CN104775130B - A kind of environment-friendly metal skimmed milk and preparation method thereof - Google Patents

A kind of environment-friendly metal skimmed milk and preparation method thereof Download PDF

Info

Publication number
CN104775130B
CN104775130B CN201510223261.4A CN201510223261A CN104775130B CN 104775130 B CN104775130 B CN 104775130B CN 201510223261 A CN201510223261 A CN 201510223261A CN 104775130 B CN104775130 B CN 104775130B
Authority
CN
China
Prior art keywords
parts
sodium
skimmed milk
environment
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201510223261.4A
Other languages
Chinese (zh)
Other versions
CN104775130A (en
Inventor
柯斌清
柯杰
柯宇杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510223261.4A priority Critical patent/CN104775130B/en
Publication of CN104775130A publication Critical patent/CN104775130A/en
Application granted granted Critical
Publication of CN104775130B publication Critical patent/CN104775130B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention provides a kind of environment-friendly metal skimmed milk, and its component and weight are:10 60 parts of sodium carbonate, 0.8 5 parts of coconut oil diethanol amide, 8 30 parts of sodium metasilicate, 0.5 3 parts of straight-chain alkyl polyoxyethylene ether sodium sulphate, 0.5 20 parts of sodium gluconate, 15 parts of capric acid diethanol amine, 16 parts of sodium hydroxide, it is good, environmentally friendly with degreasing effect, packaging, storage, convenient transportation and the features such as small freight volume.The present invention also provides the preparation method of the skimmed milk, is made at normal temperatures and pressures, and method is simple, rational technology, safe and reliable, can guarantee that product quality and industrialized production.

