Prior art keywords
core rod
mold
die sleeve
cover plate
sleeve
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510361393.3A
Other languages
Chinese (zh)
Inventor
曹永义
王刚
陈晓东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Xizhou Magnet Wires Co Ltd
Original Assignee
Wuxi Xizhou Magnet Wires Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Xizhou Magnet Wires Co Ltd filed Critical Wuxi Xizhou Magnet Wires Co Ltd
Priority to CN201510361393.3A priority Critical patent/CN105080794A/en
Publication of CN105080794A publication Critical patent/CN105080794A/en
Pending legal-status Critical Current

Links

Landscapes

  • Coating Apparatus (AREA)

Abstract

The invention provides a painting mold of a varnished wire. The painting mold can solve the problem that an existing painting mold is not prone to replacement and can effectively avoid the phenomenon that in the painting process, insulation varnish is wasted. The painting mold comprises a mold core and a mold sleeve; the mold core is arranged in the mold sleeve; and the painting mold is characterized by further comprising an upper cover plate and a lower cover plate. The mold core is formed by splicing a left half mold core body and a right half mold core body; and the mold sleeve is formed by splicing a front half mold sleeve body and a rear half mold sleeve body; the front half mold sleeve and the rear half mold sleeve are placed to be mounted on the periphery of the mold core, and the mold core is packaged in the mold sleeve through the upper cover plate and the lower cover plate; and the upper cover plate and the lower cover plate are in fastened connection with the mold core and the mold sleeve respectively through bolts.

Description

The japanning die of enamel-covered wire
Technical field
The present invention relates to the processing unit (plant) field of enamel-covered wire, be specially the japanning die of enamel-covered wire.
Background technology
The enamelling process of current enamel-covered wire generally has felt method to paint and die methods japanning, wherein the japanning of felt method has easy to operate, exchange wire gauge advantage easily, but the viscosity requirement of the method to insulated paint is higher, and paint film is wayward, needs often change felt and insulated paint is vulnerable to pollute thus affects the insulating properties of enamel-covered wire, and adopt of die methods japanning fixes japanning die 2 more, insulated paint is stored in paint cylinder 3, bare copper wire 1 from bottom to top through paint cylinder 3 after again through japanning die 2, see Fig. 1 and Fig. 2, japanning die 2 wherein comprises mould cover 2-1 and core rod 2-2, core rod 2-2 is installed in mould cover 2-1 by jump ring 2-3 in fact, its film thickness is easy to control, japanning precision is high, but need to change corresponding japanning die when processing different size enamel-covered wire, generally that bare copper wire is cut off at first mould place during replacing, then corresponding mould is changed, again the bare copper wire cut off is welded to connect, therefore its to there is die change loaded down with trivial details, labor strength is large, inefficient problem, and more during mold exchange, bare copper wire welds after cutting off again and also directly results in scrapping of bare copper wire, cause the waste of bare copper wire, in addition, existing die methods japanning is stored in paint cylinder due to edge paint, there is the phenomenon of the waste of insulated paint in lacquering process.In Fig. 1,4 is felt.
Summary of the invention
For the problems referred to above, the invention provides the japanning die of enamel-covered wire, it can solve and adopt the not easily changeable problem of existing japanning die, and effectively can reduce the insulated paint wasting phenomenon existed in lacquering process.
The japanning die of enamel-covered wire, it comprises core rod and die sleeve, described core rod is installed in die sleeve, it is characterized in that: it also comprises upper cover plate and lower cover, described core rod is made up of left half core rod and right half core rod split, described die sleeve is made up of first half die sleeve and later half die sleeve split, described first half die sleeve and later half die sleeve split are installed on the surrounding of described core rod, described core rod is packaged in described die sleeve by described upper cover plate, lower cover, and described upper cover plate, lower cover are respectively and described core rod, to be bolted connection between die sleeve.
Further, described core rod is installed on the top of described die sleeve, and the cavity between the bottom surface of described core rod and described lower cover is formed and stores up paint bath, described upper cover plate, be bolted between core rod and die sleeve fixing.
Further, described first half die sleeve and back mold half have into paint hole, described in enter to paint hole connect paint inlet tube.
The beneficial effect of japanning die of the present invention is: its core rod and die sleeve are split structure half-and-half, core rod is packaged in die sleeve by upper cover plate and lower cover simultaneously, its easy accessibility, no longer need during die change to cut off bare copper wire, therefore greatly can improve the replacing efficiency of mould and avoid because of more mold exchange and damage to naked copper money, and reduce scrapping and waste of bare copper wire, save production cost; In addition, its core rod is installed on the top of mould cover, thus between die sleeve and lower cover, form storage paint bath, first half die sleeve and back mold half have into paint hole, enter to paint hole and connect paint inlet tube, insulated paint is conveyed in the storage paint bath of mould by paint inlet tube, therefore insulated paint to be closed in mould thus effectively can to avoid the waste of insulated paint, also insulated paint can be avoided contaminated, ensure that the quality of production of enamel-covered wire.
Accompanying drawing explanation
Fig. 1 is the schematic diagram of existing mold method japanning;
Fig. 2 is the structure for amplifying schematic diagram of existing japanning die in Fig. 1;
Fig. 3 is the structural representation of japanning die of the present invention;
Fig. 4 is that the A-A of Fig. 3 is to schematic diagram.
Detailed description of the invention
See Fig. 3 and Fig. 4, the japanning die of enamel-covered wire of the present invention, it comprises core rod 10, die sleeve 20, upper cover plate 30 and lower cover 40, core rod 10 is installed in die sleeve 20, core rod 10 is made up of left half core rod 11 and right half core rod 12 split, die sleeve 20 is made up of first half die sleeve 21 and later half die sleeve 22 split, first half die sleeve 21 and the split of later half die sleeve 22 are installed on the surrounding of core rod 10, upper cover plate 30, core rod 10 is packaged in die sleeve 20 by lower cover 40, core rod 10 is installed on the top of die sleeve 20, cavity between the bottom surface of described core rod and described lower cover is formed and stores up paint bath 61, be fastenedly connected by bolt 51 between upper cover plate 30 and core rod 10, die sleeve 20 and upper cover plate 30, be connected and fixed by bolt 52 between lower cover 40.First half die sleeve 21 and back mold half 22 have into paint hole 60, enters to paint hole 60 and connect paint inlet tube.

