CN104631723B - A kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method - Google Patents

A kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method Download PDF

Info

Publication number
CN104631723B
CN104631723B CN201410807350.9A CN201410807350A CN104631723B CN 104631723 B CN104631723 B CN 104631723B CN 201410807350 A CN201410807350 A CN 201410807350A CN 104631723 B CN104631723 B CN 104631723B
Authority
CN
China
Prior art keywords
synthetic enamel
solvent
diluent
ancient building
brush
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410807350.9A
Other languages
Chinese (zh)
Other versions
CN104631723A (en
Inventor
朱殿臣
刘爱林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GANSU XINGCHENG CONSTRUCTION ENGINEERING Co Ltd
Original Assignee
GANSU XINGCHENG CONSTRUCTION ENGINEERING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GANSU XINGCHENG CONSTRUCTION ENGINEERING Co Ltd filed Critical GANSU XINGCHENG CONSTRUCTION ENGINEERING Co Ltd
Priority to CN201410807350.9A priority Critical patent/CN104631723B/en
Publication of CN104631723A publication Critical patent/CN104631723A/en
Application granted granted Critical
Publication of CN104631723B publication Critical patent/CN104631723B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method, with solve traditional method be easily generated fade, crack performance, poisoning that workmen is easily generated by oil plant, allergy, the problem of variable color.The method step is: after brill life that pillar is levigate, and putty dry tack free carries out paint application, and assorted synthetic enamel is diluted brushing according to the height of natural conditions temperature, survives for three times.The feature of the present invention is as follows: 1, use synthetic enamel, eliminates the big Resina Toxicodendri verniciflui of tradition to operator's poisoning, the injury of allergy, reduces construction safety risk, improve Business Economic Benefit.2. using assorted alkyd ready-mixed paint and assorted synthetic enamel, durability and the storage life of ancient building paint extend.After covering with paint, lacquer, colour wash, etc. 3 years, surface color is gorgeous, without variable color and mildew phenomena.Reduce construction cost.Enable timber structure to reach be full of cracks moistureproof, anti-, anticorrosion, acid rain preventing, owing to lacquer painting is smooth hard, decrease and artificial portray destruction.

