CN104460182B - The processing method and darkening ring of darkening ring - Google Patents
The processing method and darkening ring of darkening ring Download PDFInfo
- Publication number
- CN104460182B CN104460182B CN201410833306.5A CN201410833306A CN104460182B CN 104460182 B CN104460182 B CN 104460182B CN 201410833306 A CN201410833306 A CN 201410833306A CN 104460182 B CN104460182 B CN 104460182B
- Authority
- CN
- China
- Prior art keywords
- darkening ring
- hole
- darkening
- processing method
- aqueous slkali
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The present invention discloses a kind of processing method and darkening ring of the darkening ring, and described method includes following steps:Darkening ring is provided, the darkening ring includes body, is made coated on the anti-static coating on the body and the through hole being formed on the body, the body of plastic material, and the anti-static coating is carbon dust layer;Dumb light structure is formed on the hole wall of the through hole by alkali soluble corrosion.The processing method and darkening ring of the darkening ring of the present invention, darkening ring is handled in supersonic generator by aqueous slkali, to form dumb light structure on the hole wall of the through hole of darkening ring, to avoid the hole wall due to through hole it is reflective and caused by the undesirable condition such as dazzle, halation and ghost generation, and then ensure that shooting effect, improve the quality of shooting product.
Description
Technical field
The present invention relates to the processing method and darkening ring of camera technology field, more particularly to a kind of darkening ring.
Background technology
It is logical for adjusting that 3 to 5 darkening rings of placement are generally required inside camera in high-pixel mobile phone and digital camera
Optical port footpath and other veiling glares are blocked, be all with being handled after metal stamping by way of oxidizing blackening, to reach full-dull in the past
Purpose, but cost and expensive several times of plastic cement darkening ring decline to a great extent recently as cost, used instead surface band prevent it is quiet
Substituted after the direct punching press of polyethylene terephthalate (PET) raw material of the high shading coating of electricity, but as pixel is more next
Higher, the section of endoporus can leave shinny section after plastic cement punching press, and traditional nigrescence cannot be carried out as metal
Delustring is handled, so that it is bad to produce obvious dazzle, halation and ghost (FLARE) etc.
The content of the invention
It is a primary object of the present invention to provide the processing method and darkening ring of a kind of darkening ring, it is intended to solve existing screening
Aperture due to through-hole wall it is reflective and caused by the undesirable technical problem such as dazzle, halation and ghost.
To achieve the above object, the present invention provides a kind of processing method of darkening ring, the processing method bag of the darkening ring
Include following steps:
Darkening ring is provided, the darkening ring includes body, coated on the anti-static coating on the body and is formed at institute
The through hole on body is stated, the body is made of plastic material, and the anti-static coating is carbon dust layer, and the through hole passes through punching press
Formed;
Dumb light structure is formed on the hole wall of the through hole by alkali soluble corrosion.
Preferably, it is described specifically to be wrapped in the step of formation dumb light structure on the hole wall of the through hole by alkali soluble corrosion
Include:
Aqueous slkali is placed in supersonic generator;
Darkening ring is placed in the aqueous slkali, and is stirred.
Preferably, the body is made of polyethylene terephthalate, and the aqueous slkali is sodium bicarbonate solution, its
Concentration is 5%~35%.
Preferably, the temperature of the aqueous slkali is 35~55 degree, when the time of the stirring is 3~5 small.
Preferably, the power of the supersonic generator is 300~500 watts.
Preferably, the thickness of the darkening ring is 0.025 millimeter, a diameter of 2.14 millimeters of the through hole.
In addition, to achieve these goals, the present invention also provides a kind of darkening ring, the darkening ring includes body, coating
In the anti-static coating on the body and the through hole being formed on the body, the body is made of plastic material, described
Anti-static coating is carbon dust layer, and the through hole is by being stamped and formed out, formed with dumb light structure on the hole wall.
Preferably, the body is made of polyethylene terephthalate.
Preferably, the dumb light structure is formed by alkali soluble corrosion.
Preferably, the aqueous slkali is sodium bicarbonate solution, and the concentration 5%~35% of the sodium bicarbonate solution, it is warm
Spend for 35~55 degree.
Preferably, the thickness of the darkening ring is 0.025 millimeter, a diameter of 2.14 millimeters of the through hole.
The present invention darkening ring processing method and darkening ring, by aqueous slkali in supersonic generator to darkening ring into
Row processing, with the hole wall of the through hole of darkening ring formed dumb light structure, to avoid the hole wall due to through hole it is reflective and caused by
The generation of the undesirable conditions such as dazzle, halation and ghost, and then ensure that shooting effect, improve the quality of shooting product.
Brief description of the drawings
Fig. 1 is the flow chart of an embodiment of the processing method of darkening ring of the present invention;
Fig. 2 is the flow chart for forming dumb light structure on the hole wall of the through hole by alkali soluble corrosion shown in Fig. 1;
Fig. 3 is the cross-sectional view of darkening ring of the present invention.
The object of the invention is realized, the embodiments will be further described with reference to the accompanying drawings for functional characteristics and advantage.
Embodiment
It should be appreciated that the specific embodiments described herein are merely illustrative of the present invention, it is not intended to limit the present invention.
The present invention provides a kind of processing method of darkening ring, with reference to Fig. 1, in one embodiment, the processing of the darkening ring
Method includes the following steps:
Step S10, darkening ring is provided, the darkening ring includes body, coated on the anti-static coating on the body and
The through hole being formed on the body, the body are made of plastic material, and the anti-static coating is carbon dust layer, the through hole
By being stamped and formed out.
