CN104977307A - 一种冷轧板表面清洗效果检测装置及方法 - Google Patents

一种冷轧板表面清洗效果检测装置及方法 Download PDF

Info

Publication number
CN104977307A
CN104977307A CN201410143246.4A CN201410143246A CN104977307A CN 104977307 A CN104977307 A CN 104977307A CN 201410143246 A CN201410143246 A CN 201410143246A CN 104977307 A CN104977307 A CN 104977307A
Authority
CN
China
Prior art keywords
cold
working arm
handle
testing cushion
contact pad
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410143246.4A
Other languages
English (en)
Inventor
叶铁
高振宇
张勇
胡洪旭
白日
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Steel Co Ltd
Original Assignee
Angang Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Angang Steel Co Ltd filed Critical Angang Steel Co Ltd
Priority to CN201410143246.4A priority Critical patent/CN104977307A/zh
Publication of CN104977307A publication Critical patent/CN104977307A/zh
Pending legal-status Critical Current

Abstract

本发明提供一种冷轧板表面清洗效果检测装置及方法,检测装置由手柄、弹簧、工作臂、销轴、接触垫及限位螺栓组成;工作臂通过销轴连接在手柄前端,手柄与工作臂之间设有弹簧,工作臂前端固定有接触垫,接触垫下面通过螺杆连接海绵,海绵外包裹测试垫,手柄中部通过螺纹连接限位螺栓。通过手柄按压放在冷轧板表面的接触垫,压缩弹簧至工作臂后部压靠在限位螺栓上,使测试垫与被检测冷轧板表面摩擦3-10秒后移开;将测试垫与对比卡进行比对,根据测试垫颜色及残留量,即可判定冷轧板表面碱洗洗净程度。本发明可实现冷轧板表面碱洗质量的分级评定,提高判定的精确度,并避免划伤事故。

