CN1050316A - The iron pan and the manufacture method thereof that contain body trace element - Google Patents
The iron pan and the manufacture method thereof that contain body trace element Download PDFInfo
- Publication number
- CN1050316A CN1050316A CN 89105763 CN89105763A CN1050316A CN 1050316 A CN1050316 A CN 1050316A CN 89105763 CN89105763 CN 89105763 CN 89105763 A CN89105763 A CN 89105763A CN 1050316 A CN1050316 A CN 1050316A
- Authority
- CN
- China
- Prior art keywords
- zinc
- iron
- trace element
- directly
- mixed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The iron pan and the manufacture method thereof that contain body trace element are to have invented a kind of cooker, make people by cook with diet processes in replenish the trace element of needed by human naturally, the method for mixing zinc element in iron pan also is provided simultaneously.
Description
The invention belongs to daily life field (A47J class) and field of metallurgy (C23C class), is to have invented iron pan and the manufacture method thereof that contains body trace element.
The basic chemical ingredients of the iron pan of producing is iron and carbon at present, contains some impurity, mainly is silicon, manganese, phosphorus, four kinds of elements of sulphur, does not contain zinc, is a kind of invention so zinc element is mixed in the iron pan.With the present invention the patent No. 87100282 is arranged similarly, " a kind of nutritious slice ", applicant Zhou Guoliang, he proposes to mix into six kinds of elements such as zinc, does not propose zinc is mixed scheme in the iron but, and experiment shows, gasify after directly zinc being dropped into the iron liquation at once, 907 ℃ of the gasification temperatures of zinc, iron melt temperature are mixed into being difficult to of zinc more than 1600 ℃.
Medical research shows that human body is taken in an amount of zinc element every day, can suppress the harm of lead element to human body effectively, thereby memory alleviates irascible mood, and the aging course of delaying human body has very big benefit to healthy with intelligence.The objective of the invention is to make the element zinc, copper, phosphorus, selenium, germanium etc. of needed by human just to be replenished naturally, and be provided at the method for mixing zinc in the iron by the cooking, diet processes.
How elements such as zinc being mixed in the iron pan, is key of the present invention, directly mixes zinc and do not accomplish in melting, because the gasification temperature of zinc is 907 ℃, is lower than 1600 ℃ of the fusing points of iron.The invention provides two kinds and mix the zinc method: what 1. mix in iron liquid is not zinc element, but the compound of the high-melting-point of zinc or high gasification point, as zinc oxide, zinc sulphide (both fusing points are all more than 1700 ℃), they all dissolve in hydrochloric acid in gastric juice, are absorbed by the body.When 2. metallic zinc is not in melting, mix in the iron liquid, but when casting, directly pour the mold mouth into, pour in the mould with iron liquid.Also available these the two kinds of ways of other element are mixed in the iron.Zinc content can produce αGu Rongti with iron in 10% the time.The present invention allows the content of zinc be 0.2~5%, and selenium germanium (anti-cancer), copper and rare earth equal size respectively are 0.1~0.5%.
The present invention is in case input is implemented, and the user will obtain replenishing of an amount of elements such as zinc by diet every day, and this is to the human body beneficial, and especially health and the intelligence to children is of great benefit to.
Embodiment is as follows:
One, a certain proportion of zinc oxide or zinc sulphide are mixed iron liquid, make to contain zinc in the pot.
Two, metallic zinc is processed into small pieces or particle, when casting, pours the mold mouth equably in proportion into, form zinc-iron alloy with iron.
Claims (4)
1, the present invention contains the body trace element iron pan for HUMAN HEALTH provides, such as containing zinc, germanium, copper, rare earth; The method that element is mixed has three kinds: 1. element is directly mixed iron liquid, can directly mix as copper; 2. the metallic zinc gasification point is lower than the fusing point of iron, can't directly mix iron liquid, and just the compound with zinc mixes iron liquid, as zinc oxide, and zinc sulphide; 3. when casting, directly pour the small pieces or the small-particle of element into the mold mouth, together flow in the mould with iron liquid.
2, by the described method of claim 1, it is characterized in that zinc oxide or zinc sulphide are mixed in the iron liquation, make to contain zinc in the iron pan.
3, by the described method of claim 1, it is characterized in that the small-particle or the powder of zinc or zn cpds are directly poured in the mold mouth when casting equably, together inject in the mould with iron liquid.
4, by the described trace element pot of claim 1, the content of its element is: zinc 0.2~5%, copper, germanium, phosphorus, content of rare earth respectively are 0.1~0.5%.