CN104959108B - 一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法 - Google Patents

一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法 Download PDF

Info

Publication number
CN104959108B
CN104959108B CN201510365596.XA CN201510365596A CN104959108B CN 104959108 B CN104959108 B CN 104959108B CN 201510365596 A CN201510365596 A CN 201510365596A CN 104959108 B CN104959108 B CN 104959108B
Authority
CN
China
Prior art keywords
bryozoatum
attapulgite
ammonia nitrogen
filtering material
sewage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201510365596.XA
Other languages
English (en)
Other versions
CN104959108A (zh
Inventor
蔡恩扬
任浩楠
陈逸涵
李子健
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Xinyun Environmental Protection Technology Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510365596.XA priority Critical patent/CN104959108B/zh
Publication of CN104959108A publication Critical patent/CN104959108A/zh
Application granted granted Critical
Publication of CN104959108B publication Critical patent/CN104959108B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法,其由以下重量份原料制成:凹凸棒石44‑56、海浮石32‑48、硅藻泥16‑24、多孔磷酸钙12‑18、贝壳粉5‑10、沸石分子筛4‑6、纳米二氧化钛6‑8、颗粒活性炭15‑20、离子交换树脂3‑5、氨基三亚甲基膦酸五钠1‑3、细孔硅胶3‑5、纳米壳聚糖2‑4、乙醇30‑40;本发明制得的凹凸棒石/海浮石复合滤料耐高温,耐腐蚀,吸附效果好,过滤精度高,热收缩率小,具有杰出的尺寸稳定性,使用寿命长,能有效的净化污水中的氨氮等有害成份。

