CN104774983B - Anion and cation charge control resin - Google Patents

Anion and cation charge control resin Download PDF

Info

Publication number
CN104774983B
CN104774983B CN201510101113.5A CN201510101113A CN104774983B CN 104774983 B CN104774983 B CN 104774983B CN 201510101113 A CN201510101113 A CN 201510101113A CN 104774983 B CN104774983 B CN 104774983B
Authority
CN
China
Prior art keywords
resin
cation
mixed liquor
anion
leather
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201510101113.5A
Other languages
Chinese (zh)
Other versions
CN104774983A (en
Inventor
高文杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510101113.5A priority Critical patent/CN104774983B/en
Publication of CN104774983A publication Critical patent/CN104774983A/en
Application granted granted Critical
Publication of CN104774983B publication Critical patent/CN104774983B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

An anion and cation charge control resin is a finishing material used on the surface of tanning leather, and belongs to the field of leather finishing. The anion and cation charge control resin solves the problem that the leather products using Nappa leather, aniline leather and slunk as the raw materials lose the original softness, and becomes hard and poor in hand feeling in the traditional leather cleaning and maintenance process, also solves the technical problem that anion and cation resin can not be used at the same time. A technical scheme is as below: adding anion acrylic resin, polyurethane resin, protein resin and a softening agent into a container, and stirring uniformly for stand-by; adding a neutral wax liquid, a weak cation wax liquid and water into another container, and stirring uniformly. adding the cation resin into the mixed liquor of wax liquid, and stirring uniformly; and finally, adding the mixed liquor of the cation resin into the mixed liquor of the various anion resin, stirring uniformly and filtering to obtain the anion and cation charge control resin.