Description

A kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method
Technical field
The invention belongs to construction engineering technical field, particularly to cold nonirrigated farmland district historic building structure paint application method.
Background technology
Ancient Times in China construction history is long, and resource is the abundantest, is a jewel in the woods of architecture Art, in being The epitome of the national magnificent culture of China, is working people's crystallizations of wisdom in ancient times, Ye Shi China as one of the mark of ancient civilized country, Not only there is high history, science and artistic value, also there is important Exploitation Value simultaneously.
Color gorgeous paint colour painting of disputing in riotous profusion is the art that bearty in form created by ancient building, different regions, different nationalitys All there are different aesthetic taste and different religions ideas, the most each region, the traditional art of various nationalities to be respectively arranged with it special in form Point, Gansu Province is a multi-ethnic province, and the natural climate temperature difference is relatively big, in ancient building technique and other areas difference, Particularly highlighting in the paint of historic building structure and embody, workmen is easily generated by the big Resina Toxicodendri verniciflui traditional handicraft of employing Poisoning, allergic problem annoying ancient building repair protection work progress in a difficult problem.
Existing construction method uses big Resina Toxicodendri verniciflui (be commonly called as soil paint), in work progress operator be easily poisoned, allergy.Cover with paint, lacquer, colour wash, etc. After 3 years, surface blistering, colour-darkening, mouldy, poor durability after construction.
Summary of the invention
It is an object of the invention to provide a kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method, to solve tradition side Method be easily generated fade, crack performance, poisoning that workmen is easily generated by oil plant, allergy, the problem of variable color.
The technical scheme is that a kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method, at basic unit Reason, behaviour base oil, brush four road synthetic enamel solvent or diluent, sanding wax, wax polish, specifically comprise the following steps that
(1) base treatment: first the greasy dirt of Wood surface, mortar are cleaned out, then a time sand paper of mill, polish, Polish;
(2) grasping base oil: uniformly brushing base oil, base oil is allocated by weight: raw Oleum Verniciae fordii 6-7 part, alkyd varnish 2-2.5 Part, gasoline 0.1-0.5 part;
(3) brush four road synthetic enamel solvent or diluent, synthetic thinner allocates by weight: synthetic enamel 6-9 part, solvent or diluent 1- 2.8 part;
(4), sanding wax: first roughing sand wax is added kerosene chemical conversion atherosclerotic, is then coated with ancient building with polishing compound, finally uses gasoline By floating wax scrub;
(5), wax polish: smear one layer of light wax after sanding wax.
Preferably, described solvent or diluent by giving birth to Oleum Verniciae fordii, edible vegetable oil, gasoline form according to the volume ratio mix of 1:0.8:0.2.
Preferably, during brush four road synthetic enamel solvent or diluent, per pass paint interval time is 4-6h in summer, spring and autumn 10-12h, the winter Season 20-24h.
Preferably, brush first synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 6-8 part, solvent or diluent 2-2.8 Part.
Preferably, brush second synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 7-8.5: solvent or diluent 2-2.5.
Preferably, brush the 3rd road synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 8-8.7: solvent or diluent 2-2.3.
Preferably, brush the 4th road synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 8-9: solvent or diluent 1-2.
The feature of the present invention is as follows:
1, use synthetic enamel, eliminate the big Resina Toxicodendri verniciflui of tradition to operator's poisoning, the injury of allergy, reducing construction peace Full blast danger, improves Business Economic Benefit.
2. using assorted alkyd ready-mixed paint and assorted synthetic enamel, durability and the storage life of ancient building paint extend.It is coated with After adoring 3 years, surface color is gorgeous, without variable color and mildew phenomena.Reduce construction cost.Timber structure is enable to reach moistureproof, anti- Be full of cracks, anticorrosion, acid rain preventing, owing to lacquer painting is smooth hard, decrease and artificial portray destruction.
Detailed description of the invention
Term is explained: added, undercarriage is the industry slang of self-assembling formation, their boundary in paint colour painting technological process Line, typically with each eave beam hypodermis as boundary, it is added, and it is lower for undercarriage.Added big wood does colour painting more, and undercarriage does more to be covered or decorate with paint.
Following example are applied to ancient building oil colored paintings undercarriage and the big wood component such as upper trestle, Liang Fang.
In embodiment solvent or diluent by giving birth to Oleum Verniciae fordii, edible vegetable oil, gasoline mix form, raw Oleum Verniciae fordii, edible vegetable oil, gasoline proportionality are 1:0.8: 0.2.Brush per pass paint interval time, should be according to temperature at that time depending on, summer 4-6h, spring, autumn 10-12h, winter is 20-24h.
Embodiment 1.
After brill life that pillar is levigate, putty dry tack free (moisture content 1.5%) carries out paint application, and step is as follows:
(1), base treatment: first with operating on or the greasy dirt of Wood surface, mortar etc. are cleaned out, then by chunk glass Grinding a sand paper, will polish, polish, wolline stubble to grind off, and negative and positive angle glue mark to be removed, and external corner wants chamfered edge, rounding, goes up next Cause.
(2), behaviour's base oil: base oil to be brushed uniformly, can not leak brush.Base oil is allocated by weight: raw Oleum Verniciae fordii 7: alkyd Varnish 2.5: gasoline 0.5.
At knot and aperture smears gypsum putty, during modulation putty, putty is adjusted diluter by synthetic enamel to be added;Dried mill Sand paper, grinds off open country putty, cleans and cleans with wet cloth.Completely scrape gypsum putty, completely scrape one time with Puttying plate, light to be scraped, scrape Flat.Dried dry sanding paper, grinds off open country putty, cleans and cleans with wet cloth.Completely scrape second putty, big face steel disc scraper plate Scrape, flat smooth.Scraping with operating at little, inner corner trim wants straight.After putty parches, polish with No. zero sand paper, polish, clean and use Wet cloth is cleaned.
(3), brush first synthetic enamel solvent or diluent: priming paint adds synthetic thinner and adjusts the dilutest, it should be noted that smooth vertical and horizontal painting Brush, must not leak brush and stream pendant, carry out dry sanding paper, clean and clean with wet cloth after paint parches.In place of being found to have injustice, and Recurrence of disease at the same time next year smears putty, and dried local polishes, polishes, and cleans and cleans with wet cloth.First synthetic thinner is adjusted by weight Join: synthetic enamel 8: solvent or diluent 2.8.
(4), brush second synthetic enamel: brush second synthetic enamel, must not note leak brush and stream pendant.Parch rear ground wood sand Paper, as many in surface miliaria pimple, available No. 280 waterproof abrasive papers mill.As local have not only, uneven place, should and recurrence of disease at the same time next year spread putty, treat greasy After son parches, dry sanding paper, clean and clean with wet cloth.After having brushed second paint, just can carry out glaziers work.Second alcohol Acid solvent or diluent is allocated by weight: synthetic enamel 8.5: solvent or diluent 2.5.
(5), brush the 3rd road synthetic enamel: brush method with require same second, with No. 320 liquid honings, but it is noted that not Corner angle must be galled, gentle light will be reached, should clean after milled and clean with wet cloth.
3rd road synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 8.7: solvent or diluent 2.3.
(6), brush the 4th road synthetic enamel, the method for mopping and requirement are ibid.No. 320~No. 400 water are applied after having brushed 7d Sand papering, firmly wants uniformly during mill, should substantially be polished by brush stricture of vagina, and notice that corner angle must not gall, clean and with wet after milled Cloth is cleaned and is waited to do.4th road synthetic enamel its allocate by weight: synthetic enamel 9: solvent or diluent 2.
(7), sanding wax: first roughing sand wax is added kerosene chemical conversion atherosclerotic, then dips in the painting of upper polishing compound with staple and be covered with a door Face or window face, rubbed back and forth by staple with hands and come and go repeatedly, firmly want uniformly, wipe to there is half-light when rubbing, and size face is upper and lower Unanimously be as the criterion (must not gall corner angle), finally dips in gasoline by floating wax scrub with staple.
(8), wipe wax polish: with clean staple dip in wax polish very thin smear one layer, note wiping even cleaning, reach gloss satisfy Till Man.
(9), winter construction: interior paint engineering should be carried out under heating condition, and room temperature is kept in balance, and is the most preferably not less than 10 DEG C, and temperature must not change suddenly.Special messenger should be set simultaneously and be responsible for thermometric and switch door and window, in order to ventilation dehumidifying gas.
Embodiment 2. repeats the step of embodiment 1, and difference is: base oil is allocated by weight: raw Oleum Verniciae fordii 6: Alkyd varnish 2: gasoline 0.1.Brush first synthetic enamel is allocated by weight: synthetic enamel 6: solvent or diluent 2.Brush second alcohol Acid enamel paint is allocated by weight: synthetic enamel 7: solvent or diluent 2.Brush the 3rd road synthetic enamel is allocated by weight: alkyd Enamel paint 8: solvent or diluent 2.Brush the 4th road synthetic enamel is allocated by weight: synthetic enamel 8: solvent or diluent 1.

