CN104441181A - Mold pressing wood veneer pasting technology for lower mullion - Google Patents
Mold pressing wood veneer pasting technology for lower mullion Download PDFInfo
- Publication number
- CN104441181A CN104441181A CN201410671604.9A CN201410671604A CN104441181A CN 104441181 A CN104441181 A CN 104441181A CN 201410671604 A CN201410671604 A CN 201410671604A CN 104441181 A CN104441181 A CN 104441181A
- Authority
- CN
- China
- Prior art keywords
- door frame
- door leaf
- low middle
- middle door
- frame door
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a wood veneer decorative finish technology in door leaf manufacturing, in particular to a mold pressing wood veneer pasting technology for a lower mullion. The mold pressing wood veneer pasting technology includes the following steps that step1, a special mold for a lower mullion door leaf is manufactured; step2, a green body is manufactured; step3, according to assembly, the mullion part and the edge part of the finished green body, obtained in the step2, of the lower mullion door leaf are coated with adhesive in a rolled mode through a rolling coating machine, and then wood veneer containing moisture is flat laid on the finished green body of the lower mullion door leaf to form a blank, to be formed, of the lower mullion door leaf; step4, hot pressing forming is performed, and the blank, to be formed, of the lower mullion door leaf in the step3 is placed on a feeding trolley and fed into a hot pressing machine in the step1 through the feeding trolley to form the lower mullion door leaf through mold pressing; in the mold pressing process, the hot pressing temperature of the hot pressing machine is 80 DEG C-100 DEG C, and hot pressing time is 5 minutes-6 minutes. The technology improves the production efficiency, lowers the production cost and guarantees product quality.
Description
Technical field
The present invention relates to door leaf manufacture in wooden skin " finishing process, especially a kind ofly to enhance productivity, reduce production cost and wooden skin technique is pasted in the low middle door frame mold pressing of ensuring the quality of products.
Background technology
The door leaf of existing convex-concave Europe series wood skin facing, its skin is the moulding of planar band matrix, the lagging technique of this skin is: after door leaf is compressing, entirety polishes flat, middle door frame position roller coating adhesive, is laid in the veneer of moisture content and need pastes in wooden skin on door frame, adopt manual flatiron to press, make adhesive solidification, reach lagging object.This lagging mode, needs a large amount of to adopt manual flatiron manually to press, wastes time and energy, and limit by operative's technical ability, easily causes gluingly loosely occurring the phenomenons such as bubble, can not ensure the quality of products.
In sum, in the low middle door frame series door leaf of prior art, door frame wood skin attaching process causes production efficiency low, and manufacturing cost is high; And affect by operative's technical ability, of poor quality.
Summary of the invention
The object of this invention is to provide and a kind ofly to enhance productivity, reduce production cost and wooden skin technique is pasted in the low middle door frame mold pressing of ensuring the quality of products.
The technical scheme adopted for realizing above-mentioned purpose of the present invention is: wooden skin technique is pasted in a kind of low middle door frame mold pressing, wherein, comprises the steps:
The first step, makes low middle door frame door leaf particular manufacturing craft, and this low middle door frame door leaf particular manufacturing craft mates with low middle door frame door leaf, and low middle door frame door leaf particular manufacturing craft is loaded the hot pressing die orifice place of hot press;
Second step, base, the surface to low middle door frame door leaf blank carries out surface treatment by the shaping low middle door frame door leaf blank of making by sander or sander, until the surfacing of low middle door frame door leaf blank and the low middle door frame door leaf essence base of fine and smooth formation;
3rd step, assembly, in middle door frame door leaf essence base low described in second step, door frame portion and arris portion adopt coating roller roller coating adhesive, then moisture content are laid in door frame portion, arris portion and ditch portion in low middle door frame door leaf essence base respectively with the veneer that door frame portion, arris portion and ditch portion in low middle door frame door leaf essence base match and form low middle door frame door leaf blank to be formed;
4th step, hot-forming, low middle door frame door leaf blank to be formed described in 3rd step is placed on feeding trolley, by feeding trolley, low middle door frame door leaf blank to be formed is sent in hot press described in the first step, then form low middle door frame door leaf by the low middle door frame door leaf particular manufacturing craft compression molding in hot press; In this mold process, the hot pressing temperature of hot press is 80-100 DEG C, and hot pressing time is 5-6 minute.