Claims (3)

1. the japanning die of enamel-covered wire, it comprises core rod and die sleeve, described core rod is installed in die sleeve, it is characterized in that: it also comprises upper cover plate and lower cover, described core rod is made up of left half core rod and right half core rod split, described die sleeve is made up of first half die sleeve and later half die sleeve split, described first half die sleeve and later half die sleeve split are installed on the surrounding of described core rod, described core rod is packaged in described die sleeve by described upper cover plate, lower cover, and described upper cover plate, lower cover are bolted connection with described core rod, die sleeve respectively.
2. the japanning die of enamel-covered wire according to claim 1, it is characterized in that: described core rod is installed on the top of described die sleeve, cavity between the bottom surface of described core rod and described lower cover is formed and stores up paint bath, is bolted fixing between described upper cover plate and core rod.
3. the japanning die of enamel-covered wire according to claim 2, is characterized in that: described first half die sleeve and back mold half have into paint hole, described in enter to paint hole connect paint inlet tube.
CN201510361393.3A 2015-06-28 2015-06-28 Painting mold of varnished wire Pending CN105080794A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510361393.3A CN105080794A (en) 2015-06-28 2015-06-28 Painting mold of varnished wire

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510361393.3A CN105080794A (en) 2015-06-28 2015-06-28 Painting mold of varnished wire

Publications (1)

Publication Number Publication Date
CN105080794A true CN105080794A (en) 2015-11-25

Family

ID=54562651

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510361393.3A Pending CN105080794A (en) 2015-06-28 2015-06-28 Painting mold of varnished wire

