Health-care iron pan containing trace elements and manufacturing method thereof Download PDFInfo
- Publication number
- CN1103671A CN1103671A CN 93120445 CN93120445A CN1103671A CN 1103671 A CN1103671 A CN 1103671A CN 93120445 CN93120445 CN 93120445 CN 93120445 A CN93120445 A CN 93120445A CN 1103671 A CN1103671 A CN 1103671A
- Authority
- CN
- China
- Prior art keywords
- molybdenum
- selenium
- iron
- content
- magnesium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a health-care iron pan containing trace elements and a manufacturing method thereof, which is characterized in that: the cast iron for making the pan contains selenium, molybdenum and magnesium microelements; the selenium content is more than or equal to 1.5ppm, the molybdenum content is more than or equal to 80ppm, and the magnesium content is more than or equal to 0.2 ppm. The iron pan can absorb trace elements of selenium, molybdenum and magnesium during cooking and eating, has effects of preventing and resisting cancer for digestive system, and can enhance immunity. The invention also provides a manufacturing method of the iron pan containing selenium, molybdenum and magnesium.
Description
The present invention relates to a kind of health iron pan and manufacture method thereof that contains trace element, a kind of health iron pan and manufacture method thereof that contains selenium, molybdenum, magnesium trace element of saying so more specifically.
Selenium, molybdenum, magnesium are the special trace elements that human body needs, and human body is had immunization, and Digestive tract is had anti-cancer, antitumous effect, and especially the effect to esophagus cancer is more obvious (sees 1. cancer diagnosis and treatment 350 problems, Yu Rencun chief editor, publication in 1989; 2. in September, 1991, whole nation selenium The Study on Resources was understood data).Once there was the report that contains selenium health care pot in former Shaanxi, Hangzhou, but its selenium content is very low, in gastronomical process, the selenium amount in the diet of being dissolved in does not reach diseases prevention, disease-resistant health-care effect, and do not contain molybdenum and magnesium in its product, to the tumour of Digestive tract, particularly esophagus cancer does not have preventive effect.
The objective of the invention is to overcome above-mentioned the deficiencies in the prior art and the health iron pan and the manufacture method thereof of a kind of selenium that contains significant quantity, molybdenum, magnesium trace element are provided.
Technical scheme of the present invention is in order to achieve the above object:
1, the black shale ore that will contain selenium, molybdenum is pulverized, and becomes 8-20 purpose breeze with ball mill grinding, and wherein selenium content is 1500-3000ppm; Molybdenum content is 1000-3500ppm.
2, the pig iron is heated to 1100 ℃-1350 ℃, after the fusing, the breeze that will contain selenium, molybdenum is put into hot metal ladle bottom, breeze add-on: the pig iron: breeze=7~10: 0.1~0.15(weight).Fully stir, burn after 2~5 minutes, selenium content can reach 〉=1.5ppm; Preferably be controlled at selenium content 1.5~2.7ppm; Molybdenum content can reach 〉=80ppm, and preferably molybdenum content is controlled at 80-100ppm.
3, in the molten iron that contains selenium, molybdenum, add silicon magnesium-zinc alloy grain immediately after the burning of the breeze of selenium to be contained, molybdenum, after its add-on made the alloy burning, magnesium element content 〉=0.2ppm preferably was controlled at 0.2-0.5ppm.
4, the molten iron that will contain selenium, molybdenum, magnesium trace element is poured into a mould in the mould of the system of giving and is made iron pan.
The present invention's beneficial effect compared with prior art is:
Make in the cast iron of iron pan and contain the selenium human body special requirement, significant quantity, molybdenum, magnesium trace element, this pot of life-time service is cooked, trace element is dissolved in the food, can reach the content that needed by human body is wanted, to digestion, particularly esophagus cancer is played the effectively preventing effect, and can strengthen the immunizing power of human body.
Embodiment 1:
The 7kg pig iron is heated to 1350 ℃, after the pig iron is dissolved, with selenium content is 3000ppm, the 20 purpose breeze 0.1kg that contain the molybdenum amount and be 3500ppm add molten iron bag bottom, burns to add silicon magnesium-zinc alloy (press 50% calculating of Mg content combustion loss in the alloy, make its content reach 0.2ppm) 0.01kg(magnesium after 3 minutes immediately and account for 5% at alloy at content), after the fusing, selenium content is 1.6ppm in the molten iron, and molybdenum content is 109ppm, and Mg content is 0.2ppm.Pour into iron pan with the molten iron that contains selenium, molybdenum, magnesium.
Embodiment 2:
The 7kg molten iron is heated to 1100 ℃, the fusing back adds and contains selenium 3000ppm, the breeze 0.15kg that contains molybdenum 3500ppm, after the burning, leave standstill adding in 5 minutes as embodiment 1 described silicon magnesium-zinc alloy 0.025kg, after the fusing, selenium content 2.72ppm in the molten iron, molybdenum content 80ppm, Mg content 0.5ppm pours into iron pan with the molten iron that contains selenium, molybdenum, magnesium.
Claims (3)
1, a kind of health iron pan that contains trace element is characterized in that: contain selenium, molybdenum, magnesium trace element in making the cast iron of iron pan; Selenium content 〉=1.5ppm, molybdenum content 〉=80ppm, Mg content 〉=0.2ppm.
2, iron pan as claimed in claim 1 is characterized in that: make and contain selenium 1.5~2.72ppm in the iron pan cast iron; Contain molybdenum 80~100ppm; Contain magnesium 0.2~0.5ppm.
3, a kind of manufacture method of iron pan as claimed in claim 1, it is characterized in that: the black shale ore that will contain selenium 1500~3000PPM, contains molybdenum 1000~3500ppm is pulverized, become 8-20 purpose breeze through the ball mill ball milling, the pig iron is heated to 1100~1350 ℃, be fused into molten iron, the breeze that will contain selenium, molybdenum drops into hot metal ladle bottom, breeze add-on: the pig iron: breeze=7~10: 0.1~0.15(weight); Burn after 2~5 minutes selenium content 〉=1.5ppm; Molybdenum content 〉=80ppm; Add the silicon magnesium-zinc alloy after breeze has burnt immediately, silicon magnesium-zinc alloy add-on makes Mg content 〉=0.2ppm in the molten iron; In the mould of the system of giving, pour into iron pan with the molten iron that contains selenium, molybdenum, magnesium then.