Claims (7)

1. a Zhong Han nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: it includes base treatment, the behaviour end Oil, brush four road synthetic enamel solvent or diluent, sanding wax, wax polish, specifically comprise the following steps that
(1) base treatment: first the greasy dirt of Wood surface, mortar are cleaned out, then a time sand paper of mill, will polish, polish;
(2) behaviour's base oil: uniformly brushing base oil, base oil allocates by weight: raw Oleum Verniciae fordii 6-7 part, alkyd varnish 2-2.5 part, Gasoline 0.1-0.5 part;
(3) brush four road synthetic enamel solvent or diluent, synthetic enamel solvent or diluent allocates by weight: synthetic enamel 6-9 part, solvent or diluent 1- 2.8 part;
(4) sanding wax: roughing sand wax first adds kerosene chemical conversion atherosclerotic, is then coated with ancient building with polishing compound, finally will be floating with gasoline Wax scrub;
(5) wax polish: smear one layer of light wax after sanding wax.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: institute State solvent or diluent by giving birth to Oleum Verniciae fordii, edible vegetable oil, gasoline form according to the volume ratio mix of 1:0.8:0.2.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: brush During four road synthetic enamel solvent or diluents, per pass paint interval time is 4-6h in summer, spring and autumn 10-12h, winter 20-24h.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: brush First synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 6-8 part, solvent or diluent 2-2.8 part.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: brush Second synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 7-8.5 part, solvent or diluent 2-2.5 part.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: brush 3rd road synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 8-8.7 part, solvent or diluent 2-2.3 part.
One the most according to claim 1 is trembled with fear nonirrigated farmland district ancient building colors synthetic enamel construction method, it is characterised in that: brush 4th road synthetic enamel solvent or diluent is allocated by weight: synthetic enamel 8-9 part, solvent or diluent 1-2 part.
CN201410807350.9A 2014-12-23 2014-12-23 A kind of cold nonirrigated farmland district ancient building colors synthetic enamel construction method Expired - Fee Related CN104631723B (en)