CN104448441A - Rubber base plate - Google Patents
Rubber base plate Download PDFInfo
- Publication number
- CN104448441A CN104448441A CN201310434562.2A CN201310434562A CN104448441A CN 104448441 A CN104448441 A CN 104448441A CN 201310434562 A CN201310434562 A CN 201310434562A CN 104448441 A CN104448441 A CN 104448441A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber
- base plate
- accelerant
- rubber base
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a rubber base plate, belongs to the technical field of chemical industry and in particular relates to the technical field of a formula of the rubber base plate. According to the specific technical scheme, the rubber base plate is characterized by comprising 100 parts of butadiene styrene rubber, 4-8 parts of zinc oxide, 0.5-1.5 parts of stearic acid, 0.8-1.5 parts of an accelerant TMTD, 0.5-1.5 parts of an accelerant CZ, 1.0-3.0 parts of a coupling agent Si69, 30-50 parts of semi-reinforced carbon black, 50-70 parts of nano kaolin, 1-1.5 parts of an anti-aging agent 4010NA, 1-2 parts of an anti-aging agent RD, 0.5-1.5 parts of microcrystalline wax, 0.3-1.5 parts of sulfur, 40-50 parts of ethylene-alpha-olefin-non-conjugated polyene copolymer rubber and 20-30 parts of aromatic amine compounds.
Description
Technical field
A kind of rubber bearing of the present invention belongs to chemical technology field, especially relates to a kind of formula technique field of rubber bearing.
Background technology
Modern railways operational mode is for basic model with high speed, high-density, this pattern needs railway to provide satisfactory stability and rational route elasticity, and successively, the basis of railway is developed to rigidization, sweetly expensively think that neutralisation develops, this trend requires that circuit provides better elasticity.And rubber bearing just in time meets such requirement.In order to the demand of high-speed railway to rubber bearing can better be met, to adapt to the development of the high ferro of railway.Rubber is the basic raw material of rubber industry, is widely used in and manufactures tire, sebific duct, adhesive tape, cable and other various rubber items.Rubber is divided into natural rubber and synthetic rubber by raw material.Block rubber, latex, fluid rubber and powdered rubber is divided into by form.Latex is the colloidal water dispersion of rubber; Fluid rubber is the oligopolymer of rubber, is generally the liquid of thickness before unvulcanized; Powdered rubber be latex is processed into Powdered, in order to batching and processing and fabricating.The thermoplastic elastomer of the exploitation sixties in 20th century, without the need to chemicure, and adopts the working method of thermoplastics to be shaped.Rubber is divided into again universal and Special type two class by use.Be isolator, be not easy conduction, if but get wet or different temperature, likely become conductor.Conduction is the easy situation of conduction of the electronics about material interior molecules or ion.
Summary of the invention
In order to realize the rubber bearing of the present invention for the needs of high-speed railway, the invention provides following technical scheme: a kind of rubber bearing, is characterized in that: described rubber bearing comprises: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.
In order to better realize object of the present invention, described rubber bearing comprises: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.
Summary of the invention
In order to content of the present invention can better be understood, following embodiment is adopted to be explained: a kind of rubber bearing, comprising: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.
In order to better realize object of the present invention, following concrete scheme can be adopted: described rubber bearing comprises: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.
Claims (2)
1. a rubber bearing, is characterized in that: described rubber bearing comprises: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.
2. rubber bearing according to claim 1, is characterized in that: described rubber bearing comprises: styrene-butadiene rubber(SBR), 100 parts; Zinc oxide, 4 ~ 8 parts; Stearic acid part, 0.5 ~ 1.5 part; Vulcanization accelerator TMTD, 0.8 ~ 1.5 part; Accelerant CZ, 0.5 ~ 1.5 part; Coupling agent Si69 1.0 ~ 3.0 parts; Semi-reinforcing hydrocarbon black, 30 ~ 50 parts; Nano kaoline, 50 ~ 70 parts; Antioxidant 4010NA, 1 ~ 1.5 part; Anti-aging agent RD, 1 ~ 2 part; Microcrystalline Wax, 0.5 ~ 1.5 part; Sulphur, 0.3 ~ 1.5 part; Ethylene/alpha-olefin/unconjugated polyene copolymer rubber 40 ~ 50 parts; Aromatic amine based compound 20 ~ 30 parts.