Description

一种冷轧板表面清洗效果检测装置及方法
技术领域
本发明属于轧钢工艺领域,尤其涉及一种冷轧板表面清洗效果在线检测装置及方法。
背景技术
冷轧钢板进行连续退火前需要洗去轧制油,一般采用碱液清洗。为了检测碱洗的效果,常常采用湿巾或纸与碱洗后的钢板摩擦后,用肉眼观察湿巾或纸的颜色,来判定碱洗是否洗净。该方法虽然简单,但存在以下问题:
1、直接用手拿着湿巾或纸去摩擦在线运行的钢板表面,存在一定的安全隐患,操作者易被钢板划伤。
2、操作者摩擦钢板时的力量大小决定了摩擦后湿巾或纸的颜色深浅,从而直接影响对碱洗洗净情况的判定结果。
3、手拿着湿巾或纸去摩擦运行的钢板,湿巾或纸与钢板为点接触,且着力分布不均,查看时往往颜色最深的部位来判断钢板的洗净情况,难以准确反映出碱洗的真实效果。
由于存在着以上三个问题,因此,现有技术所使用的检测方法显然是不科学的,受人为因素干扰较大,无法区分出碱洗的洗净程度。
发明内容
本发明旨在提供一种可准确反映碱洗质量,提高检测精准度,并避免安全事故的冷轧板表面清洗效果在线检测装置及检测方法。
为此,本发明所采取的解决方案是:
一种冷轧板表面清洗效果检测装置,由手柄、弹簧、工作臂、销轴、接触垫及限位螺栓组成;工作臂中部通过销轴活动连接在手柄前端,手柄中部设有弹簧,弹簧另一端固定在工作臂后部,工作臂前端固定有接触垫,接触垫下面通过螺杆连接海绵,海绵外包裹测试垫,在手柄中部通过螺纹连接一限位螺栓。
所述测试垫为纸质或棉、毛、麻、化纤织物。
一种冷轧板表面清洗效果检测方法,其具体方法和步骤为:
1、检测时,检测人员手持手柄将测试垫放至运行的被检测冷轧板表面,并通过手柄按压接触垫,工作臂以销轴为轴旋转,工作臂后部压缩弹簧收缩,直至工作臂后端压靠在限位螺栓上为止。
2、保持压力,使测试垫与被检测冷轧板表面摩擦接触3-10秒后移开。
3、将卸下的测试垫与事先制备好的对比卡进行颜色比对,若测试垫上无乳液残留,则视为优良;若有少许残留,但测试垫仍保持颜色青白,则视为合格;如果测试垫已呈黑色,则视为不合格,重新调整冷轧板碱洗系统。
本发明的有益效果为:
1、安全性大大提高,避免了操作者被钢板划伤事故;
2、利用比对卡,实现了冷轧板表面碱洗质量的分级评定;
3、测试垫与钢板表面采用面接触,可全面真实放映碱洗洗净效果,提高判定的精确度;
4、为质量控制和升级提供了可靠的手段与数据支持。
附图说明
图1是冷轧板表面清洗效果检测装置结构示意图。
图中:限位螺栓1、手柄2、弹簧3、工作臂4、销轴5、接触垫6、螺杆7、海绵8、测试垫9。
具体实施方式
由图1可见,本发明冷轧板表面清洗效果检测装置系由限位螺栓1、手柄2、弹簧3、工作臂4、销轴5、接触垫6所组成。手柄2为一直杆,直杆前端加工有销轴孔;工作臂4呈“S”形,中部亦设有销轴孔;接触垫6为矩形(也可为圆形或椭圆形),在接触垫6的上表面开设有螺杆孔,螺杆孔内螺纹连接有螺杆7,用于固定海绵8和测试垫9,测试垫9包裹在海绵8的外面,测试垫9可以为纸质,也可以采用棉、毛、麻、化纤织物。工作臂4的中部通过销轴5活动连接在手柄2的前端,并可绕销轴5转动。手柄2中部设有一根弹簧3,弹簧3的另一端固定在工作臂4的后部,工作臂4的前端固定有接触垫6,在手柄2的中部、位于弹簧3的后侧通过螺纹连接一可调节伸出长度的限位螺栓1。
本发明冷轧板表面清洗效果检测方法的具体步骤为:
1、检测时,检测人员手持手柄2将测试垫9放至运行的被检测冷轧板表面,并通过手柄2按压接触垫6,在此压力作用下,工作臂4将以销轴5为轴旋转,使工作臂4后部直接压缩弹簧3收缩,直至工作臂4的后端压靠在限位螺栓1上为止。
2、继续保持该压力,使测试垫9与被检测冷轧板表面摩擦接触3-10秒后,即可将测试垫9从被检测冷轧板表面移开。
3、松动螺杆7将测试垫9从接触垫6上卸下,然后将卸下的测试垫9与事先制备好的对比卡进行颜色比对,若测试垫9上无乳液残留,则视为优良;若有少许残留,但测试垫9仍保持颜色青白,则视为合格;如果测试垫9已呈黑色,则视为不合格,需要重新调整冷轧板碱洗系统。

Claims (3)

1.一种冷轧板表面清洗效果检测装置,其特征在于,由手柄、弹簧、工作臂、销轴、接触垫及限位螺栓组成;工作臂中部通过销轴活动连接在手柄前端,手柄中部设有弹簧,弹簧另一端固定在工作臂后部,工作臂前端固定有接触垫,接触垫下面通过螺杆连接海绵,海绵外包裹测试垫,在手柄中部通过螺纹连接一限位螺栓。
2.根据权利要求1所述的冷轧板表面清洗效果检测装置,其特征在于,所述测试垫为纸质或棉、毛、麻、化纤织物。
3.一种应用权利要求1所述冷轧板表面清洗效果检测装置的方法,其特征在于,具体检测方法和步骤为:
(1)、检测时,检测人员手持手柄将测试垫放至运行的被检测冷轧板表面,并通过手柄按压接触垫,工作臂以销轴为轴旋转,工作臂后部压缩弹簧收缩,直至工作臂后端压靠在限位螺栓上为止;
(2)、保持压力,使测试垫与被检测冷轧板表面摩擦接触3-10秒后移开;
(3)、将卸下的测试垫与事先制备好的对比卡进行颜色比对,若测试垫上无乳液残留,则视为优良;若有少许残留,但测试垫仍保持颜色青白,则视为合格;如果测试垫已呈黑色,则视为不合格,重新调整冷轧板碱洗系统。
CN201410143246.4A 2014-04-10 2014-04-10 一种冷轧板表面清洗效果检测装置及方法 Pending CN104977307A (zh)