Specifically, in the present embodiment, the thickness of the darkening ring be 0.025 millimeter, a diameter of the 2.14 of the through hole
Millimeter, the body are made of polyethylene terephthalate.
Anti-static coating is coated since the manufacture of darkening ring is to be initially formed body, then in the outer surface of body, finally
Through hole is being formed on body by way of punching press, at this moment, the hole wall of the through hole is by polyethylene terephthalate
Formed, then machine can be corroded by aqueous slkali, and to form dumb light structure on hole wall, and the remainder of darkening ring is then
Covered with the anti-static coating formed by carbon dust layer, its susceptibility to aqueous slkali is poor, will not substantially be subject to aqueous slkali
Corrosion, and then ensure that the feasibility of this forwarding method.
Step S20, dumb light structure is formed on the hole wall of the through hole by alkali soluble corrosion.
Specifically, it is in the present embodiment, described to be formed by alkali soluble corrosion on the hole wall of the through hole with reference to Fig. 2
The step of dumb light structure, specifically includes:
Step S21, aqueous slkali is placed in supersonic generator.
Specifically, the aqueous slkali is sodium bicarbonate solution, its concentration is 5%~35%;The supersonic generator
Power is 300~500 watts, is preferably 400 watts.Supersonic generator sends ultrasonic wave, is placed in causing in supersonic generator
Sodium bicarbonate solution vibrations, and then ensure that corrosive effect.
Step S22, darkening ring is placed in the aqueous slkali, and stirred.
Specifically, the temperature of the sodium bicarbonate solution is 35~55 degree, when the time of the stirring is 3~5 small.Pass through
Heating and the mode of stirring, further ensure corrosive effect, while shorten etching time, improve treatment effeciency.
The processing method of the darkening ring of the present invention, is handled darkening ring in supersonic generator by aqueous slkali,
With on the hole wall of the through hole of darkening ring formed dumb light structure, to avoid the hole wall due to through hole it is reflective and caused by dazzle, light
The generation of the undesirable conditions such as dizzy and ghost, and then ensure that shooting effect, improve the quality of shooting product.
The present invention also provides a kind of darkening ring, and with reference to Fig. 3, in one embodiment, the darkening ring includes body 200, applies
The anti-static coating 300 being overlying on the body 200 and the through hole 220 being formed on the body 200, the body 200 by
Plastic material is made, and the anti-static coating 300 is carbon dust layer, and the through hole 220 is formed by being stamped and formed out on the hole wall
There is dumb light structure 222.
Specifically, in the present embodiment, the thickness of the darkening ring be 0.025 millimeter, the through hole 220 it is a diameter of
2.14 millimeter;The body 200 is made of polyethylene terephthalate;The dumb light structure 222 passes through alkali soluble corrosion
Formed.
Applied since the manufacture of darkening ring is to be initially formed body 200, then in the outer surface of body 200 coating antistatic
Layer 300, is finally forming through hole 220, at this moment, the hole wall of the through hole 220 is by gathering by way of punching press on body 200
Ethylene glycol terephthalate is formed, then machine can be corroded by aqueous slkali, to form dumb light structure on hole wall
222, and the remainder of darkening ring is then covered with the anti-static coating 300 formed by carbon dust layer, its susceptibility to aqueous slkali
It is poor, it will not substantially be corroded be subject to aqueous slkali, and then ensure that the feasibility of this forwarding method.
Further, in the present embodiment, the aqueous slkali is sodium bicarbonate solution, the concentration of the sodium bicarbonate solution
5%~35%, its temperature is 35~55 degree, by way of heating, ensure that corrosive effect, while shortens etching time,
Improve treatment effeciency.
In conclusion the darkening ring of the present invention, by forming dumb light structure on the hole wall of the through hole of darkening ring, to avoid
Due to the hole wall of through hole it is reflective and caused by the undesirable condition such as dazzle, halation and ghost generation, and then ensure that shooting effect,
Improve the quality of shooting product.
It these are only the preferred embodiment of the present invention, be not intended to limit the scope of the invention, it is every to utilize this hair
The equivalent structure or equivalent flow shift that bright specification and accompanying drawing content are made, is directly or indirectly used in other relevant skills
Art field, is included within the scope of the present invention.
Claims (2)
1. a kind of processing method of darkening ring, it is characterised in that the processing method of the darkening ring includes the following steps:
There is provided darkening ring, the darkening ring includes body, coated on the anti-static coating on the body and is formed at described
Through hole on body, the body are made of plastic material, and the anti-static coating is carbon dust layer, and the through hole passes through punching press shape
Into;
Dumb light structure is formed on the hole wall of the through hole by alkali soluble corrosion;
It is described to be specifically included by alkali soluble corrosion in the step of formation dumb light structure on the hole wall of the through hole:
Aqueous slkali is placed in supersonic generator;
Darkening ring is placed in the aqueous slkali, and is stirred;
The body is made of polyethylene terephthalate, and the aqueous slkali is sodium bicarbonate solution, its concentration for 5%~
35%;
The temperature of the aqueous slkali is 35~55 degree, when the time of the stirring is 3~5 small;
The power of the supersonic generator is 300~500 watts.
2. the processing method of darkening ring as claimed in claim 1, it is characterised in that the thickness of the darkening ring is 0.025 milli
Rice, a diameter of 2.14 millimeters of the through hole.