CN104999709A - Method for producing embossed rolled toilet paper - Google Patents
Method for producing embossed rolled toilet paper Download PDFInfo
- Publication number
- CN104999709A CN104999709A CN201510442962.7A CN201510442962A CN104999709A CN 104999709 A CN104999709 A CN 104999709A CN 201510442962 A CN201510442962 A CN 201510442962A CN 104999709 A CN104999709 A CN 104999709A
- Authority
- CN
- China
- Prior art keywords
- embossing
- thin
- paper
- surface layer
- thick
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for producing embossed rolled toilet paper. The method comprises the steps of raw paper uncoiling, surface layer fine embossing, surface layer coarse embossing, gluing, bottom layer fine embossing, rewinding and packaging. Layers of the embossed rolled toilet paper obtained by means of the method are not prone to separating, and the embossed rolled toilet paper is fluffy, has a firm hand feel and is soft and comfortable. Meanwhile, the water absorbing capacity is substantially improved by more than 30%.
Description
Technical field
The present invention relates to the method for producing coil paper, the particularly method of production embossing toiler roll.
Background technology
Tradition embossing is generally which floor paper carries out embossing by a set of embossed wheel together, not only aesthetic property is poor for the embossing toiler roll produced, and the easy absciss layer of each interlayer of the toiler roll suppressed, and paper is coarse, feel is thin, soaking effect is bad, and during use, comfort is not good.
Summary of the invention
The object of the invention is to overcome above-mentioned deficiency existing in prior art, the method for new production embossing toiler roll is provided.
In order to realize foregoing invention object, the invention provides following technical scheme:
The method of production embossing toiler roll, comprises body paper unreel, embossing, gluing, rewinding, packaging, specifically comprises the steps:
(1) body paper unreel: by body paper unreel to be embossed;
(2) the thin embossing of surface layer: one or more layers of body paper is caused upper thin knurling rolls and thin cruddy paper is obtained to the thin embossing of compacting, described thin knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on steel rod is made up of the thin embossing die unit of dense distribution, and described embossing die decorative pattern height is 0.7 ~ 0.9mm;
(3) the thick embossing of surface layer: the thin cruddy paper that step (2) obtains causes thick knurling rolls and obtains surface layer cruddy paper to carrying out thick embossing, described thick knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on thick embossing steel rod by sparse distribution and the large thick embossing die unit of the relatively thin embossing die unit of shape form, described embossing die decorative pattern height is 1.0 ~ 1.3mm;
(4) gluing: the surface layer cruddy paper that step (3) obtains causes the roller pair that cementing rubber rollers and thick embossing steel rod are formed, to the surface layer cruddy paper inboard concave surface gluing invocation point glue surface layer cruddy paper that step (3) obtains;
(5) the thin embossing of bottom: one deck body paper is caused lower thin knurling rolls and the thin cruddy paper of bottom is obtained to the thin embossing of compacting;
(6) rewinding, packaging: the thin cruddy paper rewinding of bottom that some glue surface layer cruddy paper step (4) obtained and step (5) obtain, the thick embossing concave surface of some glue surface layer cruddy paper bonds with the thin cruddy paper concave surface of bottom and is connected in rewinding process, obtains embossing toiler roll after packaging.
Further, in step (2), embossing die decorative pattern height is preferably 0.8mm.
Further, in step (3), embossing die decorative pattern height is preferably 1.2mm.
Further, the body paper adopted in step (2) is two-layer or three layers of body paper.
The embossing toiler roll of the present invention's statement is two-layer or two-layer above embossing toiler roll.
Compared with prior art, beneficial effect of the present invention: each interlayer of the embossing toiler roll not easily absciss layer that the method for production embossing toiler roll of the present invention prepares, and paper is fluffy, feel is abundant does not lose soft comfortable again, water absorbing capacity significantly promotes simultaneously, improves more than 30%.
Accompanying drawing explanation
Fig. 1 is that in embodiment 2, body paper moves towards schematic flow sheet;
Fig. 2 is the layer structure schematic diagram of multi-layer embossed toiler roll prepared by embodiment 2.
Detailed description of the invention
Below in conjunction with test example and detailed description of the invention, the present invention is described in further detail.But this should be interpreted as that the scope of the above-mentioned theme of the present invention is only limitted to following embodiment, all technology realized based on content of the present invention all belong to scope of the present invention.
