CN104975283A - 一种凝汽器铜管复合预膜液 - Google Patents
一种凝汽器铜管复合预膜液 Download PDFInfo
- Publication number
- CN104975283A CN104975283A CN201510322342.XA CN201510322342A CN104975283A CN 104975283 A CN104975283 A CN 104975283A CN 201510322342 A CN201510322342 A CN 201510322342A CN 104975283 A CN104975283 A CN 104975283A
- Authority
- CN
- China
- Prior art keywords
- parts
- copper tube
- carboxyl
- protective films
- condenser
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种凝汽器铜管复合预膜液,由以下份数的原料组分组成:20-30份硫酸镍、8-10份氯化镍、5-10份硫酸铝、5-10份硫酸铜、3-5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8-10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8-10份2-氨基苯并噻唑、3-5份石灰、3-5份碳酸钠、5-6份柠檬酸、100-120份去离子水。该凝汽器铜管复合预膜液解决了保护膜局限于偏酸性的外部环境,增强了保护膜的耐碱性,两种保护膜相互交错,使得所形成的复合保护膜适应值更广,可以适应更好的PH值变化,大大扩大了保护膜对酸碱环境的适应能力,解决了保护膜对环境问题。
Description
技术领域
本发明涉及预膜液的技术领域,尤其涉及一种凝汽器铜管复合预膜液。
背景技术
目前,我国的大多数火力发电厂的凝汽器都是用循环冷却水来对凝汽器进行冷却的,由于循环冷却水的水质特点,普遍存在着对凝汽器铜管的腐蚀,使凝汽器的使用寿命降低,危害极大,因此各个科研单位及电厂都在积极想办法来对凝汽器铜管进行保护,先后用过阴极保护法、管端采用保护套管法、硫酸亚铁成膜法,铜试剂造模法等,但这些措施只是保护凝汽器两端的水室,管板和管端,不能有效保护铜管,且铜管的表面保护膜必然受到破坏,从而影响凝汽器的使用寿命。
发明内容
本发明的目的是为了克服上述现有技术的缺点,提供一种凝汽器铜管复合预膜液,该凝汽器铜管复合预膜液解决了保护膜局限于偏酸性的外部环境,增强了保护膜的耐碱性,两种保护膜相互交错,使得所形成的的复合保护膜适应值更广,可以适应更好的PH值变化,大大扩大了保护膜对酸碱环境的适应能力,解决了保护膜对环境问题。
本发明解决其技术问题所采用的技术方案是:一种凝汽器铜管复合预膜液,由以下份数的原料组分组成:20-30份硫酸镍、8-10份氯化镍、5-10份硫酸铝、5-10份硫酸铜、3-5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8-10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8-10份2-氨基苯并噻唑、3-5份石灰、3-5份碳酸钠、5-6份柠檬酸、100-120份去离子水。
进一步的,各原料组分的份数为:20份硫酸镍、8份氯化镍、5份硫酸铝、5份硫酸铜、3份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8份2-氨基苯并噻唑、3份石灰、3份碳酸钠、5份柠檬酸、100份去离子水。
或者是,各原料组分的份数为:30份硫酸镍、10份氯化镍、10份硫酸铝、10份硫酸铜、5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、10份2-氨基苯并噻唑、5份石灰、5份碳酸钠、6份柠檬酸、120份去离子水。
综上所述,本发明的凝汽器铜管复合预膜液解决了保护膜局限于偏酸性的外部环境,增强了保护膜的耐碱性,两种保护膜相互交错,使得所形成的的复合保护膜适应值更广,可以适应更好的PH值变化,大大扩大了保护膜对酸碱环境的适应能力,解决了保护膜对环境问题。
具体实施方式
实施例1
本实施例1所描述的一种凝汽器铜管复合预膜液,由以下份数的原料组分组成:20份硫酸镍、8份氯化镍、5份硫酸铝、5份硫酸铜、3份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8份2-氨基苯并噻唑、3份石灰、3份碳酸钠、5份柠檬酸、100份去离子水。
实施例2
本实施例2所描述的一种凝汽器铜管复合预膜液,由以下份数的原料组分组成:30份硫酸镍、10份氯化镍、10份硫酸铝、10份硫酸铜、5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、10份2-氨基苯并噻唑、5份石灰、5份碳酸钠、6份柠檬酸、120份去离子水。
以上所述,仅是本发明的较佳实施例而已,并非对本发明的技术方案作任何形式上的限制。凡是依据本发明的技术实质对以上实施例所作的任何简单修改、等同变化与修饰,均仍属于本发明的技术方案的范围内。
Claims (3)
1.一种凝汽器铜管复合预膜液,其特征在于,由以下份数的原料组分组成:20-30份硫酸镍、8-10份氯化镍、5-10份硫酸铝、5-10份硫酸铜、3-5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8-10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8-10份2-氨基苯并噻唑、3-5份石灰、3-5份碳酸钠、5-6份柠檬酸、100-120份去离子水。
2.根据权利要求1所述的一种凝汽器铜管复合预膜液,其特征在于,各原料组分的份数为:20份硫酸镍、8份氯化镍、5份硫酸铝、5份硫酸铜、3份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、8份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、8份2-氨基苯并噻唑、3份石灰、3份碳酸钠、5份柠檬酸、100份去离子水。
3.根据权利要求1所述的一种凝汽器铜管复合预膜液,其特征在于,各原料组分的份数为:30份硫酸镍、10份氯化镍、10份硫酸铝、10份硫酸铜、5份2-苯并噻唑偶氮-7-(4-羧基苯偶氮)-变色酸、10份1-(2'-苯并噻唑)-3-(4'-羧基苯)三氮烯、10份2-氨基苯并噻唑、5份石灰、5份碳酸钠、6份柠檬酸、120份去离子水。