CN104817987A - High-strength leather joint - Google Patents

High-strength leather joint Download PDF

Info

Publication number
CN104817987A
CN104817987A CN201510229948.9A CN201510229948A CN104817987A CN 104817987 A CN104817987 A CN 104817987A CN 201510229948 A CN201510229948 A CN 201510229948A CN 104817987 A CN104817987 A CN 104817987A
Authority
CN
China
Prior art keywords
parts
dermatomere
acetone
maleic anhydride
modified polypropylene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510229948.9A
Other languages
Chinese (zh)
Inventor
姚红军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Tian Yan Textile Equipment Co Ltd
Original Assignee
Nantong Tian Yan Textile Equipment Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nantong Tian Yan Textile Equipment Co Ltd filed Critical Nantong Tian Yan Textile Equipment Co Ltd
Priority to CN201510229948.9A priority Critical patent/CN104817987A/en
Publication of CN104817987A publication Critical patent/CN104817987A/en
Pending legal-status Critical Current

Abstract

The invention discloses a high-strength leather joint, which includes a leather joint body being prepared by bonding a plurality layers of nonwoven cloths through an adhesive. The adhesive is composed of maleic anhydride-modified polypropylene, thermal-plastic polyamide, wheat flour, carbon tetrachloride and acetone. The high-strength leather joint is firm in structure and is long in service life.

Description

High strength dermatomere
Technical field
The present invention relates to a kind of spinning dermatome.
Background technology
Existing spinning dermatome, its dermatomere body stability is undesirable.
Summary of the invention
The object of the present invention is to provide firmly a kind of, the high strength dermatomere of long working life.
Technical solution of the present invention is:
A kind of high strength dermatomere, comprises dermatomere body, it is characterized in that: dermatomere body forms by multi-layer nonwoven fabrics tackiness agent is bonding, and adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 30-50 part
Polyamide thermoplastic 10-20 part
Wheat-flour 5-10 part
Tetracol phenixin 5-10 part
Acetone 5-10 part.
Adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 43 parts
Polyamide thermoplastic 19 parts
Wheat-flour 6 parts
7 parts, tetracol phenixin
8 parts, acetone.
Adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 32 parts
Polyamide thermoplastic 11 parts
Wheat-flour 9 parts
9 parts, tetracol phenixin
5 parts, acetone.
The firm excellent performance of the present invention, long working life.
Below in conjunction with embodiment, the invention will be further described.
Embodiment
A kind of high strength dermatomere, comprise dermatomere body, dermatomere body forms by multi-layer nonwoven fabrics tackiness agent is bonding, and adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 43 parts
Polyamide thermoplastic 19 parts
Wheat-flour 6 parts
7 parts, tetracol phenixin
8 parts, acetone.
Adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 32 parts
Polyamide thermoplastic 11 parts
Wheat-flour 9 parts
9 parts, tetracol phenixin
5 parts, acetone.

Claims (3)

1. a high strength dermatomere, comprises dermatomere body, it is characterized in that: dermatomere body forms by multi-layer nonwoven fabrics tackiness agent is bonding, and adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 30-50 part
Polyamide thermoplastic 10-20 part
Wheat-flour 5-10 part
Tetracol phenixin 5-10 part
Acetone 5-10 part.
2. high strength dermatomere according to claim 1, is characterized in that: adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 43 parts
Polyamide thermoplastic 19 parts
Wheat-flour 6 parts
7 parts, tetracol phenixin
8 parts, acetone.
3. high strength dermatomere according to claim 1, is characterized in that: adhesive therefor is made up of the component of following weight part:
Maleic anhydride modified polypropylene 32 parts
Polyamide thermoplastic 11 parts
Wheat-flour 9 parts
9 parts, tetracol phenixin
5 parts, acetone.
CN201510229948.9A 2015-05-08 2015-05-08 High-strength leather joint Pending CN104817987A (en)