The method of embodiment 1 production embossing toiler roll, comprises body paper unreel, embossing, gluing, rewinding, packaging, specifically comprises the steps:
(1) body paper unreel: by body paper unreel to be embossed;
(2) the thin embossing of surface layer: three layers of body paper are caused upper thin knurling rolls and thin cruddy paper is obtained to the thin embossing of compacting, described thin knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on steel rod is made up of the thin embossing die unit of dense distribution, and described embossing die decorative pattern height is 0.7mm;
(3) the thick embossing of surface layer: the thin cruddy paper that step (2) obtains causes thick knurling rolls and obtains surface layer cruddy paper to carrying out thick embossing, described thick knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on thick embossing steel rod by sparse distribution and the large thick embossing die unit of the relatively thin embossing die unit of shape form, described embossing die decorative pattern height is 1.0mm;
(4) gluing: the surface layer cruddy paper that step (3) obtains causes the roller pair that cementing rubber rollers and thick embossing steel rod are formed, to the surface layer cruddy paper inboard concave surface gluing invocation point glue surface layer cruddy paper that step (3) obtains;
(5) the thin embossing of bottom: one deck body paper is caused lower thin knurling rolls and the thin cruddy paper of bottom is obtained to the thin embossing of compacting;
(6) rewinding, packaging: the thin cruddy paper rewinding of bottom that some glue surface layer cruddy paper step (4) obtained and step (5) obtain, the thick embossing concave surface of some glue surface layer cruddy paper bonds with the thin cruddy paper concave surface of bottom and is connected in rewinding process, obtains embossing toiler roll after packaging.
Embodiment 2 is with reference to Fig. 1, and the method for production embossing toiler roll, comprises body paper unreel, embossing, gluing, rewinding, packaging, specifically comprise the steps:
(1) body paper unreel: by body paper unreel to be embossed;
(2) the thin embossing of surface layer: two-layer body paper is caused upper thin knurling rolls through paper carrying roll thin cruddy paper is obtained to the thin embossing of compacting, described thin knurling rolls are to for steel rod is to rubber roll (being made up of upper thin embossing rubber roll and upper thin knurling steel roll), wherein go up the embossing die decorative pattern on thin embossing steel rod to be made up of the thin embossing die unit of dense distribution, described embossing die decorative pattern height is 0.8mm;
(3) the thick embossing of surface layer: the thin cruddy paper that step (2) obtains causes thick knurling rolls and obtains surface layer cruddy paper to carrying out thick embossing, described thick knurling rolls are to for steel rod is to rubber roll (being made up of thick embossing steel rod and thick embossing rubber roll), embossing die decorative pattern wherein on thick embossing steel rod by sparse distribution and the large thick embossing die unit of the relatively thin embossing die unit of shape form, described embossing die decorative pattern height is 1.2mm;
(4) gluing: the surface layer cruddy paper that step (3) obtains causes the roller pair that cementing rubber rollers and thick embossing steel rod are formed, to the surface layer cruddy paper inboard concave surface gluing invocation point glue surface layer cruddy paper that step (3) obtains;
(5) the thin embossing of bottom: one deck body paper is caused lower thin knurling rolls and the thin cruddy paper of bottom is obtained to the thin embossing of compacting;
(6) rewinding, packaging: the thin cruddy paper of bottom that some glue surface layer cruddy paper step (4) obtained and step (5) obtain is through rewinding machine rewinding, the thick embossing concave surface of some glue surface layer cruddy paper bonds with the thin cruddy paper concave surface of bottom and is connected in rewinding process, obtains embossing toiler roll after packaging.
With reference to Fig. 2, the embossing toiler roll that the example method prepares, comprise surface layer 1, bottom 3 and be arranged on the sandwich layer 2 in the middle of surface layer 1 and bottom 3, also comprise glue layer 4, surface layer 1 is provided with surface layer embossing, sandwich layer 2 is provided with sandwich layer embossing, and bottom 3 is provided with bottom embossing, and bottom embossing concave surface 302 is connected by glue layer 4 with sandwich layer embossing concave surface 202; Surface layer embossing by dense distribution shading embossing and be arranged on the thick embossing of sparse distribution in shading embossing and form, the single embossing units of thick embossing is larger relative to the shape of shading embossing; The shading embossed height that surface layer 1 is arranged is 0.8mm; The thick embossed height that surface layer 1 is arranged is 1.2mm; Bottom embossing is made up of the bottom shading embossing of dense distribution, and the embossed height in the embossing of bottom shading is 0.8mm.
