的工艺过程为16道序,其工序工艺过程为:1、全尾砂料进入直径45m浓缩机,2、经过直径45m浓缩机处理的全尾砂料进入直径18m浓缩机,3、直径18m浓缩机处理的全尾砂料矿浆浓度达到45~55%,矿浆浓度达到45~55%的全尾砂料部分进入5序渣浆泵,清水部分进入溢流槽4序,4、溢流槽中的清水返回尾矿车间直径50m浓缩机,5、浓度达到45~55%全尾砂料浆通过渣浆泵输送给搅拌桶6序,7、水泥入料进入水泥仓,8、水泥仓中的水泥进入螺旋给料机,9、螺旋给料机中的水泥进入皮带计量装置,10、皮带计量装置按照水泥占全尾砂干重的2~3%的比例送给斗式提升机,11、斗式提升机将水泥占全尾砂干重的2~3%的水泥送进搅拌桶6序,6、搅拌桶中的全尾砂料与加入2~3%的水泥充分搅拌后输送到4台盘式真空过滤机,12、四台盘式真空过滤机将加入2~3%水泥的料浆充分搅拌后的全尾砂料浆过滤后,清水排入循环水池13序,固结滤饼晴天时直接通过皮带运输机Ⅰ14序和皮带运输机Ⅱ15序排入塌陷区16序。
固结滤饼晴天时直接排入塌陷坑,雨天需在晾晒棚晾晒三天再输送到塌陷坑。固结滤饼浓度为75~80%,全尾砂固结体28天单轴抗压强度达到0.382~0.910MPa。

Claims (1)

1.一种尾矿固结后充填到塌陷坑的方法,其特征在于:其一种尾矿固结后充填到塌陷坑的工艺过程为16道序,其工序工艺过程为:1、全尾砂料进入直径45m浓缩机,2、经过直径45m浓缩机处理的全尾砂料进入直径18m浓缩机,3、直径18m浓缩机处理的全尾砂料矿浆浓度达到45~55%,矿浆浓度达到45~55%的全尾砂料部分进入5序渣浆泵,清水部分进入溢流槽4序,4、溢流槽中的清水返回尾矿车间直径50m浓缩机,5、浓度达到45~55%全尾砂料浆通过渣浆泵输送给搅拌桶6序,7、水泥入料进入水泥仓,8、水泥仓中的水泥进入螺旋给料机,9、螺旋给料机中的水泥进入皮带计量装置,10、皮带计量装置按照水泥占全尾砂干重的2~3%的比例送给斗式提升机,11、斗式提升机将水泥占全尾砂干重的2~3%的水泥送进搅拌桶6序,6、搅拌桶中的全尾砂料与加入2~3%的水泥充分搅拌后输送到四台盘式真空过滤机,12、四台盘式真空过滤机将加入2~3%水泥的料浆充分搅拌后的全尾砂料浆过滤后,清水排入循环水池13序,固结滤饼晴天时直接通过皮带运输机Ⅰ14序和皮带运输机Ⅱ15序排入塌陷区16序。
CN201410201221.5A 2014-05-14 2014-05-14 一种尾矿固结后充填到塌陷坑的方法 Pending CN105089694A (zh)