Country Status (1)

Country Link
CN (1) CN105080794A (en)

Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH1166974A (en) * 1997-08-18 1999-03-09 Chubu Sukegawa Kogyo Kk Heat resistant insulated wire for casting metal mold
CN201082405Y (en) * 2007-08-22 2008-07-09 佛山市威奇电工材料有限公司 Changing type paint coating mould
CN201298401Y (en) * 2008-11-05 2009-08-26 无锡环宇电磁线有限公司 Separate mold for painting enamelled sheet wires
CN201799373U (en) * 2010-09-06 2011-04-20 金杯电工股份有限公司 Split type japanning die
CN102820106A (en) * 2012-08-23 2012-12-12 韩富生 Special enamel coating device for mold-process enameled wire production
CN102856013A (en) * 2012-09-18 2013-01-02 无锡锡洲电磁线有限公司 Lacquering device for varnished wire
CN203910351U (en) * 2014-04-11 2014-10-29 张家港市华发电工器材制造有限公司 Enamelled wire static painting apparatus
CN204996664U (en) * 2015-06-28 2016-01-27 无锡锡洲电磁线有限公司 Japanning mould of enameled wire

Patent Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH1166974A (en) * 1997-08-18 1999-03-09 Chubu Sukegawa Kogyo Kk Heat resistant insulated wire for casting metal mold
CN201082405Y (en) * 2007-08-22 2008-07-09 佛山市威奇电工材料有限公司 Changing type paint coating mould
CN201298401Y (en) * 2008-11-05 2009-08-26 无锡环宇电磁线有限公司 Separate mold for painting enamelled sheet wires
CN201799373U (en) * 2010-09-06 2011-04-20 金杯电工股份有限公司 Split type japanning die
CN102820106A (en) * 2012-08-23 2012-12-12 韩富生 Special enamel coating device for mold-process enameled wire production
CN102856013A (en) * 2012-09-18 2013-01-02 无锡锡洲电磁线有限公司 Lacquering device for varnished wire
CN203910351U (en) * 2014-04-11 2014-10-29 张家港市华发电工器材制造有限公司 Enamelled wire static painting apparatus
CN204996664U (en) * 2015-06-28 2016-01-27 无锡锡洲电磁线有限公司 Japanning mould of enameled wire

Similar Documents

Publication Publication Date Title
CN204996664U (en) Japanning mould of enameled wire
CN104525816A (en) Forging device and process for flange yoke of transmission shaft
CN105080794A (en) Painting mold of varnished wire
CN104043804A (en) Die mounting device and die mounting method of upright die casting machine
CN103337360B (en) A kind of novel non-casting dry type transformer high-voltage coil and low-voltage coil cover winding mold tool
CN203862986U (en) Die installation device for vertical die casting machine
CN203751016U (en) Aluminum section extruder with novel extruding device
CN102737790B (en) Improved movable enameled wire painting mould
CN203343379U (en) Core shooter
CN203370937U (en) Mould with replaceable mould cores
CN202650727U (en) Novel enameled wire japanning mould
CN202105987U (en) Socket sand core for cast iron pipe
CN204818052U (en) Foundry goods embryo mould automatic production line
CN104441736A (en) Leather strip extruder
CN102709001A (en) Novel painting die for enameled wire
CN104752050A (en) Method for enlarging diameter varying range of adjustable winding mould of transformer coil
CN205217704U (en) Electrode connection piece compression molding machine
CN205159094U (en) Vary voltage coiling mould
CN204221427U (en) Work piece holder frock in a kind of binding post process
CN204183939U (en) The automatic cold-press mould structure of diamond bead
CN102800441B (en) For the adjustable japanning die of enamelled wire processing
CN103743865A (en) Detection method of inner cavity of sand mold
CN203592326U (en) Novel crossbeam pedestal processing fixing structure
CN202623085U (en) Die with guide pillar of discharge oil cylinder
CN203779591U (en) Full-automatic cylinder sleeve unloading production line

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20151125