Description

一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制 备方法
技术领域
本发明涉及滤料技术领域,更具体地说是一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法。
背景技术
滤料是水处理过滤材料的总称,主要用于生活污水,工业污水,纯水,饮用水的过滤。滤料(filtering media)主要分为两大类,一类是用以水处理设备中的进水过滤的粒状材料,通常指石英砂,白煤或矿石等。另一类是物理分离的过滤介质,主要包括过滤布,过滤网,滤芯,滤纸,以及最新的膜。
凹凸棒石又称坡缕石或坡缕缟石,是一种具链层状结构的含水富镁硅酸盐粘土矿物。其结构属2:1型粘土矿物。在每个2:1单位结构层中,四面体晶片角顶隔一定距离方向颠倒,形成层链状。在四面体条带间形成与链平行的通道,通道横断面约3.7*6.3A°。通道中充填沸石水和结晶水。凹凸棒石矿物几乎遍及世界各地,但具有工业意义的矿床所占比例不大,仅限于美国、中国、西班牙、法国、土耳其、塞内加尔、南非、澳大利亚、巴西、以色列、沙特阿拉伯、瑞士、英国 、俄罗斯(Irkutsk ,伊尔库茨克)、吉尔吉斯斯坦、哈萨克斯坦、乌克兰、亚美尼亚、阿塞拜疆、白俄罗斯、尼泊尔等国,据不完全统计,世界探明储量约14亿吨。
海浮石化学组成有颇大的出入。一般是由铝、钾、钠的硅酸盐所成,亦即以 二氧化硅为主要成分的类似玻璃组成的矿物。 因多采自海水,则亦可能含有氯、镁等海水中存在的物质。石花主要为碳酸钙,并含少量的镁,铁及酸不溶物质。浮石 为不规则的块状,大小不一,通常直径2~7厘米,有的可达20厘米。表面粗糙,有多数大小不等的细孔,灰白色或灰黄色。质硬而松脆,易砸碎,断面粗糙有小孔,有的具绢丝样光泽或无。
本发明采用凹凸棒石和海浮石复合制得的滤料,吸附效果好,过滤精度高,能有效的净化吸附污水中的氨氮等有害物质。
发明内容
本发明的目的是为了提供一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法。该复合滤料对于污水中的氨氮等有害物质具有优异的净化吸附作用。
本发明的目的是通过以下技术方案实现的:
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料,由以下重量份原料制成:凹凸棒石44-56、海浮石32-48、硅藻泥16-24、多孔磷酸钙12-18、贝壳粉5-10、沸石分子筛4-6、纳米二氧化钛6-8、颗粒活性炭15-20、离子交换树脂3-5、氨基三亚甲基膦酸五钠1-3、细孔硅胶3-5、纳米壳聚糖2-4、乙醇30-40;
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料的制备方法,包括以下步骤:
(1)将凸凹棒石、海浮石、硅藻泥、氨基三亚甲基膦酸五钠用高速研磨机研磨至粒径为1-5μm的颗粒,与颗粒活性炭、贝壳粉混合均匀,加入乙醇,2000-3000r/min高速分散0.5-1h,然后加热至60-70℃,搅拌至至混合料乙醇全部挥发,湿法造粒;
(2)将上述湿颗粒直接放到高温环境中骤热膨胀,膨胀温度500-700℃,时间为15-20min;
(3)将膨胀成型后的颗粒经800-950℃焙烧4-8分钟后冷却至室温;
(4)将上述冷却后的颗粒与余下原料混合均匀,灭菌干燥后即可得到所需污水用复合滤料。
本发明的优点在于:
本发明制得的凹凸棒石/海浮石复合滤料耐高温,耐腐蚀,吸附效果好,过滤精度高,热收缩率小,具有杰出的尺寸稳定性,使用寿命长,能有效的净化污水中的氨氮等有害成份。
具体实施方式
实施例1
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料,由以下重量(kg)原料制成:凹凸棒石44、海浮石32、硅藻泥16、多孔磷酸钙12、贝壳粉5、沸石分子筛4、纳米二氧化钛6、颗粒活性炭15、离子交换树脂3、氨基三亚甲基膦酸五钠1、细孔硅胶3、纳米壳聚糖2、乙醇30;
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料的制备方法,包括以下步骤:
(1)将凸凹棒石、海浮石、硅藻泥、氨基三亚甲基膦酸五钠用高速研磨机研磨至粒径为1-5μm的颗粒,与颗粒活性炭、贝壳粉混合均匀,加入乙醇,2000-3000r/min高速分散0.5-1h,然后加热至60-70℃,搅拌至至混合料乙醇全部挥发,湿法造粒;
(2)将上述湿颗粒直接放到高温环境中骤热膨胀,膨胀温度500-700℃,时间为15-20min;
(3)将膨胀成型后的颗粒经800-950℃焙烧4-8分钟后冷却至室温;
(4)将上述冷却后的颗粒与余下原料混合均匀,灭菌干燥后即可得到所需污水用复合滤料。
上述制得的凹凸棒石/海浮石复合滤料的氨氮吸附率为93.6%。
实施例2
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料,由以下重量(kg)原料制成:凹凸棒石50、海浮石44、硅藻泥22、多孔磷酸钙16、贝壳粉8、沸石分子筛5、纳米二氧化钛7、颗粒活性炭18、离子交换树脂4、氨基三亚甲基膦酸五钠2、细孔硅胶4、纳米壳聚糖3、乙醇35;
凹凸棒石/海浮石复合滤料的制备方法同实施例1。
上述制得的凹凸棒石/海浮石复合滤料的氨氮吸附率为95.1%。
实施例3
一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料,由以下重量(kg)原料制成:凹凸棒石56、海浮石48、硅藻泥24、多孔磷酸钙18、贝壳粉10、沸石分子筛6、纳米二氧化钛8、颗粒活性炭20、离子交换树脂5、氨基三亚甲基膦酸五钠3、细孔硅胶5、纳米壳聚糖4、乙醇40;
凹凸棒石/海浮石复合滤料的制备方法同实施例1。
上述制得的凹凸棒石/海浮石复合滤料的氨氮吸附率为94.2%。

Claims (1)

1.一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料,其特征在于:由以下重量份原料制成:凹凸棒石44-56、海浮石32-48、硅藻泥16-24、多孔磷酸钙12-18、贝壳粉5-10、沸石分子筛4-6、纳米二氧化钛6-8、颗粒活性炭15-20、离子交换树脂3-5、氨基三亚甲基膦酸五钠1-3、细孔硅胶3-5、纳米壳聚糖2-4、乙醇30-40;
以上滤料制备方案如下:
(1)将凹凸棒石、海浮石、硅藻泥、氨基三亚甲基膦酸五钠用高速研磨机研磨至粒径为1-5μm的颗粒,与颗粒活性炭、贝壳粉混合均匀,加入乙醇,2000-3000r/min高速分散0.5-1h,然后加热至60-70℃,搅拌至混合料乙醇全部挥发,湿法造粒;
(2)将上述步骤(1)湿法造粒所得的颗粒直接放到高温环境中骤热膨胀,膨胀温度500-700℃,时间为15-20min;
(3)将膨胀成型后的颗粒经800-950℃焙烧4-8分钟后冷却至室温;
(4)将上述冷却后的颗粒与余下原料混合均匀,灭菌干燥后即可得到所需污水用复合滤料。
CN201510365596.XA 2015-06-29 2015-06-29 一种污水氨氮净化吸附用凹凸棒石/海浮石复合滤料及其制备方法 Active CN104959108B (zh)