Description

A kind of environment-friendly metal skimmed milk and preparation method thereof
Technical field
The present invention relates to a kind of cleaning agent, more particularly to a kind of environment-friendly type skimmed milk handled for metal material surface, The invention further relates to the preparation method of the skimmed milk.
Background technology
Metal works are during manufacture, transport, storage and use, and because machining and antirust etc. need, its surface is applied There is grease.These greases are the compositions based on mineral grease and vegetable fat, and added with various organic or inorganic additives Composition is formed.Therefore in metal material surface processing, degreasing is important technical process, and the degreasing degree of metal surface will be straight Connect the subsequent treatment quality for having influence on workpiece.
Surface of workpiece lubricant component is more complicated, and a class is the saponified oil based on fatty glyceride, can be passed through Removed with the saponification of alkali;Another kind of is mineral oil (non-soap carburetion), can be removed by emulsification.
At present, the auxiliary agent of most water-base metal degreasing agents is still based on phosphate, because phosphate is in degreasing agent In existing chelation, have decontamination again, and have good washing and the low feature of use cost.But as people get over Carry out more attaching importance to environmental protection, more and more stricter is required to the limitation that P elements are discharged, inexorable trend is turned into using agent of non-phosphate degreasing.
In addition, metal degreasing agent on the market is largely fluid product at present, active constituent content is limited, to packaging, Storage, transport add cost.
The content of the invention
It is an object of the invention to solve the problem of prior art is present there is provided a kind of environment-friendly metal skimmed milk, have Degreasing effect is good, environmentally friendly, packaging, storage, convenient transportation and the features such as small freight volume.
The concrete technical scheme used for:
A kind of environment-friendly metal skimmed milk, the component and its weight of the skimmed milk are:10-60 parts of sodium carbonate, 0.8-5 parts of coconut oil diethanol amide, 8-30 parts of sodium metasilicate, 0.5-3 parts of straight-chain alkyl polyoxyethylene ether sodium sulphate, glucose Sour sodium 0.5-20 parts, 1-5 parts of capric acid diethanol amine, 1-6 parts of sodium hydroxide.
It is preferred that, the skimmed milk also contains 0.2-0.8 parts of disodium ethylene diamine tetraacetate.
It is preferred that, the weight distribution ratio of disodium ethylene diamine tetraacetate is 0.5-0.8 parts in the skimmed milk.
It is preferred that, the weight of the component of the skimmed milk is:20-50 parts of sodium carbonate, coconut oil diethanol amide 1-3 parts, 15-25 parts of sodium metasilicate, 1.2-2 parts of straight-chain alkyl polyoxyethylene ether sodium sulphate, 2-18 parts of sodium gluconate, capric acid two 2-3.5 parts of monoethanolamine, 2.5-4 parts of sodium hydroxide.
Compared with prior art, the environment-friendly metal skimmed milk that the present invention is provided possesses following advantage:
1st, phosphate or polyphosphoric acid are replaced using the orthosilicate with excellent oil removing, corrosion inhibition, certain complexing Salt, possesses more preferable deoiling effect and environmental protection.
2nd, it can use at normal temperatures.
3rd, various metals, such as carbon steel, stainless steel, titanium or titanium alloy, copper and copper alloy be can be universally used in.
4th, in Chemical cleaning, electrolytic cleaned, ultrasonic cleaning technique, effect is notable.
5th, metal degreasing agent at present on the market is largely fluid product, and active constituent content is limited;The environment-friendly type Metal spent meal is powder product and active constituent content is more, and packaging, storage, convenient transportation, freight volume are small.
The present invention also provides the preparation method of the skimmed milk, and method is simple, rational technology, safe and reliable, including following step Suddenly:
A. 10-60 parts of sodium carbonate, 0.8-5 parts of coconut oil diethanol amide are added in mixer, mixes, stir;
B. the mixer is kept stirring for state, sequentially adds 8-30 parts of sodium metasilicate, straight-chain alkyl polyoxyethylene ether sulphur Sour sodium 0.5-3 parts, 0.5-20 parts of sodium gluconate, are well mixed;
C. the mixer is kept stirring for state, adds 1-5 parts of capric acid diethanol amine, 1-6 parts of sodium hydroxide, and mixing is equal Produced after even.
It is preferred that, in the step b, sequentially add sodium metasilicate, straight-chain alkyl polyoxyethylene ether sodium sulphate, gluconic acid Time interval between sodium is 2-8 minutes.
It is preferred that, in the step c, the time interval added between capric acid diethanol amine, sodium hydroxide is 2-8 minutes.
It is preferred that, the mixing time added after sodium gluconate is 2-8 minutes, and the mixing time added after sodium hydroxide is 15-25 minutes.
It is preferred that, described step a, b, c are carried out at normal temperatures and pressures.
It is preferred that, the mixer is vertical double-spiral conical mixer, and the rotating speed of the mixer is 20~60 revs/min Clock.
Compared with prior art, the preparation method for the skimmed milk that the present invention is provided possesses following advantage:
1st, it is made under normal temperature and pressure conditionses, it is simple and convenient.
2nd, the speed of mixer is 20-60 revs/min, both can guarantee that component stirred and production efficiency, and had been avoided that again Component influences properties of product because excessive friction is extruded.
3rd, method is simple, rational technology, safe and reliable, can guarantee that product quality and industrialized production.
Embodiment
Below in conjunction with the specific embodiment of the present invention, technical scheme is clearly and completely described.It is aobvious So, described embodiment is only the section Example of the present invention, rather than whole embodiments.Based on the implementation in the present invention Example, the every other embodiment that those of ordinary skill in the art are obtained on the premise of creative work is not made all belongs to In protection scope of the present invention.
Embodiment 1:
Following ingredients (parts by weight) are weighed by following proportionings:44 parts of sodium carbonate, 0.25 part of coconut oil diethanol amide, 32.8 parts of sodium metasilicate, 1 part of straight-chain alkyl polyoxyethylene ether sodium sulphate, 15 parts of sodium gluconate, disodium ethylene diamine tetraacetate 0.7 Part, 3.8 parts of sodium hydroxide, 2.5 parts of capric acid diethanol amine.
Preparation method:First by 44 parts of addition mixing and blending machines of sodium carbonate, 0.25 part of coconut oil diethanol amide is added; At normal temperatures and pressures, mixer switch is opened, regulation rotating speed is kept stirring for state to 36 revs/min.It is subsequently added into sodium metasilicate 32.8 parts, stir 5 minutes;1 part of straight-chain alkyl polyoxyethylene ether sodium sulphate is added, is stirred 5 minutes;Add sodium gluconate 15 Part, stir 5 minutes;Then, 0.7 part of disodium ethylene diamine tetraacetate is added, 2.5 parts of capric acid diethanol amine, hydroxide is subsequently added into 3.8 parts of sodium, continues to stir 20 minutes, is sufficiently mixed uniformly, produces powder product.
The rotating speed such as following table of embodiment 2-6, each component consumption and mixer, remaining operation be the same as Example 1:
The skimmed milk that the present invention is provided after testing and application, major technique and performance indications are as follows:
(1) the key technical indexes:
1st, outward appearance:White or faint yellow homogeneous solid
2nd, pH value (3% aqueous solution g/L):12.5-13.5
3rd, alkali point (3% aqueous solution g/L):≥16
4th, phosphorus content is (with PO4 2+Meter, %):≤ 0.0005%
5th, nitrogen content is (with NH4 +Meter, %):≤ 0.0002%
6th, it is biodegradable (lower 21 days of natural conditions):>=95%
(2) main performance index:
1st, tank liquor concentration (g/L):5-30
2nd, treatment temperature (DEG C):It can use at normal temperatures, optimum temperature is 60-80 DEG C.
3rd, processing time (s):8-30s can wash the greasy dirt of surface of steel plate.
4th, washing rate (%):>=95%
5th, cleaning way:Various cleaning ways are applicable to, such as sprays, impregnate, be cleaned by ultrasonic.
Several embodiments of the present invention are the foregoing is only, but protection scope of the present invention is not limited thereto, The those of ordinary skill of any skilled in the technical scope of present disclosure, the change that can readily occur in or Replace, should all cover within the scope of the present invention.Therefore, protection scope of the present invention should be with the protection of the claim Scope is defined.

