CN105001748A - 一种汽车防划白色油漆 - Google Patents
一种汽车防划白色油漆 Download PDFInfo
- Publication number
- CN105001748A CN105001748A CN201410604614.0A CN201410604614A CN105001748A CN 105001748 A CN105001748 A CN 105001748A CN 201410604614 A CN201410604614 A CN 201410604614A CN 105001748 A CN105001748 A CN 105001748A
- Authority
- CN
- China
- Prior art keywords
- parts
- acid ester
- phosphoric acid
- paint
- silicone oil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种汽车防划白色油漆,按重量份计,由以下各原料组成:氯乙烯共聚合树脂10-15、苯乙烯聚酯树脂20-24、磷酸酯12-14、环己六醇六磷酸脂3-5、钛白粉1.5-2.5、乙基纤维素0.4-0.8、火成岩粉1.5-2.5、中空玻璃球2-4、白色颜料10-12、针状硅灰石2.5-4.5、有机硅油0.3-0.8、流平剂1.2-1.5、消泡剂0.2-0.7、蒸馏水20-22;本发明实现轻量化的耐碎落涂料,可用空气喷涂、无空气喷涂、刷涂、静电喷涂等方法涂装。该涂料用于汽车底盘及车身其他部位。因而油漆的保光性、耐高温性、耐水性和耐候性较好。
Description
技术领域
本发明涉及汽车装饰涂料领域,具体属于一种汽车防划白色油漆。
背景技术
油漆是一种能牢固覆盖在物体表面,起保护、装饰、标志和其他特殊用途的化学混合物涂料。油漆为粘稠油性颜料,未干情况下易燃,不溶于水,微溶于脂肪,可溶于醇、醛、醚、苯、烷,易溶于汽油、煤油、柴油。
现在市场上汽车用油漆种类很多,但是各种油漆都是由成膜物质(各种树脂)、溶剂、颜料、干燥剂、添加剂组成。普通油漆通常用汽油作溶剂,环氧铁红底漆含少量二甲苯,浸漆主要含甲苯,也有少量苯,对人体身体影响很大。
发明内容
本发明的目的是提供一种汽车防划白色油漆,实现轻量化的耐碎落涂料,可用空气喷涂、无空气喷涂、刷涂、静电喷涂等方法涂装。该涂料用于汽车底盘及车身其他部位。因而油漆的保光性、耐高温性、耐水性和耐候性较好。
本发明采用的技术方案如下:
一种汽车防划白色油漆,按重量份计,由以下各原料组成:
氯乙烯共聚合树脂10-15、苯乙烯聚酯树脂20-24、磷酸酯12-14、环己六醇六磷酸脂3-5、钛白粉1.5-2.5、乙基纤维素0.4-0.8、火成岩粉1.5-2.5、中空玻璃球2-4、白色颜料10-12、针状硅灰石2.5-4.5、有机硅油0.3-0.8、流平剂1.2-1.5、消泡剂0.2-0.7、蒸馏水20-22;
其具体的制备方法如下:按上述重量份,将氯乙烯共聚合树脂和苯乙烯聚酯树脂、磷酸酯和三分之一的蒸馏水进行预乳化后抽入高位槽,环己六醇六磷酸脂、乙基纤维素、有机硅油用三分之二的水溶解后抽入另一高位槽,两个高位槽同时以滴加的方式进入搅拌槽,搅拌槽内温度控制在60-70℃,压力控制在1.4-2.2mpa,控制滴加速度,使反应物料在1.2-2.2h滴完,然后保温1-1.5h,然后冷却,冷却后与其余原料充分混合搅拌,即得。
汽车防划白色油漆,由以下各原料组成:氯乙烯共聚合树脂12、苯乙烯聚酯树脂22、磷酸酯13、环己六醇六磷酸脂4、钛白粉2、乙基纤维素0.6、火成岩粉2、中空玻璃球3、白色颜料11、针状硅灰石3、有机硅油0.5、流平剂1.3、消泡剂0.5、蒸馏水21。
本发明采用磷酸酯为乳化剂,与苯乙烯聚酯树脂形成成膜,原材料中不含有甲醛和三甲苯等有害物质,实现轻量化的耐碎落涂料,可用空气喷涂、无空气喷涂、刷涂、静电喷涂等方法涂装。该涂料用于汽车底盘及车身其他部位。因而油漆的保光性、耐高温性、耐水性和耐候性较好。
具体实施方式
一种汽车防划白色油漆,按重量份计,由以下各原料组成:
氯乙烯共聚合树脂12、苯乙烯聚酯树脂22、磷酸酯13、环己六醇六磷酸脂4、钛白粉2、乙基纤维素0.6、火成岩粉2、中空玻璃球3、白色颜料11、针状硅灰石3、有机硅油0.5、流平剂1.3、消泡剂0.5、蒸馏水21;
其具体的制备方法如下:按上述重量份,将氯乙烯共聚合树脂和苯乙烯聚酯树脂、磷酸酯和三分之一的蒸馏水进行预乳化后抽入高位槽,环己六醇六磷酸脂、乙基纤维素、有机硅油用三分之二的水溶解后抽入另一高位槽,两个高位槽同时以滴加的方式进入搅拌槽,搅拌槽内温度控制在60-70℃,压力控制在1.4-2.2mpa,控制滴加速度,使反应物料在1.2-2.2h滴完,然后保温1-1.5h,然后冷却,冷却后与其余原料充分混合搅拌,即得。
Claims (2)
1.一种汽车防划白色油漆,按重量份计,其特征在于,由以下各原料组成:
氯乙烯共聚合树脂10-15、苯乙烯聚酯树脂20-24、磷酸酯12-14、环己六醇六磷酸脂3-5、钛白粉1.5-2.5、乙基纤维素0.4-0.8、火成岩粉1.5-2.5、中空玻璃球2-4、白色颜料10-12、针状硅灰石2.5-4.5、有机硅油0.3-0.8、流平剂1.2-1.5、消泡剂0.2-0.7、蒸馏水20-22;
其具体的制备方法如下:按上述重量份,将氯乙烯共聚合树脂和苯乙烯聚酯树脂、磷酸酯和三分之一的蒸馏水进行预乳化后抽入高位槽,环己六醇六磷酸脂、乙基纤维素、有机硅油用三分之二的水溶解后抽入另一高位槽,两个高位槽同时以滴加的方式进入搅拌槽,搅拌槽内温度控制在60-70℃,压力控制在1.4-2.2mpa,控制滴加速度,使反应物料在1.2-2.2h滴完,然后保温1-1.5h,然后冷却,冷却后与其余原料充分混合搅拌,即得。
2.根据权利要求1所述汽车防划白色油漆,其特征在于,由以下各原料组成:氯乙烯共聚合树脂12、苯乙烯聚酯树脂22、磷酸酯13、环己六醇六磷酸脂4、钛白粉2、乙基纤维素0.6、火成岩粉2、中空玻璃球3、白色颜料11、针状硅灰石3、有机硅油0.5、流平剂1.3、消泡剂0.5、蒸馏水21。