Description

Zwitterion electric charge adjusts resin
One. technical field
The present invention relates to leather surface coating technology field, and in particular to the covering with paint used by bibulous leather surface into Film --- -- resin.After this resin is covered with paint, lacquer, colour wash, etc. on leather and fur products surface, leather surface will be formed it is a kind of it is soft, The suitable coating of light, gives leather pure and fresh, beautiful sense.
Two. technical background
1. the scheme of prior art
, for fashion and attractive in appearance, great majority are all using nappa leather, the aniline that cortex is frivolous, soft for present leather wear , used as raw material, this is leather-like due to frivolous, softness, with the sensation as silk for leather, abortive calfskin.Wear graceful elegant, U.S. Sight is generous, firmly gets consumers in general's favor.But this leather-like water imbibition is especially strong, with traditional coating method, far from Requirement is covered with paint, lacquer, colour wash, etc. in the beauty cleaning that these leather and fur products instantly can be met.
Traditional coating method.Film-forming resin is directly coated on into leather surface.Leather leather in tannery is carried Negative electrical charge, in anionic state;And film-forming resin is all the anionic materials with negative electrical charge.By anion film-forming resin Cover with paint, lacquer, colour wash, etc. on the leather with negative electrical charge, leather can not prevent the infiltration of film-forming resin.So leather just suck it is substantial amounts of it is cloudy from Sub- film-forming resin.After dry, a very thick tunic will be formed, leather will become very hard, raw hide leather goods are lost completely Pliability.The stronger leather of water imbibition, as the method with is covered with paint, lacquer, colour wash, etc., direct result is exactly the clothes of some leather and fur products can not Wear again.
Cationic Finish technology is introduced again now.Will resin cation be first sprayed on leather surface (be commonly called as envelope Bottom), then resin anion (R.A.) is sprayed on the leather of back cover again, be so in order to prevent film-forming resin from permeating toward in leather, One layer of thin film is only formed on back cover layer, leather would not suck substantial amounts of film-forming resin and be hardened.
2. the shortcoming of prior art
Cationic Finish technology now, although prevent the infiltration of film-forming resin, but because of the resin cation of back cover layer Very strong positive and negative charge is all carried with the moon for covering with paint, lacquer, colour wash, etc. film forming agent from resin itself.After positive and negative charge contacts with each other, the film of formation is Harder, the pliability of raw hide leather is not reached, change the original style of raw hide leather.This is of current leather finish field Disappearance technology.Cause the clothes of many leather and fur products into " disposable " clothes, it is impossible to which beauty cleaning is covered with paint, lacquer, colour wash, etc..
Three. the content of the invention
1. technical problem solved by the invention.
The present invention " zwitterion electric charge adjusts resin ", solve current film-forming resin makes leather be hardened during covering with paint The problem poor with feel.Also solving yin and yang resin can not be while the difficult problem for using put together.
The zwitterion electric charge of the present invention adjusts the charge density that resin weakens zwitterion, reduces charge difference, makes into The electric charge of film dies down.The present invention zwitterion electric charge adjust resin, cover with paint, lacquer, colour wash, etc. on leather will shape --- ----softness it is thin Film, has reached and has softened the leather purposefully, remains original style and features of raw hide leather.
1. first, the present invention has broken the unicity of film-forming resin.The present invention is modulated with various zwitterion film-forming resins, Mutually learn from other's strong points to offset one's weaknesses, comprehensive effect, beyond any single film-forming resin.
2. zwitterion is organically combined.Resin cation is brought in the film-forming resin of anion by auxiliary agent, the moon is made Cation combines, and forms " the zwitterion electric charge regulation tree of a kind of new filmogen, i.e. my invention Fat ".
It is well known that during leather finish, two kinds of resins of negative and positive must not be mixed and be used.If being mixed in one Rise and use, zwitterion horse back breakdown of emulsion forms block, becomes pasty state, loses validity, it is impossible to use.This is now in all teaching materials All it is so to discuss.
And the zwitterion electric charge that I invents adjusts resin, exactly solves the problems, such as that zwitterion resin can not be together. The present invention is, by auxiliary agent and special modulator approach, zwitterion resin to be combined, not breakdown of emulsion, is not tied Block.Just because of the combination of zwitterion resin, the strong of the positive and negative charge that zwitterion itself is carried greatly is reduced Degree, that is to say, that the charge density that the zwitterion electric charge of my invention is adjusted in resin is reduced.The negative and positive of my invention from Charge of the electron adjusts resin and covers with paint, lacquer, colour wash, etc. on leather, and the film of formation would not make leather be hardened, and make cortex become very soft.It is bright It is aobvious to feel than raw hide leather softness much, and brightness is suitable, and without modeling sense, resistance to complications, viscosity fastness strengthens, and combination property has very big Raising.
2. the benefit that the present invention brings
1. film forming is soft, repairs and recover the leather being hardened.
The leather fur clothing that the zwitterion electric charge of every use my invention adjusts resin covering with paint is all very soft, it will be apparent that super Go out raw hide leather, the pliability of fur clothing.Raw hide clothing is harder, touches " hitting hand ", after the zwitterion resin of my invention is covered with paint, lacquer, colour wash, etc., Just become very soft at once.Either domestic or import resin can not all reach this effect.
2. combination property strengthens
Except softness is outside one's consideration, other performances, such as cold resistance, viscosity fastness, water proofing property, tortuosity, light appropriateness are all much Beyond the function that domestic and international any single resin has.
3. low cost
A kinds:Can be raw material modulation completely by domestic resin, cost greatly reduces, break from external import resin ridge The bad phenomenon of disconnected China market.Stocked up calculating with current retail market price (Beijing retailer rather than producer stocks up)
Less than acrylic resin (18 yuan/kilogram are stocked up) 11.2%
Less than polyurethane resin (28 yuan/kilogram are stocked up) 43%
B kinds:With yuan/kilogram of external import raw material 60, modulation cost reduction by 47%
C kinds:It is that raw material modulation cost reduces by 51% with domestic and imported resin
That is
A. it is 16 yuan completely with domestic resin modulation per kilogram cost.
B. it is 31.05 yuan with import resin modulation per kilogram cost
C. closed with domestic and imported resin and adjust per kilogram cost to be 23.80 yuan
Above said that these materials were stocked up completely by retail price, well imagined if being changed to producer and stocking up, cost Can also be greatly lowered.
3rd, environmental protection
Its not only low cost but also environmental protection, it does raw material and medium without solvent-borne type material, and water miscible covering with paint is used completely Material and do medium with water.It is free from environmental pollution, cheap, easy to use, energy-saving material.
4. the present invention is through many experiments, and is proved that effect is very good in practice.
1.. I has individual fur specially to wash shop in Heilongjiang Province's Yichun, and the leather and fur products covered with paint, lacquer, colour wash, etc. with resin of the present invention is obtained Unanimously approve and approve of to consumers in general.
2.. trade Co., Ltd of Tian Chengzhong Australia of Harbin City, sign a contract with me, carry out technological cooperation.
Four. description of the drawings ----nothing
Five. specific embodiment
This cloudy anionic charge adjust resin be by acrylic resin, polyurethane resin, protein resin, softening agent, Neutral cured liquid, the cured liquid of weak cation, resin cation and water hybrid modulation are formed, and the proportioning of each composition is by weight:
1. the electric charge modulated with domestic raw material adjusts resin
A, acrylic resin:500-800
B, polyurethane resin:200-300
C, protein resin:15-30
D, softening agent:30-40
E, neutral cured liquid:50-150
The cured liquid of F, weak cation:50-150
G, resin cation:200-300
H, water (distilled water):800-1000
This zwitterion electric charge adjusts the preparation method of resin and comprises the following steps:
(1) acrylic resin, polyurethane resin, protein, softening agent, neutral cured liquid, weak cation are weighed by proportioning cured Liquid, resin cation, water (distilled water)
(2) first negative acrylic resin, polyurethane resin, protein resin, softening agent added in molten device, in room temperature Lower stirring 20-30min
(3) neutral cured liquid, the cured liquid of weak cation, water is put in another molten device again, stirred at normal temperatures 20min just may be used.
(4) and then, then resin anion (R.A.) is added to mix up cured liquid mixing in (i.e. 3) stirring 20min
(5) it is last again by the mixed liquor (i.e. 4) of resin cation and cured emulsion, then instill and modulated by various resin anion (R.A.)s Mixed liquor in (i.e. 2), the time does not limit, it is uniform till.
2. the electric charge for being prepared with imported raw material adjusts resin
A. import special type film forming agent:400-550
B. import aniline film forming agent:400-550
C. softening agent:30-40
D. neutral cured liquid:50-150
E. the cured liquid of weak cation:50-150
F. resin cation:200-300
G. water (distilled water):800-1000
This zwitterion electric charge adjusts the preparation method of resin and comprises the steps:
(1) import special type film forming agent, import aniline film forming agent, softening agent, neutral cured liquid, weak sun are weighed up from cured by proportioning Liquid, resin cation, water (distilled water)
(2) first negative special type film forming agent, aniline film forming agent, softening agent be added in molten device, 20- is stirred at room temperature 30min
(3) neutral cured liquid, the cured liquid of weak cation and water put in another molten device again, stirred at room temperature, 20min just may be used
(4) and then, then resin cation is added in the cured liquid mixed liquor for mixing up (i.e. 3) stirring 20min
(5) it is last, the mixed liquor (i.e. 4) of the cured emulsion of resin cation is added dropwise to into again what is modulated by various resin anion (R.A.)s (i.e. 2) time does not limit in mixed liquor, it is uniform till.
3. the resin and preparation method adjusted is closed with domestic and imported material:
The resin that the resin of domestic modulation is added the imported material modulation of equivalent is mixed as together, till stirring.Just Into the hybrid resin of domestic and imported resin.

