CN104634605A - Cutting method for detecting longitudinal residual stress of bar material - Google Patents

Cutting method for detecting longitudinal residual stress of bar material Download PDF

Info

Publication number
CN104634605A
CN104634605A CN201410827678.7A CN201410827678A CN104634605A CN 104634605 A CN104634605 A CN 104634605A CN 201410827678 A CN201410827678 A CN 201410827678A CN 104634605 A CN104634605 A CN 104634605A
Authority
CN
China
Prior art keywords
cutting method
residual stress
bar
cutting
longitudinal residual
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410827678.7A
Other languages
Chinese (zh)
Inventor
李国�
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Baotou Iron and Steel Group Co Ltd
Inner Mongolia Baotou Steel Union Co Ltd
Original Assignee
Baotou Iron and Steel Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Baotou Iron and Steel Group Co Ltd filed Critical Baotou Iron and Steel Group Co Ltd
Priority to CN201410827678.7A priority Critical patent/CN104634605A/en
Publication of CN104634605A publication Critical patent/CN104634605A/en
Pending legal-status Critical Current

Abstract

The invention relates to a cutting method for detecting a longitudinal residual stress of a bar material. The cutting method is characterized by comprising the following steps: cutting a rod material section with the length of 500mm from one end of a to-be-detected rod material as a detection component, respectively measuring out 15mm from a central part of a bar body of the detection component to two sides, and cutting off a test sample with the length of 30mm along the peripheral direction. The cutting method disclosed by the invention has the advantages that the cutting method is simple, a cutting part is reasonably selected, and the longitudinal residual stress of the bar material can be rapidly and accurately detected.

Description

A kind of detection bar longitudinal residual stress cutting method
Technical field
The present invention relates to a kind of detection bar longitudinal residual stress cutting method, belong to detection technique field.
Background technology
Bar is one of major product of Baogang, and be the necessity of the engineerings such as building, bridge, the unrelieved stress existed in cold-drawn bar is very high, very easily ruptures, and affects the quality of product, has direct relation with people's productive life.
Because bar residual stress test does not have standard, do not detect the report of bar with strain gauge method, the selection of patch location seems particularly important, and how to detect is the problem studied at present.
Summary of the invention
The object of the invention is in order to fast, accurately bar longitudinal residual stress can be detected, provide a kind of and detect bar longitudinal residual stress cutting method.
Technical scheme of the present invention is as follows:
Intercept the bar section of long 500mm from bar one end to be detected as detection piece, in the centre of detection piece rod body, respectively measure 15mm to both sides, along the circumferential direction cut the sample that length is 30mm.
Advantage of the present invention is: method is simple, and cutting part is chosen rationally, can detect the longitudinal residual stress of bar fast and accurately.
Accompanying drawing explanation
Fig. 1 is cutting position schematic diagram of the present invention.
Embodiment
With reference to accompanying drawing, intercept the bar section of long 500mm from bar one end to be detected as detection piece 1, in the centre of detection piece rod body, respectively measure 15mm to both sides, along the circumferential direction cut the sample that length is 30mm.
Because the stress surveyed is longitudinal residual stress, so cut direction is detection piece circumference, make detection piece when not fettering, release stress, bar longitudinal stress situation could be measured truly, cut direction is incorrect, and the stress value measured is not meridional stress value, or does not measure result or data are inaccurate.

Claims (1)

1. one kind is detected bar longitudinal residual stress cutting method, it is characterized in that: intercept the bar section of long 500mm from bar one end to be detected as detection piece, in the centre of detection piece rod body, respectively measure 15mm to both sides, along the circumferential direction cut the sample that length is 30mm.
CN201410827678.7A 2014-12-26 2014-12-26 Cutting method for detecting longitudinal residual stress of bar material Pending CN104634605A (en)