CN104804652A - 环保型建筑胶粘剂 - Google Patents
环保型建筑胶粘剂 Download PDFInfo
- Publication number
- CN104804652A CN104804652A CN201510207197.0A CN201510207197A CN104804652A CN 104804652 A CN104804652 A CN 104804652A CN 201510207197 A CN201510207197 A CN 201510207197A CN 104804652 A CN104804652 A CN 104804652A
- Authority
- CN
- China
- Prior art keywords
- parts
- environment
- friendly type
- tackiness agent
- type building
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种环保型建筑胶粘剂,由下列重量份的原料制成:草酸5-5.6份,硼砂0.8-1.3份,羟乙基尿素6-6.5份,丙酮12-16份,填料20-40份,醋酸乙稀脂40-52份,水80-90份。本发明的环保型建筑胶粘剂粘接强度高、不含甲醛、无毒无污染、成本低、施工方便,从根本上保护好环境、生产人员、施工人员及广大用户的人身健康与安全。
Description
技术领域
本发明涉及建筑胶粘剂领域,具体涉及一种环保型建筑胶粘剂。
背景技术
随着人们生活水平的提高,建筑装潢市场对建筑胶粘剂量的需求越来越大,居住环保也成了人们关注的焦点,因此在胶粘剂产品设计的思想、生产原料的选用、胶粘剂的生产过程与工艺、胶粘剂产品的应用都应该是环境友好、无毒、无害的环保产品,从根本上保护好环境、生产人员、施工人员及广大用户的人身健康与安全,这是建筑胶粘剂发展方向中的大问题。而传统的107胶水、801胶水和901胶水等均因含有害物质,长期危害人们的身体健康,而逐渐被市场淘汰。
发明内容
本发明提供一种粘接强度高、不含甲醛、无毒无污染、成本低的环保型建筑胶粘剂,从根本上保护好环境、生产人员、施工人员及广大用户的人身健康与安全。
本发明一种环保型建筑胶粘剂所采用的技术方案是:一种环保型建筑胶粘剂,由下列重量份的原料制成:草酸5-5.6份,硼砂0.8-1.3份,羟乙基尿素6-6.5份,丙酮12-16份,填料20-40份,醋酸乙稀脂40-52份,水80-90份。
进一步地,由下列最优配比的原料制成:草酸5.3份,硼砂1份,羟乙基尿素6.2份,丙酮13份,填料30份,醋酸乙稀脂44份,水86份。
进一步地,填料为石膏、钛白粉、滑石粉中的一种,也可以使用其混合物。
进一步地,其制备方法是:按配方备料;将醋酸乙稀脂和水加入反应釜中搅拌半小时,然后加热至60-70度;继续加热至80度时,再以细流方式将草酸,硼砂,羟乙基尿素及丙酮加入反应釜静置2-3小时后搅拌;20分钟后加入填料再充分搅拌,得到的产品就是环保型建筑胶粘剂;待冷却后包装。
本发明的有益效果是:本发明的环保型建筑胶粘剂粘接强度高、不含甲醛、无毒无污染、成本低、施工方便,从根本上保护好环境、生产人员、施工人员及广大用户的人身健康与安全。
具体实施方式
下面结合具体实施例对本发明作进一步说明。
实施例1:
本发明一种环保型建筑胶粘剂,由下列重量份的原料制成:草酸5份,硼砂0.8份,羟乙基尿素6份,丙酮12份,填料20份,醋酸乙稀脂40份,水80份。
填料为石膏、钛白粉、滑石粉中的一种,也可以使用其混合物。
本发明一种环保型建筑胶粘剂的其制备方法是:
1.按配方备料:草酸5份,硼砂0.8份,羟乙基尿素6份,丙酮12份,填料20份,醋酸乙稀脂40份,水80份;
2.将醋酸乙稀脂和水加入反应釜中搅拌半小时,然后加热至60-70度;
3.继续加热至80度时,再以细流方式将草酸,硼砂,羟乙基尿素及丙酮加入反应釜静置2-3小时后搅拌;
4.20分钟后加入填料再充分搅拌,得到的产品就是环保型建筑胶粘剂;
5.待冷却后包装。
实施例2:
本发明一种环保型建筑胶粘剂,由下列重量份的原料制成:草酸5.6份,硼砂1.3份,羟乙基尿素6.5份,丙酮16份,填料40份,醋酸乙稀脂52份,水90份。
填料为石膏、钛白粉、滑石粉中的一种,也可以使用其混合物。
本发明一种环保型建筑胶粘剂的其制备方法是:
1.按配方备料:草酸5.6份,硼砂1.3份,羟乙基尿素6.5份,丙酮16份,填料40份,醋酸乙稀脂52份,水90份;
2.将醋酸乙稀脂和水加入反应釜中搅拌半小时,然后加热至60-70度;
3.继续加热至80度时,再以细流方式将草酸,硼砂,羟乙基尿素及丙酮加入反应釜静置2-3小时后搅拌;
4.20分钟后加入填料再充分搅拌,得到的产品就是环保型建筑胶粘剂;
5.待冷却后包装。
实施例3,为本发明的最优实施例:
本发明一种环保型建筑胶粘剂,由下列重量份的原料制成:草酸5.3份,硼砂1份,羟乙基尿素6.2份,丙酮13份,填料30份,醋酸乙稀脂44份,水86份。
填料为石膏、钛白粉、滑石粉中的一种,也可以使用其混合物。
本发明一种环保型建筑胶粘剂的其制备方法是:
1.按配方备料:草酸5.6份,硼砂1.3份,羟乙基尿素6.5份,丙酮16份,填料40份,醋酸乙稀脂52份,水90份;
2.将醋酸乙稀脂和水加入反应釜中搅拌半小时,然后加热至60-70度;
3.继续加热至80度时,再以细流方式将草酸,硼砂,羟乙基尿素及丙酮加入反应釜静置2-3小时后搅拌;
4.20分钟后加入填料再充分搅拌,得到的产品就是环保型建筑胶粘剂;
5.待冷却后包装。
综上所述,本发明的环保型建筑胶粘剂粘接强度高、不含甲醛、无毒无污染、成本低、施工方便,从根本上保护好环境、生产人员、施工人员及广大用户的人身健康与安全。
Claims (4)
1.一种环保型建筑胶粘剂,其特征在于由下列重量份的原料制成:草酸5-5.6份,硼砂0.8-1.3份,羟乙基尿素6-6.5份,丙酮12-16份,填料20-40份,醋酸乙稀脂40-52份,水80-90份。
2.如权利要求1所述的环保型建筑胶粘剂,其特征在于由下列最优配比的原料制成:草酸5.3份,硼砂1份,羟乙基尿素6.2份,丙酮13份,填料30份,醋酸乙稀脂44份,水86份。
3.如权利要求1所述的环保型建筑胶粘剂,其特征在于:填料为石膏、钛白粉、滑石粉中的一种,也可以使用其混合物。
4.如权利要求1所述的环保型建筑胶粘剂,其特征在于:其制备方法是:
按配方备料;
将醋酸乙稀脂和水加入反应釜中搅拌半小时,然后加热至60-70度;
继续加热至80度时,再以细流方式将草酸,硼砂,羟乙基尿素及丙酮加入反应釜静置2-3小时后搅拌;
20分钟后加入填料再充分搅拌,得到的产品就是环保型建筑胶粘剂;
待冷却后包装。