CN104551226A - Cutting method for testing axial residual stress of seamless tube - Google Patents

Cutting method for testing axial residual stress of seamless tube Download PDF

Info

Publication number
CN104551226A
CN104551226A CN201410827712.0A CN201410827712A CN104551226A CN 104551226 A CN104551226 A CN 104551226A CN 201410827712 A CN201410827712 A CN 201410827712A CN 104551226 A CN104551226 A CN 104551226A
Authority
CN
China
Prior art keywords
cutting method
seamless tube
cutting
residual stress
axial residual
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410827712.0A
Other languages
Chinese (zh)
Inventor
李国�
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Baotou Iron and Steel Group Co Ltd
Inner Mongolia Baotou Steel Union Co Ltd
Original Assignee
Baotou Iron and Steel Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Baotou Iron and Steel Group Co Ltd filed Critical Baotou Iron and Steel Group Co Ltd
Priority to CN201410827712.0A priority Critical patent/CN104551226A/en
Publication of CN104551226A publication Critical patent/CN104551226A/en
Pending legal-status Critical Current

Abstract

The invention relates to a cutting method for testing axial residual stress of a seamless tube. The cutting method is characterized by comprising the following steps of cutting out a seamless tube which is 1000mm long from one end of a to-be-tested bar to serve as a tested piece; measuring for 15mm to two sides respectively from the central position in the length direction of the tested piece, and respectively describing two circles vertical to the axis; then, cutting along the two described circles to form a circular ring which is 30mm wide. The cutting method has the advantages that the method is simple, cutting position selection is reasonable, and the axial residual stress of the seamless tube can be rapidly and accurately tested.

Description

A kind of cutting method of testing the axial unrelieved stress of solid drawn tube
Technical field
The present invention relates to a kind of cutting method of testing the axial unrelieved stress of solid drawn tube, belong to detection technique field.
Background technology
What unrelieved stress physical test method adopted has: x-ray method, method of magnetic, brittle coating method, optical method, acoustic method, electric resistance strain film method, wherein: electric resistance strain film method is a kind of method of relatively generally acknowledging both at home and abroad, the residual stress test of rail adopts paster method at present, performs European EN13674-1 standard.Up to the present, the residual stress test method of weldless steel tube does not have standard, and part adopts the method estimation of theory calculate, and adopt paster method actual measurement to have no report, also nobody studies specially, and the STRESS VARIATION at each position of steel pipe is all unclear.
Adopt electric resistance strain film method (paster method) to test the axial unrelieved stress of solid drawn tube, need counter stress to discharge, how to cut tested solid drawn tube and cut direction is the key detected, the selection of cutting position seems particularly important.
Summary of the invention
The object of the invention is, in order to fast, accurately detect the axial unrelieved stress of solid drawn tube, to provide a kind of cutting method of testing the axial unrelieved stress of solid drawn tube.
Technical scheme of the present invention is as follows:
The seamless pipeline section of long 1000mm is intercepted as detection piece from bar one end to be detected, in the center of the length direction of detection piece respectively to two-sided measurement 15mm, and draw two circles perpendicular to axis respectively, then cut along drawn circle, cut out the annulus of a wide 30mm.
Advantage of the present invention is: method is simple, and cutting position is selected rationally, to detect the axial unrelieved stress of solid drawn tube fast and accurately.
Accompanying drawing explanation
Fig. 1 is cutting position schematic diagram of the present invention.
Embodiment
With reference to accompanying drawing, the seamless pipeline section of long 1000mm is intercepted as detection piece 1 from bar one end to be detected, in the center of the length direction of detection piece respectively to two-sided measurement 15mm, and draw two circles perpendicular to axis respectively, then cut along drawn circle band saw, cut out the annulus of a wide 30mm.
Because the stress surveyed is axial unrelieved stress, so cut direction is detection piece circumferencial direction, make workpiece when not fettering, release stress, weldless steel tube force-bearing situation could be measured truly, cut direction is incorrect, and the stress value measured is not meridional stress value, or does not measure result or data are inaccurate.

Claims (1)

1. test the cutting method of the axial unrelieved stress of solid drawn tube for one kind, it is characterized in that: intercept the seamless pipeline section of long 1000mm from bar one end to be detected as detection piece, in the center of the length direction of detection piece respectively to two-sided measurement 15mm, and draw two circles perpendicular to axis respectively, then cut along drawn circle, cut out the annulus of a wide 30mm.
CN201410827712.0A 2014-12-26 2014-12-26 Cutting method for testing axial residual stress of seamless tube Pending CN104551226A (en)