Claims (2)

1. a kind of covering with paint adjusts resin in the zwitterion electric charge of leather surface, by resin anion (R.A.) mixed liquor, resin cation Mixed liquor, softening agent, wax emulsion auxiliary agent and distilled water composition;
Its proportioning is by weight;
It is characterized in that described resin anion (R.A.) mixed liquor be acrylic resin, polyurethane resin, protein resin, softening agent mix Close modulation to form, described resin cation mixed liquor is by resin cation, neutral wax emulsion, weak cation wax emulsion and steaming Distilled water is constituted;
Acrylic resin, polyurethane resin, protein resin, softening agent ratio are in wherein described resin anion (R.A.) mixed liquor:
Acrylic resin: polyurethane resin: protein resin: softening agent=500-800: 200-300: 15-30: 30-40
Wherein described resin cation mixed liquor cationic resin, neutral wax emulsion, weak cation wax emulsion and distilled water Ratio be:
Resin cation: neutral wax emulsion: weak cation wax emulsion: distilled water=200-300: 50-150: 50-150: 800- 1000。
2. the zwitterion electric charge described in claim 1 adjusts the preparation method of resin, it is characterized in that comprising the following steps,
Step one resin anion (R.A.) mixed liquor:Acrylic resin 500-800, polyurethane resin 200- are weighed by weight ratio 300, protein resin 15-30, softening agent 30-40, in adding it to container, are stirred at room temperature 20min;
Step 2 resin cation mixed liquor:Neutral wax emulsion 50-150, weak cation wax emulsion 50- are weighed by weight ratio 150, resin cation 200-300, distilled water 800-1000;
A. first neutral wax emulsion, weak cation wax emulsion and distilled water are added in another container and stir 20min;
B. resin cation is added in A again and stirs 20min, resin cation mixed liquor is prepared and just completed;
Step 3 is at leisure added dropwise to resin cation mixed liquor in resin anion (R.A.) mixed liquor, instills while stirring, the time Do not limit, till dripping off;
Step 4 120 mesh filter screen filtrations, bottling.
CN201510101113.5A 2015-03-06 2015-03-06 Anion and cation charge control resin Expired - Fee Related CN104774983B (en)