With reference to Fig. 2, the embossing toiler roll that the example method prepares, surface layer embossing convex surface 101 and sandwich layer embossing convex surface 201 are fitted, and use to feel the softness of paper and smooth during friction; Bottom embossing convex surface 301 and sandwich layer embossing convex surface 201 are oppositely arranged the fluffy sense adding toiler roll; Surface layer embossing concave surface 102 and sandwich layer embossing concave surface 202 are fitted, the point glue that sandwich layer embossing concave surface 202 is arranged is bonding with bottom embossing concave surface 302, further increase the fluffy sense of embossing toiler roll of the present invention, and the paper fiber of every layer of paper is all subject to change in various degree, reduce the rigidity of fiber, increase the elasticity of fiber, expand fiber and interfibrous space simultaneously, therefore make the multi-layer embossed toiler roll water absorbing capacity of preparation be increased dramatically, water absorbing capacity improves more than 30%.
The method of embodiment 3 production embossing toiler roll, comprises body paper unreel, embossing, gluing, rewinding, packaging, specifically comprises the steps:
(1) body paper unreel: by body paper unreel to be embossed;
(2) the thin embossing of surface layer: one deck body paper is caused upper thin knurling rolls and thin cruddy paper is obtained to the thin embossing of compacting, described thin knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on steel rod is made up of the thin embossing die unit of dense distribution, and described embossing die decorative pattern height is 0.9mm;
(3) the thick embossing of surface layer: the thin cruddy paper that step (2) obtains causes thick knurling rolls and obtains surface layer cruddy paper to carrying out thick embossing, described thick knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on thick embossing steel rod by sparse distribution and the large thick embossing die unit of the relatively thin embossing die unit of shape form, described embossing die decorative pattern height is 1.3mm;
(4) gluing: the surface layer cruddy paper that step (3) obtains causes the roller pair that cementing rubber rollers and thick embossing steel rod are formed, to the surface layer cruddy paper inboard concave surface gluing invocation point glue surface layer cruddy paper that step (3) obtains; The roller that described cementing rubber rollers and glue steel rider, glue rubber rollers form is to by glue paper injection cementing rubber rollers;
(5) the thin embossing of bottom: one deck body paper is caused lower thin knurling rolls and the thin cruddy paper of bottom is obtained to the thin embossing of compacting;
(6) rewinding, packaging: the thin cruddy paper rewinding of bottom that some glue surface layer cruddy paper step (4) obtained and step (5) obtain, the thick embossing concave surface of some glue surface layer cruddy paper bonds with the thin cruddy paper concave surface of bottom and is connected in rewinding process, obtains embossing toiler roll after packaging.
Claims (4)
1. the method for production embossing toiler roll, comprises body paper unreel, embossing, gluing, rewinding, packaging, it is characterized in that, specifically comprise the steps:
(1) body paper unreel: by body paper unreel to be embossed;
(2) the thin embossing of surface layer: one or more layers of body paper is caused upper thin knurling rolls and thin cruddy paper is obtained to the thin embossing of compacting, described thin knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on steel rod is made up of the thin embossing die unit of dense distribution, and described embossing die decorative pattern height is 0.7 ~ 0.9mm;
(3) the thick embossing of surface layer: the thin cruddy paper that step (2) obtains causes thick knurling rolls and obtains surface layer cruddy paper to carrying out thick embossing, described thick knurling rolls are to for steel rod is to rubber roll, embossing die decorative pattern wherein on thick embossing steel rod by sparse distribution and the large thick embossing die unit of the relatively thin embossing die unit of shape form, described embossing die decorative pattern height is 1.0 ~ 1.3mm;
(4) gluing: the surface layer cruddy paper that step (3) obtains causes the roller pair that cementing rubber rollers and thick embossing steel rod are formed, to the surface layer cruddy paper inboard concave surface gluing invocation point glue surface layer cruddy paper that step (3) obtains;
(5) the thin embossing of bottom: one deck body paper is caused lower thin knurling rolls and the thin cruddy paper of bottom is obtained to the thin embossing of compacting;
(6) rewinding, packaging: the thin cruddy paper rewinding of bottom that some glue surface layer cruddy paper step (4) obtained and step (5) obtain, the thick embossing concave surface of some glue surface layer cruddy paper bonds with the thin cruddy paper concave surface of bottom and is connected in rewinding process, obtains embossing toiler roll after packaging.
2. method according to claim 1, is characterized in that, in step (2), embossing die decorative pattern height is 0.8mm.
3. method according to claim 1 and 2, is characterized in that, in step (3), embossing die decorative pattern height is 1.2mm.
4. method according to claim 3, is characterized in that, the body paper adopted in step (2) is two-layer or three layers of body paper.