Claims (8)

1. a kind of environment-friendly metal skimmed milk, it is characterised in that the component and its weight of the skimmed milk be:Sodium carbonate 10-60 parts, 0.8-5 parts of coconut oil diethanol amide, 8-30 parts of sodium metasilicate, straight-chain alkyl polyoxyethylene ether sodium sulphate 0.5-3 Part, 0.5-20 parts of sodium gluconate, 1-5 parts of capric acid diethanol amine, 1-6 parts of sodium hydroxide;Disodium ethylene diamine tetraacetate 0.2-0.8 Part.
2. a kind of environment-friendly metal skimmed milk according to claim 1, it is characterised in that the weight of the component of the skimmed milk Amount part, which matches, is:20-50 parts of sodium carbonate, 1-3 parts of coconut oil diethanol amide, 15-25 parts of sodium metasilicate, straight chained alkyl polyoxy second 1.2-2 parts of alkene ether sodium sulfate, 2-18 parts of sodium gluconate, 2-3.5 parts of capric acid diethanol amine, 2.5-4 parts of sodium hydroxide, ethylenediamine 0.5-0.8 parts of tetraacethyl disodium.
3. a kind of preparation method of environment-friendly metal skimmed milk as claimed in claim 1, it is characterised in that including following step Suddenly:
A. 10-60 parts of sodium carbonate, 0.8-5 parts of coconut oil diethanol amide are added in mixer, mixes, stir;
B. the mixer is kept stirring for state, sequentially adds 8-30 parts of sodium metasilicate, straight-chain alkyl polyoxyethylene ether sodium sulphate 0.5-3 parts, 0.5-20 parts of sodium gluconate, are well mixed;
C. the mixer is kept stirring for state, adds 0.2-0.8 parts of disodium ethylene diamine tetraacetate;Capric acid diethanol amine 1-5 Part, 1-6 parts of sodium hydroxide, are produced after being well mixed.
4. the preparation method of environment-friendly metal skimmed milk according to claim 3, it is characterised in that in the step b, according to The secondary time interval added between sodium metasilicate, straight-chain alkyl polyoxyethylene ether sodium sulphate, sodium gluconate is 2-8 minutes.
5. the preparation method of environment-friendly metal skimmed milk according to claim 3, it is characterised in that in the step c, plus It is 2-8 minutes to enter the time interval between capric acid diethanol amine, sodium hydroxide.
6. the preparation method of the environment-friendly metal skimmed milk according to claim 3, it is characterised in that add gluconic acid Mixing time after sodium is 2-8 minutes, and the mixing time added after sodium hydroxide is 15-25 minutes.
7. the preparation method of environment-friendly metal skimmed milk according to claim 3, it is characterised in that described step a, b, c Carry out at normal temperatures and pressures.
8. the preparation method of environment-friendly metal skimmed milk according to claim 3, it is characterised in that the mixer is vertical Formula double-spiral conical mixer, the rotating speed of the mixer is 20~60 revs/min.
CN201510223261.4A 2015-05-05 2015-05-05 A kind of environment-friendly metal skimmed milk and preparation method thereof Expired - Fee Related CN104775130B (en)