Due to above-mentioned technique, the low middle door frame door leaf of same batch of model adopts same mould, and the temperature and time when pasting wooden skin can ensure the same, product quality can effectively be ensured, adopt hot press mold pressing to paste wooden skin, improve production efficiency, reduce production cost simultaneously.
Accompanying drawing explanation
The nonlimiting examples that the present invention can be provided by accompanying drawing further illustrates.
Fig. 1 is the structural representation of the low middle door frame door leaf essence base of the present invention.
In figure: 1, arris portion; 2, ditch portion; 3, middle door frame portion.
Detailed description of the invention
Below in conjunction with drawings and Examples, the invention will be further described:
Paste wooden skin technique see the low middle door frame mold pressing in accompanying drawing 1, figure, wherein, comprise the steps:
The first step, makes low middle door frame door leaf particular manufacturing craft, and this low middle door frame door leaf particular manufacturing craft mates with low middle door frame door leaf, and low middle door frame door leaf particular manufacturing craft is loaded the hot pressing die orifice place of hot press;
Second step, base, the surface to low middle door frame door leaf blank carries out surface treatment by the shaping low middle door frame door leaf blank of making by sander or sander, until the surfacing of low middle door frame door leaf blank and the low middle door frame door leaf essence base of fine and smooth formation;
3rd step, assembly, in middle door frame door leaf essence base low described in second step, door frame portion 3 and arris portion 1 adopt coating roller roller coating adhesive, then moisture content are laid in door frame portion 3, arris portion 1 and ditch portion 2 in low middle door frame door leaf essence base respectively with the veneer that door frame portion 3, arris portion 1 and ditch portion 2 in low middle door frame door leaf essence base match and form low middle door frame door leaf blank to be formed;
4th step, hot-forming, low middle door frame door leaf blank to be formed described in 3rd step is placed on feeding trolley, by feeding trolley, low middle door frame door leaf blank to be formed is sent in hot press described in the first step, then form low middle door frame door leaf by the low middle door frame door leaf particular manufacturing craft compression molding in hot press; In this mold process, the hot pressing temperature of hot press is 80-100 DEG C, and hot pressing time is 5-6 minute.In this embodiment, ditch portion 2 no longer needs roller coating adhesive, is formed, further increase production efficiency and reduce production cost through hot press hot pressing disposal molding compacting described in the 4th step.
Obviously, all embodiments of foregoing description are a part of embodiments of the present invention, instead of whole embodiments.Based on embodiments of the invention, those of ordinary skill in the art are not making other embodiments all obtained under creative work prerequisite, all belong to the category of the present invention's protection.
In sum, invention increases production efficiency, reduce production cost and ensure that product quality.
Claims (1)
1. a wooden skin technique is pasted in low middle door frame mold pressing, it is characterized in that, comprises the steps:
The first step, makes low middle door frame door leaf particular manufacturing craft, and this low middle door frame door leaf particular manufacturing craft mates with low middle door frame door leaf, and low middle door frame door leaf particular manufacturing craft is loaded the hot pressing die orifice place of hot press;
Second step, base, the surface to low middle door frame door leaf blank carries out surface treatment by the shaping low middle door frame door leaf blank of making by sander or sander, until the surfacing of low middle door frame door leaf blank and the low middle door frame door leaf essence base of fine and smooth formation;
3rd step, assembly, in middle door frame door leaf essence base low described in second step, door frame portion (3) and arris portion (1) adopt coating roller roller coating adhesive, then by moisture content and be laid in the middle door frame portion (3) of the smart base of low middle door frame door leaf respectively with the veneer that door frame portion (3), arris portion (1) He Goubu (2) in low middle door frame door leaf essence base match, arris portion (1) He Goubu (2) forms low middle door frame door leaf blank to be formed;
4th step, hot-forming, low middle door frame door leaf blank to be formed described in 3rd step is placed on feeding trolley, by feeding trolley, low middle door frame door leaf blank to be formed is sent in hot press described in the first step, then form low middle door frame door leaf by the low middle door frame door leaf particular manufacturing craft compression molding in hot press; In this mold process, the hot pressing temperature of hot press is 80-100 DEG C, and hot pressing time is 5-6 minute.